Abstract
The use of plasmonic nanoparticles for biosensor technology is dependent on nanoparticle size and morphology. This study determined the effect of pH and pressure on synthetized silver nanoparticles size. In method 1, a mixture of NaBH4 and sodium citrate was added to a solution of AgNO3 monodispersed by ultrasound energy. In method 2 the reducer was added to the precursor-dispersant mixture solution. The effect of pH was evaluated by using buffer solutions at pH 4,0, pH 7,0, pH 10,0 and water as control. To determine the effect of pressure, AgNPs were subjected for 0, 4 and 23 hours to 1,75 MPa at 200°C. AgNPs produced with method 1 showed a more symmetric SRP and a smaller nanoparticle diameter (±6 nm). The SPR with method 1 at pH 10,0 produced a higher UV peak with a shift around 20 nm. In the case of the pressure treatment, a shift of approximately 20 nm was observed at all time conditions studied, and a higher AgNPs diameter was found in contrast to method 1. Finally, EDX and Raman analysis confirm the presence of AgNPs and a mild oxidation of these. These results suggest that alkalinity and pressure allow affect the diameter of AgNPs.

This publication has 31 references indexed in Scilit: