In‐Plane Cracking Behavior and Ultimate Strength for 2D Woven and Braided Melt‐Infiltrated SiC/SiC Composites Tensile Loaded in Off‐Axis Fiber Directions
- 30 August 2007
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 90 (10) , 3185-3193
Abstract
The tensile mechanical properties of ceramic matrix composites (CMC) in directions off the primary axes of the reinforcing fibers are important for the architectural design of CMC components that are subjected to multiaxial stress states. In this study, two‐dimensional (2D)‐woven melt‐infiltrated (MI) SiC/SiC composite panels with balanced fiber content in the 0° and 90° directions were tensile loaded in‐plane in the 0° direction and at 45° to this direction. In addition, a 2D triaxially braided MI SiC/SiC composite panel with a higher fiber content in the ±67° bias directions compared with the axial direction was tensile loaded perpendicular to the axial direction tows (i.e., 23° from the bias fibers). Stress–strain behavior, acoustic emission, and optical microscopy were used to quantify stress‐dependent matrix cracking and ultimate strength in the panels. It was observed that both off‐axis‐loaded panels displayed higher composite onset stresses for through‐thickness matrix cracking than the 2D‐woven 0/90 panels loaded in the primary 0° direction. These improvements for off‐axis cracking strength can in part be attributed to higher effective fiber fractions in the loading direction, which in turn reduces internal stresses on weak regions in the architecture, e.g., minicomposite tows oriented normal to the loading direction and/or critical flaws in the matrix for a given composite stress. Both off‐axis‐oriented panels also showed relatively good ultimate tensile strength when compared with other off‐axis‐oriented composites in the literature, both on an absolute strength basis as well as when normalized by the average fiber strength within the composites. Initial implications are discussed for constituent and architecture design to improve the directional cracking of SiC/SiC CMC components with MI matrices.Keywords
This publication has 18 references indexed in Scilit:
- SiC/SiC Composites for 1200°C and Above2005
- Stress-dependent matrix cracking in 2D woven SiC-fiber reinforced melt-infiltrated SiC matrix compositesComposites Science and Technology, 2004
- Effects of Thermal Aging on the Mechanical Properties of a Porous‐Matrix Ceramic CompositeJournal of the American Ceramic Society, 2002
- Intermediate temperature strength degradationin SiC/SiC compositesJournal of the European Ceramic Society, 2002
- Modal acoustic emission of damage accumulation in a woven SiC/SiC compositeComposites Science and Technology, 1999
- Mechanical performance of 2-D braided carbon/epoxy compositesComposites Science and Technology, 1998
- Effects of Off‐Axis Loading on the Tensile Behavior of a Ceramic‐Matrix CompositeJournal of the American Ceramic Society, 1996
- Crack Initiation in Fiber‐Reinforced Brittle LaminatesJournal of the American Ceramic Society, 1996
- In‐Plane Mechanical Properties of Several Ceramic‐Matrix CompositesJournal of the American Ceramic Society, 1995
- Model of the Nonlinear Mechanical Behavior of 2D SiC–SiC Chemical Vapor Infiltration CompositesJournal of the American Ceramic Society, 1994