TAThorbjörn Andersson

Thorbjörn Andersson

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Thorbjörn Andersson has a total of 7 co-authors. Here are the top co-authors by number of shared publications:

  • Bengt Wesslén

    Polymer Science & Technology, Lund University, Lund, Sweden

    3 shared publications
  • Tim Nielsen

    SIK – The Swedish Institute for Food and Biotechnology, Lund

    3 shared publications
  • Bengt Wesslén

    Department of Polymer Science and Engineering, Lund Institute of Technology, P.O. Box 124, SE-221 00 Lund, Sweden

    1 shared publication
  • Berit Stålbom

    Department of Material Characterisation, Tetra Pak Research & Development AB, SE 221 86 Lund, Sweden

    1 shared publication
  • Gunnar Forsgren

    Laboratory for Sensory and Chemical Analysis, Iggesund Paperboard, Strömsbruk

    1 shared publication
  • John Sandström

    Department of Material Development, Tetra Pak Research & Development AB, S-221 86 Lund, Sweden

    1 shared publication

Latest Publications

  • The effects of selected aldehydes, ketones and carboxylic acids on off-flavours in water

    by Thorbjörn Andersson, Gunnar Forsgren, Tim Nielsen

    The effects of selected aldehydes, ketones and carboxylic acids on the development of off-flavours in water were studied. Combinations of hexanal, octanal, 2-octanone, 5-nonanone, hexanoic acid and nonanoic acid were rated by the off-flavour intensities they created in water at concentrations just at or below the threshold value of each analyte. Two different sensory panels evaluated the off-flavours induced by different combinations of the analytes. The observations of the two panels agreed well. From these studies, it could be concluded that aldehydes play an important role in the development of off-flavours intensities in water. There were synergistic effects between aldehydes and ketones, as well as between aldehydes and carboxylic acids. Small amounts of aldehydes and carboxylic acids – well below their respective threshold values – caused an increase in the off-flavour intensity. No synergism between ketones and carboxylic acids could be observed.


  • Degradation of polyethylene during extrusion. II. Degradation of low‐density polyethylene, linear low‐density polyethylene, and high‐density polyethylene in film extrusion

    by Thorbjörn Andersson, Berit Stålbom, Bengt Wesslén

    The degradation of different polyethylenes—low‐density polyethylene (LDPE), linear low‐density polyethylene (LLDPE), and high‐density polyethylene (HDPE)—with and without antioxidants and at different oxygen concentrations in the polymer granulates, have been studied in extrusion coating processing. The degradation was followed by online rheometry, size exclusion chromatography, surface oxidation index measurements, and gas chromatography–mass spectrometry. The degradations start in the extruder where primary radicals are formed, which are subject to the auto‐oxidation when oxygen is present. In the extruder, crosslinking or chain scissions reactions are dominating at low and high melt temperatures, respectively, for LDPE, and chain scission is overall dominating for the more linear LLDPE and HDPE resins. Additives such as antioxidants react with primary radicals formed in the melt. Degradation taking place in the film between the die orifice, and the quenching point is mainly related to the exposure time to air oxygen. Melt temperatures above 280°C give a dominating surface oxidation, which increases with the exposure time to air between die orifice and quenching too. A number of degradation products were identified—for example, aldehydes and organic acids—which were present in homologous series. The total amount of aldehydes and acids for each number of chain carbon atoms were appeared in the order of C5>C4>C6>C7≫C2 for LDPE, C5>C6>C4>C7≫C2 for LLDPE, and C5>C6>C7>C4≫C2 for HDPE. The total amounts of oxidized compounds presented in the films were related to the processing conditions. Polymer melts exposed to oxygen at the highest temperatures and longest times showed the presence dialdehydes, in addition to the aldehydes and acids. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 91: 1525–1537, 2004


  • Degradation of low density polyethylene during extrusion. I. Volatile compounds in smoke from extruded films

    by Thorbjörn Andersson, Bengt Wesslén, John Sandström

    Many problems with odor and taste in food packaging can be traced to degradation of the packaging materials during processing. From this starting point, the degradation of polyethylene in a commercial extrusion coating process was studied by analyzing degradation products present in smoke sampled at the extruder die orifice. Two low‐density polyethylenes, A and B, with similar melt flow indexes and densities and obtained from different producers, were investigated. A third polymer, C, consisting of recycled material B, was also investigated. More than 40 aliphatic aldehydes and ketones, together with 14 different carboxylic acids, were identified in the smoke. The highest concentration was found for acetaldehyde, regardless of polymer and processing conditions. Increasing the extrusion temperatures in the range 280–325 °C increased the amounts of the oxidized products in the smoke. The extruded film thickness, 12 and 25 μm, influenced the concentrations of degradation products, with the thicker film giving higher amounts of product. The recycled polymer C generally gave lower concentrations of degradation products compared with the virgin polymer B. Differences in the product spectrum between the two virgin polymers may be related to differences in the manufacturing process. Many of the identified compounds have very characteristic taste and smell and are consequently of interest from an odor and taste point of view in food packaging applications. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 86: 1580–1586, 2002