Svea Petersen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Svea Petersen has a total of 70 co-authors. Here are the top co-authors by number of shared publications:
- Nele Espelage
Laboratory of Polymer Engineering University of Applied Sciences Osnabrück Osnabrück Germany
5 shared publications - Eva Berghaus
Laboratory of Chemistry and Surface Modification University of Applied Sciences Osnabrück Germany
3 shared publications - Marius Behnecke
Laboratory of Polymer Engineering University of Applied Sciences Osnabrück Osnabrück Germany
3 shared publications - Markus Lothar Susoff
Faculty of Engineering and Computer Science University of Applied Sciences Osnabruck Osnabruck Germany
3 shared publications - Martin Steinhart
Department of Biology/Chemistry and Center for Cellular Nanoanalytics, Osnabrück University, Barbarastr. 11, Osnabrück 49076, Germany
3 shared publications Peter Blömer
Center for Materials and Technology Private University of Applied Sciences for Business and Technology Diepholz Germany
3 shared publications
Latest Publications
- Open Access
- 17 August 2026
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 368
Deposition and roughness tailoring of calcium phosphate coatings on polyetheretherketone for orthopedic and dental implant applications
- 17 August 2026
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 368
Open AccessDeposition and roughness tailoring of calcium phosphate coatings on polyetheretherketone for orthopedic and dental implant applications
- Open Access
- 22 July 2026
- Published by Wiley in Polymers for Advanced Technologies
- Vol. 37 (7) , e70689
How the Interplay of Accelerated Aging and Sterilization by γ ‐Irradiation Influences the Recyclability of Medical Polypropylene Copolymer
Recycling of medical‐grade plastics remains challenging due to stringent quality and safety requirements. We investigated the combined effects of two injection molding/ γ ‐irradiation (25 kGy) cycles and accelerated aging simulating 1 year of service life on two compounds consisting of isotactic polypropylene copolymer containing less than 10 mol‐% ethylene (PP‐C) and different stabilizer compositions. One composition comprised the primary antioxidant Irganox 1010 (I1010), the secondary antioxidant Irgafos 168 (I168), the radiation stabilizer Tinuvin 622 (T622), and calcium stearate (CaSt) as acid scavenger, while the second composition was lacking I1010. For comparison, both compounds were subjected to the same treatments without γ ‐irradiation. We analyzed additive consumption, radiolysis product formation, molar mass evolution, rheological behavior, and crystallinity. High‐performance liquid chromatography (HPLC) and gas chromatography combined with mass spectrometry (GC–MS) revealed pronounced degradation of I1010 and I168, particularly after γ ‐irradiation. The presence of I1010 mitigated the depletion of I168, indicating synergistic stabilization. The radiolysis product 1,3‐di‐tert‐butylbenzene (DTBB) formed upon γ ‐irradiation, confirming additive decomposition. Gel permeation chromatography (GPC) and oscillatory rheometry showed a reduction in PP‐C molar mass and zero‐shear viscosity reflecting chain scission. The slope of the relation of the PP‐C radius of gyration and its molar mass M indicated that γ ‐irradiation primarily induced long chain branching in the absence of I1010. In contrast, X‐ray diffraction (XRD) revealed only minor changes in crystallinity, suggesting that the crystalline phase remained largely unaffected by the irradiation and injection molding history. Overall, irradiation effects exceeded those of reprocessing and accelerated aging, indicating that sterilization crucially impacts recyclability of PP‐C in medical products.
