Microstructure and Mechanical Properties of AlSi10MnMg Alloy with Increased Content of Recycled Scrap
Open Access
Abstract
Increasing the share of circulating scrap in produced castings is not only due to optimizing production costs, but also the need to protect the environment realized by reducing production energy intensity, generating less waste, mitigating greenhouse gas emissions, and consuming fewer natural resources. However, this is associated with maintaining the required properties of castings and considering the impact of impurities on the formation of the structure of aluminum alloys. This research concerns the AlSi10MnMg alloy, which introduces 50 to 75% (every 5%) of circulating scrap. This alloy is one of the most commonly used for producing gravity and pressure die-castings (HPDC), including engine parts and transport structural elements. Based on microscopic research, it was found that the increase in scrap content causes an increase in the share of iron, which results in pre-eutectic (from about 0.45 wt.% to 0.7 wt.% Fe) or even primary crystallization of iron phases (over 0.7 wt.% Fe), mainly the plate–needle phase β-Al5FeSi. Its unfavorable morphology and size cause the formation of numerous shrinkage porosity areas, which has an impact on the reduction in mechanical properties (reduction in UTS and YS by approx. 16% and elongation by approx. 18%, compared to the AlSi10MnMg alloy with 50% scrap content). It was found that the increase in the share of recycled scrap (from 50 to 75%) can be used only when the manganese content is increased. Its effect is to change the morphology of the β-Al5FeSi phase into α-Al15(Fe,Mn)3Si2, whose crystallization occurs in the temperature range of 540 to 555 °C and increases slightly with increasing manganese addition. It is essential to consider the appropriate value of the Mn/Fe quotient, which should be about 1/2, because a higher value may cause the formation of a sludge factor. This work aimed to determine the limiting iron content (contained in the scrap) at which the sequence of the β-Al5FeSi phase release (pre-eutectic or primary crystallization) changes. This sequence mainly affects the form of morphology, the dimensions of the β-Fe phase, and the proportion of shrinkage porosity.Keywords
This publication has 53 references indexed in Scilit:
- Use of reactive nanostructured chemicals for refinement of Si eutectic in an aluminum casting alloyJournal of Materials Science, 2019
- Structures and Mechanical Properties of Al-Al2Cu InterfacesJOM, 2019
- Secondary Al-Si-Mg High-pressure Die Casting Alloys with Enhanced DuctilityMetallurgical and Materials Transactions A, 2014
- Influence of Oxide Additions on the Porosity Development and Mechanical Properties of A356 Aluminium Alloy CastingsInternational Journal of Metalcasting, 2012
- Aluminum recycling—An integrated, industrywide approachJOM, 2010
- Modeling the Effect of Finite-Rate Hydrogen Diffusion on Porosity Formation in Aluminum AlloysMetallurgical and Materials Transactions B, 2007
- Iron-rich intermetallic phases and their role in casting defect formation in hypoeutectic Al−Si alloysMetallurgical and Materials Transactions A, 2005
- The role of iron in the formation of porosity in Al-Si-Cu-based casting alloys: Part I. Initial experimental observationsMetallurgical and Materials Transactions A, 1999
- Effect of hydrogen in aluminium and aluminium alloys: A reviewBulletin of Materials Science, 1996
- Effect of alloying elements on the solidification characteristics and microstructure of Al- Si- Cu- Mg- Fe 380 alloyMetallurgical and Materials Transactions A, 1994