- Zhengren Huang
State Key Laboratory of High Performance Ceramics and Superfine Microstructures, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 200050, China
5 shared publications - Xishi Wu
State Key Laboratory of Advanced Marine Materials, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China
3 shared publications Jian Chen
2 shared publicationsRonghua Su
Suzhou Kunlun Heavy Equipment Manufacturing Co., Ltd, Jiangsu, Kunshan, China
2 shared publicationsYan Liu
State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics Chinese Academy of Sciences, Shanghai, Shanghai, China
2 shared publicationsZhengren Huang
2 shared publications
Latest Publications
- 1 January 2025
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 40 (5) , 466
Effect of Zn2+ Catalyst on Microporous Structure of Porous Carbon Prepared from Phenolic Resin/Ethylene Glycol
- 1 January 2025
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 40 (5) , 466
Effect of Zn2+ Catalyst on Microporous Structure of Porous Carbon Prepared from Phenolic Resin/Ethylene Glycol
- Open Access
Joining of SiC Ceramic by Si–C Reaction Bonding Using Organic Resin as Carbon Precursor
In this study, the joining of silicon carbide (SiC) ceramics was achieved via a Si–C reaction bonding method using the phenolic resin (PF)–MgCl2 system as the carbon precursor. Specifically, by adding MgCl2 to the phenolic resin mixture, the average pore size of the product of carbonization of the PF resin mixture increased from 14 ± 5 nm to 524 ± 21 nm, which was beneficial for the infiltration of molten silicon at high temperature. The microstructure of the joined specimens and the effect of the inert filler on the joint strength were investigated. It was demonstrated that SiC–SiC joints with strong interfacial bonding and high flexural strength could be obtained by the Si–C reaction bonding method using a phenol formaldehyde resin/alcohol sol-gel system as the carbon precursor. The flexural strength of the joined specimens reached the highest value, i.e., 308 ± 27 MPa when the solid loading of the inert filler was 26%. Overall, stable joining of silicon carbide ceramics was achieved by the proposed method, which has significance for realizing the preparation of complex-shaped or large silicon carbide ceramic parts.
Open AccessJoining of SiC Ceramic by Si–C Reaction Bonding Using Organic Resin as Carbon Precursor
In this study, the joining of silicon carbide (SiC) ceramics was achieved via a Si–C reaction bonding method using the phenolic resin (PF)–MgCl2 system as the carbon precursor. Specifically, by adding MgCl2 to the phenolic resin mixture, the average pore size of the product of carbonization of the PF resin mixture increased from 14 ± 5 nm to 524 ± 21 nm, which was beneficial for the infiltration of molten silicon at high temperature. The microstructure of the joined specimens and the effect of the inert filler on the joint strength were investigated. It was demonstrated that SiC–SiC joints with strong interfacial bonding and high flexural strength could be obtained by the Si–C reaction bonding method using a phenol formaldehyde resin/alcohol sol-gel system as the carbon precursor. The flexural strength of the joined specimens reached the highest value, i.e., 308 ± 27 MPa when the solid loading of the inert filler was 26%. Overall, stable joining of silicon carbide ceramics was achieved by the proposed method, which has significance for realizing the preparation of complex-shaped or large silicon carbide ceramic parts.
- 1 January 2022
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 37 (12) , 1275-1280
Effect of Pore Structure of Organic Resin-based Porous Carbon on Joining Properties of Cf/SiC Composites
- 1 January 2022
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 37 (12) , 1275-1280
Effect of Pore Structure of Organic Resin-based Porous Carbon on Joining Properties of Cf/SiC Composites
- 12 March 2019
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 33 (12) , 1261-1274
Effects of random chopped short carbon fibers on microstructure and mechanical properties of joints for Cf/SiC composites by reaction bonding process
Random chopped short carbon fibers (Csf)/phenol-formaldehyde resin (PF)/SiC powder mixtures are used as filler for the joining of Cf/SiC composites to obtain SiC interlayer at the joining region. The influences of Csf on the microstructure and mechanical properties have been investigated. Research shows that the introduction of Csf can improve the microstructure uniformity of the joint and reduce residual silicon content in the interlayer. The joint achieve a high flexural strength of 232 ± 33 MPa as the carbon fiber content is 30 wt.%, which is similar to that of the Cf/SiC composites (220 ± 21 MPa). The decrease in residual silicon content and the formation of nano-sized SiC particles are the main reasons for high joining strength.
- 12 March 2019
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 33 (12) , 1261-1274
Effects of random chopped short carbon fibers on microstructure and mechanical properties of joints for Cf/SiC composites by reaction bonding process
Random chopped short carbon fibers (Csf)/phenol-formaldehyde resin (PF)/SiC powder mixtures are used as filler for the joining of Cf/SiC composites to obtain SiC interlayer at the joining region. The influences of Csf on the microstructure and mechanical properties have been investigated. Research shows that the introduction of Csf can improve the microstructure uniformity of the joint and reduce residual silicon content in the interlayer. The joint achieve a high flexural strength of 232 ± 33 MPa as the carbon fiber content is 30 wt.%, which is similar to that of the Cf/SiC composites (220 ± 21 MPa). The decrease in residual silicon content and the formation of nano-sized SiC particles are the main reasons for high joining strength.
- Open Access
- 31 January 2019
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 9 (8) , 4203-4209
Pore structure control of porous carbon obtained from phenol formaldehyde resin and ethylene glycol: the effect of H3BO3 on the pore structure
Boric acid was used as a source of complexing agent to change phase separation kinetics and dynamics of the resin-glycol system to regulate the pore structure of porous carbon. The results show that the addition of H3BO3 in the resin mixtures can change the polymerization dynamics during curing of resin-glycol mixtures. For the complexation of H3BO3 to diols, the size of the ethylene glycol-rich phase produced during the curing of the resin mixture increase with the increase of the content of H3BO3. Similarly, the pore size of porous carbon after pyrolysis increases with the increase of H3BO3 content. The average pore size of resulting porous carbon can be regulated in the range from 15 to 2754 nm. These results reveal that H3BO3 exhibited obvious effects in changing the pore structure of resin-glycol system during pyrolysis.
