Michael Pohl
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Michael Pohl has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Jens Jürgensen
Institute for Materials—Materials Testing, Ruhr-University Bochum, 44801 Bochum, Germany
2 shared publications - Marina Macias Barrientos
Faculty of Mechanical Engineering, TU Dortmund University, 44227 Dortmund, Germany
2 shared publications - Andreas Frehn
Materion Brush GmbH, 70499 Stuttgart, Germany
1 shared publication - Jens Jürgensen
Euro-Labor GmbH, Bochum, Germany
1 shared publication - Klaus Ohla
AMPCO METAL S.A., Route de Chésalles 48, 1723 Marly, Switzerland
1 shared publication Murat Mola
Institut für Werkstoffe, Ruhr-Universität Bochum , Bochum , Germany
1 shared publication
Latest Publications
- Open Access
- 22 July 2026
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 15 (5) , 1126-1143
Delayed Hydrogen-Induced Cracking: Fundamentals and Real-World Examples
Delayed hydrogen cracking represents a critical damage phenomenon in metallic materials, characterized by a temporal separation between hydrogen uptake and crack initiation. This time dependency often complicates failure analysis, as cracking may occur hours, days, or even years after manufacturing or commissioning. While hydrogen embrittlement has been extensively studied, the mechanisms governing delayed cracking are frequently discussed in isolation rather than as an integrated process. This paper presents a mechanistic framework for delayed hydrogen cracking by systematically linking hydrogen uptake, hydrogen configurations, stress-assisted hydrogen redistribution, and hydrogen-induced damage mechanisms. It is shown that the mere presence of hydrogen is insufficient to cause delayed cracking. Instead, the phenomenon arises from the ability of hydrogen to remain mobile or to be re-activated from initially benign configurations, followed by time-dependent redistribution toward regions of elevated mechanical stress and thus strain. Only when a critical local hydrogen concentration is reached do hydrogen-enhanced damage mechanisms such as hydrogen-enhanced decohesion and hydrogen-enhanced localized plasticity become operative. The resulting fracture morphologies are discussed as the fractographic manifestation of these time-dependent processes rather than as indicators of a single dominant mechanism. Differences in fracture appearance across various material classes are addressed in this context. Finally, selected technical failure cases are presented to illustrate how hydrogen introduced during manufacturing or service can lead to delayed cracking under practical operating conditions. By integrating fundamental hydrogen–material interactions with real-world failure examples, this paper provides a comprehensive understanding of why hydrogen-induced cracking may occur long after hydrogen exposure and offers a structured basis for failure analysis and risk assessment of hydrogen-exposed components.
- 22 July 2026
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 15 (5) , 1126-1143
Open AccessDelayed Hydrogen-Induced Cracking: Fundamentals and Real-World Examples
Delayed hydrogen cracking represents a critical damage phenomenon in metallic materials, characterized by a temporal separation between hydrogen uptake and crack initiation. This time dependency often complicates failure analysis, as cracking may occur hours, days, or even years after manufacturing or commissioning. While hydrogen embrittlement has been extensively studied, the mechanisms governing delayed cracking are frequently discussed in isolation rather than as an integrated process. This paper presents a mechanistic framework for delayed hydrogen cracking by systematically linking hydrogen uptake, hydrogen configurations, stress-assisted hydrogen redistribution, and hydrogen-induced damage mechanisms. It is shown that the mere presence of hydrogen is insufficient to cause delayed cracking. Instead, the phenomenon arises from the ability of hydrogen to remain mobile or to be re-activated from initially benign configurations, followed by time-dependent redistribution toward regions of elevated mechanical stress and thus strain. Only when a critical local hydrogen concentration is reached do hydrogen-enhanced damage mechanisms such as hydrogen-enhanced decohesion and hydrogen-enhanced localized plasticity become operative. The resulting fracture morphologies are discussed as the fractographic manifestation of these time-dependent processes rather than as indicators of a single dominant mechanism. Differences in fracture appearance across various material classes are addressed in this context. Finally, selected technical failure cases are presented to illustrate how hydrogen introduced during manufacturing or service can lead to delayed cracking under practical operating conditions. By integrating fundamental hydrogen–material interactions with real-world failure examples, this paper provides a comprehensive understanding of why hydrogen-induced cracking may occur long after hydrogen exposure and offers a structured basis for failure analysis and risk assessment of hydrogen-exposed components.
