Raman Bedi
Research Subjects
Research Interests
Raman Bedi has a total of 54 co-authors. Here are the top co-authors by number of shared publications:
- Ashok Kumar Bagha
Department of Mechanical Engineering, Dr B R Ambedkar National Institute of Technology Jalandhar, 144008, India
10 shared publications - Modassir Akhtar
PYROSEARCH, School of Chemical Engineering, The University of Queensland, Brisbane, QLD, 4072, Australia
8 shared publications - Rahul Samyal
Birla Institute of Technology & Science Mechanical Engineering Department Pilani
8 shared publications - Akhil Khajuria
Centre for Strategic and Sustainable Infrastructure, Indian Institute of Technology Jammu, Jammu, India
6 shared publications Akhil Khajuria
CSIR—National Metallurgical Laboratory
5 shared publications- Ashwani Kumar Singh
Deen Dayal Upadhyaya Gorakhpur University
4 shared publications
Latest Publications
- 7 November 2026
- Published by SAGE Publications in Plastics, Rubber and Composites: Macromolecular Engineering
Dual-waste valorisation of pine needle biomass and post-consumer PET into sustainable composites: Mechanical, dynamic mechanical and environmental performance
The use of lignocellulosic biomass with post-consumer polyethylene terephthalate (PET) is an attractive option for waste diversion and resource recovery. In this study, pine needle (PN) biomass was used to reinforce a commercial unsaturated polyester resin (UPR) made from recycled PET (rPET). The untreated (UPN) and NaOH-treated (TPN) fibres were added at 30 wt% using the vacuum-bagging method and subsequently characterised by tensile and flexural testing, dynamic mechanical analysis, Fourier-transform infrared (FTIR), X-ray diffraction (XRD), scanning electron microscope (SEM), and 45-day water immersion and soil burial ageing. Alkali treatment raised tensile strength from 7.32 ± 0.46 to 11.05 ± 0.53 MPa (+50.9%), flexural strength from 44.00 ± 3.16 to 64.20 ± 6.10 MPa (+45.9%), and the moisture-diffusion coefficient fell from 9.81 × 10 −13 to 3.76 × 10 −13 m 2 s −1 . TPN-rPET was superior to UPN-rPET under environmental ageing conditions. Alkaline modification, therefore, improves PN reinforcement, resulting in a waste-based composite material suitable for non-load-bearing and lightly loaded applications.
- 7 November 2026
- Published by SAGE Publications in Plastics, Rubber and Composites: Macromolecular Engineering
Dual-waste valorisation of pine needle biomass and post-consumer PET into sustainable composites: Mechanical, dynamic mechanical and environmental performance
The use of lignocellulosic biomass with post-consumer polyethylene terephthalate (PET) is an attractive option for waste diversion and resource recovery. In this study, pine needle (PN) biomass was used to reinforce a commercial unsaturated polyester resin (UPR) made from recycled PET (rPET). The untreated (UPN) and NaOH-treated (TPN) fibres were added at 30 wt% using the vacuum-bagging method and subsequently characterised by tensile and flexural testing, dynamic mechanical analysis, Fourier-transform infrared (FTIR), X-ray diffraction (XRD), scanning electron microscope (SEM), and 45-day water immersion and soil burial ageing. Alkali treatment raised tensile strength from 7.32 ± 0.46 to 11.05 ± 0.53 MPa (+50.9%), flexural strength from 44.00 ± 3.16 to 64.20 ± 6.10 MPa (+45.9%), and the moisture-diffusion coefficient fell from 9.81 × 10 −13 to 3.76 × 10 −13 m 2 s −1 . TPN-rPET was superior to UPN-rPET under environmental ageing conditions. Alkaline modification, therefore, improves PN reinforcement, resulting in a waste-based composite material suitable for non-load-bearing and lightly loaded applications.
- Open Access
- 31 December 2025
- Published by European Publishing in Population Medicine
- Vol. 7 (December) , 1-7
Global oral health policy implementation: A narrative review of the World Health Organization’s Strategic action plan 2023–2030
The World Health Organization’s Global Oral Health Action Plan (GOHAP) 2023–2030 marks a significant shift in global oral health policy, emphasizing universal coverage and primary care integration. This narrative review examines policy implementation approaches across different healthcare...
- 31 December 2025
- Published by European Publishing in Population Medicine
- Vol. 7 (December) , 1-7
Open AccessGlobal oral health policy implementation: A narrative review of the World Health Organization’s Strategic action plan 2023–2030
The World Health Organization’s Global Oral Health Action Plan (GOHAP) 2023–2030 marks a significant shift in global oral health policy, emphasizing universal coverage and primary care integration. This narrative review examines policy implementation approaches across different healthcare...
