Comparative Evaluation of Novel and Conventional Acid Etchants on the Surface Roughness of Lithium Disilicate and Zirconia Ceramics
Open Access
- 1 January 2026
- journal article
- Published by Wiley in International Journal of Dentistry
- Vol. 2026 (1) , 4245703
Abstract
Background: Establishing a durable bond to high‐strength dental ceramics, especially zirconia (Zir), is a clinical challenge. This is due to the material’s chemical inertness and its resistance to conventional etching methods. Zir lacks silica, making it unresponsive to traditional hydrofluoric acid (HF) treatments effective for glass ceramics like lithium disilicate (LiDi). This study assesses the efficacy of a novel multiacid etchant in modifying the surface roughness of LiDi and 5 mol% yttria‐stabilized Zir (5Y‐TZP), comparing its performance against three commercial HF‐based etchants. Methods: Four etchants were tested: Zircos‐E (EDOS [ZiE]), 9.5% porcelain etchant (Bisco [BIS]), 9% porcelain etch (Ultradent [ULT]), and IPS Ceramic Etching Gel (Ivoclar [IPS]). Each was applied for 20 s, 1 min, and 30 min to LiDi (Amber Mill) and 5Y Zir (IPS e.max ZirCAD Prime MT) specimens ( n = 10 per group). Surface roughness (Ra) was measured with a profilometer. Data were analyzed using two‐way analysis of variance (ANOVA) and Tukey’s honestly significant difference (HSD) test ( α = 0.05). Results: On 5Y Zir, Zircos‐E produced significantly higher surface roughness than all other etchants, reaching 0.378 µm at 30 min ( p < 0.001), indicating a greater ability to modify the Zir surface topography under the conditions evaluated in this study. On LiDi, it also resulted in the highest roughness (0.785 µm) but with signs of excessive etching and surface degradation. In contrast, the HF‐based etchants produced more controlled and uniform roughening on LiDi, without overetching. Conclusions: The novel multiacid etchant is highly effective for treating 5Y Zir, creating a favorable microretentive surface for bonding. However, its aggressive action makes it unsuitable for LiDi, where overetching can compromise structural integrity. Selection of etching agents should be material‐specific to optimize clinical outcomes while preserving ceramic quality.Keywords
This publication has 38 references indexed in Scilit:
- Is zirconia surface etching a viable alternative to airborne particle abrasion? A systematic review and meta-analysis of in vitro studiesJournal of Dentistry, 2024
- Advances in Ceramics for Dental ApplicationsDental Clinics of North America, 2022
- Chemical surface modification of lithium disilicate needles of a silica-based ceramic after HF-etching and ultrasonic bath cleaning: Impact on the chemical bonding with silaneDental Materials, 2021
- Effects of an etching solution on the adhesive properties and surface microhardness of zirconia dental ceramicsThe Journal of Prosthetic Dentistry, 2018
- The effect of surface treatments on dental zirconia: An analysis of biaxial flexural strength, surface roughness and phase transformationJournal of Dentistry, 2018
- Effect of surface treatments on the properties and morphological change of dental zirconiaThe Journal of Prosthetic Dentistry, 2016
- Effect of hydrofluoric acid concentration and etching duration on select surface roughness parameters for zirconiaThe Journal of Prosthetic Dentistry, 2015
- Insights on Ceramics as Dental Materials. Part II: Chemical Surface TreatmentsSilicon, 2011
- State of the art of zirconia for dental applicationsDental Materials, 2008
- Stabilized zirconia as a structural ceramic: An overviewDental Materials, 2008