F. H. Samuel
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
F. H. Samuel has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
A. M. Samuel
Département des Sciences appliquées, Université du Québec à Chicoutimi, Chicoutimi (Québec), Canada G7H 2B1
4 shared publicationsC. Villeneuve
Département des Sciences appliquées, Université du Québec à Chicoutimi, Chicoutimi (Québec), Canada G7H 2B1
4 shared publicationsS. Valtierra
Research and Development, Corporativo Nemak, S.A. de C.V., Garza Garcia, NL 66221, Mexico
4 shared publicationsH. W. Doty
General Motors Powertrain, Metallurgical Processing Group, Metal Casting Technology, Inc., Milford, NH 03055, USA
3 shared publicationsP. Ouellet
Département des Sciences appliquées, Université du Québec à Chicoutimi, 555, boulevard de l'Université, Chicoutimi (Québec), Canada G7H 2B1
2 shared publicationsA. Pennors
Département des Sciences appliquées, Université du Québec à Chicoutimi, Chicoutimi (Québec), Canada G7H 2B1
1 shared publication
Latest Publications
- 1 September 2001
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 14 (2) , 97-120
Effect of trace elements on β-Al5FeSi characteristics, porosity and tensile properties of Al-Si-Cu (319) cast alloys
This study was performed on an Al-6.2% Si-3.7% Cu-0.37% Fe-0.095% Mn (A319.2) alloy, to study the effect of trace elements on the β-Al5FeSi intermetallic phase characteristics observed in the alloy and the resultant tensile properties. The results show that increasing the iron content leads to precipitation of long, branched platelets of the β-Al5FeSi phase. These platelets (or needles as they appear in the microstructure) often result in the formation of large shrinkage cavities due to the inability of the liquid metal to fill the spaces between the branched platelets. The alloy tensile properties are greatly improved by: a) Sr addition in the range 200–400 ppm, b) increasing the Mn/Fe ratio to 0.7, c) addition of 0.08%Be, d) addition of 0.08% Be+ 0.02% Sr. The results indicate that the classic neutralization treatment of using a Mn addition with or without Cr could be replaced by the combined 0.08%Be + 0.02%Sr addition. The latter combination produces a much better improvement in the alloy ductility. The rupture mode changes from transgranular to intergranular as the iron concentration is increased from 0.5% to 1.5%. Fragmentation of the β-Al5FeSi platelets using Sr or Be + Sr, or their transformation into α-Al15(Fe, Mn, Cr)3Si2 in the form of Chinese script or sludge particles (using Mn or Mn + Cr) results in a ductile dimpled rupture surface.
- 1 September 2001
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 14 (2) , 97-120
Effect of trace elements on β-Al5FeSi characteristics, porosity and tensile properties of Al-Si-Cu (319) cast alloys
This study was performed on an Al-6.2% Si-3.7% Cu-0.37% Fe-0.095% Mn (A319.2) alloy, to study the effect of trace elements on the β-Al5FeSi intermetallic phase characteristics observed in the alloy and the resultant tensile properties. The results show that increasing the iron content leads to precipitation of long, branched platelets of the β-Al5FeSi phase. These platelets (or needles as they appear in the microstructure) often result in the formation of large shrinkage cavities due to the inability of the liquid metal to fill the spaces between the branched platelets. The alloy tensile properties are greatly improved by: a) Sr addition in the range 200–400 ppm, b) increasing the Mn/Fe ratio to 0.7, c) addition of 0.08%Be, d) addition of 0.08% Be+ 0.02% Sr. The results indicate that the classic neutralization treatment of using a Mn addition with or without Cr could be replaced by the combined 0.08%Be + 0.02%Sr addition. The latter combination produces a much better improvement in the alloy ductility. The rupture mode changes from transgranular to intergranular as the iron concentration is increased from 0.5% to 1.5%. Fragmentation of the β-Al5FeSi platelets using Sr or Be + Sr, or their transformation into α-Al15(Fe, Mn, Cr)3Si2 in the form of Chinese script or sludge particles (using Mn or Mn + Cr) results in a ductile dimpled rupture surface.
- 1 December 2000
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 13 (4) , 231-253
Effect of cooling rate and Sr-modification on porosity and Fe-intermetallics formation in Al-6.5% Si-3.5% Cu-Fe alloys
Together with porosity, the problems created by the formation of iron intermetallics in Al-Si alloys pose serious concerns in regard to their use in structural components. The presence of these intermetallics, particularly the brittle β-Al5FeSi phase, tends to reduce the alloy properties and casting quality. In order to optimise the iron intermetallics in Al-6.5% Si-3.5% Cu-Fe alloys, the effects of cooling rate, Sr modification, other melt additions, and heat treatment were studied, with a view to determining the means of their formation and dissolution, in relation to their effect on porosity formation and alloy properties. The iron levels selected for study were 0.5%, 1.0% and 1.5%, covering the range of levels normally observed in foundry alloys. Castings were prepared using a cooling fin sand mould (DAS range: 25–85 μm) for microstructural analysis, and a Stahl permanent mould for tensile testing purposes. Samples of molten metal quenched in cold water provided much smaller DASs. Microstructural characterisation was carried out using optical microscopy and thermal, image and electron microprobe analyses. Tensile properties (T6 condition) were determined at room temperature and a strain rate of 4 × 10−4/s using an Instron Universal testing machine. The results show that at any Fe level, the average β-Al5FeSi platelet length is strongly determined by the DAS. Strontium (250–350 ppm) is effective in reducing the β-platelet size through its fragmentation/dissolution effect on the latter. At higher Sr concentrations, both coarsening of the β-platelets (i.e., “overmodification”) and their decomposition (through Si rejection ahead of the platelets) occur. Addition of P increases β-phase formation (due to the presence of AIP particles that act as possible nucleation sites). Melt superheating (900 °C) thereafter reduces the effect. At Fe levels of 1% or more, α-Chinese script or sludge particles form only at slow cooling rates or with superheating. Tensile properties of alloys containing up to 1 % Fe are improved with Mn, Mn + Cr, Sr or Be additions. Best overall properties are achieved with Mn at Mn/Fe = 0.7. Also, Sr additions of 200–300 ppm are best, higher levels giving rise to increased porosity levels and, hence, lower properties. For a given Fe level, the optimum Sr concentration depends on the cooling rate and Si content of the alloy. Iron levels of 1.5% are not recommended for Al-6.5% Si-3.5% Cu (319.2) alloys as the properties cannot be improved by any of the above means.
- 1 December 2000
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 13 (4) , 231-253
Effect of cooling rate and Sr-modification on porosity and Fe-intermetallics formation in Al-6.5% Si-3.5% Cu-Fe alloys
Together with porosity, the problems created by the formation of iron intermetallics in Al-Si alloys pose serious concerns in regard to their use in structural components. The presence of these intermetallics, particularly the brittle β-Al5FeSi phase, tends to reduce the alloy properties and casting quality. In order to optimise the iron intermetallics in Al-6.5% Si-3.5% Cu-Fe alloys, the effects of cooling rate, Sr modification, other melt additions, and heat treatment were studied, with a view to determining the means of their formation and dissolution, in relation to their effect on porosity formation and alloy properties. The iron levels selected for study were 0.5%, 1.0% and 1.5%, covering the range of levels normally observed in foundry alloys. Castings were prepared using a cooling fin sand mould (DAS range: 25–85 μm) for microstructural analysis, and a Stahl permanent mould for tensile testing purposes. Samples of molten metal quenched in cold water provided much smaller DASs. Microstructural characterisation was carried out using optical microscopy and thermal, image and electron microprobe analyses. Tensile properties (T6 condition) were determined at room temperature and a strain rate of 4 × 10−4/s using an Instron Universal testing machine. The results show that at any Fe level, the average β-Al5FeSi platelet length is strongly determined by the DAS. Strontium (250–350 ppm) is effective in reducing the β-platelet size through its fragmentation/dissolution effect on the latter. At higher Sr concentrations, both coarsening of the β-platelets (i.e., “overmodification”) and their decomposition (through Si rejection ahead of the platelets) occur. Addition of P increases β-phase formation (due to the presence of AIP particles that act as possible nucleation sites). Melt superheating (900 °C) thereafter reduces the effect. At Fe levels of 1% or more, α-Chinese script or sludge particles form only at slow cooling rates or with superheating. Tensile properties of alloys containing up to 1 % Fe are improved with Mn, Mn + Cr, Sr or Be additions. Best overall properties are achieved with Mn at Mn/Fe = 0.7. Also, Sr additions of 200–300 ppm are best, higher levels giving rise to increased porosity levels and, hence, lower properties. For a given Fe level, the optimum Sr concentration depends on the cooling rate and Si content of the alloy. Iron levels of 1.5% are not recommended for Al-6.5% Si-3.5% Cu (319.2) alloys as the properties cannot be improved by any of the above means.