- 25 October 2024
- Published by IOP Publishing in Engineering Research Express
- Vol. 6 (4) , 045413
A novel route of carburizing through microwave hybrid heating
Carburizing is a surface treatment process by diffusing carbon into the steel. These days, manufacturing industries demand highly efficient processes that consume low power. Microwave processing is a newly evolving process that consumes low power. This study proposes a novel route for carburizing mild steel (substrate) through experimental and simulation studies using a microwave heating. Charcoal powder was used as a susceptor to convert microwave energy into heat energy and to deposit carbon on the surface of the specimen. The mild steel specimens were exposed to the microwave power input of 900 W and 360 W for exposure time of 1500 s and 1980 s naming it as S2 and S3 respectively. The microstructural analysis of specimens S2 and S3 confirms the formation of pearlite structures at the surface. However, the amount of pearlite structure was significantly higher for the S3. The higher carbon content is confirmed through energy-dispersive x-ray spectroscopy (EDS) analysis of specimen S3. The average hardness of the S3 specimen was determined to be 220.8 HV, which shows an increase of 38.36% compared to the S1 (base metal). x-ray diffraction (XRD) results indicate the additional cementite peaks (Fe3C) and ferrite-confirming phase transformations for carburized samples. The wear analysis of S2 and S3 was conducted through pin-on-disk testing. The peak COF of 0.73 and 0.64 was observed for S2 and S3 respectively. The hard surface of S3 resists the penetration of the counter body to a greater extent due to the fine morphology of pearlite. From the FEM study, the maximum value of 7.96 × 10 3 (V/m) was determined at the center region for the electric field distribution in the microwave cavity, which is the optimum value for efficient heating. The maximum temperature of the mild steel obtained during the carburization process was 900 °C in 1800 s. The microwave carburizing process requires relatively less time than the conventional carburizing process which will save energy consumption.
- 25 October 2024
- Published by IOP Publishing in Engineering Research Express
- Vol. 6 (4) , 045413
A novel route of carburizing through microwave hybrid heating
Carburizing is a surface treatment process by diffusing carbon into the steel. These days, manufacturing industries demand highly efficient processes that consume low power. Microwave processing is a newly evolving process that consumes low power. This study proposes a novel route for carburizing mild steel (substrate) through experimental and simulation studies using a microwave heating. Charcoal powder was used as a susceptor to convert microwave energy into heat energy and to deposit carbon on the surface of the specimen. The mild steel specimens were exposed to the microwave power input of 900 W and 360 W for exposure time of 1500 s and 1980 s naming it as S2 and S3 respectively. The microstructural analysis of specimens S2 and S3 confirms the formation of pearlite structures at the surface. However, the amount of pearlite structure was significantly higher for the S3. The higher carbon content is confirmed through energy-dispersive x-ray spectroscopy (EDS) analysis of specimen S3. The average hardness of the S3 specimen was determined to be 220.8 HV, which shows an increase of 38.36% compared to the S1 (base metal). x-ray diffraction (XRD) results indicate the additional cementite peaks (Fe3C) and ferrite-confirming phase transformations for carburized samples. The wear analysis of S2 and S3 was conducted through pin-on-disk testing. The peak COF of 0.73 and 0.64 was observed for S2 and S3 respectively. The hard surface of S3 resists the penetration of the counter body to a greater extent due to the fine morphology of pearlite. From the FEM study, the maximum value of 7.96 × 10 3 (V/m) was determined at the center region for the electric field distribution in the microwave cavity, which is the optimum value for efficient heating. The maximum temperature of the mild steel obtained during the carburization process was 900 °C in 1800 s. The microwave carburizing process requires relatively less time than the conventional carburizing process which will save energy consumption.
