Jin‐Feng Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Jin‐Feng Li has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
X. Tan
The Key Laboratory of Nonferrous Metal Materials Science and Engineering Ministry of Education Changsha 410083 (P. R. China)
2 shared publicationsC. Cai
School of Chemistry and Chemical Engineering, Ningxia University, Yinchuan 750001 (P. R. China)
1 shared publicationC. X. Li
School of Materials Science and Engineering, Central South University, Changsha 410083 (P. R. China)
1 shared publicationC.‐X. Li
Guangdong General Research Institute of Industrial Technology (Guangzhou Research Institute of Non‐ferrous Metals) Guangzhou 510650 (P. R. China)
1 shared publicationF. L. Zeng
School of Materials Science and Engineering, Central South University, Changsha 410083 (P. R. China)
1 shared publicationN. Jiang
College of Materials Science and Engineering, Central South University, Changsha 410083, P. R. China
1 shared publication
Latest Publications
- 2 July 2013
- Published by Wiley in Materials and Corrosion
- Vol. 65 (11) , 1062-1072
Potential change and corrosion behavior of two Al-Mg-Si alloys with different Si content under MgCl2 drops in 33% relative humidity
The Volta potential change and corrosion behaviors of alloys Al‐0.63Mg‐0.28Si and Al‐0.52Mg‐0.63Si under MgCl2 drops with the initial concentration of 0.1–1.0 M in environments with relative humidity (RH) 33% were studied using a Kelvin probe (KP). For the alloy Al‐0.63Mg‐0.28Si, the Volta potential curve was mainly featured with many potential transients in the form of a sudden drop followed by an immediate recovery along the potential baseline at a higher potential value of −0.35 to −0.5 VSHE, which were associated with initiation and repassivation of metastable pits with diameter less than 3 μm. For the alloy Al‐0.52Mg‐0.63Si containing excess Si particles, the potential curve was featured with potential change in the form of slow increase followed by a sudden drop along the potential baseline at a lower potential value of about −0.7 VSHE. The sudden potential drop and stabilizing at the lower potential level were associated with corrosion initiation and growth, respectively. In the case of lower initial concentration and higher Si content leading to excess Si particles, the corrosion rating was higher. However, the excess Si particles showed a greater impact than the initial concentration.
- 2 July 2013
- Published by Wiley in Materials and Corrosion
- Vol. 65 (11) , 1062-1072
Potential change and corrosion behavior of two Al-Mg-Si alloys with different Si content under MgCl2 drops in 33% relative humidity
The Volta potential change and corrosion behaviors of alloys Al‐0.63Mg‐0.28Si and Al‐0.52Mg‐0.63Si under MgCl2 drops with the initial concentration of 0.1–1.0 M in environments with relative humidity (RH) 33% were studied using a Kelvin probe (KP). For the alloy Al‐0.63Mg‐0.28Si, the Volta potential curve was mainly featured with many potential transients in the form of a sudden drop followed by an immediate recovery along the potential baseline at a higher potential value of −0.35 to −0.5 VSHE, which were associated with initiation and repassivation of metastable pits with diameter less than 3 μm. For the alloy Al‐0.52Mg‐0.63Si containing excess Si particles, the potential curve was featured with potential change in the form of slow increase followed by a sudden drop along the potential baseline at a lower potential value of about −0.7 VSHE. The sudden potential drop and stabilizing at the lower potential level were associated with corrosion initiation and growth, respectively. In the case of lower initial concentration and higher Si content leading to excess Si particles, the corrosion rating was higher. However, the excess Si particles showed a greater impact than the initial concentration.
- 11 July 2012
- Published by Wiley in Materials and Corrosion
- Vol. 65 (5) , 476-484
Corrosion behavior of 1420 Al–Li alloy under MgCl2 drops in 33% relative humidity
The corrosion behaviors of 1420 Al–Li alloy under 4 μl MgCl2 drops with initial concentration of 0.1–1.0 M in relative humidity (RH) 33% were studied using a Kelvin Probe. In all cases, the equilibrium MgCl2 concentration was 4.9 M. The corrosion was highly dependent on the initial MgCl2 concentration. After equilibration with the environment RH, the whole available cathodic limiting current associated with oxygen reduction was decreased with increasing the initial MgCl2 concentration. Accordingly, the corrosion rate was decreased. Under the MgCl2 drops with initial 0.1 and 0.3 M concentrations, the main corrosion form was filiform‐like corrosion. While, as the initial concentration was increased to 1.0 M, the main corrosion form was meta‐stable pitting corrosion. In the case of 0.1 and 0.3 M initial concentrations, along the Volta potential baseline at −0.7 to −0.8 VSHE, there existed many potential transients in the form of rapid increase followed by immediate drop, which should be associated with the filiform‐like corrosion growth stop and initiation. In the case of 1.0 M initial concentration, much more potential transients appeared in the form of sudden drop followed by a recovery, which was associated with the initiation and re‐passivation of meta‐stable pits.