- 29 November 1999
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 12 (3) , 197-210
Microstructural observations on Fe-intermetallics in unmodified and Sr-modified Al-Si-Cu (A380.1) die casting alloy
The present work was performed on an Al-9%Si-3.2 % Cu-1 % Fe-0.17 % Mn-0.04 % Mg (A380.1) alloy, in the unmodified and Sr-modified (350 ppm Sr) conditions. Three pouring temperatures, 750 °C, 720 °C and 620 °C, were used in each case. The liquid metal was poured into a hot graphite mould, cold metallic mould and cold water which produced castings whose microstructures exhibited average dendrite arm spacings (DASs) of ∼45 μm, ∼15 μm, and ∼5 μm, respectively. The microstructures were analysed using optical microscopy, and electron microprobe analysis (EMPA) coupled with energy dispersive X-ray (EDX) analysis. Tensile test bars were also prepared using a Stahl permanent mould (type ASTM 108-B), each Stahl mould casting providing two test bars. The test bars were tensile tested in the T6 condition (6–8 bars per composition). The results obtained show that the presence of Sr leads to precipitation of a large part of the iron intermetallics in the form of coarse pre-dendritic particles situated within the α-Al dendrites, instead of in the interdendritic regions. This is expected to homogenise the stress distribution across the alloy matrix, and hence lead to better tensile properties. In the alloy containing a higher Fe-content (1.4% Fe), but the same amount of Mn, addition of 0.08% Be together with 0.02% Sr is equivalent to the addition of 1% Mn (for an Mn/Fe ratio of 0.7) in terms of the tensile properties. The results are discussed in detail in the paper.
- 29 November 1999
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 12 (3) , 197-210
Microstructural observations on Fe-intermetallics in unmodified and Sr-modified Al-Si-Cu (A380.1) die casting alloy
The present work was performed on an Al-9%Si-3.2 % Cu-1 % Fe-0.17 % Mn-0.04 % Mg (A380.1) alloy, in the unmodified and Sr-modified (350 ppm Sr) conditions. Three pouring temperatures, 750 °C, 720 °C and 620 °C, were used in each case. The liquid metal was poured into a hot graphite mould, cold metallic mould and cold water which produced castings whose microstructures exhibited average dendrite arm spacings (DASs) of ∼45 μm, ∼15 μm, and ∼5 μm, respectively. The microstructures were analysed using optical microscopy, and electron microprobe analysis (EMPA) coupled with energy dispersive X-ray (EDX) analysis. Tensile test bars were also prepared using a Stahl permanent mould (type ASTM 108-B), each Stahl mould casting providing two test bars. The test bars were tensile tested in the T6 condition (6–8 bars per composition). The results obtained show that the presence of Sr leads to precipitation of a large part of the iron intermetallics in the form of coarse pre-dendritic particles situated within the α-Al dendrites, instead of in the interdendritic regions. This is expected to homogenise the stress distribution across the alloy matrix, and hence lead to better tensile properties. In the alloy containing a higher Fe-content (1.4% Fe), but the same amount of Mn, addition of 0.08% Be together with 0.02% Sr is equivalent to the addition of 1% Mn (for an Mn/Fe ratio of 0.7) in terms of the tensile properties. The results are discussed in detail in the paper.
