Quentin Auzoux
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Quentin Auzoux has a total of 39 co-authors. Here are the top co-authors by number of shared publications:
- Frantz Martin
Université Paris-Saclay, CEA, Service de recherche en Corrosion et Comportement des Matériaux, 91191 Gif Sur Yvette, France
5 shared publications Laurence Latu-Romain
4 shared publicationsYves Wouters
4 shared publicationsFrédéric Datcharry
3 shared publications- Cyriac Christophe2 shared publications
Frantz Martin
2 shared publications
Latest Publications
- Open Access
- 6 April 2026
- Published by Elsevier in Nuclear Materials and Energy
- Vol. 47
Hydrogen uptake of Ti64 and surface–nitrided Ti64 in flowing pressurized water at 300 °C
- 6 April 2026
- Published by Elsevier in Nuclear Materials and Energy
- Vol. 47
Open AccessHydrogen uptake of Ti64 and surface–nitrided Ti64 in flowing pressurized water at 300 °C
- Open Access
- 10 June 2025
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 615
Flow-accelerated corrosion of Ti64 and surface-nitrided Ti64 in pressurised water at 300 °C
- 10 June 2025
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 615
Open AccessFlow-accelerated corrosion of Ti64 and surface-nitrided Ti64 in pressurised water at 300 °C
- 3 April 2025
- Published by Elsevier in Corrosion Science
- Vol. 251
Effect of nitriding on the corrosion of Ti64 in purified pressurized water at 300 °C
- 3 April 2025
- Published by Elsevier in Corrosion Science
- Vol. 251
Effect of nitriding on the corrosion of Ti64 in purified pressurized water at 300 °C
- 23 April 2024
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 67, 577-591
Experimental study of the hydrogen-microstructure interactions in a pre-strained 316L austenitic stainless steel
- 23 April 2024
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 67, 577-591
Experimental study of the hydrogen-microstructure interactions in a pre-strained 316L austenitic stainless steel
- Open Access
Hydrogen Embrittlement Characterization of 1.4614 and 1.4543 Martensitic Precipitation Hardened Stainless Steels
Hydrogen embrittlement (HE) of 1.4614 and 1.4543 maraging stainless steels is characterized with fine structural TEM-ASTAR, hydrogen electrochemical permeation, thermodesorption and tensile testing (with slow strain rate during H cathodic charging) experiments. Both solutions annealed and 550 °C aged states are studied. When aged, 1.4614 grade contains nanometric hexagonal Ni3Ti precipitates whereas 1.4543 grade contains three families of nanometric precipitates, namely, hexagonal Ni3Ti, non fcc-rich Cu and G-phase rich in Si, Ti and Ni with cube-cube relations with martensite. From the permeation and thermodesorption results, it appears that austenite and nanometric precipitates seem to constitute deep traps for hydrogen in both grades. From tensile tests with in situ H charging, 1.4614 and 1.4543 maraging grades show a high susceptibility to HE with relative reduction of area (RRA) strictly superior to 80% for both metallurgical states. The presence of retained austenite does not seem to bring any HE resistance because of its transformation into martensite during deformation.
Open AccessHydrogen Embrittlement Characterization of 1.4614 and 1.4543 Martensitic Precipitation Hardened Stainless Steels
Hydrogen embrittlement (HE) of 1.4614 and 1.4543 maraging stainless steels is characterized with fine structural TEM-ASTAR, hydrogen electrochemical permeation, thermodesorption and tensile testing (with slow strain rate during H cathodic charging) experiments. Both solutions annealed and 550 °C aged states are studied. When aged, 1.4614 grade contains nanometric hexagonal Ni3Ti precipitates whereas 1.4543 grade contains three families of nanometric precipitates, namely, hexagonal Ni3Ti, non fcc-rich Cu and G-phase rich in Si, Ti and Ni with cube-cube relations with martensite. From the permeation and thermodesorption results, it appears that austenite and nanometric precipitates seem to constitute deep traps for hydrogen in both grades. From tensile tests with in situ H charging, 1.4614 and 1.4543 maraging grades show a high susceptibility to HE with relative reduction of area (RRA) strictly superior to 80% for both metallurgical states. The presence of retained austenite does not seem to bring any HE resistance because of its transformation into martensite during deformation.
- 1 September 2021
- Published by Elsevier in Corrosion Science
- Vol. 190
Corrosion of titanium alloys in pressurised water at 300 °C: Kinetics and modelling
- 1 September 2021
- Published by Elsevier in Corrosion Science
- Vol. 190
Corrosion of titanium alloys in pressurised water at 300 °C: Kinetics and modelling
- Open Access
- 12 October 2020
- Published by EDP Sciences in MATEC Web of Conferences
- Vol. 321, 06006
Corrosion of titanium alloys in pressurized water at 300 °C and 15 MPa
Commercially pure titanium (Ti CP) and two titanium alloys (Ti 64 and Ti10-2-3) representative of different metallurgical classes were exposed to pressurized water at 300 °C, 15 MPa in a dedicated stainless steel corrosion loop up to 1632 h.Mass uptake measurements as well as extensive characterization of the oxides formed on the polished samples using scanning and transmission electron microscopy, Raman spectroscopy, X-ray diffraction, X-ray photoelectron spectroscopy, photoelectrochemistry and glow discharge optical emission spectroscopy led to the following main conclusions:• The oxide scale was made of a thin and continuous TiO2 layer topped by small TiO2 anatase crystallites and large FeTiO3 ilmenite crystallites.• The interface tortuosity increased with exposure duration, as well as the amount of crystallites. From 217 h exposure, the thickness of the thin continuous TiO2 layer remained constant with exposure duration.• The mass uptake increased approximately linearly with exposure duration.These observations were consistent with a corrosion mechanism involving simultaneous oxide growth, dissolution and precipitation. The corrosion rate of the three studied materials was estimated to be around 3 µm/year.
- 12 October 2020
- Published by EDP Sciences in MATEC Web of Conferences
- Vol. 321, 06006
Open AccessCorrosion of titanium alloys in pressurized water at 300 °C and 15 MPa
Commercially pure titanium (Ti CP) and two titanium alloys (Ti 64 and Ti10-2-3) representative of different metallurgical classes were exposed to pressurized water at 300 °C, 15 MPa in a dedicated stainless steel corrosion loop up to 1632 h.Mass uptake measurements as well as extensive characterization of the oxides formed on the polished samples using scanning and transmission electron microscopy, Raman spectroscopy, X-ray diffraction, X-ray photoelectron spectroscopy, photoelectrochemistry and glow discharge optical emission spectroscopy led to the following main conclusions:• The oxide scale was made of a thin and continuous TiO2 layer topped by small TiO2 anatase crystallites and large FeTiO3 ilmenite crystallites.• The interface tortuosity increased with exposure duration, as well as the amount of crystallites. From 217 h exposure, the thickness of the thin continuous TiO2 layer remained constant with exposure duration.• The mass uptake increased approximately linearly with exposure duration.These observations were consistent with a corrosion mechanism involving simultaneous oxide growth, dissolution and precipitation. The corrosion rate of the three studied materials was estimated to be around 3 µm/year.
- 1 April 2019
- Published by Elsevier in Corrosion Science
- Vol. 150, 32-41
Oxide formation on titanium alloys in primary water of nuclear pressurised water reactor
- 1 April 2019
- Published by Elsevier in Corrosion Science
- Vol. 150, 32-41
Oxide formation on titanium alloys in primary water of nuclear pressurised water reactor
- Open Access
- 1 February 2018
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 499, 641-651
Stress corrosion crack initiation of Zircaloy-4 cladding tubes in an iodine vapor environment during creep, relaxation, and constant strain rate tests
- 1 February 2018
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 499, 641-651
Open AccessStress corrosion crack initiation of Zircaloy-4 cladding tubes in an iodine vapor environment during creep, relaxation, and constant strain rate tests