Margo Cauwels
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Margo Cauwels has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
- Kim Verbeken
Ghent University, Ghent, Belgium
5 shared publications - Tom Depover
Ghent University
4 shared publications - Wim De Waele
Department of Electromechanical, Systems and Metal Engineering, Ghent University, Ghent, Belgium
4 shared publications - Robin Depraetere
Department of Electromechanical, Systems and Metal Engineering, Ghent University, Technologiepark-Zwijnaarde 46, 9052 Ghent, Belgium
3 shared publications - Stijn Hertelé
Soete Laboratory, Ghent University, Technologiepark Zwijnaarde 903, Zwijnaarde 9052, Belgium
3 shared publications Tom Depover
2 shared publications
Latest Publications
- Open Access
Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part I: Structure, Mechanical Properties and Susceptibility to Hydrogen Embrittlement
The utilization of hydrogen as a clean energy carrier requires an assessment of existing natural gas pipelines with respect to hydrogen embrittlement (HE). In this study, the structural integrity and hydrogen sensitivity of X52 (L360) pipeline steel from the Bulgarian gas transmission network after 31 years of service were investigated, focusing on production (longitudinal) and girth (circumferential) welded joints. Hydrogen content was measured in the base metal, production weld and girth weld before and after electrochemical charging, while in situ hydrogen charging during tensile testing was applied to simulate service conditions. Mechanical behavior was evaluated by tensile tests, and microstructural and fracture characteristics were analyzed by SEM and TEM. The results show significant spatial variations in hydrogen concentration, related to local microstructural heterogeneity and hydrogen trapping. In the as-operated state, fracture was localized mainly in the heat-affected zone. Hydrogen charging led to a pronounced reduction in ductility (approximately twofold), whereas yield and tensile strengths were only slightly affected. Failure analyses indicate a transition toward more brittle fracture mechanisms, dominated by quasi-cleavage and intergranular cracking in the as-charged state, with hydrogen embrittlement susceptibility indices demonstrating higher hydrogen sensitivity of the girth-welded joints.
Open AccessInvestigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part I: Structure, Mechanical Properties and Susceptibility to Hydrogen Embrittlement
The utilization of hydrogen as a clean energy carrier requires an assessment of existing natural gas pipelines with respect to hydrogen embrittlement (HE). In this study, the structural integrity and hydrogen sensitivity of X52 (L360) pipeline steel from the Bulgarian gas transmission network after 31 years of service were investigated, focusing on production (longitudinal) and girth (circumferential) welded joints. Hydrogen content was measured in the base metal, production weld and girth weld before and after electrochemical charging, while in situ hydrogen charging during tensile testing was applied to simulate service conditions. Mechanical behavior was evaluated by tensile tests, and microstructural and fracture characteristics were analyzed by SEM and TEM. The results show significant spatial variations in hydrogen concentration, related to local microstructural heterogeneity and hydrogen trapping. In the as-operated state, fracture was localized mainly in the heat-affected zone. Hydrogen charging led to a pronounced reduction in ductility (approximately twofold), whereas yield and tensile strengths were only slightly affected. Failure analyses indicate a transition toward more brittle fracture mechanisms, dominated by quasi-cleavage and intergranular cracking in the as-charged state, with hydrogen embrittlement susceptibility indices demonstrating higher hydrogen sensitivity of the girth-welded joints.
- Open Access
Modeling of Hydrogen-Charged Notched Tensile Tests of an X70 Pipeline Steel with a Hydrogen-Informed Gurson Model
Hydrogen can degrade the mechanical properties of steel components, which is commonly referred to as “hydrogen embrittlement” (HE). Quantifying the effect of HE on the structural integrity of components and structures remains challenging. The authors investigated an X70 pipeline steel through uncharged and hydrogen-charged (notched) tensile tests. This paper presents a combination of experimental results and numerical simulations using a micro-mechanics-inspired damage model. Four specimen geometries and three hydrogen concentrations (including uncharged) were targeted, which allowed for the construction of a fracture locus that depended on the stress triaxiality and hydrogen concentration. The multi-physical finite element model includes hydrogen diffusion and damage on the basis of the complete Gurson model. Hydrogen-Assisted degradation was implemented through an acceleration of the void nucleation process, as supported by experimental observations. The damage parameters were determined through inverse analysis, and the numerical results were in good agreement with the experimental data. The presented model couples micro-mechanical with macro-mechanical results and makes it possible to evaluate the damage evolution during hydrogen-charged mechanical tests. In particular, the well-known ductility loss due to hydrogen was captured well in the form of embrittlement indices for the different geometries and hydrogen concentrations. The limitations of the damage model regarding the stress state are discussed in this paper.
