Abstract
The paper examines composite binders based on Portland cement and volcanic sand, subjected to mechanical activation in a vibrating mill. Rational grinding parameters (10, 30, and 50 minutes) and filler content (10-30%) were determined. It was found that under optimal conditions, the specific surface area reaches 731.2 m2/kg, and the compressive strength increases to 90.34 MPa after 28 days, which is 77.8% higher than that of commercial cement. Laser granulometry and X-ray phase analysis revealed the hardening mechanisms associated with the amorphization of the structure, a decrease in the average diameter of the particles and the formation of additional hydrosilicate phases. The possibility of saving Portland cement up to 30% without loss of strength characteristics is shown

This publication has 3 references indexed in Scilit: