NVNitesh Vashishtha

Nitesh Vashishtha

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Nitesh Vashishtha has a total of 28 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Tribological Performance Comparison of Lubricating Greases for Electric Vehicle Bearings

    by Deepika Shekhawat, Ayush Jain, Nitesh Vashishtha, Arendra Pal Singh, Rahul Kumar

    EV motors and machine elements operate at higher speeds, generate significant heat and noise (vibration), and subject lubricants (bearings) to multiple degrading factors, requiring thermal stability, wear protection, mitigating wear mechanisms like pitting and scuffing, and low electrical conductivity to prevent arcing damage to bearings. This study evaluates the tribological performance of four types of greases—PUEs, PUPao, PUEth (polyurea-based), and LiPAO (lithium–calcium complex-based)—to determine their suitability for electric motor bearings. Key performance metrics include tribological properties, electrical resistivity, leakage, bearing noise, and wear behavior. A four-ball wear test ranks the greases by scar diameter as PUPao < PUEs < PUEth < LiPAO, while the coefficient of friction is observed in the range of 0.15–0.18, with LiPAO exhibiting the lowest friction. Electrical resistivity tests reveal that PUEs grease has the lowest resistivity. Electrical leakage tests, conducted with a voltage differential across bearings, assess pitting damage, with PUEth and LiPAO showing evidence of surface pitting. Optical microscopy and scanning electron microscopy analysis is carried out to examine the pitting. In bearing noise tests, PUEs demonstrates the lowest noise levels, whereas LiPAO produces the highest. Visual and microscopic examination of the greases further characterizes their lubricating properties. Based on overall performance, the greases are ranked in suitability for electric motor applications as PUEs > PUPao > PUEth > LiPAO. The findings highlight the critical need for selecting appropriate grease formulations to ensure optimal bearing performance under varying operational conditions.


  • Effect of WC/C coated rolling element to improve bearing life

    by Ayush Jain, Nitesh Vashishtha, Kannan P. Rajesh

    The research is aimed to understand the effect of WC/C coating on the bearing rolling elements to improve fatigue life in surface distress conditions. The 1–1.5 microns optimized coating thickness was deposited on the steel substrate using the PVD process. The coating's physical and chemical properties were analysed by X-ray diffraction, scanning electron microscope, contact profilometer, nanoindentation hardness, and micro scratch indenter. The wear properties were compared on a ball-on-disc tribometer with and without a coated specimen. The bearing tests were performed in contaminated and clean lubrication conditions to prove the coating's effect on bearing life in surface distress conditions. Results show that coated roller bearings perform at least two times that of the standard bearing. The overall benefit of less friction and wear resistance was due to the polishing action and coating transfer mechanism of multi-layer coating which increases oil film thickness between contacts and hence improve bearing life.


  • Evaluation of hybrid sol-gel alumina coating for electrical resistance applications

    by Shubham Vishvakarma, Rajesh Kannan, Nitesh Vashishtha, Arendra Pal Singh

    In an electric motor, bearing plays a vital role in the performance and reliability which fails frequently due to electrical pitting. To avoid this issue, the bearing can be coated with insulation material. In this present investigation, hybrid sol-gel coating was carried out on bearing steel by dip-coating method. The hybrid sol-gel was prepared using aluminium isopropoxide and calcined alumina powder. The ratio of Sol-Gel to calcined alumina and thickness of the coating was optimized to attain a crack-free surface coating. The crack behaviour was studied. The characterization of Hybrid Sol-Gel was carried out using Fourier-transform infrared spectroscopy and the surface morphology was observed using an optical microscope. The electrical resistance of the coating was measured using an insulation resistance tester. The crack-free surface coating of 40 microns was achieved at a low sol-gel to calcined alumina ratio. The electrical resistance of the coating is found suitable for bearing application. The thermodynamically stable hybrid sol-gel i.e., α alumina -ϒ alumina coating surface is proposed for electrical insulation coating.


  • Friction energy map for sliding wear of Al 2 O 3 -TiO 2 and Cr 2 O 3 -TiO 2 coatings

    by Sanket Anil Mehar, Sanjay G Sapate, Nitesh Vashishtha, Pranay Bagde, Avishkar B Rathod

