Friction surfacing and cold spray deposition for surface crack repair in austenitic stainless steels
- 18 October 2022
- journal article
- research article
- Published by Elsevier in Materials Today Communications
- Vol. 33, 104692
Abstract
No abstract availableKeywords
Funding Information
- Materials Research Science and Engineering Center, Harvard University
- National Science Foundation (DMR-1720415)
- U.S. Department of Energy (DE-NE0008801)
- University of Wisconsin-Madison
This publication has 11 references indexed in Scilit:
- Leak-tight crack repair for 304L stainless steel using friction surfacingJournal of Manufacturing Processes, 2022
- Cold spray deposition of 304L stainless steel to mitigate chloride-induced stress corrosion cracking in canisters for used nuclear fuel storageJournal of Nuclear Materials, 2020
- Solid state crack repair by friction stir processing in 304L stainless steelJournal of Materials Science & Technology, 2018
- Microstructural Evolutions During Annealing of Plastically Deformed AISI 304 Austenitic Stainless Steel: Martensite Reversion, Grain Refinement, Recrystallization, and Grain GrowthMetallurgical and Materials Transactions A, 2016
- Friction surfacing—A reviewJournal of Materials Processing Technology, 2014
- Dynamic recrystallization in friction surfaced austenitic stainless steel coatingsMaterials Characterization, 2012
- Microstructural Evolution During Friction Surfacing of Austenitic Stainless Steel AISI 304 on Low Carbon SteelMetallurgical and Materials Transactions A, 2012
- Effects of laser peening on stress corrosion cracking (SCC) of ANSI 304 austenitic stainless steelCorrosion Science, 2012
- Rapid formation of the sigma phase in 304 stainless steel during friction stir weldingScripta Materialia, 2003
- Weld Repair of Irradiated MaterialsMaterials Characterization, 1999