Thickness and yttria percentage influences the fracture resistance of laminate veneer zirconia restorations
Open Access
- 13 September 2022
- journal article
- research article
- Published by Wiley in Clinical and Experimental Dental Research
- Vol. 8 (6) , 1413-1420
Abstract
Objectives: Mechanical properties are cardinal for the long‐term clinical success of laminate veneer restorations but the selection of new restorative materials should ideally be based on clinical evidence, therefore, in vitro testing of dental materials is a good alternative to evaluate their properties and understand their behavior so this study aimed to compare and evaluate the effect of two different thicknesses and yttria percentage on the fracture resistance of laminate veneer zirconia restorations.Materials and Methods: Forty laminate veneer restoration prepared from partial sintering zirconia of 3Y (yttria), 5Y (yttria), combined 3Y&5Y (yttria), and lithium disilicate. Specimens were assigned into four main groups according to their percentage of yttria content (n = 10) and subgrouped into two thicknesses (0.5 mm thickness and 0.3 mm thickness) (n = 5) as follows: Group I, II, III, and IV (Group I for lithium disilicate (control), Group II for 3Y zirconia, Group III for 5Y zirconia, and Group IV for combined 3Y&5Y zirconia), each of them subdivided according to their thickness into two subgroups (n = 5 for each one) and resistance to fracture for each restoration was evaluated using a universal testing machine. Data were analyzed using a one‐way analysis of variance and Duncan's tests at a 5% level of significance.Results: The thickness of laminate veneer restoration significantly affects the fracture resistance value of all type of laminate veneers restorations (fracture resistance mean value was highest for 0.5 mm thickness and lower for 0.3 mm thickness restorations) and yttria percentage significantly affect fracture resistance value of zirconia laminate veneer restorations (fracture resistance mean value was highest for 0.5 mm thickness of 3Y zirconia [865 N] and combined 3Y&5Y zirconia [846 N]).Conclusions: Reducing the thickness of laminate zirconia veneer restorations to 0.3 mm reduces its fracture resistance and increasing yttria percentage had an adverse effect on fracture resistance of zirconia laminate veneer restorations.Keywords
This publication has 28 references indexed in Scilit:
- Novel Zirconia Materials in DentistryJournal of Dental Research, 2017
- Comparison of the effect of different surface treatments on the bond strength of different cements with nickel chromium metal alloy: An in vitro studyJournal of Clinical and Experimental Dentistry, 2017
- Effects of pretreatments and hydrothermal aging on biaxial flexural strength of lithium di-silicate and Mg-PSZ ceramicsJournal of Dentistry, 2016
- Effect of grain size on the monoclinic transformation, hardness, roughness, and modulus of aged partially stabilized zirconiaDental Materials, 2015
- The clinical success of tooth‐ and implant‐supported zirconia‐based fixed dental prostheses. A systematic reviewJournal of Oral Rehabilitation, 2015
- Survival of Porcelain Laminate Veneers with Different Degrees of Dentin Exposure: 2-year Clinical Results2014
- The failure load of CAD/CAM generated zirconia and glass-ceramic laminate veneers with different preparation designsThe Journal of Prosthetic Dentistry, 2012
- Fracture resistance of all‐ceramic crowns placed on a preparation with a slice‐formed finishing lineJournal of Oral Rehabilitation, 2009
- A comparison of fracture strength of yttrium‐oxide‐ partially‐stabilized zirconia ceramic crowns with varying core thickness, shapes and veneer ceramicsJournal of Oral Rehabilitation, 2004
- Measurement of enamel thickness in relation to reduction for etched laminate veneers.1992