Shane Durbach
Research Subjects
Shane Durbach has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Pranav K. Tripathi
DST-NRF Centre of Excellence in Strong Materials and the Molecular Sciences Institute, School of Chemistry, University of the Witwatersrand, Johannesburg 2050, South Africa
3 shared publications Ahmed Shaikjee
DST-NRF Centre of Excellence in Strong Materials, University of the Witwatersrand (Wits), Johannesburg 2050, South Africa
1 shared publication- Ahmed Shaikjee
DST-NRF Centre of Excellence in Strong Materials, University of the Witwatersrand (Wits), Private Bag 3, Johannesburg 2050, South Africa
1 shared publication - David Gordon Billing
University of the Witwatersrand
1 shared publication - Deena Naidoo
School of Physics, University of the Witwatersrand, Johannesburg 2050, South Africa
1 shared publication - Hilary Masenda
Materials Physics Research Institute, School of Physics, University of the Witwatersrand 1 , Johannesburg 2050
1 shared publication
Latest Publications
- Open Access
- 8 August 2016
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 6 (80) , 76773-76779
Morphological and crystallinity differences in nitrogen-doped carbon nanotubes grown by chemical vapour deposition decomposition of melamine over coal fly ash
Millions of tons of coal fly ash (CFA) are produced each year in thermoelectric coal powered stations as a waste-product. Until recently few researchers have endeavored to use CFA as a catalyst in the formation of carbon nanomaterials (CNMs). In this study a two-stage tube furnace was used to synthesize N-doped carbon nanotubes (NCNTs) by chemical vapor deposition using melamine as the source of nitrogen and carbon, with CFA as a catalyst, at temperatures ranging from 800 to 900 °C. The masses of the NCNTs formed were found to have increased with increased synthesis temperature. The morphology and crystallinity of the NCNTs along with the amount of nitrogen incorporated into these were found to vary with the synthesis temperature. NCNTs synthesized at 800 °C were found to be typical multiwalled carbon nanotubes by transmission electron microscopy, whereas those at 850 and 900 °C were found to be chain-like and bamboo-like compartmentalised nanotubes respectively. The NCNTs synthesized at 800 °C were found to contain the least incorporation of nitrogen by elemental analysis and were the most crystalline (as determined by using the IG/ID ratio and the G-band position from laser Raman spectroscopy), whereas those at 850 °C were the least crystalline but had the highest incorporation of nitrogen. NCNTs synthesised at 800 °C were the most thermally stable, whereas those synthesized at 850 °C were the least stable. NCNTs synthesized at 900 °C had a crystallinity, thermal stability and nitrogen content which lay between the other two.
- 8 August 2016
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 6 (80) , 76773-76779
Open AccessMorphological and crystallinity differences in nitrogen-doped carbon nanotubes grown by chemical vapour deposition decomposition of melamine over coal fly ash
Millions of tons of coal fly ash (CFA) are produced each year in thermoelectric coal powered stations as a waste-product. Until recently few researchers have endeavored to use CFA as a catalyst in the formation of carbon nanomaterials (CNMs). In this study a two-stage tube furnace was used to synthesize N-doped carbon nanotubes (NCNTs) by chemical vapor deposition using melamine as the source of nitrogen and carbon, with CFA as a catalyst, at temperatures ranging from 800 to 900 °C. The masses of the NCNTs formed were found to have increased with increased synthesis temperature. The morphology and crystallinity of the NCNTs along with the amount of nitrogen incorporated into these were found to vary with the synthesis temperature. NCNTs synthesized at 800 °C were found to be typical multiwalled carbon nanotubes by transmission electron microscopy, whereas those at 850 and 900 °C were found to be chain-like and bamboo-like compartmentalised nanotubes respectively. The NCNTs synthesized at 800 °C were found to contain the least incorporation of nitrogen by elemental analysis and were the most crystalline (as determined by using the IG/ID ratio and the G-band position from laser Raman spectroscopy), whereas those at 850 °C were the least crystalline but had the highest incorporation of nitrogen. NCNTs synthesised at 800 °C were the most thermally stable, whereas those synthesized at 850 °C were the least stable. NCNTs synthesized at 900 °C had a crystallinity, thermal stability and nitrogen content which lay between the other two.
- Open Access
- 2 June 2015
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 5 (66) , 53776-53781
The effect of CO2 on the CVD synthesis of carbon nanomaterials using fly ash as a catalyst
Carbon nanomaterials (CNMs) can be derived from waste materials such as: coal fly ash and CO2, with CO2 and C2H2 as carbon sources respectively.
- 2 June 2015
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 5 (66) , 53776-53781
Open AccessThe effect of CO2 on the CVD synthesis of carbon nanomaterials using fly ash as a catalyst
Carbon nanomaterials (CNMs) can be derived from waste materials such as: coal fly ash and CO2, with CO2 and C2H2 as carbon sources respectively.
- Open Access
- 10 August 2014
- Published by Springer Nature in Discover Nano
- Vol. 9 (1) , 387
Direct synthesis of carbon nanofibers from South African coal fly ash
Carbon nanofibers (CNFs), cylindrical nanostructures containing graphene, were synthesized directly from South African fly ash (a waste product formed during the combustion of coal). The CNFs (as well as other carbonaceous materials like carbon nanotubes (CNTs)) were produced by the catalytic chemical vapour deposition method (CCVD) in the presence of acetylene gas at temperatures ranging from 400°C to 700°C. The fly ash and its carbonaceous products were characterized by transmission electron microscopy (TEM), thermogravimetric analysis (TGA), laser Raman spectroscopy and Brunauer-Emmett-Teller (BET) surface area measurements. It was observed that as-received fly ash was capable of producing CNFs in high yield by CCVD, starting at a relatively low temperature of 400°C. Laser Raman spectra and TGA thermograms showed that the carbonaceous products which formed were mostly disordered. Small bundles of CNTs and CNFs observed by TEM and energy-dispersive spectroscopy (EDS) showed that the catalyst most likely responsible for CNF formation was iron in the form of cementite; X-ray diffraction (XRD) and Mössbauer spectroscopy confirmed these findings.
- 10 August 2014
- Published by Springer Nature in Discover Nano
- Vol. 9 (1) , 387
Open AccessDirect synthesis of carbon nanofibers from South African coal fly ash
Carbon nanofibers (CNFs), cylindrical nanostructures containing graphene, were synthesized directly from South African fly ash (a waste product formed during the combustion of coal). The CNFs (as well as other carbonaceous materials like carbon nanotubes (CNTs)) were produced by the catalytic chemical vapour deposition method (CCVD) in the presence of acetylene gas at temperatures ranging from 400°C to 700°C. The fly ash and its carbonaceous products were characterized by transmission electron microscopy (TEM), thermogravimetric analysis (TGA), laser Raman spectroscopy and Brunauer-Emmett-Teller (BET) surface area measurements. It was observed that as-received fly ash was capable of producing CNFs in high yield by CCVD, starting at a relatively low temperature of 400°C. Laser Raman spectra and TGA thermograms showed that the carbonaceous products which formed were mostly disordered. Small bundles of CNTs and CNFs observed by TEM and energy-dispersive spectroscopy (EDS) showed that the catalyst most likely responsible for CNF formation was iron in the form of cementite; X-ray diffraction (XRD) and Mössbauer spectroscopy confirmed these findings.