Chunming Zou
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Chunming Zou has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
- Zunjie Wei
Harbin Institute of Technology
9 shared publications - Hongwei Wang
School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China
7 shared publications - Rong Zhang
School of Materials Science and Engineering, Fujian University of Technology, Fuzhou 350118, China
5 shared publications - Bo Gao
National Key Laboratory for Precision Hot Processing of Metals, School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China
2 shared publications - Rui Wang
School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China
2 shared publications - Yanfei Sui
National Key Laboratory for Precision Hot Processing of Metals, School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China
2 shared publications
Latest Publications
- Open Access
First-Principles Study of Interfacial Properties and Fracture Behavior of (3C and 4H) SiC/Al Interfaces
First-principles calculations based on density functional theory (DFT) are performed to investigate the interfacial properties and fracture behavior of 3C-SiC(111)/Al(111) and 4H-SiC(0001)/Al(111) interfaces. To mitigate surface effects through adequate slab thickness, the interface models are constructed by positioning a seven-layer Al(111) slab atop eight-layer 3C-SiC(111) and 14-layer 4H-SiC(0001) slabs, respectively. Accounting for the distinct surface terminations and stacking sequences of each polytype, six interface configurations are established: C-top, -center, and -hollow; Si-top, -center, and -hollow. Based on the simulation results of surface energy, work of separation, and electron density distribution, the C-top configuration yields the most stable SiC/Al interface structure, exhibiting the highest work of separation. The ultimate tensile strengths of the C-top interfaces are 6.603 GPa (3C-SiC/Al) and 6.851 GPa (4H-SiC/Al), with corresponding tensile strains of 10% and 12%, respectively. Tensile fracture initiates exclusively within the Al slab for all C-top interfaces, but at distinct atomic layers: fracture occurs between the second and third Al layers (Al2–Al3) for 3C-SiC/Al; and between the first and second Al layers (Al1–Al2) for 4H-SiC/Al. This distinction reflects the influence of different interfacial configurations on the bonding strength between aluminum atomic layers. In summary, an atomic-scale investigation of the interfacial properties and fracture behavior of SiC/Al interfaces provides critical insights for the design and fabrication of novel ceramic/metal composites.
Open AccessFirst-Principles Study of Interfacial Properties and Fracture Behavior of (3C and 4H) SiC/Al Interfaces
First-principles calculations based on density functional theory (DFT) are performed to investigate the interfacial properties and fracture behavior of 3C-SiC(111)/Al(111) and 4H-SiC(0001)/Al(111) interfaces. To mitigate surface effects through adequate slab thickness, the interface models are constructed by positioning a seven-layer Al(111) slab atop eight-layer 3C-SiC(111) and 14-layer 4H-SiC(0001) slabs, respectively. Accounting for the distinct surface terminations and stacking sequences of each polytype, six interface configurations are established: C-top, -center, and -hollow; Si-top, -center, and -hollow. Based on the simulation results of surface energy, work of separation, and electron density distribution, the C-top configuration yields the most stable SiC/Al interface structure, exhibiting the highest work of separation. The ultimate tensile strengths of the C-top interfaces are 6.603 GPa (3C-SiC/Al) and 6.851 GPa (4H-SiC/Al), with corresponding tensile strains of 10% and 12%, respectively. Tensile fracture initiates exclusively within the Al slab for all C-top interfaces, but at distinct atomic layers: fracture occurs between the second and third Al layers (Al2–Al3) for 3C-SiC/Al; and between the first and second Al layers (Al1–Al2) for 4H-SiC/Al. This distinction reflects the influence of different interfacial configurations on the bonding strength between aluminum atomic layers. In summary, an atomic-scale investigation of the interfacial properties and fracture behavior of SiC/Al interfaces provides critical insights for the design and fabrication of novel ceramic/metal composites.