- Open Access
Effect of Hydrogen Charging on the Mechanical Properties of High-Strength Copper-Base Alloys, Austenitic Stainless Steel AISI 321, Inconel 625 and Ferritic Steel 1.4511
Hydrogen embrittlement (HE) poses the risk of premature failure for many metals, especially high-strength steels. Due to the utilization of hydrogen as an environmentally friendly energy source, efforts are made to improve the resistance to HE at elevated pressures and temperatures. In addition, applications in hydrogen environments might require specific material properties in terms of thermal and electrical conductivity, magnetic properties as well as corrosion resistance. In the present study, three high-strength Cu-base alloys (Alloy 25, PerforMet® and ToughMet® 3) as well as austenitic stainless AISI 321, Ni-base alloy IN 625 and ferritic steel 1.4511 are charged in pressurized hydrogen and subsequently tested by means of Slow Strain Rate Testing (SSRT). The results show that high-strength Cu-base alloys exhibit a great resistance to HE and could prove to be suitable for materials for a variety of hydrogen applications with rough conditions such as high pressure, elevated temperature and corrosive environments.
Open AccessEffect of Hydrogen Charging on the Mechanical Properties of High-Strength Copper-Base Alloys, Austenitic Stainless Steel AISI 321, Inconel 625 and Ferritic Steel 1.4511
Hydrogen embrittlement (HE) poses the risk of premature failure for many metals, especially high-strength steels. Due to the utilization of hydrogen as an environmentally friendly energy source, efforts are made to improve the resistance to HE at elevated pressures and temperatures. In addition, applications in hydrogen environments might require specific material properties in terms of thermal and electrical conductivity, magnetic properties as well as corrosion resistance. In the present study, three high-strength Cu-base alloys (Alloy 25, PerforMet® and ToughMet® 3) as well as austenitic stainless AISI 321, Ni-base alloy IN 625 and ferritic steel 1.4511 are charged in pressurized hydrogen and subsequently tested by means of Slow Strain Rate Testing (SSRT). The results show that high-strength Cu-base alloys exhibit a great resistance to HE and could prove to be suitable for materials for a variety of hydrogen applications with rough conditions such as high pressure, elevated temperature and corrosive environments.
- Open Access
Local Hydrogen Measurements in Multi-Phase Steel C60E by Means of Electrochemical Microcapillary Cell Technique
By utilizing hydrogen as an eco-friendly energy source, many metals are exposed to gaseous (pressurized) hydrogen. High-strength steels with an ultimate tensile strength of 800 MPa and above are especially susceptible to hydrogen-induced fracturing, also referred to as hydrogen embrittlement (HE). Both the microstructure and phase fractions within the steel, as well as lattice distortion, carbide precipitation, residual stress, etc., significantly affect the susceptibility to HE. Among others, one important cause for this observation is found in the locally varying hydrogen solubility within different microstructural phases such as martensite, bainite, pearlite, and ferrite. Both a thorough understanding of the HE mechanisms and taking countermeasures in the form of alloying design require an accurate analysis of local diffusive hydrogen concentrations within the material. Thermal analysis methods such as Thermal Desorption Mass Spectrometry only display an integral hydrogen concentration throughout the whole sample volume. To analyze the local diffusive hydrogen concentration, novel measuring techniques with a high special resolution must therefore be utilized. The current research presents first-of-its-kind hydrogen analyses by means of the electrochemical microcapillary cell. Using a 10 µm tip opening diameter allows for conducting local diffusive hydrogen measurements within individual grains of multi-phase carbon steel C60E (1.1221). The results confirm that hydrogen is distributed heterogeneously within multi-phase steels. Considering the individual phase fractions and the respective local diffusive hydrogen concentrations, a total diffusive hydrogen concentration can be calculated. The obtained value is in good agreement with reference thermal hydrogen analyses. Our results suggest that electrochemical microcapillary cell measurements offer great potential for further studies, which will provide a better understanding of HE and local hydrogen accumulation.
