Lourenço Correr-Sobrinho
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Lourenço Correr-Sobrinho has a total of 211 co-authors. Here are the top co-authors by number of shared publications:
- Américo Bortolazzo Correr
State University of Campinas, Brazil
33 shared publications - Ana Rosa Costa
Department of Orthodontics, Hermínio Ometto Foundation - FHO, Araras, SP, Brazil
17 shared publications - Mário Alexandre Coelho Sinhoreti
University of Campinas
15 shared publications - Silvia Amélia Scudeler Vedovello
Universidade Estadual de Campinas, Brasil
11 shared publications Ana Rosa Costa
Universidade Estadual de Campinas, Brazil
10 shared publications- Regina Maria Puppin-Rontani
Universidade Estadual de Campinas, Brasil
8 shared publications
Latest Publications
- Open Access
- 1 January 2026
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 37
Torque expression in conventional and self-ligating orthodontic brackets: An in vitro study
This study assessed torque expression at different angulations of conventional, interactive, and passive self-ligating brackets, with or without metal ligatures, and evaluated surface morphology and chemical composition (%). All brackets (Roth prescription, 0.022" x 0.028" slot) were fixed to round acrylic cylinders with cyanoacrylate adhesive. Five hundred segments of rectangular archwires (0.019" x 0.025") were bent and welded (20 mm x 10 mm), then fixed to the brackets either with or without 0.010" metal ligatures in ten experimental groups (n = 10). The assembled specimens were then mounted on a universal testing machine, and a vertical force was applied to the free end of the archwire, resulting in a 10 mm displacement. Mean torque values (N·mm) at specified torque angles of 0° to 25°, as well as the mean torque angles (°) corresponding to 5 and 20 N·mm, were analyzed using ANOVA and Tukey’s test (α = 0.05). Bracket design and chemical composition were examined by SEM/EDS. Slot angulation and dimensional measurements were evaluated using ImageJ. Passive self-ligating brackets, without and with ligatures, showed the smallest torque angles, statistically smaller than those of the other groups (p < 0.001). Bracket clips were composed predominantly of nickel and titanium. Passive self-ligating brackets, either ligated or not, showed the highest torque expression at both 5 and 20 N·mm. Overall, torque expression was influenced more by the dimensional characteristics of brackets and rectangular archwires than by the type of ligature used. Clinically, passive self-ligating brackets may facilitate earlier torque expression during orthodontic treatment.
- 1 January 2026
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 37
Open AccessTorque expression in conventional and self-ligating orthodontic brackets: An in vitro study
This study assessed torque expression at different angulations of conventional, interactive, and passive self-ligating brackets, with or without metal ligatures, and evaluated surface morphology and chemical composition (%). All brackets (Roth prescription, 0.022" x 0.028" slot) were fixed to round acrylic cylinders with cyanoacrylate adhesive. Five hundred segments of rectangular archwires (0.019" x 0.025") were bent and welded (20 mm x 10 mm), then fixed to the brackets either with or without 0.010" metal ligatures in ten experimental groups (n = 10). The assembled specimens were then mounted on a universal testing machine, and a vertical force was applied to the free end of the archwire, resulting in a 10 mm displacement. Mean torque values (N·mm) at specified torque angles of 0° to 25°, as well as the mean torque angles (°) corresponding to 5 and 20 N·mm, were analyzed using ANOVA and Tukey’s test (α = 0.05). Bracket design and chemical composition were examined by SEM/EDS. Slot angulation and dimensional measurements were evaluated using ImageJ. Passive self-ligating brackets, without and with ligatures, showed the smallest torque angles, statistically smaller than those of the other groups (p < 0.001). Bracket clips were composed predominantly of nickel and titanium. Passive self-ligating brackets, either ligated or not, showed the highest torque expression at both 5 and 20 N·mm. Overall, torque expression was influenced more by the dimensional characteristics of brackets and rectangular archwires than by the type of ligature used. Clinically, passive self-ligating brackets may facilitate earlier torque expression during orthodontic treatment.