- 3 May 2024
- Published by Elsevier in Journal of Cleaner Production
- Vol. 457, 142417
A review of composite materials based on rice straw and future trends for sustainable composites
- 3 May 2024
- Published by Elsevier in Journal of Cleaner Production
- Vol. 457, 142417
A review of composite materials based on rice straw and future trends for sustainable composites
- 23 January 2024
- Published by Taylor & Francis in Materials and Manufacturing Processes
- Vol. 39 (6) , 815-824
Microwave joining of additive manufactured SS316 with conventional SS316 for hybrid structural applications
- 23 January 2024
- Published by Taylor & Francis in Materials and Manufacturing Processes
- Vol. 39 (6) , 815-824
Microwave joining of additive manufactured SS316 with conventional SS316 for hybrid structural applications
- 7 February 2023
- Published by IOP Publishing in Physica Scripta
- Vol. 98 (3) , 035701
Fatigue life analysis and damage evaluation in glass fiber reinforced composite materials based on recycled polyethylene terephthalate
Viability of recycling polyethylene terephthalate (PET) can be enhanced by increasing its usage as a matrix material in manufacturing of composite materials. Structural applications of composite materials almost always involve fatigue loading and evaluation of fatigue behaviour is essential to explore the full potential of composite materials based on recycled PET. With an aim to increase the acceptability of recycled PET based resins, fatigue performance of glass fiber reinforced composite materials based on unsaturated polyester resin derived from recycled PET (rPET-UPR) has been evaluated in the present research. Glass fiber composites laminates of stacking sequence [0/(±45)2/0]T have been fabricated using vacuum infusion process. Fatigue tests were performed at the stress ratio of 0.1, where the stress level varied from 40%–80% of the ultimate tensile strength (UTS). The results of fatigue tests show that the fatigue lives of composites based on rPET-UPR were lower as compared to virgin polyester matrix composites. However, Statistical analysis of the fatigue life data using two parameter Weibull distribution, established that there is no deleterious effect on the scatter observed in fatigue lives of these composites, as compared to composites based on virgin polyester resin. Due to higher degradation of rPET-UPR matrix as well as weak interfacial properties, 13% higher self generated temperature was observed during fatigue loading in comparison to virgin resin based composite materials. A three phase stiffness degradation curve has been observed for these composite materials indicating stiffness loss in the range of 20%–35% till the time of failure, which correlates well with the experimental damage observations. A nonuniform and rapid damage growth was observed at high-stress levels, whereas a more uniform damage zone was observed at the low-stress levels.
- 7 February 2023
- Published by IOP Publishing in Physica Scripta
- Vol. 98 (3) , 035701
Fatigue life analysis and damage evaluation in glass fiber reinforced composite materials based on recycled polyethylene terephthalate
Viability of recycling polyethylene terephthalate (PET) can be enhanced by increasing its usage as a matrix material in manufacturing of composite materials. Structural applications of composite materials almost always involve fatigue loading and evaluation of fatigue behaviour is essential to explore the full potential of composite materials based on recycled PET. With an aim to increase the acceptability of recycled PET based resins, fatigue performance of glass fiber reinforced composite materials based on unsaturated polyester resin derived from recycled PET (rPET-UPR) has been evaluated in the present research. Glass fiber composites laminates of stacking sequence [0/(±45)2/0]T have been fabricated using vacuum infusion process. Fatigue tests were performed at the stress ratio of 0.1, where the stress level varied from 40%–80% of the ultimate tensile strength (UTS). The results of fatigue tests show that the fatigue lives of composites based on rPET-UPR were lower as compared to virgin polyester matrix composites. However, Statistical analysis of the fatigue life data using two parameter Weibull distribution, established that there is no deleterious effect on the scatter observed in fatigue lives of these composites, as compared to composites based on virgin polyester resin. Due to higher degradation of rPET-UPR matrix as well as weak interfacial properties, 13% higher self generated temperature was observed during fatigue loading in comparison to virgin resin based composite materials. A three phase stiffness degradation curve has been observed for these composite materials indicating stiffness loss in the range of 20%–35% till the time of failure, which correlates well with the experimental damage observations. A nonuniform and rapid damage growth was observed at high-stress levels, whereas a more uniform damage zone was observed at the low-stress levels.