- 29 November 1999
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 12 (3) , 145-160
Fragmentation and dissolution of β-Al5FeSi phase during solution heat treatment of Al-13wt%Si-Fe alloys
The dissolution of the platelet/needle-like/β-Al5FeSi phase in unmodified and Sr-modified Al-12wt% Si-0.35 wt% Mg alloys was studied, using three levels of iron viz., 0.5, 1.0, and 1.5%. The alloys were cast in the form of tensile test bars (dendrite arm spacing ∼22 μm) using a Stahl permanent mould (type ASTM B-108). The test bars were solution heat-treated at 540 °C for times up to 200 h. The results indicate that a sufficiently high concentration of Sr (∼350 ppm) breaks down the β-needles into small, thin fragments through (a) splitting of the needles into two halves, and (b) fragmentation due to Si rejection. Minimal β-needle lengths are achieved after 30 h and 10 h for the unmodified and Sr-modified alloys, respectively. The fragmentation process results in stabilising the alloy tensile properties during the period of solution treatment, in that not much variation in the tensile parameters is observed up to 100 h at 540 °C. In the Sr-modified alloys, the YS levels are 50 MPa higher than those obtained from the unmodified alloys treated similarly. Dissolution of the β-phase occurs by decomposition of β-Al5FeSi into Al6Fe and Si particles. While the fragmentation and dissolution of the β-phase is associated with the formation of dimple ruptured surfaces, however, a large proportion of the sample failure occurs by cleavage mode due to persistence of the largest β-phase needles observed in the structure even after solution treatment.
- 29 November 1999
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 12 (3) , 145-160
Fragmentation and dissolution of β-Al5FeSi phase during solution heat treatment of Al-13wt%Si-Fe alloys
The dissolution of the platelet/needle-like/β-Al5FeSi phase in unmodified and Sr-modified Al-12wt% Si-0.35 wt% Mg alloys was studied, using three levels of iron viz., 0.5, 1.0, and 1.5%. The alloys were cast in the form of tensile test bars (dendrite arm spacing ∼22 μm) using a Stahl permanent mould (type ASTM B-108). The test bars were solution heat-treated at 540 °C for times up to 200 h. The results indicate that a sufficiently high concentration of Sr (∼350 ppm) breaks down the β-needles into small, thin fragments through (a) splitting of the needles into two halves, and (b) fragmentation due to Si rejection. Minimal β-needle lengths are achieved after 30 h and 10 h for the unmodified and Sr-modified alloys, respectively. The fragmentation process results in stabilising the alloy tensile properties during the period of solution treatment, in that not much variation in the tensile parameters is observed up to 100 h at 540 °C. In the Sr-modified alloys, the YS levels are 50 MPa higher than those obtained from the unmodified alloys treated similarly. Dissolution of the β-phase occurs by decomposition of β-Al5FeSi into Al6Fe and Si particles. While the fragmentation and dissolution of the β-phase is associated with the formation of dimple ruptured surfaces, however, a large proportion of the sample failure occurs by cleavage mode due to persistence of the largest β-phase needles observed in the structure even after solution treatment.
