Abhendra K. Singh
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Abhendra K. Singh has a total of 31 co-authors. Here are the top co-authors by number of shared publications:
Zach Benedict
3 shared publicationsBrian Kitt
Spirit AeroSystems, Inc., Wichita, KS, USA
2 shared publicationsBrianna Ortega
Department of Mechanical Engineering, Baylor University, Waco, TX, USA
2 shared publications- Keeley Lee2 shared publications
- Nicholas Parolini
Department of Mechanical Engineering, Baylor University, Waco, TX 76706, USA
2 shared publications - Shankar Mall
Air Force Institute of Technology
2 shared publications
Latest Publications
- Open Access
Fatigue Behavior of Hybrid Additive/Subtractive Manufactured Ti-6Al-4V
Additive–subtractive hybrid manufacturing (ASHM) allows for the rapid manufacturing of metal components with complex and precise geometries for ready-to-use or near-ready-to-use applications. Laser wire-directed energy deposition (LW-DED) can be used to quickly manufacture metal components, while CNC machining can achieve precise geometric tolerances. In this study, Ti-6Al-4V alloy specimens were fabricated using an LW-DED process combined with CNC machining and tested to evaluate the effects of ASHM on mechanical performance. Post fabrication, the Ti-6Al-4V material was evaluated through hardness mapping, monotonic tensile testing, and fully reversed axial fatigue testing. Vicker’s micro-hardness mapping showed a range of hardness results from 300 to 350 HV in the ASHM Ti-6Al-4V that remained consistent throughout the build. Tensile results showed a similar response to cast and wrought Ti-6Al-4V, with an average yield stress of 819.4 MPa, ultimate tensile strength of 935.5 MPa, and modulus of 119 GPa. When tested in fatigue, the material had a reduced life compared to wrought Ti-6Al-4V, which is attributed to defects originating from the additive process. While no run-outs were observed from the testing, the fatigue results remain aligned with trends reported for other methods of additively manufactured Ti-6Al-4V. Fully reversed high-cycle fatigue loading revealed that the ASHM-fabricated Ti-6Al-4V fell into a Basquin power-law fit with a fatigue strength coefficient of 1942 MPa with a fatigue strength exponent of −0.115. The fatigue life of the ASHM material is found to be dependent on the resulting porosity of the material that stems from the LW-DED process used in the ASHM process described.
Open AccessFatigue Behavior of Hybrid Additive/Subtractive Manufactured Ti-6Al-4V
Additive–subtractive hybrid manufacturing (ASHM) allows for the rapid manufacturing of metal components with complex and precise geometries for ready-to-use or near-ready-to-use applications. Laser wire-directed energy deposition (LW-DED) can be used to quickly manufacture metal components, while CNC machining can achieve precise geometric tolerances. In this study, Ti-6Al-4V alloy specimens were fabricated using an LW-DED process combined with CNC machining and tested to evaluate the effects of ASHM on mechanical performance. Post fabrication, the Ti-6Al-4V material was evaluated through hardness mapping, monotonic tensile testing, and fully reversed axial fatigue testing. Vicker’s micro-hardness mapping showed a range of hardness results from 300 to 350 HV in the ASHM Ti-6Al-4V that remained consistent throughout the build. Tensile results showed a similar response to cast and wrought Ti-6Al-4V, with an average yield stress of 819.4 MPa, ultimate tensile strength of 935.5 MPa, and modulus of 119 GPa. When tested in fatigue, the material had a reduced life compared to wrought Ti-6Al-4V, which is attributed to defects originating from the additive process. While no run-outs were observed from the testing, the fatigue results remain aligned with trends reported for other methods of additively manufactured Ti-6Al-4V. Fully reversed high-cycle fatigue loading revealed that the ASHM-fabricated Ti-6Al-4V fell into a Basquin power-law fit with a fatigue strength coefficient of 1942 MPa with a fatigue strength exponent of −0.115. The fatigue life of the ASHM material is found to be dependent on the resulting porosity of the material that stems from the LW-DED process used in the ASHM process described.
- 31 July 2022
- Published by Elsevier in Ceramics International
- Vol. 48 (21) , 32491-32503
Damage evolution in quasi-statically indented alumina based oxide/oxide ceramic matrix composites: An experimental investigation
- 31 July 2022
- Published by Elsevier in Ceramics International
- Vol. 48 (21) , 32491-32503
Damage evolution in quasi-statically indented alumina based oxide/oxide ceramic matrix composites: An experimental investigation
- 18 July 2022
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 56 (22) , 3483-3494
Effects of moisture ingression on the impact damage resistance and damage tolerance of alumina based oxide/oxide ceramic matrix composites
In this study the effects of moisture ingression on the impact damage resistance and damage tolerance of NextelTM610/alumina-silicate ceramic matrix composites were experimentally evaluated. Thin and thick composite laminates with balanced and symmetric layups were placed inside an environmental chamber at 80°C and 85% relative humidity till moisture saturation was reached. The laminates were then subjected to low velocity impacts using a hemispherical steel impactor at energy levels of 2.5 J and 10 J for the thin and thick laminates, respectively. This resulted in similar damage depths on the impactor side between the two sets of laminates. The resultant damage was characterized non-destructively with the damage metrics of external dent area, dent depth and planar internal damage area quantitatively determined. Impacted laminates were subject to in-plane compression loading and the residual strengths were evaluated. Planar internal damage area was larger for the moisture exposed laminates in comparison to their pristine counterparts for both the thin and thick laminates. Also, larger internal damage area resulted in lower compression-after-impact strength and thus, less damage tolerant laminates. This was true for the pristine and moisture exposed cases for both the laminate thicknesses.
- 18 July 2022
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 56 (22) , 3483-3494
Effects of moisture ingression on the impact damage resistance and damage tolerance of alumina based oxide/oxide ceramic matrix composites
In this study the effects of moisture ingression on the impact damage resistance and damage tolerance of NextelTM610/alumina-silicate ceramic matrix composites were experimentally evaluated. Thin and thick composite laminates with balanced and symmetric layups were placed inside an environmental chamber at 80°C and 85% relative humidity till moisture saturation was reached. The laminates were then subjected to low velocity impacts using a hemispherical steel impactor at energy levels of 2.5 J and 10 J for the thin and thick laminates, respectively. This resulted in similar damage depths on the impactor side between the two sets of laminates. The resultant damage was characterized non-destructively with the damage metrics of external dent area, dent depth and planar internal damage area quantitatively determined. Impacted laminates were subject to in-plane compression loading and the residual strengths were evaluated. Planar internal damage area was larger for the moisture exposed laminates in comparison to their pristine counterparts for both the thin and thick laminates. Also, larger internal damage area resulted in lower compression-after-impact strength and thus, less damage tolerant laminates. This was true for the pristine and moisture exposed cases for both the laminate thicknesses.
- Open Access
- 15 March 2022
- Published by Wiley in Polymer Composites
- Vol. 43 (5) , 3085-3095
Effects of midplane carbon nanotube sheet interleave on the strength and impact damage resistance of carbon fiber reinforced polymer composites
The effects of embedding a midplane carbon nanotube (CNT) sheet on the impact damage resistance, tensile strength and propensity for interlaminar shear failure in a carbon fiber reinforced polymer matrix composite is experimentally evaluated. External and internal damage in the impacted composite laminates were characterized via surface profilometry and ultrasonic C‐scan, respectively. The external dent areas and dent depths were greater for impacted laminates without the CNT sheet interleave, while the planar internal damage areas were greater for the impacted laminates with the CNT sheet. Destructive evaluation of the impacted laminates showed significant delaminations and matrix cracks in the vicinity of the midplane for the laminates with the CNT sheet, while damage was more distributed through the thickness in the non‐CNT sheet ones. While a single CNT sheet interleave did not significantly affect the tensile strength of the laminate, residual strength after impact and the corresponding strain to failure was higher because of the CNT sheet interleave. The propensity for interlaminar shear failure was greater for laminates without the CNT sheet than those with the CNT sheet.
- 15 March 2022
- Published by Wiley in Polymer Composites
- Vol. 43 (5) , 3085-3095
Open AccessEffects of midplane carbon nanotube sheet interleave on the strength and impact damage resistance of carbon fiber reinforced polymer composites
The effects of embedding a midplane carbon nanotube (CNT) sheet on the impact damage resistance, tensile strength and propensity for interlaminar shear failure in a carbon fiber reinforced polymer matrix composite is experimentally evaluated. External and internal damage in the impacted composite laminates were characterized via surface profilometry and ultrasonic C‐scan, respectively. The external dent areas and dent depths were greater for impacted laminates without the CNT sheet interleave, while the planar internal damage areas were greater for the impacted laminates with the CNT sheet. Destructive evaluation of the impacted laminates showed significant delaminations and matrix cracks in the vicinity of the midplane for the laminates with the CNT sheet, while damage was more distributed through the thickness in the non‐CNT sheet ones. While a single CNT sheet interleave did not significantly affect the tensile strength of the laminate, residual strength after impact and the corresponding strain to failure was higher because of the CNT sheet interleave. The propensity for interlaminar shear failure was greater for laminates without the CNT sheet than those with the CNT sheet.
