The influence of shear on phase transformations in glassy carbon compressed at room temperature using diamond anvil cells (DAC) both with and without active rotation of an anvil (rDAC) is investigated. We demonstrate that increasing shear significantly lowers the pressure required for the formation of highdensity carbon phases, including diamond. The use of a softer gasket material in a DAC was found to be an effective method to increase shear, while actively applying shear in the rDAC resulted in diamond formation at pressures as low as 15 GPa, much lower than previously reported from this precursor material. In both types of cells, most of the diamond was found in buried shear bands within a graphitic matrix. Samples prepared in the rDAC also contained a nanodiamondrich surface layer consistent with the expected intense levels of shear at the sample/anvil interface. Distinct regions of tetrahedral amorphous carbon (taC) were also found in the rDAC samples, attributed to shear zones insufficient to induce diamond crystallisation. Collectively, these findings reveal that shear provides a promising, energyefficient pathway for synthesising diamond and sp³rich carbon materials which have the potential to be exploited commercially.