- 22 July 2026
- Published by Wiley in Polymers for Advanced Technologies
- Vol. 37 (7) , e70689
Open AccessHow the Interplay of Accelerated Aging and Sterilization by γ ‐Irradiation Influences the Recyclability of Medical Polypropylene Copolymer
Recycling of medical‐grade plastics remains challenging due to stringent quality and safety requirements. We investigated the combined effects of two injection molding/ γ ‐irradiation (25 kGy) cycles and accelerated aging simulating 1 year of service life on two compounds consisting of isotactic polypropylene copolymer containing less than 10 mol‐% ethylene (PP‐C) and different stabilizer compositions. One composition comprised the primary antioxidant Irganox 1010 (I1010), the secondary antioxidant Irgafos 168 (I168), the radiation stabilizer Tinuvin 622 (T622), and calcium stearate (CaSt) as acid scavenger, while the second composition was lacking I1010. For comparison, both compounds were subjected to the same treatments without γ ‐irradiation. We analyzed additive consumption, radiolysis product formation, molar mass evolution, rheological behavior, and crystallinity. High‐performance liquid chromatography (HPLC) and gas chromatography combined with mass spectrometry (GC–MS) revealed pronounced degradation of I1010 and I168, particularly after γ ‐irradiation. The presence of I1010 mitigated the depletion of I168, indicating synergistic stabilization. The radiolysis product 1,3‐di‐tert‐butylbenzene (DTBB) formed upon γ ‐irradiation, confirming additive decomposition. Gel permeation chromatography (GPC) and oscillatory rheometry showed a reduction in PP‐C molar mass and zero‐shear viscosity reflecting chain scission. The slope of the relation of the PP‐C radius of gyration and its molar mass M indicated that γ ‐irradiation primarily induced long chain branching in the absence of I1010. In contrast, X‐ray diffraction (XRD) revealed only minor changes in crystallinity, suggesting that the crystalline phase remained largely unaffected by the irradiation and injection molding history. Overall, irradiation effects exceeded those of reprocessing and accelerated aging, indicating that sterilization crucially impacts recyclability of PP‐C in medical products.
- Open Access
- 1 January 2026
- Published by Wiley in Advances in Polymer Technology
- Vol. 2026 (1)
Interactive Effects of Antioxidants, Acid Scavengers, and HALS on the Material Properties of Polypropylene Copolymer Considering γ‐Radiation Sterilization and Recycling for Medical Devices
Global plastic production and consumption have risen continuously over past decades, increasing the need for sustainable end‐of‐life strategies. The present study provides a systematic assessment of how repeated processing and γ‐irradiation affect the stability, additive consumption, and performance of polypropylene copolymers (PP‐C) intended for closed‐loop recycling in medical technology. Applying a design of experiments approach with Irganox 1010, Irgafos 168, Tinuvin 622, and calcium stearate (CaSt), the results identify γ‐irradiation as the dominant factor dominating additive depletion, molecular degradation, and optical aging. Phenolic and phosphite antioxidants were rapidly consumed after irradiation, frequently falling below quantifiable levels, whereas processing alone caused only moderate degradation. Pronounced synergistic interactions between Irganox 1010 and Irgafos 168 were confirmed, particularly in combination with CaSt, enabling both stabilizers to remain effective over multiple cycles. Tinuvin 622 exhibited fluctuating behavior consistent with regeneration mechanisms associated with the Denisov cycle. Changes in yellowness, tensile properties, and zero shear viscosity further demonstrate that irradiation, rather than mechanical recycling, drives deterioration and rheological instability. These findings underline that successful recycling of γ‐sterilized PP‐C requires tailored additive systems and highlight stabilizer engineering as a key factor for ensuring material safety, performance, and sustainability in circular medical plastics.
- 1 January 2026
- Published by Wiley in Advances in Polymer Technology
- Vol. 2026 (1)
Open AccessInteractive Effects of Antioxidants, Acid Scavengers, and HALS on the Material Properties of Polypropylene Copolymer Considering γ‐Radiation Sterilization and Recycling for Medical Devices
Global plastic production and consumption have risen continuously over past decades, increasing the need for sustainable end‐of‐life strategies. The present study provides a systematic assessment of how repeated processing and γ‐irradiation affect the stability, additive consumption, and performance of polypropylene copolymers (PP‐C) intended for closed‐loop recycling in medical technology. Applying a design of experiments approach with Irganox 1010, Irgafos 168, Tinuvin 622, and calcium stearate (CaSt), the results identify γ‐irradiation as the dominant factor dominating additive depletion, molecular degradation, and optical aging. Phenolic and phosphite antioxidants were rapidly consumed after irradiation, frequently falling below quantifiable levels, whereas processing alone caused only moderate degradation. Pronounced synergistic interactions between Irganox 1010 and Irgafos 168 were confirmed, particularly in combination with CaSt, enabling both stabilizers to remain effective over multiple cycles. Tinuvin 622 exhibited fluctuating behavior consistent with regeneration mechanisms associated with the Denisov cycle. Changes in yellowness, tensile properties, and zero shear viscosity further demonstrate that irradiation, rather than mechanical recycling, drives deterioration and rheological instability. These findings underline that successful recycling of γ‐sterilized PP‐C requires tailored additive systems and highlight stabilizer engineering as a key factor for ensuring material safety, performance, and sustainability in circular medical plastics.
