Ti‐Doped Nanocomposite Pr2Fe14B/α‐Fe Ribbons with High Coercivity
Authors:
- 10 December 2023
- journal article
- research article
- Published by Wiley in Physica Status Solidi (a)
- Vol. 221 (4)
Abstract
Nanocomposite permanent magnetic alloys are prepared by the melt‐spinning technique with wheel speed ranging from 21 to 33 ms−1. X‐ray diffraction results show that the as‐spun ribbon is rich of soft α‐Fe, hard Pr2Fe14B magnetic phases, and no other metastable phases are found in our alloy ribbon. Initial magnetization curves reveal that the coercivity mechanism of the ribbons vary with the content of Ti. For x = 2, coercivity is mainly determined by pure pinning; while for x = 1, 3, and 4, it is mainly controlled by the mixture of nucleation of domain and localized pinning at grain boundaries. The coercivity value of 1026 kA m−1, the highest value reported so far, is mainly generated from a pure pinning mechanism in the ribbon with x = 2. The recoil permeability shows a minimum value range from to for x = 2 alloy, suggesting strong exchange coupling between the magnetic grains and then leading to the concurrent reversal of soft and hard phase grains during the demagnetization process. The Henkel plots demonstrate only exchange interaction for x = 1 and exchange interaction with slightly magnetostatic interaction for x = 2, 3, and 4. The exchange interaction exhibits maximum strength for x = 2, which is the reason for high coercivity.Keywords
Funding Information
- National Natural Science Foundation of China (12074220 and 11627805)
- Natural Science Foundation of Shandong Province (ZR2016EMM14)
This publication has 31 references indexed in Scilit:
- Magnetic force microscopy investigation of the domain structure of nanocomposite Nd2Fe14B/Fe3B magnetsActa Materialia, 2011
- Lean neodymium Nd–Fe–B magnets containing minor addition of titaniumPhysica Status Solidi (a), 2010
- Phase evolution and magnetic properties of PrxFe82−x−yTiyCo10B4C4 (x=9–10.5; y=0, 2) nanocompositesJournal of Alloys and Compounds, 2007
- Effect of Ti substitution on the magnetic properties, microstructure, and aftereffect of melt spun PrFeB nanocompositesScripta Materialia, 2006
- Study on the magnetic properties, phase evolution and microstructure of PrxFe82.2−yTiyB17.8−x (x=5–11.8; y=2.5–5.5) nanocompositesJournal of Magnetism and Magnetic Materials, 2006
- Effect of Fe substitution by Ti or Nb/V/Zr on phase stability and magnetic properties of Pr2Fe23(B, C)3 ribbonsJournal of Magnetism and Magnetic Materials, 2004
- Effect of wheel speed on the microstructure and exchange coupling interaction of nanocomposite Nd2Fe14B/α-Fe magnetsMaterials Science and Engineering: A, 2003
- A comparative study of melt-spun ribbons of Nd12Fe82B6and Nd15Fe77B8Journal of Physics D: Applied Physics, 1998
- Remanenzverhalten und Wechselwirkungen in hartmagnetischen TeilchenkollektivenPhysica Status Solidi (b), 1964
- The Scherrer Formula for X-Ray Particle Size DeterminationPhysical Review B, 1939