Open AccessModeling of Hydrogen-Charged Notched Tensile Tests of an X70 Pipeline Steel with a Hydrogen-Informed Gurson Model
Hydrogen can degrade the mechanical properties of steel components, which is commonly referred to as “hydrogen embrittlement” (HE). Quantifying the effect of HE on the structural integrity of components and structures remains challenging. The authors investigated an X70 pipeline steel through uncharged and hydrogen-charged (notched) tensile tests. This paper presents a combination of experimental results and numerical simulations using a micro-mechanics-inspired damage model. Four specimen geometries and three hydrogen concentrations (including uncharged) were targeted, which allowed for the construction of a fracture locus that depended on the stress triaxiality and hydrogen concentration. The multi-physical finite element model includes hydrogen diffusion and damage on the basis of the complete Gurson model. Hydrogen-Assisted degradation was implemented through an acceleration of the void nucleation process, as supported by experimental observations. The damage parameters were determined through inverse analysis, and the numerical results were in good agreement with the experimental data. The presented model couples micro-mechanical with macro-mechanical results and makes it possible to evaluate the damage evolution during hydrogen-charged mechanical tests. In particular, the well-known ductility loss due to hydrogen was captured well in the form of embrittlement indices for the different geometries and hydrogen concentrations. The limitations of the damage model regarding the stress state are discussed in this paper.
- 26 December 2022
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 864
Influence of stress triaxiality on hydrogen assisted ductile damage in an X70 pipeline steel
- 26 December 2022
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 864
Influence of stress triaxiality on hydrogen assisted ductile damage in an X70 pipeline steel
- Open Access
- 7 December 2019
- Published by Gruppo Italiano Frattura in Fracture and Structural Integrity
- Vol. 14 (51) , 449-458
The hydrogen embrittlement sensitivity of duplex stainless steel with different phase fractions evaluated by in-situ mechanical testing
The influence of the austenite (γ) phase fraction on the hydrogen embrittlement of duplex stainless steel is investigated. Heat treatments are performed to create two duplex stainless steel specimens, containing 50% and 44% of austenite, respectively. Mechanical testing with and without hydrogen charging reveals that significant embrittlement occurs regardless of the austenite fraction. A higher austenite fraction results in a reduced ductility loss under the presence of hydrogen. Samples with a higher ferrite fraction are embrittled more due to their higher hydrogen diffusivity. In-situ tensile tests, interrupted at the ultimate tensile strength, show hydrogen-assisted cracks on the specimen surface both in austenite and ferrite and across the α/γ interface.
- 7 December 2019
- Published by Gruppo Italiano Frattura in Fracture and Structural Integrity
- Vol. 14 (51) , 449-458
Open AccessThe hydrogen embrittlement sensitivity of duplex stainless steel with different phase fractions evaluated by in-situ mechanical testing
The influence of the austenite (γ) phase fraction on the hydrogen embrittlement of duplex stainless steel is investigated. Heat treatments are performed to create two duplex stainless steel specimens, containing 50% and 44% of austenite, respectively. Mechanical testing with and without hydrogen charging reveals that significant embrittlement occurs regardless of the austenite fraction. A higher austenite fraction results in a reduced ductility loss under the presence of hydrogen. Samples with a higher ferrite fraction are embrittled more due to their higher hydrogen diffusivity. In-situ tensile tests, interrupted at the ultimate tensile strength, show hydrogen-assisted cracks on the specimen surface both in austenite and ferrite and across the α/γ interface.