Retentive Strength of CAD/CAM-Fabricated All-Ceramic Crowns Luted on Titanium Implant Abutments Using Different Ceramic Materials and Luting Agents: An In Vitro Study
Open Access
Abstract
Objectives: This study aimed to determine the retentive strength of monolithic hybrid-all-ceramic crowns luted on titanium implant abutments. Material and Methods: In total, 450 crowns (75 each of Mark II, Empress CAD, e.max CAD, Suprinity, Enamic, Celtra Duo) were milled using a CAD/CAM system. The crowns were cemented onto sandblasted titanium implant abutments using five luting agents (Multilink Implant, Variolink II, RelyX Unicem, Fujicem, and Panavia 2.0). After thermocycling was performed (5000 cycles: 5–55 °C, 30-s dwell time), the crowns were removed using a universal testing machine. The location of luting-agent residue on the abutment and inner crown surfaces was evaluated. Analyses of variance (ANOVA) with the Bonferroni correction were performed to evaluate differences of retentive strength depending on the crown material and the kind of the luting agent. Results: The retentive strengths for the different ceramic materials were Vita Mark II: 652N-759N (SD:134N-146N), Empress CAD: 681N-822N (SD: 89N-146N), e.max CAD: 784N-1044N (SD: 109N-176N), Vita Enamic: 716N-1177N (SD: 132N-220N), Vita Suprinity: 867N-1488N (SD: 202N-278N), and Celtra Duo 772N-1335N (SD:151N-229N). After the removal trials, the visual documentation showed different adhesive residue location depending on the ceramic materials. Furthermore, the pull-off force was dependent on the choice of adhesives. No significant differences were found between different luting agents and the ceramic material Vita Mark II and Empress CAD. EmaxCAD showed significant differences with Unicem and FujiCem compared to Panavia, as did VitaSuprinity, VitaEnamic, and Celtra Duo (p < 0.001). Conclusions: The ceramic material used seems to influence the retentive strength and the use of certain luting agents results in a higher retentive strength for some ceramic materials.Keywords
All Related Versions
This publication has 36 references indexed in Scilit:
- Fracture Strength of Monolithic All-Ceramic Crowns on Titanium Implant AbutmentsThe International Journal of Oral and Maxillofacial Implants, 2016
- Effect of surface topography of implant abutments on retention of cemented single-tooth crowns.2010
- Effect of Surface Conditioning and Taper Angle on the Retention of IPS e.max Press CrownsJournal of Prosthodontics, 2010
- Influence of different luting concepts on long term retentive strength of zirconia crowns.2009
- Effects of Surface Conditioning on the Retentiveness of Titanium Crowns Over Short Implant AbutmentsImplant Dentistry, 2007
- In vitro retentive strength of zirconium oxide ceramic crowns using different luting agentsThe Journal of Prosthetic Dentistry, 2005
- The effects of abutment taper, length and cement type on resistance to dislodgement of cement‐retained, implant‐supported restorationsJournal of Prosthodontics, 2003
- Shear bond strength of resin cements to both ceramic and dentinThe Journal of Prosthetic Dentistry, 2002
- Weibull parameters of composite resin bond strengths to porcelain and noble alloy using the Rocatec systemDental Materials, 2002
- Influence of different convergence angles and tooth preparation heights on the internal adaptation of Cerec crownsThe Journal of Prosthetic Dentistry, 2002