- Open Access
A Design of Experiment (DoE) Approach to Evaluate the Recyclability of a Polypropylene Copolymer in Medical Technology Under the Aspect of Additive Composition
This study evaluates the influence of repeated processing, γ-irradiation (25 kGy), and additive formulation including Irgafos 168 (I168), Tinuvin 622 (T622), and Calcium Stearate (CaSt) on a polypropylene copolymer (PP-C). Motivated by medical technology applications, the study assessed effects on optical properties, yellowing, crystallization, mechanical performance, and viscosity using a full factorial design of experiments (DoE). Results showed γ-irradiation had the most significant impact, especially on zero-shear viscosity, which decreased by 84% after the first irradiation. The Yellowness Index (YI) changed measurably, but discoloration remained imperceptible. Crystallization temperature was influenced mainly by additive interactions, while specific enthalpy was affected by processing and γ-irradiation. Elongation at break and tensile strength were predominantly influenced by γ-irradiation, with elongation at break being a sensitive indicator of degradation. Zero-shear viscosity, correlating with molecular weight, was mainly controlled by γ-irradiation, indicating chain scission without critical embrittlement. Overall, γ-irradiation exerted a stronger effect than processing or additive formulation. Zero-shear viscosity proved a reliable measure of degradation, while elongation at break offered complementary insights. Despite significant viscosity reduction, mechanical properties remained high, confirming the material’s suitability for its intended applications.
Open AccessA Design of Experiment (DoE) Approach to Evaluate the Recyclability of a Polypropylene Copolymer in Medical Technology Under the Aspect of Additive Composition
This study evaluates the influence of repeated processing, γ-irradiation (25 kGy), and additive formulation including Irgafos 168 (I168), Tinuvin 622 (T622), and Calcium Stearate (CaSt) on a polypropylene copolymer (PP-C). Motivated by medical technology applications, the study assessed effects on optical properties, yellowing, crystallization, mechanical performance, and viscosity using a full factorial design of experiments (DoE). Results showed γ-irradiation had the most significant impact, especially on zero-shear viscosity, which decreased by 84% after the first irradiation. The Yellowness Index (YI) changed measurably, but discoloration remained imperceptible. Crystallization temperature was influenced mainly by additive interactions, while specific enthalpy was affected by processing and γ-irradiation. Elongation at break and tensile strength were predominantly influenced by γ-irradiation, with elongation at break being a sensitive indicator of degradation. Zero-shear viscosity, correlating with molecular weight, was mainly controlled by γ-irradiation, indicating chain scission without critical embrittlement. Overall, γ-irradiation exerted a stronger effect than processing or additive formulation. Zero-shear viscosity proved a reliable measure of degradation, while elongation at break offered complementary insights. Despite significant viscosity reduction, mechanical properties remained high, confirming the material’s suitability for its intended applications.
- Open Access
- 14 November 2025
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 143 (6)
Exposition of Radiation‐Stabilized Polypropylene Copolymer to Repeated Injection Molding and γ ‐Radiation
High‐quality requirements for plastic components in healthcare limit their recyclability. This study examined the stability of a representative polypropylene copolymer (PP‐C) containing Tinuvin 622 (T622) as a light stabilizer and calcium stearate (CaSt) as an acid scavenger during successive recycling steps involving γ ‐irradiation, mimicking medical sterilization. Chemical, thermal, rheological and mechanical properties of PP‐C were analyzed throughout various recycling stages. Differential scanning calorimetry and x‐ray scattering revealed little impact of γ ‐irradiation on crystallinity and polymorph formation. The influence of γ ‐irradiation on the chemical and mechanical properties of the PP‐C specimens was large compared to the processing‐related changes to the material properties. T622 content decreased by 22% after four cycles involving γ ‐irradiation, while the formation of volatile substances increased substantially. Zero‐shear viscosity dropped by 80%, indicating a corresponding decrease in molecular weight. Elongation at break increased with each cycle without γ ‐irradiation and decreased with γ ‐irradiation. Since elongation at break did not drop below critical levels, molecular weight likely remained above the threshold for maintaining the required mechanical properties. The decisive influence of γ ‐irradiation over processing effects suggests that although performance declines with γ ‐irradiation, PP‐C retains sufficient stability. These findings support the feasibility of recycling PP‐C for healthcare applications under the conditions considered.
