Zheng Lv
Zheng Lv has a total of 47 co-authors. Here are the top co-authors by number of shared publications:
Wentao Tang
3 shared publicationsXueping Ren
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, People’s Republic of China
3 shared publicationsC. Mao
State Key Laboratory of Advanced Materials for Intelligent Sensing, Beijing 100088, China
2 shared publications- Changhui Mao
State Key Laboratory of Advanced Materials for Intelligent Sensing, GRINM Group Co., Ltd., Beijing 100088, China
2 shared publications He Dai
State Key Laboratory of Advanced Materials for Intelligent Sensing, GRINM Group Co., Ltd., Beijing, China
2 shared publicationsJ. Wang
Advanced Electronic Materials Institute, GRIMAT Engineering Institute Co. Ltd, Beijing 101407, China
2 shared publications
Latest Publications
- 17 March 2026
- Published by Springer Nature in Journal of Materials Science
- Vol. 61 (18) , 12764-12780
Synergizing composition optimization and rapid powder rolling in Al–W–Ce composites: a strategy for optimized microstructure and mechanical performance
- 17 March 2026
- Published by Springer Nature in Journal of Materials Science
- Vol. 61 (18) , 12764-12780
Synergizing composition optimization and rapid powder rolling in Al–W–Ce composites: a strategy for optimized microstructure and mechanical performance
- Open Access
- 19 September 2025
- Published by IOP Publishing in Nuclear Fusion
- Vol. 65 (10) , 106026
Microstructure, mechanical properties and oxidation resistance of bulk W-B-Fe-Cr for fusion shielding
In this work, a bulk W-B-Fe-Cr shielding material with lower boron content (9.6 at.%) has been fabricated by hot isostatic pressing (HIP) for potential engineering applications in compact fusion reactors. The microstructure, mechanical properties and oxidation resistance of W-B-Fe-Cr were systematically investigated. By HIP sintering at 1250 °C, the uniform, dense and crack-free microstructure of W-B-Fe-Cr was obtained. The results of the phase analysis show that W-B-Fe-Cr is mainly composed of W, (Fe,Cr)WB and (Fe,Cr)7W6. In the range of 500 °C–1000 °C, the low-boron W-B-Fe-Cr possesses higher flexural strength than the reported high-boron (16 ∼ 30 at.%) W2B-W owing to its W-rich composition, which can more effectively exploit both the toughness of the W phase and the hardening effect of the boride phase. The results show that although the neutron shielding property is degraded by the reduction of the boron content, conversly the strength is enhanced. Therefore, for W-B based shielding reactive sintered borides (RSBs), prudent balancing between shielding capability and mechanical performance is essential for the design of the boron content. To evaluate the oxidation resistance of W-B-Fe-Cr, the bare specimen and its Si-coated counterpart were subjected to oxidation tests in air at 1000 °C. The underlying WSi2-(FeWCr)Si x dual-phase reaction layer was formed by coating Si, which was transformed into the dense SiO2 protective film at high temperature to effectively prevent exposure of the substrate. The scientific discoveries and constraints of the low-boron W-B-Fe-Cr research are systematically summarized, and the prospective strategies for mechanical performance optimization in high-boron derivatives are reviewed.
- 19 September 2025
- Published by IOP Publishing in Nuclear Fusion
- Vol. 65 (10) , 106026
Open AccessMicrostructure, mechanical properties and oxidation resistance of bulk W-B-Fe-Cr for fusion shielding
In this work, a bulk W-B-Fe-Cr shielding material with lower boron content (9.6 at.%) has been fabricated by hot isostatic pressing (HIP) for potential engineering applications in compact fusion reactors. The microstructure, mechanical properties and oxidation resistance of W-B-Fe-Cr were systematically investigated. By HIP sintering at 1250 °C, the uniform, dense and crack-free microstructure of W-B-Fe-Cr was obtained. The results of the phase analysis show that W-B-Fe-Cr is mainly composed of W, (Fe,Cr)WB and (Fe,Cr)7W6. In the range of 500 °C–1000 °C, the low-boron W-B-Fe-Cr possesses higher flexural strength than the reported high-boron (16 ∼ 30 at.%) W2B-W owing to its W-rich composition, which can more effectively exploit both the toughness of the W phase and the hardening effect of the boride phase. The results show that although the neutron shielding property is degraded by the reduction of the boron content, conversly the strength is enhanced. Therefore, for W-B based shielding reactive sintered borides (RSBs), prudent balancing between shielding capability and mechanical performance is essential for the design of the boron content. To evaluate the oxidation resistance of W-B-Fe-Cr, the bare specimen and its Si-coated counterpart were subjected to oxidation tests in air at 1000 °C. The underlying WSi2-(FeWCr)Si x dual-phase reaction layer was formed by coating Si, which was transformed into the dense SiO2 protective film at high temperature to effectively prevent exposure of the substrate. The scientific discoveries and constraints of the low-boron W-B-Fe-Cr research are systematically summarized, and the prospective strategies for mechanical performance optimization in high-boron derivatives are reviewed.
- 28 February 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (11) , 10754-10763
Characterization of the Microstructure and High-temperature Mechanical Properties of Ce-modified 2024 Aluminum Alloy
- 28 February 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (11) , 10754-10763
Characterization of the Microstructure and High-temperature Mechanical Properties of Ce-modified 2024 Aluminum Alloy
- Open Access
- 11 July 2024
- Published by Elsevier in Nuclear Materials and Energy
- Vol. 40
Microstructure, mechanical properties and corrosion behavior of W-B-Ni-Fe shielding cermets synthesized by reactive boride sintering
- 11 July 2024
- Published by Elsevier in Nuclear Materials and Energy
- Vol. 40
Open AccessMicrostructure, mechanical properties and corrosion behavior of W-B-Ni-Fe shielding cermets synthesized by reactive boride sintering
- Open Access
Crystallization of Fe-W-B Amorphous Powder Prepared by Gas Atomization
In this work, the effects of master alloy composition and annealing temperature on the amorphization and crystallization behavior of Fe-W-B powders prepared by gas atomization using compacts of Fe, W and B powder mixture were systematically studied. The results show that only the master alloy with high content of W (19.9 at.%) and B (13.6 at.%) of the six alloys studied yielded amorphous Fe-W-B powders. The alloying elements W and B are believed to have a glass-forming ability (GFA)-enhancing effect, which together with the high cooling rate of gas atomization leads to the formation of amorphization. The difference in the average particle size of 3–10 μm for the six atomized powders indicates that the master alloys with different W and B contents have different superheat and melt viscosity at the same atomization temperature. The Fe-W-B amorphous powder is structurally stable within 600 °C and crystallizes from the edge of the particles when the temperature increases to 700 °C, and its crystalline precipitates include α-Fe, FeWB and Fe7W6. The nuclear shielding tests and Monte Carlo N Particle Transport Code (MCNP) calculated results revealed that the Fe-W-B amorphous powder has a much better shielding performance for γ-rays and neutrons than that of iron. This work provides an efficient strategy for fabricating Fe-W-B amorphous powder with promising nuclear shielding potential and sheds light on the crystallization behaviors of this alloy.
Open AccessCrystallization of Fe-W-B Amorphous Powder Prepared by Gas Atomization
In this work, the effects of master alloy composition and annealing temperature on the amorphization and crystallization behavior of Fe-W-B powders prepared by gas atomization using compacts of Fe, W and B powder mixture were systematically studied. The results show that only the master alloy with high content of W (19.9 at.%) and B (13.6 at.%) of the six alloys studied yielded amorphous Fe-W-B powders. The alloying elements W and B are believed to have a glass-forming ability (GFA)-enhancing effect, which together with the high cooling rate of gas atomization leads to the formation of amorphization. The difference in the average particle size of 3–10 μm for the six atomized powders indicates that the master alloys with different W and B contents have different superheat and melt viscosity at the same atomization temperature. The Fe-W-B amorphous powder is structurally stable within 600 °C and crystallizes from the edge of the particles when the temperature increases to 700 °C, and its crystalline precipitates include α-Fe, FeWB and Fe7W6. The nuclear shielding tests and Monte Carlo N Particle Transport Code (MCNP) calculated results revealed that the Fe-W-B amorphous powder has a much better shielding performance for γ-rays and neutrons than that of iron. This work provides an efficient strategy for fabricating Fe-W-B amorphous powder with promising nuclear shielding potential and sheds light on the crystallization behaviors of this alloy.
- Open Access
Evolution of Microstructure, Texture and Mechanical Properties for Multilayered Al Matrix Composites by Accumulative Roll Bonding
Carbon nanotubes (CNTs) reinforced aluminum matrix nanocomposites were fabricated by Accumulative Roll Bonding (ARB). The surface morphologies, mechanical properties, grains texture and orientation of the Al/CNTs nanocomposites were characterized, and the mechanisms and influences of CNTs contents and ARB cycles on the mechanical performance and grain textures of Al/CNTs were investigated and revealed. The strength of the composites rose with increase of the CNTs content, and the ARB cycles showed a 26% improvement when the CNTs content varied from 0 to 1 volume percent (vol.%). The increase in the mass fraction of the carbon nanotubes made the grain distribution in the Al/CNTs nanocomposite samples more diffuse. Besides, the stable texture of the hot rolled crystal grains on the α orientation are constantly turning to {011}< 011> with the mass fraction of the reinforcing phase increased.
Open AccessEvolution of Microstructure, Texture and Mechanical Properties for Multilayered Al Matrix Composites by Accumulative Roll Bonding
Carbon nanotubes (CNTs) reinforced aluminum matrix nanocomposites were fabricated by Accumulative Roll Bonding (ARB). The surface morphologies, mechanical properties, grains texture and orientation of the Al/CNTs nanocomposites were characterized, and the mechanisms and influences of CNTs contents and ARB cycles on the mechanical performance and grain textures of Al/CNTs were investigated and revealed. The strength of the composites rose with increase of the CNTs content, and the ARB cycles showed a 26% improvement when the CNTs content varied from 0 to 1 volume percent (vol.%). The increase in the mass fraction of the carbon nanotubes made the grain distribution in the Al/CNTs nanocomposite samples more diffuse. Besides, the stable texture of the hot rolled crystal grains on the α orientation are constantly turning to {011}< 011> with the mass fraction of the reinforcing phase increased.
- Open Access
Interfacial Microstructure in W/2024Al Composite and Inhibition of W-Al Direct Reaction by CeO2 Doping: Formation and Crystallization of Al-Ce-Cu-W Amorphous Layers
In this work, interfacial microstructure in W/2024Al composite and inhibition of the W-Al direct reaction by CeO2 doping were investigated. The composites were prepared through powder sintering, and after preparation the composites were treated by annealing at 823 K. For the prepared W/2024Al composite, a multi-phase thin layer composed of WAl12 and WAl5 compounds were formed at the interface due to the W-Al direct reaction. While doping CeO2 in the composite, Al-Ce-Cu-W amorphous substituting of W-Al compounds were formed at the interfacial reaction layer. In an annealed state, the composite with CeO2 doping shows a significant inhibitory effect on W-Al compounds, which was attributed to the crystallized layer that evolved from Al-Ce-Cu-W amorphous as an interfacial obstacle. The crystallization product for Al-Ce-Cu-W amorphous layer was identified as bcc-structure Al-Ce-Cu-W phase without any binary/ternary Ce-containing phases. Therefore, by doping CeO2 in W/2024Al composite, W-Al direct reaction was markedly inhibited during both preparation and annealing.
Open AccessInterfacial Microstructure in W/2024Al Composite and Inhibition of W-Al Direct Reaction by CeO2 Doping: Formation and Crystallization of Al-Ce-Cu-W Amorphous Layers
In this work, interfacial microstructure in W/2024Al composite and inhibition of the W-Al direct reaction by CeO2 doping were investigated. The composites were prepared through powder sintering, and after preparation the composites were treated by annealing at 823 K. For the prepared W/2024Al composite, a multi-phase thin layer composed of WAl12 and WAl5 compounds were formed at the interface due to the W-Al direct reaction. While doping CeO2 in the composite, Al-Ce-Cu-W amorphous substituting of W-Al compounds were formed at the interfacial reaction layer. In an annealed state, the composite with CeO2 doping shows a significant inhibitory effect on W-Al compounds, which was attributed to the crystallized layer that evolved from Al-Ce-Cu-W amorphous as an interfacial obstacle. The crystallization product for Al-Ce-Cu-W amorphous layer was identified as bcc-structure Al-Ce-Cu-W phase without any binary/ternary Ce-containing phases. Therefore, by doping CeO2 in W/2024Al composite, W-Al direct reaction was markedly inhibited during both preparation and annealing.
- 1 June 2017
- Published by American Scientific Publishers in Journal of Nanoscience and Nanotechnology
- Vol. 17 (6) , 4022-4031
Application of Accumulative Roll Bonding Process for Manufacturing Mg/2 wt.%CNTs Nanocomposite with Superior Mechanical Properties
In present work, magnesium matrix nanocomposites (MMNC) containing 2 wt.%CNTs were fabricated through accumulative roll bonding (ARB). The microstructure and mechanical properties of Mg/2 wt.%CNTs nanocomposites are reported for various ARB cycles. To evaluate microstructure of the nanocomposites, the field emission scanning electron microscope (FESEM), X-ray diffractometer and transmission electron microscope (TEM) were applied. After fourteen ARB cycles, the nanocomposite showed a homogeneous distribution of reinforcements and significant reduction in average matrix grain size. Meanwhile, the nanocomposite revealed higher percentage of substructured grains and lower intensity of basal texture as compared to monolithic Mg. Mechanical properties were investigated through tensile and microhardness tests. The strength and elastic modulus and microhardness of Mg/2 wt.%CNTs were found to improve significantly from eight ARB cycles and reach maximum values at fourteen ARB cycles. The ultimate tensile strength, yield strength, microhardness and elastic modulus of Mg/2 wt.%CNTs are significantly increased by 17.9%, 64.9%, 93.3% and 89.4% as compared to raw Mg, respectively.
