The objective of this study was to evaluate fracture strength of high-translucent (HTZ) and low-translucent (LTZ) zirconia and glass-ceramic (LDS) crowns. HTZ and LTZ crowns were made with thicknesses of; 0.3 mm, 0.5 mm, 0.7 mm, 1.0 mm, and 1.5 mm; and LDS crowns of 1.0 mm and 1.5 mm thicknesses. Each group consisted of 10 crowns. All crowns underwent artificial aging before loading until fracture. Mean fracture strengths varied from 450 N to 3,248 N in the LTZ group, 438 N to 3,487 N in the HTZ group, and 1,030 N to 1,431 N in the LDS group. The load at fracture of HTZ and LTZ crowns was equal. The load at fracture of yttria-stabilized tetragonal zirconia polycrystals crowns was significantly greater than LDS crowns (P = 0.000). Two types of fractures were recorded; complete and partial crack-like fracture. The crack type fracture occurred most frequently in all groups except in the thicker LTZ groups (1.0 mm and 1.5 mm). According to this study, there is no difference in strength between crowns made of high-translucent or low-translucent zirconia. At equal thickness, the strength of zirconia crowns was significantly greater than that of lithium-disilicate glass-ceramic.Keywords
This publication has 19 references indexed in Scilit:
- Edge chipping and flexural resistance of monolithic ceramicsDental Materials, 2013
- Clinical Evaluation of 1,132 Zirconia-Based Single Crowns: A Retrospective Cohort Study from the AIOP Clinical Research GroupThe International Journal of Prosthodontics, 2013
- Fracture strength of monolithic all-ceramic crowns made of high translucent yttrium oxide-stabilized zirconium dioxide compared to porcelain-veneered crowns and lithium disilicate crownsActa Odontologica Scandinavica, 2013
- Translucency of dental ceramics with different thicknessesThe Journal of Prosthetic Dentistry, 2013
- Fracture Strength of Yttria‐Stabilized Zirconium‐Dioxide (Y‐TZP) Fixed Dental Prostheses (FDPs) with Different Abutment Core Thicknesses and Connector DimensionsJournal of Prosthodontics, 2013
- Randomized, Controlled Clinical Trial of Bilayer Ceramic and Metal‐Ceramic Crown PerformanceJournal of Prosthodontics, 2012
- Clinical results of lithium-disilicate crowns after up to 9 years of serviceClinical Oral Investigations, 2012
- All-Ceramic Systems: Laboratory and Clinical PerformanceDental Clinics of North America, 2011
- Performance of Dental Ceramics: Challenges for ImprovementsJournal of Dental Research, 2011
- Three-year clinical evaluation of two ceramic crown systems: A preliminary studyThe Journal of Prosthetic Dentistry, 2010