- 11 July 2012
- Published by Wiley in Materials and Corrosion
- Vol. 65 (5) , 476-484
Corrosion behavior of 1420 Al–Li alloy under MgCl2 drops in 33% relative humidity
The corrosion behaviors of 1420 Al–Li alloy under 4 μl MgCl2 drops with initial concentration of 0.1–1.0 M in relative humidity (RH) 33% were studied using a Kelvin Probe. In all cases, the equilibrium MgCl2 concentration was 4.9 M. The corrosion was highly dependent on the initial MgCl2 concentration. After equilibration with the environment RH, the whole available cathodic limiting current associated with oxygen reduction was decreased with increasing the initial MgCl2 concentration. Accordingly, the corrosion rate was decreased. Under the MgCl2 drops with initial 0.1 and 0.3 M concentrations, the main corrosion form was filiform‐like corrosion. While, as the initial concentration was increased to 1.0 M, the main corrosion form was meta‐stable pitting corrosion. In the case of 0.1 and 0.3 M initial concentrations, along the Volta potential baseline at −0.7 to −0.8 VSHE, there existed many potential transients in the form of rapid increase followed by immediate drop, which should be associated with the filiform‐like corrosion growth stop and initiation. In the case of 1.0 M initial concentration, much more potential transients appeared in the form of sudden drop followed by a recovery, which was associated with the initiation and re‐passivation of meta‐stable pits.
- 21 June 2012
- Published by Wiley in Materials and Corrosion
- Vol. 64 (9) , 811-820
Corrosion dependence of an Al-Mg-Si alloy under MgCl2 solution drop on initial concentration and humidity
- 21 June 2012
- Published by Wiley in Materials and Corrosion
- Vol. 64 (9) , 811-820
Corrosion dependence of an Al-Mg-Si alloy under MgCl2 solution drop on initial concentration and humidity
- 5 June 2012
- Published by Wiley
- p. 443-450
Corrosion and Potentiostatic Polarization of an Al‐Cu‐Li Alloy under Tensile Stress
- 5 June 2012
- Published by Wiley
- p. 443-450
Corrosion and Potentiostatic Polarization of an Al‐Cu‐Li Alloy under Tensile Stress
- 10 June 2009
- Published by Wiley in Materials and Corrosion
- Vol. 60 (6) , 407-414
Exfoliation corrosion of 7150 Al alloy with various tempers and its electrochemical impedance spectroscopy in EXCO solution
The exfoliation corrosion susceptibility and electrochemical impedance spectroscopy (EIS) of 7150 Al alloys with T6, T73, and RRA (retrogression at 175 °C for 3 h) tempers in EXCO solution were investigated. The anodic equilibrium precipitate η(MgZn2) is continuous or closely spaced at the grain boundaries in the 7150‐T6 Al alloy, resulting in its greatest susceptibility to exfoliation corrosion. The grain boundary η precipitates in the RRA and T73 treated 7150 Al alloys are coarsened and show a clear discontinuous nature; they possess similar exfoliation corrosion sensitivity and their exfoliation corrosion resistance is greatly increased. At the beginning of immersion in EXCO solution, the EIS plot of the 7150 Al alloys is composed of a capacitive arc in the high to medium frequency range and an inductive component in the medium to low frequency range. As immersion time is increased, exfoliation corrosion with different corrosion ratings occurs on the surface of the 7150 Al alloy with various tempers, two capacitive arcs appear in the high to medium and medium to low frequency ranges, respectively. The fitted medium to low frequency capacitance C2 of 7150‐T6 Al alloy, corresponding to the new surface caused by the exfoliation corrosion, is much greater than that of the T73 and RRA treated 7150 Al alloy, which is consistent with the greatest exfoliation corrosion susceptibility of the 7150‐T6 Al alloy.