- 28 August 2025
- Published by Springer Nature in Clinical Oral Investigations
- Vol. 29 (9) , 1-10
Effect of charcoal-based dentifrices on the surface integrity and gloss of lithium disilicate glass-ceramics
Objectives To evaluate the effects of commercially charcoal-based dentifrices on the surface roughness and gloss retention of glazed lithium disilicate glass-ceramics subjected to simulated toothbrushing. Materials and methods Seventy-two glazed lithium disilicate specimens (IPS e.max CAD) were randomly assigned to three dentifrice groups (n = 24): two charcoal-based (Carvvo (CVV), Curaprox Black is White (CBW)) and one conventional (Colgate Total 12 (C12)), the control. Toothbrushing simulations were performed for 5,000, 10,000, and 20,000 cycles. Roughness (Ra) and gloss (GU) were measured at baseline and after each cycle. Surface characterization was performed using three-dimensional profilometry and scanning electron microscopy (SEM), which also analyzed abrasive particles. Data were analyzed using two-way repeated measures ANOVA and Tukey’s post-hoc test (α = 0.05). Results Roughness was affected only by dentifrice type (p = 0.004), with CVV producing higher mean values than C12, and CBW not differing from the others. Brushing cycle (p = 0.164) and interaction (p = 0.095) were non-significant. Gloss was affected by dentifrice (p < 0.001), brushing cycle (p < 0.001), and their interaction (p < 0.001). Charcoal-based dentifrices caused gloss reductions (CVV: 80.77GU baseline to 67.41GU at 20,000 cycles; CBW: 86.39GU baseline to 69.62GU at 20,000 cycles). In contrast, C12 increased gloss, reaching up to 95.97GU at 20,000 cycles. Conclusions Charcoal-based dentifrices significantly compromise the surface integrity of glazed lithium disilicate ceramics by increasing roughness and reducing gloss. Conventional dentifrices demonstrate no deleterious effect on ceramic surfaces and may even enhance gloss. Clinical relevance Routine use of charcoal-based dentifrices may accelerate surface wear and reduce optical properties of ceramic restorations, potentially compromising longevity and esthetic outcomes.
- 28 August 2025
- Published by Springer Nature in Clinical Oral Investigations
- Vol. 29 (9) , 1-10
Effect of charcoal-based dentifrices on the surface integrity and gloss of lithium disilicate glass-ceramics
Objectives To evaluate the effects of commercially charcoal-based dentifrices on the surface roughness and gloss retention of glazed lithium disilicate glass-ceramics subjected to simulated toothbrushing. Materials and methods Seventy-two glazed lithium disilicate specimens (IPS e.max CAD) were randomly assigned to three dentifrice groups (n = 24): two charcoal-based (Carvvo (CVV), Curaprox Black is White (CBW)) and one conventional (Colgate Total 12 (C12)), the control. Toothbrushing simulations were performed for 5,000, 10,000, and 20,000 cycles. Roughness (Ra) and gloss (GU) were measured at baseline and after each cycle. Surface characterization was performed using three-dimensional profilometry and scanning electron microscopy (SEM), which also analyzed abrasive particles. Data were analyzed using two-way repeated measures ANOVA and Tukey’s post-hoc test (α = 0.05). Results Roughness was affected only by dentifrice type (p = 0.004), with CVV producing higher mean values than C12, and CBW not differing from the others. Brushing cycle (p = 0.164) and interaction (p = 0.095) were non-significant. Gloss was affected by dentifrice (p < 0.001), brushing cycle (p < 0.001), and their interaction (p < 0.001). Charcoal-based dentifrices caused gloss reductions (CVV: 80.77GU baseline to 67.41GU at 20,000 cycles; CBW: 86.39GU baseline to 69.62GU at 20,000 cycles). In contrast, C12 increased gloss, reaching up to 95.97GU at 20,000 cycles. Conclusions Charcoal-based dentifrices significantly compromise the surface integrity of glazed lithium disilicate ceramics by increasing roughness and reducing gloss. Conventional dentifrices demonstrate no deleterious effect on ceramic surfaces and may even enhance gloss. Clinical relevance Routine use of charcoal-based dentifrices may accelerate surface wear and reduce optical properties of ceramic restorations, potentially compromising longevity and esthetic outcomes.
