Biaxial flexural strength of Turkom-Cera core compared to two other all-ceramic systems
Open Access
- 1 December 2010
- journal article
- research article
- Published by FapUNIFESP (SciELO) in Journal of Applied Oral Science
- Vol. 18 (6) , 607-612
Abstract
The aim of this study was to compare the biaxial flexural strength of three core ceramic materials. Three groups of 10 disc-shaped specimens (16 mm diameter x 1.2 mm thickness - in accordance with ISO-6872, 1995) were made from the following ceramic materials: Turkom-Cera Fused Alumina [(Turkom-Ceramic (M) Sdn Bhd, Puchong, Selangor, Malaysia)], In-Ceram (Vita Zahnfabrik, Bad Säckingen, Baden-Württemberg, Germany) and Vitadur-N (Vita Zahnfabrik, Bad Säckingen, Baden-Württemberg, Germany), which were sintered according to the manufacturer's recommendations. The specimens were subjected to biaxial flexural strength test in a universal testing machine at a crosshead speed of 0.5 mm/min. The definitive fracture load was recorded for each specimen and the biaxial flexural strength was calculated from an equation in accordance with ISO-6872. The mean biaxial flexural strength values were: Turkom-Cera: 506.8±87.01 MPa, In-Ceram: 347.4±28.83 MPa and Vitadur-N: 128.7±12.72 MPa. The results were analyzed by the Levene's test and Dunnett's T3 post-hoc test (SPSS software V11.5.0 for Windows, SPSS, Chicago, IL, USA ) at a preset significance level of 5% because of unequal group variances (P<0.001). There was statistically significant difference between the three core ceramics (P<0.05). Turkom-Cera showed the highest biaxial flexural strength, followed by In-Ceram and Vitadur-N. Turkom-Cera core had significantly higher flexural strength than In-Ceram and Vitadur-N ceramic core materials.Keywords
This publication has 33 references indexed in Scilit:
- CAD/CAM Zirconia vs. slip-cast glass-infiltrated Alumina/Zirconia all-ceramic crowns: 2-year results of a randomized controlled clinical trialJournal of Applied Oral Science, 2009
- RESIN BOND TO DENTAL CERAMICS, PART II: HIGH‐STRENGTH CERAMICSJournal of Esthetic and Restorative Dentistry, 2004
- A comparison of fracture strength of yttrium‐oxide‐ partially‐stabilized zirconia ceramic crowns with varying core thickness, shapes and veneer ceramicsJournal of Oral Rehabilitation, 2004
- Mechanical properties of commercial high strength ceramic core materialsDental Materials, 2004
- The effect of cement type and mixing on the bi-axial fracture strength of cemented aluminous core porcelain discsDental Materials, 2003
- Interpenetrating Phase CompositesJournal of the American Ceramic Society, 1992
- Relative flexural strength of dental restorative ceramicsDental Materials, 1990
- Toughening of a Particulate‐Reinforced Ceramic‐Matrix Composite by Thermal Residual StressJournal of the American Ceramic Society, 1990
- Unilateral, isometric bite force in 8‐68‐year‐old women and men related to occlusal factorsEuropean Journal of Oral Sciences, 1990
- Improvements in Mechanical Properties in SiC by the Addition of TiC ParticlesJournal of the American Ceramic Society, 1984