Open AccessLocal Hydrogen Measurements in Multi-Phase Steel C60E by Means of Electrochemical Microcapillary Cell Technique
By utilizing hydrogen as an eco-friendly energy source, many metals are exposed to gaseous (pressurized) hydrogen. High-strength steels with an ultimate tensile strength of 800 MPa and above are especially susceptible to hydrogen-induced fracturing, also referred to as hydrogen embrittlement (HE). Both the microstructure and phase fractions within the steel, as well as lattice distortion, carbide precipitation, residual stress, etc., significantly affect the susceptibility to HE. Among others, one important cause for this observation is found in the locally varying hydrogen solubility within different microstructural phases such as martensite, bainite, pearlite, and ferrite. Both a thorough understanding of the HE mechanisms and taking countermeasures in the form of alloying design require an accurate analysis of local diffusive hydrogen concentrations within the material. Thermal analysis methods such as Thermal Desorption Mass Spectrometry only display an integral hydrogen concentration throughout the whole sample volume. To analyze the local diffusive hydrogen concentration, novel measuring techniques with a high special resolution must therefore be utilized. The current research presents first-of-its-kind hydrogen analyses by means of the electrochemical microcapillary cell. Using a 10 µm tip opening diameter allows for conducting local diffusive hydrogen measurements within individual grains of multi-phase carbon steel C60E (1.1221). The results confirm that hydrogen is distributed heterogeneously within multi-phase steels. Considering the individual phase fractions and the respective local diffusive hydrogen concentrations, a total diffusive hydrogen concentration can be calculated. The obtained value is in good agreement with reference thermal hydrogen analyses. Our results suggest that electrochemical microcapillary cell measurements offer great potential for further studies, which will provide a better understanding of HE and local hydrogen accumulation.
- 16 June 2017
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 6 (4) , 282-288
Failure Analysis to Clarify Unambiguous Hydrogen Fracturing in Steels
- 16 June 2017
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 6 (4) , 282-288
Failure Analysis to Clarify Unambiguous Hydrogen Fracturing in Steels
- 3 October 2013
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 2 (5) , 343-351
Duplex Steels. Part II: Carbides and Nitrides
- 3 October 2013
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 2 (5) , 343-351
Duplex Steels. Part II: Carbides and Nitrides
- 9 April 2013
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 2 (2) , 113-121
Duplex Steels: Part I: Genesis, Formation, Structure
- 9 April 2013
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 2 (2) , 113-121
Duplex Steels: Part I: Genesis, Formation, Structure
- 1 July 2005
- Published by Walter de Gruyter GmbH in International Journal of Materials Research
- Vol. 96 (7) , 749-752
Numeric simulation of the α/γ-phase ratio of ferritic-austenitic duplex steels
In the past, the necessity to predict the α/γ-phase ratio in duplex steels gave rise to a number of empirical equations and diagrams, which, however, do not guarantee a reliable prediction. Due to the insufficient agreement between experiment and empirical calculation, the new and further development of duplex steels is still carried out by means of very time-consuming and costly experiments. The CALPHAD method (CALculation of PHAse Diagrams) [1], whose calculational realization is effected by the software program Thermo-Calc [2] in connection with the optimized thermodynamic database TCFE2 (Thermo-Calc FErrum Database, Version 2), can now be used to establish a reliable (parameter optimization), thermodynamic database for duplex steels and to estimate the phase ratio.
- 1 July 2005
- Published by Walter de Gruyter GmbH in International Journal of Materials Research
- Vol. 96 (7) , 749-752
Numeric simulation of the α/γ-phase ratio of ferritic-austenitic duplex steels
In the past, the necessity to predict the α/γ-phase ratio in duplex steels gave rise to a number of empirical equations and diagrams, which, however, do not guarantee a reliable prediction. Due to the insufficient agreement between experiment and empirical calculation, the new and further development of duplex steels is still carried out by means of very time-consuming and costly experiments. The CALPHAD method (CALculation of PHAse Diagrams) [1], whose calculational realization is effected by the software program Thermo-Calc [2] in connection with the optimized thermodynamic database TCFE2 (Thermo-Calc FErrum Database, Version 2), can now be used to establish a reliable (parameter optimization), thermodynamic database for duplex steels and to estimate the phase ratio.