- 27 April 2025
- Published by Elsevier in Journal of Dentistry
- Vol. 158, 105785
Simple post-curing methods to optimize the depth of cure and physicochemical properties of 3D printed resin
- 27 April 2025
- Published by Elsevier in Journal of Dentistry
- Vol. 158, 105785
Simple post-curing methods to optimize the depth of cure and physicochemical properties of 3D printed resin
- Open Access
- 1 January 2025
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 36, e24-6106
Enamel Deproteinization with Sodium Hypochlorite: Effects on Ceramic Bracket Bond Strength
To assess the efficiency of different concentrations of sodium hypochlorite (NaOCl) on the bonding of ceramic brackets to dental enamel using different bonding protocols. Ceramic, a polycrystalline bracket, was bonded to 90 extracted bovine incisors using primer + Transbond XT (P+TXT); Optibond S adhesive + Transbond XT (OS+TXT), and OS + Orthocem (OS+OC). Three concentrations of NaOCl (0%, 2.5%, and 5.25%) were used for each material, resulting in nine experimental groups (n=10). The shear bond strength (SBS) assay was performed on a universal testing machine. The surface morphology of the enamel and tooth/bonding material interface was examined under a scanning electron microscope. Kruskal-Wallis and Dunn’s tests were performed to compare the non-parametric data (ARI scores). SBS data were analyzed using a generalized linear model. All analyses were performed using the R program and with a significance level of 5%. No significant differences in SBS between the groups with different concentrations of NaOCl (p>0.05). OS+OC group yielded the lowest bond strength values (3.35 MPa_0%, 4.90 MPa_2.5%, 4.68 MPa_5.25%) compared to the other groups, regardless of NaOCl (p0.05). OS+TXT-5.25% showed significantly higher scores (14.4 MPa) than OS+TXT-2.5% (9.17 MPa) (p<0.05). The surface morphology analysis revealed a change in the etching pattern for types 1 and 2 when NaOCl was used. The different concentrations of NaOCl previously applied onto the enamel surface did not enhance bond strength. OS+OC should not be recommended for bonding with fixed ceramic orthodontic devices.
- 1 January 2025
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 36, e24-6106
Open AccessEnamel Deproteinization with Sodium Hypochlorite: Effects on Ceramic Bracket Bond Strength
To assess the efficiency of different concentrations of sodium hypochlorite (NaOCl) on the bonding of ceramic brackets to dental enamel using different bonding protocols. Ceramic, a polycrystalline bracket, was bonded to 90 extracted bovine incisors using primer + Transbond XT (P+TXT); Optibond S adhesive + Transbond XT (OS+TXT), and OS + Orthocem (OS+OC). Three concentrations of NaOCl (0%, 2.5%, and 5.25%) were used for each material, resulting in nine experimental groups (n=10). The shear bond strength (SBS) assay was performed on a universal testing machine. The surface morphology of the enamel and tooth/bonding material interface was examined under a scanning electron microscope. Kruskal-Wallis and Dunn’s tests were performed to compare the non-parametric data (ARI scores). SBS data were analyzed using a generalized linear model. All analyses were performed using the R program and with a significance level of 5%. No significant differences in SBS between the groups with different concentrations of NaOCl (p>0.05). OS+OC group yielded the lowest bond strength values (3.35 MPa_0%, 4.90 MPa_2.5%, 4.68 MPa_5.25%) compared to the other groups, regardless of NaOCl (p0.05). OS+TXT-5.25% showed significantly higher scores (14.4 MPa) than OS+TXT-2.5% (9.17 MPa) (p<0.05). The surface morphology analysis revealed a change in the etching pattern for types 1 and 2 when NaOCl was used. The different concentrations of NaOCl previously applied onto the enamel surface did not enhance bond strength. OS+OC should not be recommended for bonding with fixed ceramic orthodontic devices.
- Open Access
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Journal of Applied Oral Science
- Vol. 32, e20240172
Physicochemical properties of flowable composites using isobornyl methacrylate as diluent monomer
This study sought to evaluate the effect of isobornyl methacrylate (IBOMA) as a diluent monomer on the physicochemical properties of experimental flowable resin composites.
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Journal of Applied Oral Science
- Vol. 32, e20240172
Open AccessPhysicochemical properties of flowable composites using isobornyl methacrylate as diluent monomer
This study sought to evaluate the effect of isobornyl methacrylate (IBOMA) as a diluent monomer on the physicochemical properties of experimental flowable resin composites.