- 10 June 2009
- Published by Wiley in Materials and Corrosion
- Vol. 60 (6) , 407-414
Exfoliation corrosion of 7150 Al alloy with various tempers and its electrochemical impedance spectroscopy in EXCO solution
The exfoliation corrosion susceptibility and electrochemical impedance spectroscopy (EIS) of 7150 Al alloys with T6, T73, and RRA (retrogression at 175 °C for 3 h) tempers in EXCO solution were investigated. The anodic equilibrium precipitate η(MgZn2) is continuous or closely spaced at the grain boundaries in the 7150‐T6 Al alloy, resulting in its greatest susceptibility to exfoliation corrosion. The grain boundary η precipitates in the RRA and T73 treated 7150 Al alloys are coarsened and show a clear discontinuous nature; they possess similar exfoliation corrosion sensitivity and their exfoliation corrosion resistance is greatly increased. At the beginning of immersion in EXCO solution, the EIS plot of the 7150 Al alloys is composed of a capacitive arc in the high to medium frequency range and an inductive component in the medium to low frequency range. As immersion time is increased, exfoliation corrosion with different corrosion ratings occurs on the surface of the 7150 Al alloy with various tempers, two capacitive arcs appear in the high to medium and medium to low frequency ranges, respectively. The fitted medium to low frequency capacitance C2 of 7150‐T6 Al alloy, corresponding to the new surface caused by the exfoliation corrosion, is much greater than that of the T73 and RRA treated 7150 Al alloy, which is consistent with the greatest exfoliation corrosion susceptibility of the 7150‐T6 Al alloy.
- 3 April 2007
- Published by Wiley in Materials and Corrosion
- Vol. 58 (4) , 273-279
Exfoliation corrosion and electrochemical impedance spectroscopy of an Al‐Li alloy in EXCO solution
- 3 April 2007
- Published by Wiley in Materials and Corrosion
- Vol. 58 (4) , 273-279
Exfoliation corrosion and electrochemical impedance spectroscopy of an Al‐Li alloy in EXCO solution
- 1 March 2005
- Published by Wiley in Materials and Corrosion
- Vol. 56 (3) , 192-196
Study on localized corrosion mechanism of 2195 Al‐Li alloy in 4.0% NaCl solution (pH 6.5) using a three‐electrode coupling system
Localized corrosion morphologies of 2195 Al‐Li alloy with various heat treatment in 4.0% NaCl solution (pH 6.5) were investigated, and its corrosion mechanism was studied using a three‐electrode coupling system of α (Al) substituting for the precipitate‐free zone (PFZ), simulated bulk θ′ (Al2Cu) and T1 (Al2CuLi). θ′ acts as cathodic zone in the alloy. At the initial stage, T1 phase is active with respect to θ′ and α (Al), and endures the main anodic current, indicating that anodic dissolution occurs on T1. However, its potential moves to positive direction with immersion time, due to dealloying of Li from T1. As a result, the main anodic dissolution occurs on α (Al) at a later stage. At this stage, as only T1 and α (Al) are coupled, T1 is cathodic to α (Al). In real 2195 alloy, T1 phase is very tiny, and anodic dissolution of T1 and PFZ occurs alternately. These results show that its intergranular corrosion or intersubgranular corrosion is caused by alternate anodic dissolution of T1 phase and PFZ along grain and subgrain boundaries.
- 1 March 2005
- Published by Wiley in Materials and Corrosion
- Vol. 56 (3) , 192-196
Study on localized corrosion mechanism of 2195 Al‐Li alloy in 4.0% NaCl solution (pH 6.5) using a three‐electrode coupling system
Localized corrosion morphologies of 2195 Al‐Li alloy with various heat treatment in 4.0% NaCl solution (pH 6.5) were investigated, and its corrosion mechanism was studied using a three‐electrode coupling system of α (Al) substituting for the precipitate‐free zone (PFZ), simulated bulk θ′ (Al2Cu) and T1 (Al2CuLi). θ′ acts as cathodic zone in the alloy. At the initial stage, T1 phase is active with respect to θ′ and α (Al), and endures the main anodic current, indicating that anodic dissolution occurs on T1. However, its potential moves to positive direction with immersion time, due to dealloying of Li from T1. As a result, the main anodic dissolution occurs on α (Al) at a later stage. At this stage, as only T1 and α (Al) are coupled, T1 is cathodic to α (Al). In real 2195 alloy, T1 phase is very tiny, and anodic dissolution of T1 and PFZ occurs alternately. These results show that its intergranular corrosion or intersubgranular corrosion is caused by alternate anodic dissolution of T1 phase and PFZ along grain and subgrain boundaries.