Zhongming Ren has a total of 28 co-authors. Here are the top co-authors by number of shared publications:
Weili Ren
4 shared publicationsKang Deng
3 shared publicationsYunbo Zhong
3 shared publicationsChuanjun Li
2 shared publicationsJian-Bo Yu
2 shared publicationsJianbo Yu
Shanghai Univ, Dept Mat Sci & Engn, Shanghai Enhanced Lab Ferromet, Shanghai 200072, Peoples R China
2 shared publications
Latest Publications
- 7 June 2018
- Published by DEStech Publications in DEStech Transactions on Computer Science and Engineering
- No. icmsa
Study on the Liquid Metal Flow Field in Narrow-Side-Patter-Mold of Slab Continuous Casting
The flow pattern and velocity distribution of liquid metal in the Narrow-Side-Patter-Mold (NSP-Mold) have been investigated with a mercury model as analogue to molten steel in the continuous casting. The Ultrasonic Doppler Velocimeter (UDV) has measured the velocity under various magnetic distribution and flux density. The impingement intensity of liquid metal to mold narrow wall have been calculated based on the measured data, and the influence of magnetic flux density on the liquid metal flow in the mold has been analyzed. The results show that with narrow-side-patter magnet and increase of the magnetic field, the surface of the melt gets weak and the free surface fluctuation is suppressed, the impingement intensity of liquid metal to mold narrow wall gets weak, impacting depth becomes shallow and a plug flow can be rapidly formed.
- 7 June 2018
- Published by DEStech Publications in DEStech Transactions on Computer Science and Engineering
- No. icmsa
Study on the Liquid Metal Flow Field in Narrow-Side-Patter-Mold of Slab Continuous Casting
The flow pattern and velocity distribution of liquid metal in the Narrow-Side-Patter-Mold (NSP-Mold) have been investigated with a mercury model as analogue to molten steel in the continuous casting. The Ultrasonic Doppler Velocimeter (UDV) has measured the velocity under various magnetic distribution and flux density. The impingement intensity of liquid metal to mold narrow wall have been calculated based on the measured data, and the influence of magnetic flux density on the liquid metal flow in the mold has been analyzed. The results show that with narrow-side-patter magnet and increase of the magnetic field, the surface of the melt gets weak and the free surface fluctuation is suppressed, the impingement intensity of liquid metal to mold narrow wall gets weak, impacting depth becomes shallow and a plug flow can be rapidly formed.
- Open Access
- 1 January 2015
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 30 (2) , 147-152
Preparing Porous Si-based Ceramic Core Using Thermosetting Silicon Resin Injection Method
The porous Si-based ceramic core was prepared using injection method, where quartz glass powders were used as original materials and thermosetting silicon resin was used as plasticizer. The effect of sintering temperature and holding time on the properties of the samples were examined. It was found that the process of devitrification was accelerated with the increase of sintering temperature while the glass phase transforms into cristobalite gradually. When sintering temperature was at 1250℃, the amount of cristobalite increased with the extension of holding time. Linear shrinkage rate and weight loss of the samples slightly increased with the increase of sintering temperature. But the holding time showed less effect on linear shrinkage rate and weight loss of the samples. In fact, the weight loss of the sample was mainly caused by decomposition of silicon resin. The sample sintered at 1250 for ℃ 10 h showed linear shrinkage of 0.93%, the porosity of 32.8% and bending strength of 9.08 MPa.
- 1 January 2015
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 30 (2) , 147-152
Open AccessPreparing Porous Si-based Ceramic Core Using Thermosetting Silicon Resin Injection Method
The porous Si-based ceramic core was prepared using injection method, where quartz glass powders were used as original materials and thermosetting silicon resin was used as plasticizer. The effect of sintering temperature and holding time on the properties of the samples were examined. It was found that the process of devitrification was accelerated with the increase of sintering temperature while the glass phase transforms into cristobalite gradually. When sintering temperature was at 1250℃, the amount of cristobalite increased with the extension of holding time. Linear shrinkage rate and weight loss of the samples slightly increased with the increase of sintering temperature. But the holding time showed less effect on linear shrinkage rate and weight loss of the samples. In fact, the weight loss of the sample was mainly caused by decomposition of silicon resin. The sample sintered at 1250 for ℃ 10 h showed linear shrinkage of 0.93%, the porosity of 32.8% and bending strength of 9.08 MPa.
