Effect of Washing on Nickel-Rich Layered Oxides: Methodology to Quantify the Lithium/Proton-Exchange Kinetics, the Inserted Protons, and the Structural Changes
Due to their high specific capacity, the market share of nickel-rich layered lithium nickel cobalt manganese oxides (NCMs, LiNixCoyMnzO2, x+y+z = 1) as cathode active materials (CAMs) for lithium-ion batteries is constantly growing. With higher nickel content, the available capacity is increased [1]; however, the higher reactivity of nickel increases unwanted contaminants on the surface of the NCM particles [2]. These contaminants comprise lithium salts, which remain from the lithium excess added during the synthesis of the CAM [3] or are formed during improper storage owed to the high sensitivity towards moisture [4]. In the cell, these compounds then lead to extensive gassing upon decomposition during the first charge/discharge cycles [5], to hydrolysis of electrolyte components [6], as well as to impedance build-up and therefore to capacity fading during cell operation [7]. Due to these negative effects, these contaminants are commonly removed by washing the CAM in water; however, this essential process is accompanied by the cation exchange of intercalated near-surface lithium ions from the NCM by protons from the solution when nickel-rich NCMs are exposed to liquid water [8] or to humid air [9]. To reveal the kinetics of this unwanted cation exchange as well as its implications on the electrochemical behavior, a comprehensive study on the exchange process during the washing is presented here for a nickel-rich NCM831205 (LiNi0.83Co0.12Mn0.05O2). In the first part of this work, washed NCM samples were prepared using a variety of process conditions (e.g., washing time, water-to-CAM mass ratio, and washing temperature) [10]. To determine the proton amount being introduced into the CAM and consequently describe the kinetics of the cation exchange, a set of five independent methods is applied, all capable of quantifying the proton amount xH⁺ (in units of mol%) exchanged into the CAM: i) By titrating the washing solution, its concentration of lithium hydroxide cLiOH is determined, what can be converted into xH⁺ of the CAM. ii) Upon irradiation with neutrons, the protons (as well as the atomic nuclei of the metals) in the NCM emit γ-rays with distinct energies, allowing to quantify xH⁺ by prompt-gamma activation analysis (PGAA). iii) Through thermogravimetric analysis coupled with mass spectrometry (TGA-MS), the observed mass loss of the thermal decomposition of the protonated phase up to 450 °C can be converted into xH⁺. iv) As the protonated layered phase converts to a rock-salt-type structure upon heating, the amount of the rock-salt phase of a heated and washed NCM sample is determined by Rietveld refinement of the powder X-ray diffraction (XRD) data, from which xH⁺ was obtained by the ratio of layered and rock-salt-type phase. v) The layer of the delithiated/protonated surface layer is quantified through X-ray photoelectron spectroscopy (XPS). For the differently washed NCM samples, proton amounts between 0.5 mol% and 25 mol% are obtained. Additionally, this study provides insights into the exchange kinetics, the thermal-decomposition mechanism of the protonated phase, as well as the bulk properties, e.g., the change of lattice parameters and the proton distribution within the particles. In the second part of this study [11], the impact of the protonation on the electrochemical behavior of the NCM is illuminated. References: [1] S. Oswald and H. A. Gasteiger, J. Electrochem. Soc. 170 030506 (2023). [2] W. Li, E. M. Erickson, and A. Manthiram, Nature Energy 5 26 (2020). [3] H.-J. Noh, S. Youn, C. S. Yoon, and Y.-K. Sun, J. Power Sources 233 121 (2013). [4] J. Sicklinger, M. Metzger, H. Beyer, D. Pritzl, and H. A. Gasteiger, J. Electrochem. Soc. 166 A2322 (2019). [5] S. Renfrew and B. D. McCloskey, J. Am. Chem. Soc. 139 17853 (2017). [6] M. Metzger, B. Strehle, S. Solchenbach, and H. A. Gasteiger, J. Electrochem. Soc. 163 A1219 (2016). [7] R. Jung, R. Morasch, P. Karayaylali, K. Phillips, F. Maglia, C. Stinner, Y. Shao-Horn, and H. A. Gasteiger, J. Electrochem. Soc. 165 A132 (2018). [8] D. Pritzl, T. Teufl, A.T.S. Freiberg, B. Strehle, J. Sicklinger, H. Sommer, P. Hartmann, and H. A. Gasteiger, J. Electrochem. Soc. 166 A4056 (2019). [9] L. Hartmann, D. Pritzl, H. Beyer, and H. A. Gasteiger, J. Electrochem. Soc. 168 070507 (2021). [10] S. Oswald, R. Wilhelm, T. Kratky, L. Szentmiklósi, B. Maróti, I. Harsányi, S. A. Hallweger, G. Kieslich, S. Günther, and H. A. Gasteiger, J. Mater. Chem. A 12 25140 (2024). [11] R. Wilhelm, S. Oswald, S. Helmer, and H. A. Gasteiger, in preparation. Figure 1