- Open Access
Microstructural Evolution and Mechanical Properties of SiC/Al-40Si Composites Fabricated by High Pressure Solidification
The microstructure and mechanical properties of SiC/Al-40Si composites prepared under high pressure were studied. As the pressure increases from 1 atm to 3 GPa, the primary Si phase in the Al-40Si alloy is refined. With increasing pressure, the composition of the eutectic point increases, the solute diffusion coefficient decreases exponentially, and the concentration of Si solute at the front of the solid–liquid interface of the primary Si is low, which contributes to the refining of the primary Si and inhibiting its faceted growth. The bending strength of SiC/Al-40Si composite prepared under 3 GPa was 334 MPa, which was 66% higher compared to the Al-40Si alloy prepared under the same pressure.
Open AccessMicrostructural Evolution and Mechanical Properties of SiC/Al-40Si Composites Fabricated by High Pressure Solidification
The microstructure and mechanical properties of SiC/Al-40Si composites prepared under high pressure were studied. As the pressure increases from 1 atm to 3 GPa, the primary Si phase in the Al-40Si alloy is refined. With increasing pressure, the composition of the eutectic point increases, the solute diffusion coefficient decreases exponentially, and the concentration of Si solute at the front of the solid–liquid interface of the primary Si is low, which contributes to the refining of the primary Si and inhibiting its faceted growth. The bending strength of SiC/Al-40Si composite prepared under 3 GPa was 334 MPa, which was 66% higher compared to the Al-40Si alloy prepared under the same pressure.
- Open Access
Nano-Phase and SiC–Si Spherical Microstructure in SiC/Al-50Si Composites Solidified under High Pressure
The formation of coarse primary Si is the main scientific challenge faced in the preparation of high-Si Al matrix composites. The SiC/Al-50Si composites are prepared by high pressure solidification, which allows the primary Si to form a SiC–Si spherical microstructure with SiC, while the solubility of Si in Al is increased by high pressure to reduce the proportion of primary Si, thus enhancing the strength of the composites. The results show that the high melt viscosity under high pressure makes the SiC particles almost “fixed” in situ. The SEM analysis shows that the presence of SiC in the growth front of the primary Si will hinder its continued growth and eventually form SiC–Si spherical microstructure. Through aging treatment, a large number of dispersed nanoscale Si phases are precipitated in the α-Al supersaturated solid solution. The TEM analysis shows that a semi-coherent interface is formed between the α-Al matrix and the nanoscale Si precipitates. The three-point bending tests shows that the bending strength of the aged SiC/Al-50Si composites prepared at 3 GPa is 387.6 MPa, which is 18.6% higher than that of the unaged composites.
Open AccessNano-Phase and SiC–Si Spherical Microstructure in SiC/Al-50Si Composites Solidified under High Pressure
The formation of coarse primary Si is the main scientific challenge faced in the preparation of high-Si Al matrix composites. The SiC/Al-50Si composites are prepared by high pressure solidification, which allows the primary Si to form a SiC–Si spherical microstructure with SiC, while the solubility of Si in Al is increased by high pressure to reduce the proportion of primary Si, thus enhancing the strength of the composites. The results show that the high melt viscosity under high pressure makes the SiC particles almost “fixed” in situ. The SEM analysis shows that the presence of SiC in the growth front of the primary Si will hinder its continued growth and eventually form SiC–Si spherical microstructure. Through aging treatment, a large number of dispersed nanoscale Si phases are precipitated in the α-Al supersaturated solid solution. The TEM analysis shows that a semi-coherent interface is formed between the α-Al matrix and the nanoscale Si precipitates. The three-point bending tests shows that the bending strength of the aged SiC/Al-50Si composites prepared at 3 GPa is 387.6 MPa, which is 18.6% higher than that of the unaged composites.