- 31 January 2023
- Published by IOP Publishing in Physica Scripta
- Vol. 98 (2) , 025709
Investigation of mechanical properties of microwave welded SS304-SS202 lap joints
The joint between dissimilar materials is always challenging to develop through traditional techniques due to the different properties of the parent materials. However, a novel non-traditional route of joining similar and dissimilar materials through energy conversion and absorption has been developed called SMHH (selective microwave hybrid heating). It has gained much attention due to its unique heating abilities. In the present work, the lap joint between SS202-SS304 is developed through SMHH placing nickel powder as an interlayer. The lap joint was characterized mechanically through shear tests and microhardness. Since the sheared area of the joint is large, it is challenging to achieve a good joint. Thus, to develop a solid joint, laser surface texturing (LST) was introduced to the joining surfaces, and the joints were characterized. After LST was introduced, a fully diffused joint interlayer region was observed through scanning electron microscopy (SEM). The EDS results confirmed the complete metallurgical bonding occurred by the diffusion of elements across the weld zone. From the XRD spectrum, the formation of intermetallic compounds like FeNi, FeNi3, C3Fe7, and M23C6 were identified at the joint region. The mean microhardness of 355 ± 10 HV was determined at the joint region of lap joints with LST. A lap joint with LST exhibits 217 MPa of shear strength, which is significantly higher than the joints without LST. Fractography of the shear failure specimens pointed out that partial heating of the interlayer caused incomplete bonding of the base metal and interlayer for without LST lap joints. However, mixed mode failure of SS202 near the overlap region of the LST lap joint occurred. It is concluded that the addition of LST on the lap joint has made a colossal impact on enhancing joint strength and intermetallic bonding. In addition, temperature-time profiling was studied to understand the heating mechanism involved in SMHH using thermocouples.
- 31 January 2023
- Published by IOP Publishing in Physica Scripta
- Vol. 98 (2) , 025709
Investigation of mechanical properties of microwave welded SS304-SS202 lap joints
The joint between dissimilar materials is always challenging to develop through traditional techniques due to the different properties of the parent materials. However, a novel non-traditional route of joining similar and dissimilar materials through energy conversion and absorption has been developed called SMHH (selective microwave hybrid heating). It has gained much attention due to its unique heating abilities. In the present work, the lap joint between SS202-SS304 is developed through SMHH placing nickel powder as an interlayer. The lap joint was characterized mechanically through shear tests and microhardness. Since the sheared area of the joint is large, it is challenging to achieve a good joint. Thus, to develop a solid joint, laser surface texturing (LST) was introduced to the joining surfaces, and the joints were characterized. After LST was introduced, a fully diffused joint interlayer region was observed through scanning electron microscopy (SEM). The EDS results confirmed the complete metallurgical bonding occurred by the diffusion of elements across the weld zone. From the XRD spectrum, the formation of intermetallic compounds like FeNi, FeNi3, C3Fe7, and M23C6 were identified at the joint region. The mean microhardness of 355 ± 10 HV was determined at the joint region of lap joints with LST. A lap joint with LST exhibits 217 MPa of shear strength, which is significantly higher than the joints without LST. Fractography of the shear failure specimens pointed out that partial heating of the interlayer caused incomplete bonding of the base metal and interlayer for without LST lap joints. However, mixed mode failure of SS202 near the overlap region of the LST lap joint occurred. It is concluded that the addition of LST on the lap joint has made a colossal impact on enhancing joint strength and intermetallic bonding. In addition, temperature-time profiling was studied to understand the heating mechanism involved in SMHH using thermocouples.
- 10 November 2022
- Published by IOP Publishing in Physica Scripta
- Vol. 97 (12) , 125704
Comparative performance of various susceptor materials and vertical cavity shapes for selective microwave hybrid heating (SMHH)
The microwave processing of materials is gaining popularity over the past decade due to its unique heating abilities. The microwave hybrid heating (MHH) technique has effectively processed bulk metallic materials. MHH is assisted by susceptor material which forces metals to absorb microwave radiations. Further, MHH is modified to selective microwave hybrid heating (SMHH) to increase the efficiency of the process. This work examines the performance of Graphite and Charcoal susceptors with a conical vertical cavity for SMHH using FEM simulation. It is observed that the maximum temperature achieved by Graphite was 215 °C at an exposure time of 300 s, whereas, for Charcoal susceptor, it is 655 °C. Further, the effect of different vertical cavity shapes (cylindrical and conical) on the SMHH technique is presented for Charcoal susceptor. For an exposure time of 300 s, the temperature rise in the conical and cylindrical cavity is 655 °C and 319 °C, respectively. From resistive heat flow, time-temperature profile and temperature distribution, it is clear how SMHH is significantly effective for a conical vertical cavity having Charcoal susceptor. In addition, the performance of the conical vertical cavity having Charcoal susceptor was validated through experimental study. The real-time temperature profile was determined through testo 885/testo 890 thermal imaging camera. The observed maximum temperature of the susceptor after heating for 300 s was 639.9 °C.