- Open Access
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Oral Research
- Vol. 38, e078
Effect of adding arginine at different concentrations to experimental orthodontic resins: an in vitro study
The aim of this study was to assess the effect of adding arginine at different concentrations to commercial and experimental orthodontic resins on shear bond strength (SBS), as well as on the antimicrobial activity of arginine against S. mutans. Metal brackets were bonded onto the surface of 120 bovine incisors using Transbond, OrthoCem, and an experimental resin (ER), adding 0, 2.5, 5, and 7 wt.% of arginine. The SBS test was performed in deionized water at 37 ºC for 24 h, at 0.5 mm/min. SBS test results were subjected to two-way ANOVA and Tukey’s test (α = 0.05). CFU/mL data (antimicrobial assessment) were assessed by Kruskal-Wallis and Dunn’s tests (α = 0.05). No statistical difference between the resins was observed in untreated groups (p > 0.05). The addition of arginine at 2.5% (27.7 MPa) and 5% (29.0 MPa) increased the SBS of Transbond when compared (p < 0.05) to OrthoCem (18.5 and 15.6 MPa, respectively) and ER (16.3 and 18.1 MPa, respectively). Arginine at 7% improved the SBS of Transbond (24.1 MPa) and ER (21.0 MPa), which was statistically higher (p < 0.05) than OrthoCem (12.6 MPa). OrthoCem did not show a statistically significant difference at the three concentrations of arginine (p > 0.05). The addition of arginine to resins reduced the count of S. mutans (p < 0.05). As for ER, all concentrations of arginine significantly decreased CFU/mL (p < 0.05). Among commercial resins, only 7% of arginine significantly reduced CFU/mL. The addition of arginine did not interfere with the bond strength and demonstrated antibacterial activity against S. mutans.
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Oral Research
- Vol. 38, e078
Open AccessEffect of adding arginine at different concentrations to experimental orthodontic resins: an in vitro study
The aim of this study was to assess the effect of adding arginine at different concentrations to commercial and experimental orthodontic resins on shear bond strength (SBS), as well as on the antimicrobial activity of arginine against S. mutans. Metal brackets were bonded onto the surface of 120 bovine incisors using Transbond, OrthoCem, and an experimental resin (ER), adding 0, 2.5, 5, and 7 wt.% of arginine. The SBS test was performed in deionized water at 37 ºC for 24 h, at 0.5 mm/min. SBS test results were subjected to two-way ANOVA and Tukey’s test (α = 0.05). CFU/mL data (antimicrobial assessment) were assessed by Kruskal-Wallis and Dunn’s tests (α = 0.05). No statistical difference between the resins was observed in untreated groups (p > 0.05). The addition of arginine at 2.5% (27.7 MPa) and 5% (29.0 MPa) increased the SBS of Transbond when compared (p < 0.05) to OrthoCem (18.5 and 15.6 MPa, respectively) and ER (16.3 and 18.1 MPa, respectively). Arginine at 7% improved the SBS of Transbond (24.1 MPa) and ER (21.0 MPa), which was statistically higher (p < 0.05) than OrthoCem (12.6 MPa). OrthoCem did not show a statistically significant difference at the three concentrations of arginine (p > 0.05). The addition of arginine to resins reduced the count of S. mutans (p < 0.05). As for ER, all concentrations of arginine significantly decreased CFU/mL (p < 0.05). Among commercial resins, only 7% of arginine significantly reduced CFU/mL. The addition of arginine did not interfere with the bond strength and demonstrated antibacterial activity against S. mutans.
- Open Access
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 35, e24-5669
Effect of hydrofluoric acid concentration and aging on the bond strength ceramics to a resin cement
This study evaluated the influence of hydrofluoric acid (HF) concentration and thermal cycling on the microshear bond strength (µSBS) of a resin luting agent to IPS e.max® CAD and Rosetta® SM. Ceramic specimens (12.0 x 14.0 x 1.5mm) were randomized into 8 groups (n=10) according to HF concentration, commercial brand, and aging. Immediately after polishing, and etching, all specimens were silanized and a layer of adhesive was applied. A PVS mold of 3 mm thickness and 10mm diameter with (four) 1.0mm holes was fabricated, placed on each specimen, and then filled with a resin luting agent. Half of the specimens were subjected to the µSBS test using an Instron at a speed of 1.0 mm/min, following a 24-hour storage in deionized water at 37ºC. The remaining specimens were subjected to thermal cycling (5ºC-55ºC, 30 seconds per bath) and µSBS. The data were evaluated utilizing a three-way ANOVA and Tukey's post-hoc test (α=0.05). Significant differences were found for HF concentration and aging (p<0.0001). No significant difference in µSBS was found for commercial brands (p=0.085). The interaction between brand and HF concentration (p=0.358), brand and aging (p=0.135), and HF concentration and aging (p=0.138) were not statistically significant. The triple interaction among these factors was not statistically significant (p=0.610). In conclusion, the bond strength is affected by the HF concentration. No statistical difference was observed between the two ceramics. Thermal cycling significantly reduced µSBS.