- 14 November 2025
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 143 (6)
Open AccessExposition of Radiation‐Stabilized Polypropylene Copolymer to Repeated Injection Molding and γ ‐Radiation
High‐quality requirements for plastic components in healthcare limit their recyclability. This study examined the stability of a representative polypropylene copolymer (PP‐C) containing Tinuvin 622 (T622) as a light stabilizer and calcium stearate (CaSt) as an acid scavenger during successive recycling steps involving γ ‐irradiation, mimicking medical sterilization. Chemical, thermal, rheological and mechanical properties of PP‐C were analyzed throughout various recycling stages. Differential scanning calorimetry and x‐ray scattering revealed little impact of γ ‐irradiation on crystallinity and polymorph formation. The influence of γ ‐irradiation on the chemical and mechanical properties of the PP‐C specimens was large compared to the processing‐related changes to the material properties. T622 content decreased by 22% after four cycles involving γ ‐irradiation, while the formation of volatile substances increased substantially. Zero‐shear viscosity dropped by 80%, indicating a corresponding decrease in molecular weight. Elongation at break increased with each cycle without γ ‐irradiation and decreased with γ ‐irradiation. Since elongation at break did not drop below critical levels, molecular weight likely remained above the threshold for maintaining the required mechanical properties. The decisive influence of γ ‐irradiation over processing effects suggests that although performance declines with γ ‐irradiation, PP‐C retains sufficient stability. These findings support the feasibility of recycling PP‐C for healthcare applications under the conditions considered.
- Open Access
- 20 December 2023
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 141 (10)
Stability assessment of a commercial polypropylene copolymer and Irgafos 168 under repeated injection molding and γ‐irradiation cycles
Despite the increasing importance of recycling, the medical sector is hardy engaged at this time due to regulatory issues. The aim of this study was to evaluate the influence of γ‐radiation sterilization (48–52 kGy) on the repetitive injection molding of a polypropylene copolymer for medical applications. For this purpose, the material was analyzed after injection molding and irradiation. To evaluate the irradiation and reprocessing influence, optical, rheological, and mechanical properties were investigated in addition to chromatography. The latter comprised the quantitative determination of Irgafos 168 and the qualitative comparison of volatile degradation products formed, including the radiolysis product 1,3‐di‐tert‐butylbenzene. The influence of irradiation on the content of Irgafos 168, volatile organic compounds, and 1,3‐di‐tert‐butylbenzene was greatest after the first irradiation, with a decrease of Irgafos 168 content by 40%. The yellowness index and melting enthalpy were influenced by irradiation and processing, but showed no direct relationship to the individual process steps. The zero viscosity correlated directly with gas chromatography–mass spectrometry results and decreased by 80% after the first irradiation. In addition, the elongation at break was reduced by 95% after the second irradiation. The influence of irradiation on the studied characteristics was high, whereas the influence of repetitive processing did not show any measurable differences
- 20 December 2023
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 141 (10)
Open AccessStability assessment of a commercial polypropylene copolymer and Irgafos 168 under repeated injection molding and γ‐irradiation cycles
Despite the increasing importance of recycling, the medical sector is hardy engaged at this time due to regulatory issues. The aim of this study was to evaluate the influence of γ‐radiation sterilization (48–52 kGy) on the repetitive injection molding of a polypropylene copolymer for medical applications. For this purpose, the material was analyzed after injection molding and irradiation. To evaluate the irradiation and reprocessing influence, optical, rheological, and mechanical properties were investigated in addition to chromatography. The latter comprised the quantitative determination of Irgafos 168 and the qualitative comparison of volatile degradation products formed, including the radiolysis product 1,3‐di‐tert‐butylbenzene. The influence of irradiation on the content of Irgafos 168, volatile organic compounds, and 1,3‐di‐tert‐butylbenzene was greatest after the first irradiation, with a decrease of Irgafos 168 content by 40%. The yellowness index and melting enthalpy were influenced by irradiation and processing, but showed no direct relationship to the individual process steps. The zero viscosity correlated directly with gas chromatography–mass spectrometry results and decreased by 80% after the first irradiation. In addition, the elongation at break was reduced by 95% after the second irradiation. The influence of irradiation on the studied characteristics was high, whereas the influence of repetitive processing did not show any measurable differences
- Open Access
- 12 May 2023
- Published by Springer Nature in Journal of Materials Science: Materials in Medicine
- Vol. 34 (5) , 1-13
Degree of conversion and residual monomer elution of 3D-printed, milled and self-cured resin-based composite materials for temporary dental crowns and bridges