- 31 January 2019
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 9 (8) , 4203-4209
Open AccessPore structure control of porous carbon obtained from phenol formaldehyde resin and ethylene glycol: the effect of H3BO3 on the pore structure
Boric acid was used as a source of complexing agent to change phase separation kinetics and dynamics of the resin-glycol system to regulate the pore structure of porous carbon. The results show that the addition of H3BO3 in the resin mixtures can change the polymerization dynamics during curing of resin-glycol mixtures. For the complexation of H3BO3 to diols, the size of the ethylene glycol-rich phase produced during the curing of the resin mixture increase with the increase of the content of H3BO3. Similarly, the pore size of porous carbon after pyrolysis increases with the increase of H3BO3 content. The average pore size of resulting porous carbon can be regulated in the range from 15 to 2754 nm. These results reveal that H3BO3 exhibited obvious effects in changing the pore structure of resin-glycol system during pyrolysis.
- 1 January 2019
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 34 (9) , 4-1020
Preparation and Mechanical Properties of Short Carbon Fiber Reinforced Silicon Carbide Matrix Composites
- 1 January 2019
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 34 (9) , 4-1020
Preparation and Mechanical Properties of Short Carbon Fiber Reinforced Silicon Carbide Matrix Composites
- 1 October 2016
- Published by Elsevier in Materials Letters
- Vol. 181, 278-281
HoAlO3: A novel liquid aid for low temperature densification of SiC ceramics
- 1 October 2016
- Published by Elsevier in Materials Letters
- Vol. 181, 278-281
HoAlO3: A novel liquid aid for low temperature densification of SiC ceramics
- 1 December 2014
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 34 (15) , 4111-4115
Environment-friendly deposition of SiCN interlayer for reinforcing carbon fibers in C/SiC composites
- 1 December 2014
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 34 (15) , 4111-4115
Environment-friendly deposition of SiCN interlayer for reinforcing carbon fibers in C/SiC composites
- 16 February 2007
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 90 (3) , 969-972
Fabricating 2.5D SiC f /SiC Composite Using Polycarbosilane/SiC/Al Mixture for Matrix Derivation
2.5D SiC f /SiC composites were produced by a modified polymer infiltration and pyrolysis process. Fine Al and SiC powders were first infiltrated into large inter‐bundle pores. During pyrolytic decomposition of the polymer, the active Al filler reacts with small carbon‐bearing polymer fragments, and reactive nitrogen atmosphere to form new phases of carbide or nitride. The volume expansion compensates for polymer shrinkage to a certain degree. The microstructural evolution and mechanical performances were characterized. The result indicates that the addition of Al fillers has significant influence on the mechanical properties of the composites. For the composite with Al loading, a proportional‐limit stress of 380 MPa and a maximum stress of 441 MPa are achieved.
- 16 February 2007
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 90 (3) , 969-972
Fabricating 2.5D SiC f /SiC Composite Using Polycarbosilane/SiC/Al Mixture for Matrix Derivation
2.5D SiC f /SiC composites were produced by a modified polymer infiltration and pyrolysis process. Fine Al and SiC powders were first infiltrated into large inter‐bundle pores. During pyrolytic decomposition of the polymer, the active Al filler reacts with small carbon‐bearing polymer fragments, and reactive nitrogen atmosphere to form new phases of carbide or nitride. The volume expansion compensates for polymer shrinkage to a certain degree. The microstructural evolution and mechanical performances were characterized. The result indicates that the addition of Al fillers has significant influence on the mechanical properties of the composites. For the composite with Al loading, a proportional‐limit stress of 380 MPa and a maximum stress of 441 MPa are achieved.
- 7 November 2006
- Published by Wiley in Physica Status Solidi (RRL) – Rapid Research Letters
- Vol. 1 (2) , R59-R61
Polymer‐filler derived ceramics with low shrinkage using PCS/SiC/Al mixture
Active Al and inert SiC powders were dispersed in the polycarbosilane to manufacture SiC ceramic composites by a new process of active‐filler‐controlled pyrolysis of polymer. 40 wt% of active Al fillers, 40 wt% of inert SiC fillers and 20 wt% of PCS, were homogenized. The samples were obtained by pyrolysis at 1100 °C for different soaking time. The results showed that due to the incorporation of active Al fillers, formation of crystallite phases such as Al4C3, Al4Si3 and AlN occured due to the of reaction of Al particles with the polymer decomposition products and the reactive nitrogen atmosphere. The microstructural and mechanical characterization results of the composites are presented in the paper.
- 7 November 2006
- Published by Wiley in Physica Status Solidi (RRL) – Rapid Research Letters
- Vol. 1 (2) , R59-R61
Polymer‐filler derived ceramics with low shrinkage using PCS/SiC/Al mixture
Active Al and inert SiC powders were dispersed in the polycarbosilane to manufacture SiC ceramic composites by a new process of active‐filler‐controlled pyrolysis of polymer. 40 wt% of active Al fillers, 40 wt% of inert SiC fillers and 20 wt% of PCS, were homogenized. The samples were obtained by pyrolysis at 1100 °C for different soaking time. The results showed that due to the incorporation of active Al fillers, formation of crystallite phases such as Al4C3, Al4Si3 and AlN occured due to the of reaction of Al particles with the polymer decomposition products and the reactive nitrogen atmosphere. The microstructural and mechanical characterization results of the composites are presented in the paper.