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 35, e24-5669
Open AccessEffect of hydrofluoric acid concentration and aging on the bond strength ceramics to a resin cement
This study evaluated the influence of hydrofluoric acid (HF) concentration and thermal cycling on the microshear bond strength (µSBS) of a resin luting agent to IPS e.max® CAD and Rosetta® SM. Ceramic specimens (12.0 x 14.0 x 1.5mm) were randomized into 8 groups (n=10) according to HF concentration, commercial brand, and aging. Immediately after polishing, and etching, all specimens were silanized and a layer of adhesive was applied. A PVS mold of 3 mm thickness and 10mm diameter with (four) 1.0mm holes was fabricated, placed on each specimen, and then filled with a resin luting agent. Half of the specimens were subjected to the µSBS test using an Instron at a speed of 1.0 mm/min, following a 24-hour storage in deionized water at 37ºC. The remaining specimens were subjected to thermal cycling (5ºC-55ºC, 30 seconds per bath) and µSBS. The data were evaluated utilizing a three-way ANOVA and Tukey's post-hoc test (α=0.05). Significant differences were found for HF concentration and aging (p<0.0001). No significant difference in µSBS was found for commercial brands (p=0.085). The interaction between brand and HF concentration (p=0.358), brand and aging (p=0.135), and HF concentration and aging (p=0.138) were not statistically significant. The triple interaction among these factors was not statistically significant (p=0.610). In conclusion, the bond strength is affected by the HF concentration. No statistical difference was observed between the two ceramics. Thermal cycling significantly reduced µSBS.
- Open Access
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 35, e24-5674
Surface treatments of the zirconia-reinforced lithium disilicate ceramic in the adhesion to the resin cement
This study verified the effect of surface treatments of the zirconia-reinforced lithium disilicate ceramic bonded to resin cement. Ceramic blocks were divided according to treatments (n=10): FA+SRX (Fluoric acid + silane RX), FA+MDP (Fluoric acid + MDP), FA+SCF+MDP (Fluoric acid + silane CF + MDP), FA+MEP (Fluoric acid + MEP), and MEP (Self-etch primer). Resin cement cylinders were made in the ceramic blocks, photoactivated with 1,200 mW/cm² for 40s, stored in water at 37°C for 24h, and evaluated by the microshear strength test, optical failure descriptive analysis (%), surface characterization (SEM) and contact angle (Goniometer). Other samples were submitted to 10,000 thermocycles between 5°C and 55°C. Bond strength data were submitted to two-way ANOVA and Tukey’s test. Contact angle to one-way ANOVA and Games-Howell's test (5%). At 24h, MEP showed higher bond strength, and FA+SRX the lower. FA+MDP and FA+SCF+MDP showed similar values and FA+MEP was intermediate. After thermocycling, FA+SCF+MDP, FA+MEP, and MEP showed higher values, and FA+SRX the lower while FA+MDP was intermediate. When the periods were compared, FA+MDP, FA+SCF+MDP, FA+MEP, and MEP showed higher values for 24h while FA+SRX was similar. SEM showed retentive surface and crystal exposure when treated with FA+SCF+MDP. The less retentive surface was obtained with MEP, and the other treatments promoted intermediate irregularities. In conclusion, surface treatment and thermocycling promoted different values of adhesive strength and contact angle in a zirconia-reinforced lithium silicate ceramic. Failures were predominantly adhesive, and the ceramic surface was characterized by different levels of roughness and selective exposure of crystals.