The aim of this work was to investigate the elution of residual monomers as a function of the manufacturing process, which are CAD/CAM manufacturing, self-curing and 3D printing. The experimental materials used consisted of the base monomers TEGDMA, Bis-GMA and Bis-EMA and 50 wt.% fillers. Additionally, a 3D printing resin without fillers was tested. The elution of the base monomers into the different media (water, ethanol and ethanol/water (75/25 vol. %)) at 37 °C over a period of up to 120 d as well as the degree of conversion (DC) by FTIR were investigated. No monomer elution could be detected in water. Most residual monomers in both other media were released from the self-curing material whereas the 3D printing composite released relatively little. The CAD/CAM blanks released hardly any quantitatively detectable amounts of monomers. Relative to the base composition, TEGDMA eluted less than Bis-GMA and Bis-EMA. DC did not correlate with residual monomer release; thus, leaching was determined not only by the amount of residual monomers present but by further factors as possibly network density and structure. The CAD/CAM blanks and the 3D printing composite showed similar high DC but lower residual monomer release from the CAD/CAM blank, likewise the self-curing composite and the 3D printing resin exhibited similar DC but different monomer elution. In terms of residual monomer elution and DC, the 3D printing composite seems promising as a new material class for the use as temporary dental crowns and bridges. Graphical Abstract
- 12 May 2023
- Published by Springer Nature in Journal of Materials Science: Materials in Medicine
- Vol. 34 (5) , 1-13
Open AccessDegree of conversion and residual monomer elution of 3D-printed, milled and self-cured resin-based composite materials for temporary dental crowns and bridges
The aim of this work was to investigate the elution of residual monomers as a function of the manufacturing process, which are CAD/CAM manufacturing, self-curing and 3D printing. The experimental materials used consisted of the base monomers TEGDMA, Bis-GMA and Bis-EMA and 50 wt.% fillers. Additionally, a 3D printing resin without fillers was tested. The elution of the base monomers into the different media (water, ethanol and ethanol/water (75/25 vol. %)) at 37 °C over a period of up to 120 d as well as the degree of conversion (DC) by FTIR were investigated. No monomer elution could be detected in water. Most residual monomers in both other media were released from the self-curing material whereas the 3D printing composite released relatively little. The CAD/CAM blanks released hardly any quantitatively detectable amounts of monomers. Relative to the base composition, TEGDMA eluted less than Bis-GMA and Bis-EMA. DC did not correlate with residual monomer release; thus, leaching was determined not only by the amount of residual monomers present but by further factors as possibly network density and structure. The CAD/CAM blanks and the 3D printing composite showed similar high DC but lower residual monomer release from the CAD/CAM blank, likewise the self-curing composite and the 3D printing resin exhibited similar DC but different monomer elution. In terms of residual monomer elution and DC, the 3D printing composite seems promising as a new material class for the use as temporary dental crowns and bridges. Graphical Abstract
- Open Access
- 1 August 2022
- Published by Walter de Gruyter GmbH in Current Directions in Biomedical Engineering
- Vol. 8 (2) , 281-284
Effect of enzymatic degradation and hydrolysis on 3D-printed resin-based composite material for temporary dental crowns and bridges
Additive manufacturing of dental prostheses e.g. composite materials is continuously finding broader application in dentistry. In the oral environment, the materials are subjected to hydrolysis and accelerated hydrolysis by enzymes. With the aim to compare an additively manufactured composite with a self-curing and a CAD/CAM material of the same composition, the effect of enzymatic degradation and hydrolysis on the materials were investigated. The experimental composites consisted of 50 wt. % inorganic filler and 50 wt. % monomer matrix (BisEMA, BisGMA, TEGDMA). The influence of hydrolysis via a buffer system was investigated in comparison to enzymatic degradation by cholesterol esterase over 22 days. The detection of degradation products over time was conducted by HPLC-DAD analysis. Degradation products and monomers calibrated were: TEGDMA, BisGMA, BisEMA, MA, TEGMA, Bis-HPPP and E-bis-PA. Surface roughness of polished specimens was measured by AFM and hardness with a Vickers micro hardness tester. After enzymatic degradation and hydrolysis, BisGMA was detected in the eluates of the additively manufactured composites. The samples fabricated by CAD/CAM behaved similar during hydrolysis, where additionally MA was detected. After enzymatic degradation, furthermore TEGMA and BisEMA were detected qualitatively. In contrast, the self-curing material exhibited traces of MA, TEGMA, TEGDMA and BisGMA after enzymatic degradation. Hereof detectable upon hydrolysis were MA, TEGMA and BisGMA. Surface roughness was comparable for all manufactured samples whereas the hardness was lowest of the 3D printed material. Enzymatic degradation and hydrolysis had no effect on surface roughness and hardness. The additively manufactured composite appeared to have low susceptibility to enzymatic degradation and hydrolysis. Due to the manufacturing process, the polishability and initial hardness are poorer.
