Frantz Martin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Frantz Martin has a total of 52 co-authors. Here are the top co-authors by number of shared publications:
- Quentin Auzoux
Université Paris-Saclay, CEA, Service de recherche en Corrosion et Comportement des Matériaux, 91191 Gif Sur Yvette, France
5 shared publications Frédéric Datcharry
3 shared publications- Loïc Marchetti
CEA Saclay
3 shared publications Yves Wouters
3 shared publicationsFrançois Jomard
2 shared publicationsJacques Chêne
UMR 8587 CEA/CNRS, Équipe Hydrogène/Matériaux de structure, CEA, DEN, DPC, SCCME, Laboratoire d’Étude de la Corrosion Aqueuse, F-91191 Gif-Sur-Yvette, France
2 shared publications
Latest Publications
- Open Access
- 6 April 2026
- Published by Elsevier in Nuclear Materials and Energy
- Vol. 47
Hydrogen uptake of Ti64 and surface–nitrided Ti64 in flowing pressurized water at 300 °C
- 6 April 2026
- Published by Elsevier in Nuclear Materials and Energy
- Vol. 47
Open AccessHydrogen uptake of Ti64 and surface–nitrided Ti64 in flowing pressurized water at 300 °C
- Open Access
- 10 June 2025
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 615
Flow-accelerated corrosion of Ti64 and surface-nitrided Ti64 in pressurised water at 300 °C
- 10 June 2025
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 615
Open AccessFlow-accelerated corrosion of Ti64 and surface-nitrided Ti64 in pressurised water at 300 °C
- 9 May 2025
- Published by Elsevier in Corrosion Science
- Vol. 253
Corrosion mechanism and rate limiting step for hydrogen absorption of the M5Framatome alloy
- 9 May 2025
- Published by Elsevier in Corrosion Science
- Vol. 253
Corrosion mechanism and rate limiting step for hydrogen absorption of the M5Framatome alloy
- 23 April 2024
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 67, 577-591
Experimental study of the hydrogen-microstructure interactions in a pre-strained 316L austenitic stainless steel
- 23 April 2024
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 67, 577-591
Experimental study of the hydrogen-microstructure interactions in a pre-strained 316L austenitic stainless steel
- Open Access
Hydrogen Embrittlement Characterization of 1.4614 and 1.4543 Martensitic Precipitation Hardened Stainless Steels
Hydrogen embrittlement (HE) of 1.4614 and 1.4543 maraging stainless steels is characterized with fine structural TEM-ASTAR, hydrogen electrochemical permeation, thermodesorption and tensile testing (with slow strain rate during H cathodic charging) experiments. Both solutions annealed and 550 °C aged states are studied. When aged, 1.4614 grade contains nanometric hexagonal Ni3Ti precipitates whereas 1.4543 grade contains three families of nanometric precipitates, namely, hexagonal Ni3Ti, non fcc-rich Cu and G-phase rich in Si, Ti and Ni with cube-cube relations with martensite. From the permeation and thermodesorption results, it appears that austenite and nanometric precipitates seem to constitute deep traps for hydrogen in both grades. From tensile tests with in situ H charging, 1.4614 and 1.4543 maraging grades show a high susceptibility to HE with relative reduction of area (RRA) strictly superior to 80% for both metallurgical states. The presence of retained austenite does not seem to bring any HE resistance because of its transformation into martensite during deformation.
Open AccessHydrogen Embrittlement Characterization of 1.4614 and 1.4543 Martensitic Precipitation Hardened Stainless Steels
Hydrogen embrittlement (HE) of 1.4614 and 1.4543 maraging stainless steels is characterized with fine structural TEM-ASTAR, hydrogen electrochemical permeation, thermodesorption and tensile testing (with slow strain rate during H cathodic charging) experiments. Both solutions annealed and 550 °C aged states are studied. When aged, 1.4614 grade contains nanometric hexagonal Ni3Ti precipitates whereas 1.4543 grade contains three families of nanometric precipitates, namely, hexagonal Ni3Ti, non fcc-rich Cu and G-phase rich in Si, Ti and Ni with cube-cube relations with martensite. From the permeation and thermodesorption results, it appears that austenite and nanometric precipitates seem to constitute deep traps for hydrogen in both grades. From tensile tests with in situ H charging, 1.4614 and 1.4543 maraging grades show a high susceptibility to HE with relative reduction of area (RRA) strictly superior to 80% for both metallurgical states. The presence of retained austenite does not seem to bring any HE resistance because of its transformation into martensite during deformation.
- 12 February 2022
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 562
Hydrogen trapping by irradiation-induced defects in 316 Lstainless steel: A combined experimental and modeling study
- 12 February 2022
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 562
Hydrogen trapping by irradiation-induced defects in 316 Lstainless steel: A combined experimental and modeling study
- 1 September 2021
- Published by Elsevier in Corrosion Science
- Vol. 190
Corrosion of titanium alloys in pressurised water at 300 °C: Kinetics and modelling
- 1 September 2021
- Published by Elsevier in Corrosion Science
- Vol. 190
Corrosion of titanium alloys in pressurised water at 300 °C: Kinetics and modelling
- 1 May 2021
- Published by Elsevier in Corrosion Science
- Vol. 184
Corrosion of carbon steel in clay compact environments at 90 °C: Effect of confined conditions
- 1 May 2021
- Published by Elsevier in Corrosion Science
- Vol. 184
Corrosion of carbon steel in clay compact environments at 90 °C: Effect of confined conditions
- 1 November 2018
- Published by Elsevier in Corrosion Science
- Vol. 144, 1-12
Kinetics of hydrogen permeation through a Ni-base alloy membrane exposed to primary medium of pressurized water reactors
- 1 November 2018
- Published by Elsevier in Corrosion Science
- Vol. 144, 1-12
Kinetics of hydrogen permeation through a Ni-base alloy membrane exposed to primary medium of pressurized water reactors