    The present study deals with the development of friction energy map for plasma sprayed Al 2 O 3 -TiO 2 and Cr 2 O 3 -TiO 2 coatings. Al 2 O 3 -TiO 2 and Cr 2 O 3 -TiO 2 coatings were deposited by atmospheric plasma spray technique. The structural and mechanical properties of coatings were studied using Scanning Electron Microscopy (SEM), x-ray Diffraction (XRD) and Vickers macro and micro hardness test. Sliding wear tests were performed on coated specimens over a range of sliding speed and load using pin on disc test apparatus. The analysis of worn surface and wear debris was carried by SEM, XRD and Raman Spectroscopy. Cr 2 O 3 -TiO 2 coating showed higher hardness and elastic modulus and relatively lower fracture toughness than Al 2 O 3 -TiO 2 coating. Al 2 O 3 -TiO 2 coatings exhibited 1.8 times better wear resistance and 11%–30% lower friction coefficient, as compared to Cr 2 O 3 -TiO 2 coating, depending upon the wear test conditions. The reduction in friction coefficient and wear rate at higher sliding speed was due to the formation of tribofilms on worn surface. A good correlation was observed between friction energy and contact severity; which incorporates mechanical properties of coatings. Friction energy map was used to rationalize wear rates of Al 2 O 3 -TiO 2 and Cr 2 O 3 -TiO 2 coatings, for the identification of various wear regimes and failure modes of the coating.


  • Microstructure evolution and mechanical properties of Al 2 O 3 -40%TiO 2 coating by Hybrid-Low Velocity OxyFuel process

    by Satish Tailor, Nitesh Vashishtha, Ankur Modi, S C Modi

    This study presents a new thermal spray coating manufacturing process to deposit high performance ceramic coatings named ‘Hybrid-LVOF’ (Low Velocity OxyFuel). By this process, both thin and thick ceramic coatings can be deposited on metallic or ceramic substrates. In this work, the microstructural and mechanical properties of H-LVOF sprayed Al 2 O 3 -TiO 2 coatings were compared with plasma sprayed (PS) Al 2 O 3 -TiO 2 coatings; with the additional condition that typical bond coat was not applied. The α -Al 2 O 3 and γ -Al 2 O 3 contents have been quantified in the as-sprayed coatings. As-sprayed Hybrid-LVOF coatings show better properties than conventional plasma-sprayed coatings including better fracture toughness. Noise and radiation levels are very low in the hybrid-LVOF process. Furthermore, a 50% reduction in overall production cost was achieved. H-LVOF could be therefore a possible alternative to a conventional plasma spray process.


  • Open Access

    One-step fabrication of thermal sprayed polymer coating on metals

    by Satish Tailor, Nitesh Vashishtha, Ankur Modi, S C Modi

    This study presents the polymer coating onto metal-based structures by the thermal spray process. The deposition of polymers onto metal substrate has been developed by controlling the temperature in conventional thermal spray process. Properties of final polymer coating are investigated, such as microstructural, crystallization, mechanical, friction and corrosion properties. The objective of this is to deposit a polymer coating by controlling temperature in conventional thermal spray process and evaluate the coating properties for specific applications such as polymer coating on vacuum pump screws as abrasion resistant coating and on Kevlar fabric to provide strength for bullet proof soft armor vest for defense application. This study reports that as-sprayed coating can be used without post processing like annealing and filing. As-sprayed PEEK coating has a considerable hardness and adhesion strength found to be 17 ± 5 HV, 16 ± 3.0 MPa, respectively. However, post annealing treatment may introduce further improvements in wear and friction resistant properties of the final polymer coating system. The microhardness value has increased from 17 HV to 29 HV in average. The annealed semi-crystalline coatings exhibit the slightly lower friction coefficient than amorphous coating (as-sprayed); 0.31 in average versus 0.36. The wear rate of annealed coating is lower than the as-sprayed coating, decreased by approx 50% (10.5 in average versus 20.5 × 10− 6 mm3 N−1 m−1). The PEEK coating protects the base metal against corrosion and life against corrosion is found to be 25.4 μm.y−1; 81.75% efficiency in reduction of corrosion with respect to steel exposed in 5% NaCl solution.


  • Tribological properties of HVOF sprayed WC-Cr3C2-Ni coating

    by Ayush Kumar Goyal, S G Sapate, S Mehar, N Vashishtha, P Bagde, A Rathod


  • Open Access

    Effect of Experimental Parameters on Wear Response of Thermally Sprayed Carbide Based Coatings

    by Nitesh Vashishtha, Sanjay Sapate

    Friction and abrasive wear response of WC-12 Co and Cr3C2-25 NiCr coatings was studied. Abrasive wear experiments were conducted with SiC abrasive particles with varying load and sliding speeds. The results were analyzed using SEM, XRD and XPS observations of worn surfaces, wear debris and worn out abrasive paper. Friction coefficient diminished with rise in sliding speed and increased for increase in load while wear rates decreased for increasing sliding speed for both coatings. WC-12 Co coating had better wear resistance than Cr3C2-25 NiCr coating while Cr3C2-25 NiCr coating displayed lower friction coefficient. The variation in wear rate and friction response of coatings was due to combined effects of adhesion, abrasion and tribo oxidation effects. The composition of tribo films was strongly influenced by load and sliding velocity and altered friction and wear response of the coatings.