Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part I: Structure, Mechanical Properties and Susceptibility to Hydrogen Embrittlement
Authors:
- Boris YanachkovBYBoris Yanachkov
- Kateryna ValuiskaKVKateryna Valuiska
- Yana MourdjevaYMYana Mourdjeva
- Rumen KrastevRKRumen Krastev
- Vanya DyakovaVDVanya Dyakova
- Tatiana SimeonovaTSTatiana Simeonova
- Roumen H. PetrovRoumen H. Petrov
- Krasimir KolevKKKrasimir Kolev
- Margo CauwelsMCMargo Cauwels
- Tom DepoverTDTom Depover
- Rumyana LazarovaRumyana Lazarova
Open Access
Abstract
The utilization of hydrogen as a clean energy carrier requires an assessment of existing natural gas pipelines with respect to hydrogen embrittlement (HE). In this study, the structural integrity and hydrogen sensitivity of X52 (L360) pipeline steel from the Bulgarian gas transmission network after 31 years of service were investigated, focusing on production (longitudinal) and girth (circumferential) welded joints. Hydrogen content was measured in the base metal, production weld and girth weld before and after electrochemical charging, while in situ hydrogen charging during tensile testing was applied to simulate service conditions. Mechanical behavior was evaluated by tensile tests, and microstructural and fracture characteristics were analyzed by SEM and TEM. The results show significant spatial variations in hydrogen concentration, related to local microstructural heterogeneity and hydrogen trapping. In the as-operated state, fracture was localized mainly in the heat-affected zone. Hydrogen charging led to a pronounced reduction in ductility (approximately twofold), whereas yield and tensile strengths were only slightly affected. Failure analyses indicate a transition toward more brittle fracture mechanisms, dominated by quasi-cleavage and intergranular cracking in the as-charged state, with hydrogen embrittlement susceptibility indices demonstrating higher hydrogen sensitivity of the girth-welded joints.Keywords
Funding Information
- National Recovery and Resilience Fund of Bulgaria (PVU-51/BG-RRP-2.017-0022-C02)
This publication has 36 references indexed in Scilit:
- Investigation of hydrogen embrittlement in welded joints of the L360MH pipeline steel for hydrogen transportationCorrosion Science, 2025
- Investigating variations in hydrogen-assisted crack propagation of X52 pipeline steel with different microstructural characteristicsCorrosion Science, 2024
- Investigations of temperature effects on hydrogen diffusion and hydrogen embrittlement of X80 pipeline steel under electrochemical hydrogen charging environmentCorrosion Science, 2023
- Hydrogen embrittlement characteristics in cold-drawn high-strength stainless steel wiresCorrosion Science, 2023
- Key factors affecting hydrogen trapping at the inclusions in steels: A combined study using microprint technique and theoretical modelingCorrosion Science, 2022
- A comparative fracture analysis on as-received and electrochemically hydrogen charged API X60 and API X60SS pipeline steels subjected to tensile testingEngineering Failure Analysis, 2021
- Effects of multiple welding thermal cycles on hydrogen permeation parameters of X80 steelCorrosion Science, 2021
- Inclusion Characteristics and Acicular Ferrite Nucleation in Ti‐Containing Weld Metals of X70 Pipeline SteelSteel Research International, 2017
- A focus on different factors affecting hydrogen induced cracking in oil and natural gas pipeline steelEngineering Failure Analysis, 2017
- The diffusion and trapping of hydrogen in steelActa Metallurgica, 1970