Damage behavior of tungsten fiber‐reinforced copper matrix composite after high‐speed impact

Authors:

Abstract
W f /Cu 82 Al 10 Fe 4 Ni 4 composite was fabricated by means of infiltration casting. By the microstructure observation of the composite with the aid of scanning electron microscopy (SEM) and transmission electron microscopy (TEM), it can be found that there are (Fe, Ni), AlFe, Al 3 Ni, and Cu 3 Al precipitated phases existing in the matrix alloy. By two‐stage light gas gun, W f /Cu 82 Al 10 Fe 4 Ni 4 composite hypervelocity projectile into concrete target test with the speed of 2.2 km·s −1 is finished. By microstructure observation, it can be found that the failure mode of W f /Cu 82 Al 10 Fe 4 Ni 4 composite projectile during penetration is the rapid peeling of tungsten fibers from the projectile, which makes the projectile display good self‐sharpening property. Meanwhile, it can be found that microstructure morphology change of W f /Cu 82 Al 10 Fe 4 Ni 4 composite occurs after hypervelocity impact. The density of dislocations around the large‐dimensional (Fe, Ni), AlFe, Al 3 Ni, and Cu 3 Al precipitated phases in the matrix alloy rises sharply. At the same time, there are large‐dimensional deformed twins existing in local regions and stacking faults existing inside the twins.
Funding Information
  • Fundamental Research Funds for the Central Universities (DL12BB04)
  • National Natural Science Foundation of China (31200434)
  • National Natural Science Foundation of China (31370566)

This publication has 24 references indexed in Scilit: