Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Fabio Scenini has a total of 125 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Influence of Surface Preparation on the High-Temperature Oxidation of Alloy 800HT in Impure Helium

    by Matthew Brayne, James Rafferty, Yahya H. Mozumder, Aya Shin, Marc Chevalier, Mia Maric, Fabio Scenini

    High-temperature oxidation of Alloy 800HT in impure helium can affect structural integrity through grain-boundary-controlled subsurface degradation. This study compared oxidation behaviour at 800°C between a P600-ground surface, containing a deformation-induced ultrafine-grained layer (UFGL), and a deformation-free Oxide Polishing Suspension (OPS)-polished surface representing the bulk microstructure. Grinding accelerated chromia formation, yielding a thin, unprotective, continuous scale. However, the UFGL recrystallised during exposure, generating grain boundaries susceptible to preferential intergranular oxidation (PIO). Both surfaces converged to a long-term degradation mode governed by bulk grain-boundary character, with non-Σ3 boundaries promoting PIO while Σ3 boundaries largely arrested penetration. Bowed grain boundary morphologies were consistent with diffusion-induced grain boundary migration (DIGM) as a plausible PIO precursor, though Ni/Cr solute partitioning was not retained after prolonged homogenisation. These findings demonstrate that surface finish influences oxidation only transiently, whereas long-term environmental degradation, is dictated by the intrinsic grain‐boundary network, with important implications for crack‐initiation susceptibility under stress.

  • Open Access

    The Mechanism of Austenitisation in Low-Alloy Steels Studied In-Situ: Austenite Memory and Autogenous Recrystallisation

    by Mark Taylor, Rhys Thomas, Albert Smith, Grace Fidler, Yahya H. Mozumder, Gabor Ribarik, Tamas Ungar, Christopher Hutchinson, Fabio Scenini, P.B. Prangnell, et al.

    Austenitisation is a mainstay of steel processing and is required to form strong microstructures, e.g., martensite. It is known that austenitisation can proceed by a two-step mechanism, which first involves a 'memory effect' that regenerates the original prior-austenite grains (PAGs), and second a recrystallisation step, which generates a new grain structure. However, the mechanisms of these processes are not fully understood, especially in low-alloy steels. Here, we use in-situ high-temperature electron backscatter diffraction and synchrotron X-ray diffraction to investigate austenitisation in two martensitic low-alloy steels. Both exhibited the memory effect, but only one subsequently recrystallised. The memory effect progressed by the growth of acicular austenite consistent with a mixed displacive/diffusive reaction. Growth of pre-existing retained austenite was unlikely to be responsible for the memory effect, as memory was observed in alloys without measurable retained austenite, and multiple variants of austenite nucleated within a PAG at the transformation start. The growth of the memory variant along martensite-martensite grain boundaries was favoured over other variants. Evidence strongly suggests that the driving force for the recrystallisation step is dominated by the dislocations generated during the transformation itself, and not by those inherited from martensite. The occurrence of recrystallisation is dependent on the competition between dislocation recovery and recrystallisation in memory orientation austenite, which is influenced by an alloy’s austenitisation temperature, and heating rates through austenitisation. This new understanding may enable improved heat treatment practices that exploit the two-step nature of the process to promote improved PAG.

  • Open Access

    Preferential oxidation of martensite in austenitic stainless steel in high-temperature water: Implications for stress corrosion cracking

    by Kudzanai Mukahiwa, M. G. Burke, Fabio Scenini

    The oxidation behaviour of martensitic phases in hydrogen-charged Type 316L austenitic stainless steel exposed to deoxygenated high-temperature water representative of pressurized water reactor (PWR) primary coolant conditions was investigated using a suite of advanced and complementary techniques, including SEM-EDXS, TKD, and STEM-EDX. These characterization techniques enabled detailed analysis of phase transformations and microstructural changes in hydrogen-charged material, as well as characterization of oxide morphology and chemistry. Cathodic hydrogen charging induced extensive transformation of the distorted γ-matrix into body-centred cubic (α’) and hexagonal close-packed (ε) martensitic laths. Subsequent hydrogen outgassing promoted crystallographic cracking along prior austenite {111} planes. Grain orientation was found to influence transformation susceptibility, whereby grains with {001} planes perpendicular to the charging direction exhibited resistance to both martensite formation and crack initiation. Oxidation analysis at 250 °C and 300 °C revealed preferential corrosion of α′ and ε martensite, leading to the formation of a defective, porous chromium-rich spinel inner oxide, while adjacent γ grains remained largely unaffected. These findings elucidate the interplay between martensitic phase and localized oxidation. The new insights offered by these results are discussed in the context of stress corrosion crack mechanisms in high-temperature water environments.

  • Open Access

    Controlling microsegregation–induced phase formation and pitting corrosion in wire-arc additively manufactured precipitation-hardened martensitic stainless steel

    by Y.H. Mozumder, M. Taylor, V. Bongiorno, Y. Lu, J. Wang, S. Williams, P.B. Prangnell, E.J. Pickering, F. Scenini

  • Characterization and Performance Testing of Additively Manufactured Alloy 625 in High-Temperature Water

    by James Hall, Yahya H. Mozumder, Jonathan Duff, Karen Perkins, Tim Watkins, Ed Pickering, Fabio Scenini

    Additive manufacturing (AM) of nickel-based alloys offers design flexibility and reduced lead times for critical components in pressurized water reactors. However, its influence on stress corrosion cracking (SCC) behavior remains poorly understood. This work investigates the microstructural evolution and SCC initiation susceptibility of laser powder bed fusion (LPBF) Alloy 625, with emphasis on the role of hot isostatic pressing (HIP). The as-built LPBF microstructure revealed a columnar dendritic structure with pronounced interdendritic segregation of Nb, Mo, and Ti. HIP treatment effectively homogenized the microstructure, resulting in equiaxed grains containing Nb-enriched grain boundary carbides. Cold work introduced fractured Nb-rich grain boundary carbides and nanoscale cavities, providing a mechanical baseline for distinguishing purely deformation-induced damage from environmentally assisted cracking. Accelerated oxidation tests of HIP-AM samples in hydrogenated steam at 480°C revealed selective degradation of Nb-rich carbides, forming voids along grain boundaries. Slow strain rate tensile (SSRT) tests were conducted on 20% cold-rolled HIP-AM specimens in simulated PWR water (342°C, 30 cc/kg H2). Minimal intergranular SCC (IGSCC) was observed at 4.8% strain, whereas clear IGSCC initiation occurred at 26% strain, indicating high but finite SCC resistance under combined mechanical and environmental loading. These findings highlight that while HIP improves microstructural homogeneity, it introduces grain boundary features susceptible to oxidation-assisted degradation. The results provide critical insights for optimizing postprocessing strategies and assessing the long-term integrity of AM Alloy 625 in high-temperature reactor water.

  • Creep Crack Growth of 316H Stainless Steel in a Simulated Advanced Gas-Cooled Reactor Environment

    by James Rafferty, Fabio Scenini

    This study investigates the role of environmental exposure on creep crack growth in AISI 316H stainless steel, a material widely used in advanced gas-cooled reactors (AGRs). Notched specimens subjected to sustained loading under simulated AGR conditions (CO2 with 1% CO, 500 ppm H2O, 300 ppm CH4, and 100 ppm H2) revealed enhanced intergranular cracking at stress intensity factors above 13 MPa√m, accompanied by grain boundary cavitation and crack branching. To distinguish the individual contributions of creep, oxidation, and carburization, comparative tests were conducted in inert argon and hydrogenated steam environments. The inert atmosphere was used to isolate the mechanical effects of creep alone, while the hydrogenated steam environment allowed oxidation to be studied independently of carbon ingress. Both conditions resulted in significantly reduced crack growth compared to AGR exposure, indicating that carburization plays a critical role in accelerating damage. Electron probe microanalysis suggests elevated carbon concentrations along cavitated grain boundaries, suggesting that carbon segregation contributes to embrittlement and facilitates crack propagation under creep conditions. These findings provide insights into the environmental degradation mechanisms affecting reactor-grade stainless steels. Importantly, the insights gained from this study are directly relevant to high-temperature gas-cooled reactors, where similar alloy-environment interactions may influence long-term structural integrity under service conditions.

  • Evaluating the Use of Phosphate to Mitigate Caustic-PbSCC of Alloy 690TT

    by Giulia B. Mazzei, Jonathan Duff, D. Anthony Horner, M. Grace Burke, Fabio Scenini

    Phosphate additions to Pb-caustic water chemistry were investigated as a potential mitigation strategy for lead-assisted stress corrosion cracking (PbSCC) of Alloy 690TT at approximately 310°C. Autoclave tests were performed for 500 h using C-ring specimens strained in the plastic regime and exposed to four caustic environments (pH_high-T ∼10) containing different PbO and phosphate concentrations. Two surface conditions were examined: as-received and OPS-polished. Results showed that 1,700 ppm phosphate provided only a minor benefit in reducing PbSCC severity, while 3,000 ppm phosphate mitigated cracking for as-received surfaces but promoted localized attack on polished surfaces. Advanced microstructural characterization (scanning electron microscope, focused ion beam-transmission electron microscopy, and scanning transmission electron microscopy with energy-dispersive x-ray) revealed similar crack-tip oxide compositions across all environments, with Pb incorporated in a (Cr,Fe)_3O_4 spinel phase at approximately 1 wt% to 3 wt%. These findings show that phosphate reduces PbSCC kinetics by partially sequestering Pb from solution rather than altering crack-tip chemistry. Although mitigation was incomplete, the results provide insight into inhibitor performance under concentrated crevice-like conditions and highlight the complexity of controlling PbSCC. These findings inform inhibitor selection and water chemistry strategies aimed at improving long-term PWR steam generator integrity.