- 1 July 1999
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 12 (1) , 49-65
Measurements of oxide films in Al-(6–17) wt%Si foundry alloys using the Qualiflash filtration technique
The Qualiflash technique was used to assess the melt cleanliness of Al-Si foundry alloys. This is a simple filtration technique where the melt cleanliness is gauged by the number of steps covered by the liquid metal that filters through into a step-like ingot mould placed underneath the filter. The present work was performed on A356 and A390 aluminum foundry alloys. The main objectives were to validate the reliability of the Qualiflash technique in measuring the oxide content, and to determine the role of grain-refining and Si-eutectic modification agents in relation to oxide formation. The results indicate that Qualiflash is a quick and simple technique to determine the concentration of aluminum oxides (films and massive particles), as well as other oxides, i.e. MgO, MgAl2O4, in terms of the number of ingot steps of filtered metal obtained. Grain-refining or modification agents themselves do not create oxides. However, the method of their introduction into the molten metal contributes to oxide formation. The number of ingot steps varies linearly with the alloy melt temperature. The slope is strongly related to the amount of oxide films that exist in the liquid metal prior to filtration. Such a relationship is expressed in terms of the Quality Temperature Index (QTI). The effect of oxide concentration on the QTI was investigated in detail for the two alloys studied. The results show that the relationship between the amount of oxides and the number of ingot steps is exponential, with a fitness coefficient of the order of 0.87.
- 1 July 1999
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 12 (1) , 49-65
Measurements of oxide films in Al-(6–17) wt%Si foundry alloys using the Qualiflash filtration technique
The Qualiflash technique was used to assess the melt cleanliness of Al-Si foundry alloys. This is a simple filtration technique where the melt cleanliness is gauged by the number of steps covered by the liquid metal that filters through into a step-like ingot mould placed underneath the filter. The present work was performed on A356 and A390 aluminum foundry alloys. The main objectives were to validate the reliability of the Qualiflash technique in measuring the oxide content, and to determine the role of grain-refining and Si-eutectic modification agents in relation to oxide formation. The results indicate that Qualiflash is a quick and simple technique to determine the concentration of aluminum oxides (films and massive particles), as well as other oxides, i.e. MgO, MgAl2O4, in terms of the number of ingot steps of filtered metal obtained. Grain-refining or modification agents themselves do not create oxides. However, the method of their introduction into the molten metal contributes to oxide formation. The number of ingot steps varies linearly with the alloy melt temperature. The slope is strongly related to the amount of oxide films that exist in the liquid metal prior to filtration. Such a relationship is expressed in terms of the Quality Temperature Index (QTI). The effect of oxide concentration on the QTI was investigated in detail for the two alloys studied. The results show that the relationship between the amount of oxides and the number of ingot steps is exponential, with a fitness coefficient of the order of 0.87.
- 29 November 1997
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 10 (3) , 147-157
Modification of iron intermetallics by magnesium and strontium in Al-Si alloys
The present study was carried out using three alloys viz., Al-0.05wt% Si-0.1 wt% Fe (1XXX alloy), Al-6.5 wt% Si-3.5wt% Cu-0.5wt% Fe (A319.2 primary alloy), and Al-6.5 wt% Si-3.5 wt% Cu-0.9 wt% Fe-0.34 wt% Mn (A319.1 secondary alloy). The alloy ingots were cut into smaller pieces, melted at 750°C in a SiC crucible and poured into a graphite mould preheated at 600°C. Prior to pouring, measured amounts of Mg, Sr or (Mg + Sr) were added to the molten alloys. Melts thus cast into the graphite mould produced cylindrical ingots of 60 mm diameter and ∼84 mm length. The results show that addition of Mg to 1XXX alloys promotes the first peritectic reaction in this system, leading to precipitation of the a- Al8Fe2Si Chinese script phase in rounded form caused by the reduction in surface energy. Modification of an 1XXX alloy (Fe/Si > 2) with Sr leads to a refinement of the dendrite arm spacing of the α-Al8Fe2Si Chinese script phase (from ∼3-5μm to ∼0.1–0.3μm). Addition of Mg to 319 type alloys transforms a large proportion of the β-Al5FeSi needles into the Al8Mg3FeSi6 compacted Chinese script phase, whereas Sr tends to dissolve the β-needles in the aluminum matrix without transformation into any other type of intermetallic.
- 29 November 1997
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 10 (3) , 147-157
Modification of iron intermetallics by magnesium and strontium in Al-Si alloys
The present study was carried out using three alloys viz., Al-0.05wt% Si-0.1 wt% Fe (1XXX alloy), Al-6.5 wt% Si-3.5wt% Cu-0.5wt% Fe (A319.2 primary alloy), and Al-6.5 wt% Si-3.5 wt% Cu-0.9 wt% Fe-0.34 wt% Mn (A319.1 secondary alloy). The alloy ingots were cut into smaller pieces, melted at 750°C in a SiC crucible and poured into a graphite mould preheated at 600°C. Prior to pouring, measured amounts of Mg, Sr or (Mg + Sr) were added to the molten alloys. Melts thus cast into the graphite mould produced cylindrical ingots of 60 mm diameter and ∼84 mm length. The results show that addition of Mg to 1XXX alloys promotes the first peritectic reaction in this system, leading to precipitation of the a- Al8Fe2Si Chinese script phase in rounded form caused by the reduction in surface energy. Modification of an 1XXX alloy (Fe/Si > 2) with Sr leads to a refinement of the dendrite arm spacing of the α-Al8Fe2Si Chinese script phase (from ∼3-5μm to ∼0.1–0.3μm). Addition of Mg to 319 type alloys transforms a large proportion of the β-Al5FeSi needles into the Al8Mg3FeSi6 compacted Chinese script phase, whereas Sr tends to dissolve the β-needles in the aluminum matrix without transformation into any other type of intermetallic.
- 1 September 1997
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 10 (2) , 67-78
Effect of Mg content on the dimensional stability and tensile properties of heat treated Al-Si-Cu (319) type alloys
The present study was performed on A319.2 aluminum alloy containing 6.2% Si, 3.46% Cu, 0.35% Fe, 0.1% Mg. Small amounts of additives were added to the molten metal as follows: 0.5% Mg, (0.5%Mg + 0.03% Sr), (0.5%Mg + 0.03% Sr + 0.02% TiB2). The fluidity of the molten metal as a function of temperature in the range 620–740 °C was measured using the Ragone testing technique. Two solution treatments were applied to test bars prepared from these alloy compositions: 6–8 h at 470 °C, and 6–8 h at 505 °C. In both cases, the test bars were quenched in hot water (60 °C), followed by immediate ageing for 5 h at 180 °C. The results reveal that Sr slightly improves the fluidity of the molten metal (∼12%) at 720 °C. The addition of Mg leads to a noticeable increase in the alloy length (∼2%) when the solution temperature is above 500 °C. At this temperature, incipient melting of Al5Mg8Si6Cu2 and Al2Cu phase particles located at the grain boundaries was significant. Ageing at 180 °C contributes significantly to the alloy strength without much change in the dimension. The magnitude of the increase in alloy strength is strongly related to the solution temperature. Solution treatment for 8–10 h at 500 °C may be recommended.
- 1 September 1997
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 10 (2) , 67-78
Effect of Mg content on the dimensional stability and tensile properties of heat treated Al-Si-Cu (319) type alloys
The present study was performed on A319.2 aluminum alloy containing 6.2% Si, 3.46% Cu, 0.35% Fe, 0.1% Mg. Small amounts of additives were added to the molten metal as follows: 0.5% Mg, (0.5%Mg + 0.03% Sr), (0.5%Mg + 0.03% Sr + 0.02% TiB2). The fluidity of the molten metal as a function of temperature in the range 620–740 °C was measured using the Ragone testing technique. Two solution treatments were applied to test bars prepared from these alloy compositions: 6–8 h at 470 °C, and 6–8 h at 505 °C. In both cases, the test bars were quenched in hot water (60 °C), followed by immediate ageing for 5 h at 180 °C. The results reveal that Sr slightly improves the fluidity of the molten metal (∼12%) at 720 °C. The addition of Mg leads to a noticeable increase in the alloy length (∼2%) when the solution temperature is above 500 °C. At this temperature, incipient melting of Al5Mg8Si6Cu2 and Al2Cu phase particles located at the grain boundaries was significant. Ageing at 180 °C contributes significantly to the alloy strength without much change in the dimension. The magnitude of the increase in alloy strength is strongly related to the solution temperature. Solution treatment for 8–10 h at 500 °C may be recommended.