- 1 August 2022
- Published by Walter de Gruyter GmbH in Current Directions in Biomedical Engineering
- Vol. 8 (2) , 281-284
Open AccessEffect of enzymatic degradation and hydrolysis on 3D-printed resin-based composite material for temporary dental crowns and bridges
Additive manufacturing of dental prostheses e.g. composite materials is continuously finding broader application in dentistry. In the oral environment, the materials are subjected to hydrolysis and accelerated hydrolysis by enzymes. With the aim to compare an additively manufactured composite with a self-curing and a CAD/CAM material of the same composition, the effect of enzymatic degradation and hydrolysis on the materials were investigated. The experimental composites consisted of 50 wt. % inorganic filler and 50 wt. % monomer matrix (BisEMA, BisGMA, TEGDMA). The influence of hydrolysis via a buffer system was investigated in comparison to enzymatic degradation by cholesterol esterase over 22 days. The detection of degradation products over time was conducted by HPLC-DAD analysis. Degradation products and monomers calibrated were: TEGDMA, BisGMA, BisEMA, MA, TEGMA, Bis-HPPP and E-bis-PA. Surface roughness of polished specimens was measured by AFM and hardness with a Vickers micro hardness tester. After enzymatic degradation and hydrolysis, BisGMA was detected in the eluates of the additively manufactured composites. The samples fabricated by CAD/CAM behaved similar during hydrolysis, where additionally MA was detected. After enzymatic degradation, furthermore TEGMA and BisEMA were detected qualitatively. In contrast, the self-curing material exhibited traces of MA, TEGMA, TEGDMA and BisGMA after enzymatic degradation. Hereof detectable upon hydrolysis were MA, TEGMA and BisGMA. Surface roughness was comparable for all manufactured samples whereas the hardness was lowest of the 3D printed material. Enzymatic degradation and hydrolysis had no effect on surface roughness and hardness. The additively manufactured composite appeared to have low susceptibility to enzymatic degradation and hydrolysis. Due to the manufacturing process, the polishability and initial hardness are poorer.
- Open Access
- 11 March 2022
- Published by MDPI AG in Dentistry Journal
- Vol. 10 (3) , 46
Abrasion Behavior of Different Charcoal Toothpastes on Human Dentin When Using Electric Toothbrushes
The aim of this study was to investigate abrasion on human dentin after brushing with activated charcoal toothpastes. A self-designed brushing machine was used to brush five groups (Group A: Water, Group B: Sensodyne Pro Schmelz, Group C: Splat Blackwood, Group D: Curaprox Black is White, and Group E: Prokudent Black Brilliant) with electrically powered toothbrushes for 4 h. The abrasive dentin wear was calculated using profilometry data. Furthermore, thermogravimetric analyses and scanning electron microscopy were used to analyze the composition of the toothpastes. Mean dentin loss by brushing were (71 ± 28) µm (Splat Blackwood), (44 ± 16) µm (Curaprox Black is White), (38 ± 13) µm (Prokudent Black Brilliant), (28 ± 14) µm (Sensodyne Pro Schmelz), and (28 ± 13) µm (Water). Groups A/B/D/E and group C each lie in one subset, which is statistically different from the other subset according to a post hoc Tukey test (p = 0.05). Within the limitations, it can be concluded that the content of activated charcoal in charcoal toothpastes had little influence on the observed abrasive behavior, although one of the charcoal toothpastes showed the highest abrasion on dentin.
