Effect of charcoal-based dentifrices on the surface integrity and gloss of lithium disilicate glass-ceramics
Authors:
- Victor Martins StabileVSVictor Martins Stabile
- Ana Caroline Lima ColombinoACAna Caroline Lima Colombino
- Andrey Gonçalves EmídioAEAndrey Gonçalves Emídio
- Lourenço Correr-SobrinhoLCLourenço Correr-Sobrinho
- Roberta Caroline Bruschi AlonsoRARoberta Caroline Bruschi Alonso
- Regina Maria Puppin-RontaniRegina Maria Puppin-Rontani
- 28 August 2025
- journal article
- research article
- Published by Springer Nature in Clinical Oral Investigations
- Vol. 29 (9) , 1-10
Abstract
Objectives To evaluate the effects of commercially charcoal-based dentifrices on the surface roughness and gloss retention of glazed lithium disilicate glass-ceramics subjected to simulated toothbrushing. Materials and methods Seventy-two glazed lithium disilicate specimens (IPS e.max CAD) were randomly assigned to three dentifrice groups (n = 24): two charcoal-based (Carvvo (CVV), Curaprox Black is White (CBW)) and one conventional (Colgate Total 12 (C12)), the control. Toothbrushing simulations were performed for 5,000, 10,000, and 20,000 cycles. Roughness (Ra) and gloss (GU) were measured at baseline and after each cycle. Surface characterization was performed using three-dimensional profilometry and scanning electron microscopy (SEM), which also analyzed abrasive particles. Data were analyzed using two-way repeated measures ANOVA and Tukey’s post-hoc test (α = 0.05). Results Roughness was affected only by dentifrice type (p = 0.004), with CVV producing higher mean values than C12, and CBW not differing from the others. Brushing cycle (p = 0.164) and interaction (p = 0.095) were non-significant. Gloss was affected by dentifrice (p < 0.001), brushing cycle (p < 0.001), and their interaction (p < 0.001). Charcoal-based dentifrices caused gloss reductions (CVV: 80.77GU baseline to 67.41GU at 20,000 cycles; CBW: 86.39GU baseline to 69.62GU at 20,000 cycles). In contrast, C12 increased gloss, reaching up to 95.97GU at 20,000 cycles. Conclusions Charcoal-based dentifrices significantly compromise the surface integrity of glazed lithium disilicate ceramics by increasing roughness and reducing gloss. Conventional dentifrices demonstrate no deleterious effect on ceramic surfaces and may even enhance gloss. Clinical relevance Routine use of charcoal-based dentifrices may accelerate surface wear and reduce optical properties of ceramic restorations, potentially compromising longevity and esthetic outcomes.Keywords
All Related Versions
Funding Information
- Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (001, 001, 001, 001, 001)
This publication has 44 references indexed in Scilit:
- Retrospective clinical study on the performance and aesthetic outcome of pressed lithium disilicate restorations in posterior teeth up to 8.3 yearsClinical Oral Investigations, 2023
- Does glaze firing affect the strength of advanced lithium disilicate after simulated defects?Clinical Oral Investigations, 2023
- Effect of glazing technique and firing on surface roughness and flexural strength of an advanced lithium disilicateClinical Oral Investigations, 2023
- Wear behavior and abrasiveness of monolithic CAD/CAM ceramics after simulated masticationClinical Oral Investigations, 2022
- Investigation of surface roughness values of various restorative materials after brushing with blue covarine containing whitening toothpaste by two different methods: AFM and profilometerMicroscopy Research and Technique, 2021
- Activated charcoal toothpastes do not increase erosive tooth wearJournal of Dentistry, 2021
- Charcoal and charcoal-based dentifricesThe Journal of the American Dental Association, 2017
- Influence of degradation conditions on dentin bonding durability of three universal adhesivesJournal of Dentistry, 2016
- Abrasive Finishing and Polishing in Restorative Dentistry: A State-of-the-Art ReviewDental Clinics of North America, 2007
- Surface roughness and gloss of dental materials as a function of force and polishing time in vitroDental Materials, 2006