- Open Access
Microstructure Evolution of Mg-Sn-Y Alloy Solidified under High Pressure and Temperature Gradient
The microstructures of Mg-1Sn-2.5Y (wt%) alloys solidified under high pressures were investigated. In addition, a mathematical model was established to analyze the effects of solidification pressure and cooling rate on the average grain size. The results show that the alloy was solidified under high pressure and temperature gradient using the cooling rate difference in the high pressure chamber, resulting in the formation of the outer equiaxed zone, the columnar zone, and the equiaxed zone in the sample. With an increase in the solidification pressure, the columnar-to-equiaxed transition was inhibited in Mg-1Sn-2.5Y alloy. In the outer fine equiaxed zone and the columnar zone, the solubility of Sn in the Mg matrix increased with an increase in solidification pressure. The average secondary dendrite arm spacing decreased from 14–17 μm under 1 GPa to 9–11 μm under 1.5 GPa. Increases in pressure and cooling rate resulted in a reduction in average grain size.
Open AccessMicrostructure Evolution of Mg-Sn-Y Alloy Solidified under High Pressure and Temperature Gradient
The microstructures of Mg-1Sn-2.5Y (wt%) alloys solidified under high pressures were investigated. In addition, a mathematical model was established to analyze the effects of solidification pressure and cooling rate on the average grain size. The results show that the alloy was solidified under high pressure and temperature gradient using the cooling rate difference in the high pressure chamber, resulting in the formation of the outer equiaxed zone, the columnar zone, and the equiaxed zone in the sample. With an increase in the solidification pressure, the columnar-to-equiaxed transition was inhibited in Mg-1Sn-2.5Y alloy. In the outer fine equiaxed zone and the columnar zone, the solubility of Sn in the Mg matrix increased with an increase in solidification pressure. The average secondary dendrite arm spacing decreased from 14–17 μm under 1 GPa to 9–11 μm under 1.5 GPa. Increases in pressure and cooling rate resulted in a reduction in average grain size.
- 1 January 2022
- Published by Springer Nature in China Foundry
- Vol. 19 (1) , 81-88
Regulative effect of Mg/Si ratio on microstructure evolution and mechanical properties of cast Al-Li-Mg-Si alloys
- 1 January 2022
- Published by Springer Nature in China Foundry
- Vol. 19 (1) , 81-88
Regulative effect of Mg/Si ratio on microstructure evolution and mechanical properties of cast Al-Li-Mg-Si alloys
- Open Access
Effect of High Pressure and Temperature on the Evolution of Si Phase and Eutectic Spacing in Al-20Si Alloys
The microstructure of the Si phase in Al-20Si alloys solidified under high pressure was investigated. The results demonstrate that the morphology of Si phase transformed (bulk→short rod→long needle) with the increase of superheat temperature under high pressure. At a pressure of 3 GPa and a superheat temperature of 100 K, a microstructure with a uniform distribution of fine Si phases on the α-Al matrix was obtained in the Al-20Si alloy. In addition, a mathematical model was developed to analyze the spacing variation of the lamellar Al-Si eutectics under the effect of pressure. The lamellar Al-Si eutectics appeared at 2 GPa and superheat temperatures of 70–150 K, and at 3 GPa and superheat temperatures of 140–200 K. With the increase of pressure from 2 GPa to 3 GPa, the average spacing of lamellar Al-Si eutectics decreased from 1.2–1.6 μm to 0.9–1.1 μm. In binary alloys, the effect of pressure on the eutectic spacing is related to the volume change of the solute phase from liquid to solid. When the volume change of the solute phase from liquid to solid is negative, the lamellar eutectic spacing decreases with increasing pressure. When it is positive, the eutectic spacing increases with increasing pressure.