- 11 March 2022
- Published by MDPI AG in Dentistry Journal
- Vol. 10 (3) , 46
Open AccessAbrasion Behavior of Different Charcoal Toothpastes on Human Dentin When Using Electric Toothbrushes
The aim of this study was to investigate abrasion on human dentin after brushing with activated charcoal toothpastes. A self-designed brushing machine was used to brush five groups (Group A: Water, Group B: Sensodyne Pro Schmelz, Group C: Splat Blackwood, Group D: Curaprox Black is White, and Group E: Prokudent Black Brilliant) with electrically powered toothbrushes for 4 h. The abrasive dentin wear was calculated using profilometry data. Furthermore, thermogravimetric analyses and scanning electron microscopy were used to analyze the composition of the toothpastes. Mean dentin loss by brushing were (71 ± 28) µm (Splat Blackwood), (44 ± 16) µm (Curaprox Black is White), (38 ± 13) µm (Prokudent Black Brilliant), (28 ± 14) µm (Sensodyne Pro Schmelz), and (28 ± 13) µm (Water). Groups A/B/D/E and group C each lie in one subset, which is statistically different from the other subset according to a post hoc Tukey test (p = 0.05). Within the limitations, it can be concluded that the content of activated charcoal in charcoal toothpastes had little influence on the observed abrasive behavior, although one of the charcoal toothpastes showed the highest abrasion on dentin.
- 22 December 2021
- Published by Wiley in European Journal of Oral Sciences
- Vol. 130 (2) , e12840
Antimicrobial agents in dental restorative materials: Effect on long‐term drug release and material properties
The present study reports on the long‐term drug release and mechanical properties of bioactive dental filling materials based on chlorhexidine diacetate (CHX) or octinidine (di)hydrochloride (ODH) incorporated in a composite based on dimethacrylates or an ormocer. CHX or ODH were added to a nano‐hybrid ormocer (O) and a nano‐hybrid composite (C) with the amount of 2 wt% to achieve four matrix‐drug combinations: O‐CHX, O‐ODH, C‐CHX, and C‐ODH. Drug extraction and release were measured using high‐performance liquid chromatography with diode‐array detection (HPLC‐DAD), while drug distribution was assessed by using energy dispersive X‐ray spectroscopy (EDX). Drug release in water at 37°C was observed over 87 d. To determine the material properties, the water absorption, water solubility, flexural strength and hardness were measured and compared to the reference materials. Persistent drug release over 87 d was observed for both ODH‐based systems and both ormocer‐systems, with the longest duration of activity seen for the O‐ODH combination. Persistent drug release was achieved via the loosening of the polymer network indicated via decreasing polymerization enthalpies, enhanced water absorption, and water solubility. As a consequence, the flexural strengths of the materials were reduced. However, surface hardness was hardly reduced. ODH seems to be more adequate than CHX for the design of bioactive dental filling materials based on nano‐hybrid ormocer and composites.
- 22 December 2021
- Published by Wiley in European Journal of Oral Sciences
- Vol. 130 (2) , e12840
Antimicrobial agents in dental restorative materials: Effect on long‐term drug release and material properties
The present study reports on the long‐term drug release and mechanical properties of bioactive dental filling materials based on chlorhexidine diacetate (CHX) or octinidine (di)hydrochloride (ODH) incorporated in a composite based on dimethacrylates or an ormocer. CHX or ODH were added to a nano‐hybrid ormocer (O) and a nano‐hybrid composite (C) with the amount of 2 wt% to achieve four matrix‐drug combinations: O‐CHX, O‐ODH, C‐CHX, and C‐ODH. Drug extraction and release were measured using high‐performance liquid chromatography with diode‐array detection (HPLC‐DAD), while drug distribution was assessed by using energy dispersive X‐ray spectroscopy (EDX). Drug release in water at 37°C was observed over 87 d. To determine the material properties, the water absorption, water solubility, flexural strength and hardness were measured and compared to the reference materials. Persistent drug release over 87 d was observed for both ODH‐based systems and both ormocer‐systems, with the longest duration of activity seen for the O‐ODH combination. Persistent drug release was achieved via the loosening of the polymer network indicated via decreasing polymerization enthalpies, enhanced water absorption, and water solubility. As a consequence, the flexural strengths of the materials were reduced. However, surface hardness was hardly reduced. ODH seems to be more adequate than CHX for the design of bioactive dental filling materials based on nano‐hybrid ormocer and composites.