- 1 February 2022
- Published by Elsevier in Ceramics International
- Vol. 48 (3) , 3544-3553
Thermal shock effects on the impact resistance, tolerance and flexural strength of alumina based oxide/oxide ceramic matrix composites
- 1 February 2022
- Published by Elsevier in Ceramics International
- Vol. 48 (3) , 3544-3553
Thermal shock effects on the impact resistance, tolerance and flexural strength of alumina based oxide/oxide ceramic matrix composites
- 20 August 2017
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 15 (1) , 16-27
Tensile and fatigue behavior of oxide/oxide ceramic matrix composite with simulated foreign object damage in combustion environment
In this study, oxide/oxide ceramic matrix composite test coupons were quasi‐statically indented and tested for tensile strength and fatigue life in a combustion environment. The combustion environment simulated the gas turbine engine environment in an aircraft. Two different dent sizes were created on two different sets of test coupons with a blunt conical indentor. During mechanical testing, the combustion flame simultaneously impinged on the dent region resulting in a maximum test coupon surface temperature of 1250 ± 50°C. For a life of 90 000 cycles, the fatigue limit in the combustion environment was 85% of the postindentation degraded tensile strength. Microscopy images of the failed test coupons showed damage modes of fiber fracture and matrix cracking at the dent site. The run‐out test coupons which did not fail within 90 000 cycles showed residual strength that was not significantly different from that of their virgin counterparts.
- 20 August 2017
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 15 (1) , 16-27
Tensile and fatigue behavior of oxide/oxide ceramic matrix composite with simulated foreign object damage in combustion environment
In this study, oxide/oxide ceramic matrix composite test coupons were quasi‐statically indented and tested for tensile strength and fatigue life in a combustion environment. The combustion environment simulated the gas turbine engine environment in an aircraft. Two different dent sizes were created on two different sets of test coupons with a blunt conical indentor. During mechanical testing, the combustion flame simultaneously impinged on the dent region resulting in a maximum test coupon surface temperature of 1250 ± 50°C. For a life of 90 000 cycles, the fatigue limit in the combustion environment was 85% of the postindentation degraded tensile strength. Microscopy images of the failed test coupons showed damage modes of fiber fracture and matrix cracking at the dent site. The run‐out test coupons which did not fail within 90 000 cycles showed residual strength that was not significantly different from that of their virgin counterparts.
- 9 August 2017
- Published by SAGE Publications in Advances in Applied Ceramics: Structural, Functional and Bioceramics
- Vol. 117 (1) , 30-41
Creep-rupture behaviour of notched oxide/oxide ceramic matrix composite in combustion environment
Creep-rupture tests were performed in the combustion environment on double-edge notch and centre hole oxide/oxide ceramic matrix composite specimens. The specimens were exposed to the maximum temperature of 1250 ± 50°C in the notch region where the combustion flame directly impinged. Specimens were loaded to the desired creep load levels and the loads were sustained till either the specimens ruptured or a run-out time of 25 h was achieved. Optical and scanning electron microscopes were used to characterise specimen damage. The test results were compared to its counterparts in 1200°C (isothermal) laboratory air environment. At a given creep life, the applied creep stress for both the notch types was generally lower in the combustion environment than the laboratory air environment. Finite element simulations attributed lower applied creep stress in the combustion environment to the presence of thermal gradient stresses, which were not present in the isothermal laboratory air environment.
- 9 August 2017
- Published by SAGE Publications in Advances in Applied Ceramics: Structural, Functional and Bioceramics
- Vol. 117 (1) , 30-41
Creep-rupture behaviour of notched oxide/oxide ceramic matrix composite in combustion environment
Creep-rupture tests were performed in the combustion environment on double-edge notch and centre hole oxide/oxide ceramic matrix composite specimens. The specimens were exposed to the maximum temperature of 1250 ± 50°C in the notch region where the combustion flame directly impinged. Specimens were loaded to the desired creep load levels and the loads were sustained till either the specimens ruptured or a run-out time of 25 h was achieved. Optical and scanning electron microscopes were used to characterise specimen damage. The test results were compared to its counterparts in 1200°C (isothermal) laboratory air environment. At a given creep life, the applied creep stress for both the notch types was generally lower in the combustion environment than the laboratory air environment. Finite element simulations attributed lower applied creep stress in the combustion environment to the presence of thermal gradient stresses, which were not present in the isothermal laboratory air environment.