- 20 August 2012
- Published by China Science Publishing & Media Ltd. in Journal of Inorganic Materials
- Vol. 27 (8) , 807-812
Microstructure and Mechanical Performance of Silicon Nitride Ceramics with Seeds Addition
With Y2O3:Al2O3 of different weight ratios as sintering additives and 3wt% β-Si3N4 seeds addition, silicon nitride ceramics were prepared by gas pressure sintering. The phase composition, density, microstructure, room temperature as well as elevated temperature mechanical properties were investigated. The experimental results indicated that the α→β phase transformation of silicon nitride would be finished at 1800¡䟦or 2 h, and the densities of all specimens were over 97% of theoretical density. Compared with the specimen without seeds addition, the room temperature bending strength, the elevated temperature flexural strength at 1200¡䟡nd the fracture toughness of the specimen with 6wt%Y2O3-4.5wt%Al2O3 and 3wt% β-Si3N4 seeds addition can be improved by 20%, 16% and 8%, respectively
- 20 August 2012
- Published by China Science Publishing & Media Ltd. in Journal of Inorganic Materials
- Vol. 27 (8) , 807-812
Microstructure and Mechanical Performance of Silicon Nitride Ceramics with Seeds Addition
With Y2O3:Al2O3 of different weight ratios as sintering additives and 3wt% β-Si3N4 seeds addition, silicon nitride ceramics were prepared by gas pressure sintering. The phase composition, density, microstructure, room temperature as well as elevated temperature mechanical properties were investigated. The experimental results indicated that the α→β phase transformation of silicon nitride would be finished at 1800¡䟦or 2 h, and the densities of all specimens were over 97% of theoretical density. Compared with the specimen without seeds addition, the room temperature bending strength, the elevated temperature flexural strength at 1200¡䟡nd the fracture toughness of the specimen with 6wt%Y2O3-4.5wt%Al2O3 and 3wt% β-Si3N4 seeds addition can be improved by 20%, 16% and 8%, respectively
- 11 May 2012
- Published by China Science Publishing & Media Ltd. in ACTA METALLURGICA SINICA
- Vol. 48 (5) , 629-635
EFFECT OF LONGITUDINAL MAGNETIC FIELD ON THE MICROSTRUCTURE OF DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ417G WITH DIFFERENT SIZES
- 11 May 2012
- Published by China Science Publishing & Media Ltd. in ACTA METALLURGICA SINICA
- Vol. 48 (5) , 629-635
EFFECT OF LONGITUDINAL MAGNETIC FIELD ON THE MICROSTRUCTURE OF DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ417G WITH DIFFERENT SIZES
- 6 March 2012
- Published by China Science Publishing & Media Ltd. in Journal of Inorganic Materials
- Vol. 27 (3) , 239-244
Fabrication and Properties of Porous Alumina-based Ceramic Core
Considering the difficulty of sintering and leachability of alumina―based ceramic core, different contents of silica were added to the specimens. The porous alumina―based ceramic core was prepared using the dry pressing processes. The effect of different contents of silica, sintering temperature and sintering time on the properties of the alumina―based ceramic core were investigated. The results indicated that the linear shrinkages of the specimens sintered at 1500¡䟡nd 1600¡䟦or 2 h were nearly the same. When the sample was sintered at 1700¡䟦or 2 h, the bending strength was decreased and the porosity was increased due to the evaporation of SiO2. The shrinkage, bending strength, porosity and bulk―density of the specimens sintered at 1500¡䟷ere invariable when the holding time exceeded 4 h. The sample sintered at 1500¡䟦or 2 h had linear shrinkage of 1.1%, bending strength of 63 MPa, the porosity of 35.5% and bulk―density of 2.29 g/cm3, which was hopeful to be the core candidate materials in high temperature application
- 6 March 2012
- Published by China Science Publishing & Media Ltd. in Journal of Inorganic Materials
- Vol. 27 (3) , 239-244
Fabrication and Properties of Porous Alumina-based Ceramic Core
Considering the difficulty of sintering and leachability of alumina―based ceramic core, different contents of silica were added to the specimens. The porous alumina―based ceramic core was prepared using the dry pressing processes. The effect of different contents of silica, sintering temperature and sintering time on the properties of the alumina―based ceramic core were investigated. The results indicated that the linear shrinkages of the specimens sintered at 1500¡䟡nd 1600¡䟦or 2 h were nearly the same. When the sample was sintered at 1700¡䟦or 2 h, the bending strength was decreased and the porosity was increased due to the evaporation of SiO2. The shrinkage, bending strength, porosity and bulk―density of the specimens sintered at 1500¡䟷ere invariable when the holding time exceeded 4 h. The sample sintered at 1500¡䟦or 2 h had linear shrinkage of 1.1%, bending strength of 63 MPa, the porosity of 35.5% and bulk―density of 2.29 g/cm3, which was hopeful to be the core candidate materials in high temperature application
- 1 January 2010
- Published by The Electromagnetics Academy in Progress In Electromagnetics Research Letters
- Vol. 18, 71-84
NUCLEATION AND GROWTH BEHAVIORS OF PRIMARY PHASE IN AL-CU HYPEREUTECTIC ALLOY IN HIGH MAGNETIC FIELDS
- 1 January 2010
- Published by The Electromagnetics Academy in Progress In Electromagnetics Research Letters
- Vol. 18, 71-84
NUCLEATION AND GROWTH BEHAVIORS OF PRIMARY PHASE IN AL-CU HYPEREUTECTIC ALLOY IN HIGH MAGNETIC FIELDS
- 1 January 2009
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 49 (8) , 1150-1155
Refining Mechanism of Pure Aluminum under Local Electromagnetic Vibration
- 1 January 2009
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 49 (8) , 1150-1155
Refining Mechanism of Pure Aluminum under Local Electromagnetic Vibration
- Open Access
- 1 April 2008
- Published by Taylor & Francis in Science and Technology of Advanced Materials
- Vol. 9 (2) , 024202
Effects of a high-gradient magnetic field on the migratory behavior of primary crystal silicon in hypereutectic Al–Si alloy
The migration of primary Si grains during the solidification of Al-18 wt%Si alloy under a high-gradient magnetic field has been investigated experimentally. It was found that under a gradient magnetic field, the primary Si grains migrated toward one end of the specimen, forming a Si-rich layer, and the thickness of the Si-rich layer increased with increasing magnetic flux density. No movement of Si grains was apparent under a magnetic field below 2.3 T. For magnetic fields above 6.6 T, however, the thickness of the Si-rich layer was almost constant. It was shown that the static field also played a role in impeding the movement of the grains. The primary Si grains were refined in the Si layer, even though the primary silicon grains were very dense. The effect of the magnetic flux density on the migratory behavior is discussed.
- 1 April 2008
- Published by Taylor & Francis in Science and Technology of Advanced Materials
- Vol. 9 (2) , 024202
Open AccessEffects of a high-gradient magnetic field on the migratory behavior of primary crystal silicon in hypereutectic Al–Si alloy
The migration of primary Si grains during the solidification of Al-18 wt%Si alloy under a high-gradient magnetic field has been investigated experimentally. It was found that under a gradient magnetic field, the primary Si grains migrated toward one end of the specimen, forming a Si-rich layer, and the thickness of the Si-rich layer increased with increasing magnetic flux density. No movement of Si grains was apparent under a magnetic field below 2.3 T. For magnetic fields above 6.6 T, however, the thickness of the Si-rich layer was almost constant. It was shown that the static field also played a role in impeding the movement of the grains. The primary Si grains were refined in the Si layer, even though the primary silicon grains were very dense. The effect of the magnetic flux density on the migratory behavior is discussed.
- 1 May 2007
- Published by Wiley in Steel Research International
- Vol. 78 (5) , 371-372
Electromagnetic Processing of Metals: Editorial by our Guest Editors Prof. Dr. Zhongming Ren and Dr. Gunter Gerbeth
- 1 May 2007
- Published by Wiley in Steel Research International
- Vol. 78 (5) , 371-372
Electromagnetic Processing of Metals: Editorial by our Guest Editors Prof. Dr. Zhongming Ren and Dr. Gunter Gerbeth