Effect of Silicon Compounds on Stress Corrosion Cracking of Alloy 600 in Caustic Solutions
Authors:
- M. NavasMNM. Navas
- D. Gómez-BriceñoDGD. Gómez-Briceño
- 1 July 1999
- journal article
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 55 (7) , 674-685
Abstract
Silicon compounds are abundant in both steam generator tube deposits removed from operating plants and in the hide-out return analyses performed during plant operation. Despite their abundance, the effect of these compounds on the susceptibility to intergranular attack (IGA) and stress corrosion cracking (SCC) of alloy 600 (UNS N06600) has not been established clearly in laboratory tests or under operating conditions. The present work studied the effect of different compounds of silicon, such as silica (SiO2) and sodium metasilicate (Na2SiO3), on the susceptibility to IGA/ SCC of alloy 600 in caustic solutions, with and without impurities. Experimental work included measurement of potentiodynamic polarization curves and development of stress corrosion tests with potentiostatic control at 315°C. Results of both tests indicated an inhibiting effect of silicon compounds on stress corrosion of mill-annealed (MA) alloy 600. Polarization curves in solutions with silicon compounds showed a wider range of passivation and a reduction in passive current density and anodic dissolution compared to the curves obtained in sodium hydroxide (NaOH). In corrosion tests performed in solutions containing silicon compounds, cracking appeared at only some of the potentials tested and with much reduced depth. Judging by the results obtained from analyses of the surface deposits, the inhibiting effect appeared to be related to the incorporation of silicon in the oxide layer. Regarding the effect of impurities, these have been observed not to be harmful for the response of alloy 600MA to IGA/SCC, and would appear even to improve this response in solutions containing silicon compounds, probably caused by the formation of insoluble silicates.Keywords
This publication has 9 references indexed in Scilit:
- Revised pourbaix diagrams for chromium at 25–300 °CCorrosion Science, 1997
- Effect of Partial Pressure of Hydrogen on IGSCC of Alloy 600 in PWR Primary WaterCorrosion, 1991
- Sodium Silicates—Stress Corrosion Cracking Agents for Alloys 600 and 690 at 315 CCorrosion, 1985
- Neutralization of tubesheet crevice corrosion. Final report1983
- Optimization of metallurgical variables to improve the stress corrosion resistance of Inconel 6001980
- Prediction of stress corrosion cracking in 10% caustic soda solutions at 315°C (600°F)Corrosion Science, 1980
- Stress Corrosion Cracking Studies of High Nickel Austenitic Alloys in Several High Temperature Aqueous Solutions1979
- Stress Corrosion Cracking of Stainless Steel and Nickel Alloys at Controlled Potentials in 10% Caustic Soda Solutions at 550°FJournal of the Electrochemical Society, 1976
- The system water-sodium oxide-silicon dioxide at 200, 250, and 300.degree.Inorganic Chemistry, 1967