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 35, e24-5674
Open AccessSurface treatments of the zirconia-reinforced lithium disilicate ceramic in the adhesion to the resin cement
This study verified the effect of surface treatments of the zirconia-reinforced lithium disilicate ceramic bonded to resin cement. Ceramic blocks were divided according to treatments (n=10): FA+SRX (Fluoric acid + silane RX), FA+MDP (Fluoric acid + MDP), FA+SCF+MDP (Fluoric acid + silane CF + MDP), FA+MEP (Fluoric acid + MEP), and MEP (Self-etch primer). Resin cement cylinders were made in the ceramic blocks, photoactivated with 1,200 mW/cm² for 40s, stored in water at 37°C for 24h, and evaluated by the microshear strength test, optical failure descriptive analysis (%), surface characterization (SEM) and contact angle (Goniometer). Other samples were submitted to 10,000 thermocycles between 5°C and 55°C. Bond strength data were submitted to two-way ANOVA and Tukey’s test. Contact angle to one-way ANOVA and Games-Howell's test (5%). At 24h, MEP showed higher bond strength, and FA+SRX the lower. FA+MDP and FA+SCF+MDP showed similar values and FA+MEP was intermediate. After thermocycling, FA+SCF+MDP, FA+MEP, and MEP showed higher values, and FA+SRX the lower while FA+MDP was intermediate. When the periods were compared, FA+MDP, FA+SCF+MDP, FA+MEP, and MEP showed higher values for 24h while FA+SRX was similar. SEM showed retentive surface and crystal exposure when treated with FA+SCF+MDP. The less retentive surface was obtained with MEP, and the other treatments promoted intermediate irregularities. In conclusion, surface treatment and thermocycling promoted different values of adhesive strength and contact angle in a zirconia-reinforced lithium silicate ceramic. Failures were predominantly adhesive, and the ceramic surface was characterized by different levels of roughness and selective exposure of crystals.
- Open Access
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 35, e24-5619
Effect of Ceramic Thickness on the Bond Strength to Resin-Luting Agents before and after Thermal Cycling
This study investigated microshear bond strength (µSBS) of two (2) dual-cured resin-luting agents (RelyX™ Ultimate and RelyX™ U200) when photoactivated through varying thicknesses of lithium disilicate, with or without thermal cycling. Discs of IPS e.max Press of 0.5, 1.5, and 2 mm in thickness were obtained. Elastomer molds (3.0 mm in thickness) with four cylinder-shaped orifices 1.0 mm in diameter, were placed onto the ceramic surfaces and filled with resin-luting agents. A Mylar strip, glass plate, and load of 250 grams were placed over the filled mold. The load was removed and the resin-luting agents were photoactivated through the ceramics using a single-peak LED (Radii Plus.) All samples were stored in distilled water at 37oC for 24 h. Half of the samples were subjected to thermal cycling (3,000 cycles; 5ºC and 55ºC). All samples were then submitted to µSBS test using a universal testing machine (Instron 4411) at a crosshead speed of 0.5 mm/min. Data were submitted to three-way ANOVA and Tukey post-hoc test (α=0.05). The mean µSBS at 24 h was significantly higher than after thermal cycling (p 0.05). The mean µSBS for groups photoactivated through 0.5 mm ceramic were significantly higher than 1.5 mm and 2.0 mm (p < 0.05). In conclusion, increased ceramic thicknesses reduced the bond strength of tested resin-luting agents to lithium disilicate. No differences were found between resin-luting agents. Thermal cycling reduced the bond strength of both resin-luting agents.
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 35, e24-5619
Open AccessEffect of Ceramic Thickness on the Bond Strength to Resin-Luting Agents before and after Thermal Cycling
This study investigated microshear bond strength (µSBS) of two (2) dual-cured resin-luting agents (RelyX™ Ultimate and RelyX™ U200) when photoactivated through varying thicknesses of lithium disilicate, with or without thermal cycling. Discs of IPS e.max Press of 0.5, 1.5, and 2 mm in thickness were obtained. Elastomer molds (3.0 mm in thickness) with four cylinder-shaped orifices 1.0 mm in diameter, were placed onto the ceramic surfaces and filled with resin-luting agents. A Mylar strip, glass plate, and load of 250 grams were placed over the filled mold. The load was removed and the resin-luting agents were photoactivated through the ceramics using a single-peak LED (Radii Plus.) All samples were stored in distilled water at 37oC for 24 h. Half of the samples were subjected to thermal cycling (3,000 cycles; 5ºC and 55ºC). All samples were then submitted to µSBS test using a universal testing machine (Instron 4411) at a crosshead speed of 0.5 mm/min. Data were submitted to three-way ANOVA and Tukey post-hoc test (α=0.05). The mean µSBS at 24 h was significantly higher than after thermal cycling (p 0.05). The mean µSBS for groups photoactivated through 0.5 mm ceramic were significantly higher than 1.5 mm and 2.0 mm (p < 0.05). In conclusion, increased ceramic thicknesses reduced the bond strength of tested resin-luting agents to lithium disilicate. No differences were found between resin-luting agents. Thermal cycling reduced the bond strength of both resin-luting agents.