Corrosion and Magnetite Growth on Carbon Steels in Water at 310 C —Effect of Dissolved Oxygen, pH, and EDTA Addition

Authors:
  • HGH. S. Gadiyar
    H. S. Gadiyar

Abstract
The formation of magnetite at 310 C on carbon steels has been studied at pH 7.0 and 10.5 in presence of two oxygen levels (<0.05 and 3.5 ppm) by kinetics, scanning electron microscopy, and electrochemical measurements. An adherent and protective magnetite of thickness 1.8 μ was observed after 530 hours of exposure at pH 10.5 and oxygen <0.05 ppm. Higher oxygen and neutral pH conditions resulted in only a slight increase in the overall corrosion rates, but the magnetite was still adherent and protective. Two stages in the oxide formation were seen. During the first stage, the oxide growth was nearly parabolic and continued up to a thickness of about 4 microns followed by the second stage under steady state conditions, with a low corrosion rate of 0.015 mm/y or less. The addition of EDTA up to 300 ppm has resulted in improving the adherence of the oxide and decreasing the corrosion metal loss. Room temperature electrochemical measurements have shown that the passivity proceeds in two stages, Fe(OH)2 formation and its subsequent conversion to FeO OH layer in the absence of dissolved oxygen. At high temperature, this FeO OH apparently oxidizes to protective magnetite. In the presence of oxygen, chemical oxidation of ferrous to ferric oxide has also been postulated.

This publication has 13 references indexed in Scilit: