Low-Temperature Solution Synthesis of Zinc Oxide Nanotubes
Authors:
- 15 July 2013
- journal article
- research article
- Published by Taylor & Francis in Synthesis and Reactivity in Inorganic, Metal-Organic, and Nano-Metal Chemistry
- Vol. 43 (10) , 1501-1505
Abstract
Zinc oxide nanotubes (ZnO-NTs) have been successfully synthesized at ∼60°C using wet chemical method. ZnO-NTs have diameters of 100–200 nm and lengths of 1–2 μm. Transmission electron microscopy shows that as-synthesized NTs are single-crystal hexagonal structure and grown along [0001] direction. X-ray diffraction, ultravisible absorption, and photoluminescence results reveal that thermal treatments at low temperature of <500°C in air cannot apparently improve the crystal properties of as-synthesized ZnO.Keywords
This publication has 21 references indexed in Scilit:
- The influence of annealing temperature on the structure, morphologies and optical properties of ZnO nanoparticlesSuperlattices and Microstructures, 2010
- Efficient synthesis of ZnO nanoparticles, nanowalls, and nanowires by thermal decomposition of zinc acetate at a low temperatureApplied Physics A, 2008
- Controllable Growth of ZnO Nanostructures by a Simple Solvothermal ProcessThe Journal of Physical Chemistry C, 2007
- ZnO Nanowire TransistorsThe Journal of Physical Chemistry B, 2004
- Morphology and Thermal Stability of the Active Layer in Poly(p-phenylenevinylene)/Methanofullerene Plastic Photovoltaic DevicesMacromolecules, 2004
- Efficient field emission from ZnO nanoneedle arraysApplied Physics Letters, 2003
- Metalorganic vapor-phase epitaxial growth of vertically well-aligned ZnO nanorodsApplied Physics Letters, 2002
- A simple and novel route for the preparation of ZnO nanorodsSolid State Communications, 2002
- Room-Temperature Ultraviolet Nanowire NanolasersScience, 2001
- Thermal decomposition of graphite oxidation products DSC studies of internal combustion of graphite oxideMaterials Research Bulletin, 1987