Eliminating surface transverse cracks in the novel vertical bending continuous casting of pure aluminum 1070 thin slabs
Open Access
- 4 March 2025
- journal article
- research article
- Published by Springer Nature in Scientific Reports
- Vol. 15 (1) , 1-14
Abstract
To achieve high-efficiency continuous production of aluminum, vertical bending continuous casting equipment has been designed. However, the formation of surface transverse cracks during casting presents a significant challenge, particularly when producing thin slabs of pure aluminum 1070. This study investigates the high-temperature tensile properties of pure aluminum 1070 thin slabs and conducts numerical simulations of the temperature and stress fields in the vertical bending continuous casting process. The results indicate that a thick solidified shell at the mold outlet, combined with sufficient high-temperature strength and plasticity at the center of the wide surface (1170 mm from the arc section inlet), is essential for resisting thermal and mechanical stresses, thus preventing the formation of surface transverse cracks. The solidified shell thickness at the mold outlet is optimized to no less than 10.8 mm. Additionally, the temperature at the center of the wide surface at an arc length of 1170 mm from the inlet of the arc section and at the outlet of the arc section are effectively controlled to a maximum of 414.0 °C and 365.1 °C, respectively. These adjustments effectively prevent surface transverse cracks in the produced pure aluminum 1070 thin slabs. The novelty of this work lies in the precise regulation of both the temperature and stress fields, offering a solution to the surface crack issue. This study makes significant contributions to optimizing casting parameters for the novel process and enhancing the overall efficiency of aluminum alloy production.Keywords
Funding Information
- The financial support of the State Key Laboratory of Rolling and Automation.
This publication has 39 references indexed in Scilit:
- Investigation into the Performance of TIG and MIG Welded Joints of Al6061 Plates2024
- Analysis into Mechanical Properties and Microstructural Behavior of Friction Stir Welded Al 6061-T6 Alloy Joints2022
- Tensile Properties of a Cast Al-Si-Mg Alloy with Reduced Si Content and Cr Addition at High TemperatureJournal of Materials Engineering and Performance, 2019
- The Influences of Grain Size and Morphology on the Hot Tearing Susceptibility, Contraction, and Load Behaviors of AA7050 Alloy Inoculated with Al-5Ti-1B Master AlloyMetallurgical and Materials Transactions A, 2016
- Direct‐Chill Casting of Light Alloys2013
- Observation and Prediction of the Hot Tear Susceptibility of Ternary Al-Si-Mg AlloysMetallurgical and Materials Transactions A, 2012
- Rheological behavior of Al-Mg-Si-Cu alloys in the mushy state obtained by partial remelting and partial solidification at high cooling rateMetallurgical and Materials Transactions A, 2006
- Rheological behavior of Al-Cu alloys during solidification constitutive modeling, experimental identification, and numerical studyMetallurgical and Materials Transactions A, 2005
- The use of water cooling during the continuous casting of steel and aluminum alloysMetallurgical and Materials Transactions A, 2005
- Effects of alloy composition and casting speed on structure formation and hot tearing during direct-chill casting of Al-Cu alloysMetallurgical and Materials Transactions A, 2004