Open AccessEffect of High Pressure and Temperature on the Evolution of Si Phase and Eutectic Spacing in Al-20Si Alloys
The microstructure of the Si phase in Al-20Si alloys solidified under high pressure was investigated. The results demonstrate that the morphology of Si phase transformed (bulk→short rod→long needle) with the increase of superheat temperature under high pressure. At a pressure of 3 GPa and a superheat temperature of 100 K, a microstructure with a uniform distribution of fine Si phases on the α-Al matrix was obtained in the Al-20Si alloy. In addition, a mathematical model was developed to analyze the spacing variation of the lamellar Al-Si eutectics under the effect of pressure. The lamellar Al-Si eutectics appeared at 2 GPa and superheat temperatures of 70–150 K, and at 3 GPa and superheat temperatures of 140–200 K. With the increase of pressure from 2 GPa to 3 GPa, the average spacing of lamellar Al-Si eutectics decreased from 1.2–1.6 μm to 0.9–1.1 μm. In binary alloys, the effect of pressure on the eutectic spacing is related to the volume change of the solute phase from liquid to solid. When the volume change of the solute phase from liquid to solid is negative, the lamellar eutectic spacing decreases with increasing pressure. When it is positive, the eutectic spacing increases with increasing pressure.
- Open Access
Effects of Cooling Rate on the Solidification and Microstructure of Nickel-Based Superalloy GTD222
In this work, the microstructure and solidification behavior of nickel-based superalloy GTD222 at different cooling rates are studied. The solidification of the superalloy GTD222 proceeds as follows: L → L + γ, L → L + γ + MC, L → L + (γ/γ′)-Eutectic and L → η phase. Due to alloying element redistribution, the temperature of the solidus GTD222 superalloy, 1310 °C, is slightly lower than the temperature of the liquidus, which is 1360 °C. It was found that the dendrite arm spacing of the alloy decreased with the increase of the cooling rate from 200 μm at 2.5 K/min to 100 μm at 20 K/min.
Open AccessEffects of Cooling Rate on the Solidification and Microstructure of Nickel-Based Superalloy GTD222
In this work, the microstructure and solidification behavior of nickel-based superalloy GTD222 at different cooling rates are studied. The solidification of the superalloy GTD222 proceeds as follows: L → L + γ, L → L + γ + MC, L → L + (γ/γ′)-Eutectic and L → η phase. Due to alloying element redistribution, the temperature of the solidus GTD222 superalloy, 1310 °C, is slightly lower than the temperature of the liquidus, which is 1360 °C. It was found that the dendrite arm spacing of the alloy decreased with the increase of the cooling rate from 200 μm at 2.5 K/min to 100 μm at 20 K/min.
- Open Access
- 8 May 2019
- Published by MDPI AG in Preprints.org
Effects of Solidification Cooling Rate on the Microstructure of Nickel Based Superalloy GTD222
The microstructure and solidification behavior of nickel based GTD222 superalloy at different cooling rates are studied. The solidification of the GTD222 superalloy proceeds as follows: L→L+γ, L→L+γ+MC, L→L+(γ/γ ′)-Eutectic and L→η phase. The temperature of liquidus of GTD222 superalloy is 1360 °C while the solidus is slightly lower at 1310 °C, which due to the alloying elements redistribution. It was found that the dendrite arm spacing of the alloy decreased with the increase of cooling rate (From 200 μm at 2.5 K/min to 100 μm at 20 K/min).
- 8 May 2019
- Published by MDPI AG in Preprints.org
Open AccessEffects of Solidification Cooling Rate on the Microstructure of Nickel Based Superalloy GTD222
The microstructure and solidification behavior of nickel based GTD222 superalloy at different cooling rates are studied. The solidification of the GTD222 superalloy proceeds as follows: L→L+γ, L→L+γ+MC, L→L+(γ/γ ′)-Eutectic and L→η phase. The temperature of liquidus of GTD222 superalloy is 1360 °C while the solidus is slightly lower at 1310 °C, which due to the alloying elements redistribution. It was found that the dendrite arm spacing of the alloy decreased with the increase of cooling rate (From 200 μm at 2.5 K/min to 100 μm at 20 K/min).
- 1 November 2016
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 686, 727-732
Modeling of yield strength in binary hypoeutectic alloy under high pressure solidification
- 1 November 2016
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 686, 727-732
Modeling of yield strength in binary hypoeutectic alloy under high pressure solidification