- 1 June 2017
- Published by American Scientific Publishers in Journal of Nanoscience and Nanotechnology
- Vol. 17 (6) , 4022-4031
Application of Accumulative Roll Bonding Process for Manufacturing Mg/2 wt.%CNTs Nanocomposite with Superior Mechanical Properties
In present work, magnesium matrix nanocomposites (MMNC) containing 2 wt.%CNTs were fabricated through accumulative roll bonding (ARB). The microstructure and mechanical properties of Mg/2 wt.%CNTs nanocomposites are reported for various ARB cycles. To evaluate microstructure of the nanocomposites, the field emission scanning electron microscope (FESEM), X-ray diffractometer and transmission electron microscope (TEM) were applied. After fourteen ARB cycles, the nanocomposite showed a homogeneous distribution of reinforcements and significant reduction in average matrix grain size. Meanwhile, the nanocomposite revealed higher percentage of substructured grains and lower intensity of basal texture as compared to monolithic Mg. Mechanical properties were investigated through tensile and microhardness tests. The strength and elastic modulus and microhardness of Mg/2 wt.%CNTs were found to improve significantly from eight ARB cycles and reach maximum values at fourteen ARB cycles. The ultimate tensile strength, yield strength, microhardness and elastic modulus of Mg/2 wt.%CNTs are significantly increased by 17.9%, 64.9%, 93.3% and 89.4% as compared to raw Mg, respectively.
- Open Access
- 6 November 2016
- Published by Wiley in Journal of Nanomaterials
- Vol. 2016, 1-12
Microstructure and Mechanical Properties of Mg/2 wt.%SiCp Nanocomposite Fabricated by ARB Process
Magnesium matrix nanocomposites (MMNC, the same below) containing 2 wt.% nanosized were fabricated through accumulative roll bonding (ARB). The microstructure and mechanical properties of Mg/2 wt.% nanocomposites are reported for various ARB cycles. To evaluate microstructure of the nanocomposites, the field emission scanning electron microscope (FE-SEM), X-ray diffractometer (XRD), and transmission electron microscope (TEM) were applied. After fourteen ARB cycles, the nanocomposite showed a homogeneous distribution of reinforcements and a significant reduction in average matrix grain size. Meanwhile, the nanocomposite revealed a higher percentage of recrystallization and lower intensity of basal texture as compared to monolithic Mg. Mechanical properties were investigated through tensile and microhardness tests. The strength and elastic modulus and microhardness of Mg/2 wt.% were found to be improved significantly from eight ARB cycles and reach maximum values at fourteen ARB cycles. The ultimate tensile strength, yield strength, microhardness, and elastic modulus of Mg/2 wt.% are considerably increased by 17.6%, 61.0%, 72.7%, and 80.8% as compared to raw Mg, respectively.- 6 November 2016
- Published by Wiley in Journal of Nanomaterials
- Vol. 2016, 1-12
Open AccessMicrostructure and Mechanical Properties of Mg/2 wt.%SiCp Nanocomposite Fabricated by ARB Process
Magnesium matrix nanocomposites (MMNC, the same below) containing 2 wt.% nanosized were fabricated through accumulative roll bonding (ARB). The microstructure and mechanical properties of Mg/2 wt.% nanocomposites are reported for various ARB cycles. To evaluate microstructure of the nanocomposites, the field emission scanning electron microscope (FE-SEM), X-ray diffractometer (XRD), and transmission electron microscope (TEM) were applied. After fourteen ARB cycles, the nanocomposite showed a homogeneous distribution of reinforcements and a significant reduction in average matrix grain size. Meanwhile, the nanocomposite revealed a higher percentage of recrystallization and lower intensity of basal texture as compared to monolithic Mg. Mechanical properties were investigated through tensile and microhardness tests. The strength and elastic modulus and microhardness of Mg/2 wt.% were found to be improved significantly from eight ARB cycles and reach maximum values at fourteen ARB cycles. The ultimate tensile strength, yield strength, microhardness, and elastic modulus of Mg/2 wt.% are considerably increased by 17.6%, 61.0%, 72.7%, and 80.8% as compared to raw Mg, respectively.