- 10 November 2022
- Published by IOP Publishing in Physica Scripta
- Vol. 97 (12) , 125704
Comparative performance of various susceptor materials and vertical cavity shapes for selective microwave hybrid heating (SMHH)
The microwave processing of materials is gaining popularity over the past decade due to its unique heating abilities. The microwave hybrid heating (MHH) technique has effectively processed bulk metallic materials. MHH is assisted by susceptor material which forces metals to absorb microwave radiations. Further, MHH is modified to selective microwave hybrid heating (SMHH) to increase the efficiency of the process. This work examines the performance of Graphite and Charcoal susceptors with a conical vertical cavity for SMHH using FEM simulation. It is observed that the maximum temperature achieved by Graphite was 215 °C at an exposure time of 300 s, whereas, for Charcoal susceptor, it is 655 °C. Further, the effect of different vertical cavity shapes (cylindrical and conical) on the SMHH technique is presented for Charcoal susceptor. For an exposure time of 300 s, the temperature rise in the conical and cylindrical cavity is 655 °C and 319 °C, respectively. From resistive heat flow, time-temperature profile and temperature distribution, it is clear how SMHH is significantly effective for a conical vertical cavity having Charcoal susceptor. In addition, the performance of the conical vertical cavity having Charcoal susceptor was validated through experimental study. The real-time temperature profile was determined through testo 885/testo 890 thermal imaging camera. The observed maximum temperature of the susceptor after heating for 300 s was 639.9 °C.
- 5 October 2022
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 53 (10) , 1167-1183
Boron addition to AISI A213/P91 steel: Preliminary investigation on microstructural evolution and microhardness at simulated heat‐affected zone
The motivation behind present investigation has been a step to create preliminary understanding towards structure‐property correlation i. e., microstructure and microhardness in presence of boron in P91 steel and in its subzones of heat‐affected zone with Gleeble simulation. For microstructure characterization and its comparison amongst selected two steels, light microscopy for prior austenite grain size, morphology of prior austenite grain boundaries and scanning electron microscopy at low‐resolution and high‐resolution in order to study evolution of sub‐structure i. e. martensitic lath block structure and nano‐precipitates were employed. Electron backscatter diffraction measurements of all coupons were done to understand the distribution and contribution of relative fraction of various grain and sub‐grain boundaries within local microstructure. Main effects of addition of 100 ppm boron to standard P91 steel as observed from present microstructural evaluation are; existence of fine nano‐precipitates P91‐coarse grained heat affected zone than its P91B counterpart, grain refinement in fine‐grained heat‐affected zone of both steels with partial dissolution of nano‐precipitates, coarsened nano‐precipitates in P91‐fine‐grained heat‐affected zone after post weld heat treatment, mixed‐structure of partially transformed martensite and coarsened undissolved prior austenite grains with nano‐precipitates in P91‐inter‐critical heat‐affected zone than P91B‐inter‐critical heat‐affected zone. However, difference in microhardness was primarily owing to variation of nano‐precipitates fraction area. In addition, present work induced grounds for microstructure stability i. e., grain boundary hardening in P91B weldments that suppresses type IV failure.
- 5 October 2022
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 53 (10) , 1167-1183
Boron addition to AISI A213/P91 steel: Preliminary investigation on microstructural evolution and microhardness at simulated heat‐affected zone
The motivation behind present investigation has been a step to create preliminary understanding towards structure‐property correlation i. e., microstructure and microhardness in presence of boron in P91 steel and in its subzones of heat‐affected zone with Gleeble simulation. For microstructure characterization and its comparison amongst selected two steels, light microscopy for prior austenite grain size, morphology of prior austenite grain boundaries and scanning electron microscopy at low‐resolution and high‐resolution in order to study evolution of sub‐structure i. e. martensitic lath block structure and nano‐precipitates were employed. Electron backscatter diffraction measurements of all coupons were done to understand the distribution and contribution of relative fraction of various grain and sub‐grain boundaries within local microstructure. Main effects of addition of 100 ppm boron to standard P91 steel as observed from present microstructural evaluation are; existence of fine nano‐precipitates P91‐coarse grained heat affected zone than its P91B counterpart, grain refinement in fine‐grained heat‐affected zone of both steels with partial dissolution of nano‐precipitates, coarsened nano‐precipitates in P91‐fine‐grained heat‐affected zone after post weld heat treatment, mixed‐structure of partially transformed martensite and coarsened undissolved prior austenite grains with nano‐precipitates in P91‐inter‐critical heat‐affected zone than P91B‐inter‐critical heat‐affected zone. However, difference in microhardness was primarily owing to variation of nano‐precipitates fraction area. In addition, present work induced grounds for microstructure stability i. e., grain boundary hardening in P91B weldments that suppresses type IV failure.