Widi Astuti
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Widi Astuti has a total of 48 co-authors. Here are the top co-authors by number of shared publications:
- Slamet Sumardi
National Research and Innovation Agency
4 shared publications - Azwar Manaf
Universitas Indonesia
3 shared publications - Fajar Nurjaman
Research Center of Mining Technology, National Research and Innovation Agency of Indonesia
3 shared publications - Fathan Bahfie
Research Center for Mineral Technology, National Research and Innovation Agency, Tanjung Bintang, Lampung Selatan 35361, Indonesia
3 shared publications - Himawan Tri Bayu Murti Petrus
Department of Chemical Engineering, Faculty of Engineering, Universitas Gadjah Mada, Yogyakarta, Indonesia
3 shared publications - Aisyah Minzikrina Masbar Rus
Department of Metallurgical Engineering, Faculty of Mining and Petroleum Engineering, Institut Teknologi Bandung, Bandung, Indonesia
2 shared publications
Latest Publications
- 29 October 2025
- Published by Springer Nature in Journal of Sustainable Metallurgy
- Vol. 11 (4) , 3646-3658
Sustainable Recovery of Rare Earth Elements from Coal Fly Ash via Biohydrometallurgy Using Alicyclobacillus ferrooxydans: Effects of Pulp Density and Pyrite Amendment
- 29 October 2025
- Published by Springer Nature in Journal of Sustainable Metallurgy
- Vol. 11 (4) , 3646-3658
Sustainable Recovery of Rare Earth Elements from Coal Fly Ash via Biohydrometallurgy Using Alicyclobacillus ferrooxydans: Effects of Pulp Density and Pyrite Amendment
- Open Access
- 1 September 2025
- Published by Wydawnictwo Naukowe Gabriel Borowski (WNGB) in Journal of Ecological Engineering
- Vol. 26 (9) , 20-37
Characterization and genomic profiling of potential iron-reducing bacteria isolated from red mud for bioremediation
Red mud is waste from the alumina (Al2O3) production process of bauxite ore processing through the bayer process. The production of one ton of alumina produces between 1-1.5 tons of red mud. The high amount of waste has a negative impact on the environment, resulting in infertile soil and posing...
- 1 September 2025
- Published by Wydawnictwo Naukowe Gabriel Borowski (WNGB) in Journal of Ecological Engineering
- Vol. 26 (9) , 20-37
Open AccessCharacterization and genomic profiling of potential iron-reducing bacteria isolated from red mud for bioremediation
Red mud is waste from the alumina (Al2O3) production process of bauxite ore processing through the bayer process. The production of one ton of alumina produces between 1-1.5 tons of red mud. The high amount of waste has a negative impact on the environment, resulting in infertile soil and posing...
- Open Access
- 26 May 2025
- Published by Chemical Engineering Department, Syiah Kuala University in Jurnal Rekayasa Kimia & Lingkungan
- Vol. 20 (1) , 13-21
Heavy Metal Adsorption Using Cellulose Xanthate from Sugarcane Bagasse: A Fixed-Bed Column Study
In recent years, various environmentally friendly adsorbents have been developed to address the removal of heavy metals from industrial wastewater. This study focuses on the adsorption of lead (Pb²⁺) and copper (Cu²⁺) using cellulose xanthate derived from sugarcane bagasse as an adsorbent. The adsorption experiments were conducted in a fixed-bed column with dimensions of 2.4 cm in diameter and 8 cm in height. Atomic Absorption Spectrophotometry (AAS) was used to analyze the concentrations of Pb²⁺ and Cu²⁺ before and after adsorption, while the adsorbent composition was characterized using X-Ray Fluorescence (XRF). The breakthrough times for Pb²⁺ and Cu²⁺ adsorption was found to be 8 and 6 minutes, respectively, with total adsorption durations of 18.584 and 17.543 minutes. The Thomas Model was employed to evaluate the kinetics and adsorption capacity, yielding kinetic constants (KTH) of 0.00283 and 0.0006 mL/mg.min for Pb²⁺ and Cu²⁺, respectively, and adsorption capacities (qeq) of 712.89 and 181.18 mg/g. These results provide valuable insights into the adsorbent’s efficiency, kinetics, and potential applications in environmental remediation and wastewater treatment.
- 26 May 2025
- Published by Chemical Engineering Department, Syiah Kuala University in Jurnal Rekayasa Kimia & Lingkungan
- Vol. 20 (1) , 13-21
Open AccessHeavy Metal Adsorption Using Cellulose Xanthate from Sugarcane Bagasse: A Fixed-Bed Column Study
In recent years, various environmentally friendly adsorbents have been developed to address the removal of heavy metals from industrial wastewater. This study focuses on the adsorption of lead (Pb²⁺) and copper (Cu²⁺) using cellulose xanthate derived from sugarcane bagasse as an adsorbent. The adsorption experiments were conducted in a fixed-bed column with dimensions of 2.4 cm in diameter and 8 cm in height. Atomic Absorption Spectrophotometry (AAS) was used to analyze the concentrations of Pb²⁺ and Cu²⁺ before and after adsorption, while the adsorbent composition was characterized using X-Ray Fluorescence (XRF). The breakthrough times for Pb²⁺ and Cu²⁺ adsorption was found to be 8 and 6 minutes, respectively, with total adsorption durations of 18.584 and 17.543 minutes. The Thomas Model was employed to evaluate the kinetics and adsorption capacity, yielding kinetic constants (KTH) of 0.00283 and 0.0006 mL/mg.min for Pb²⁺ and Cu²⁺, respectively, and adsorption capacities (qeq) of 712.89 and 181.18 mg/g. These results provide valuable insights into the adsorbent’s efficiency, kinetics, and potential applications in environmental remediation and wastewater treatment.
- 20 March 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 77-86
Titanium Dioxide Production from Low-Grade Ilmenite Ore: Mineral Characterization and Optimization
The characterization of low-grade ilmenite ore from Banten (Indonesia) is investigated, as well as the effects of particle size, NaOH:Ti ratio, and fusion time on Ti and Fe content in TiO2 products. Mineral separation of low-grade ilmenite ore was performed using wet gravity, followed by sieving. Each sample size’s magnetization (using 10,000 Gauss magnets) is followed by weighing the magnetization results. The sifted and magnetized samples were then analyzed with XRF for composition analysis and XRD for compound determination. FE-SEM was applied to analyze morphology. A microscope was used for metalografi analysis. The fusion temperature of the optimization process was determined using STA. Fusion times were 10, 30, 60, 90, and 150 minutes at 850°C, with a NaOH:Ti ratio (w/w) of 1:2, 2:1, and 4:1, and particle sizes of 0.177-0.149 mm, 0.149-0.105 mm, and 0.105-0.074 mm. The minerals ilmenite (FeTiO3), magnetite (Fe3O4), and coesite (SiO2) dominate the characterization of Banten low-grade ilmenite ore. Sixty minutes of fusion at 850°C with a 2:1 NaOH:Ti ratio (w/w) and 0.177-0.149 mm with 94.44% TiO2 in a product was optimal.
- 20 March 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 77-86
Titanium Dioxide Production from Low-Grade Ilmenite Ore: Mineral Characterization and Optimization
The characterization of low-grade ilmenite ore from Banten (Indonesia) is investigated, as well as the effects of particle size, NaOH:Ti ratio, and fusion time on Ti and Fe content in TiO2 products. Mineral separation of low-grade ilmenite ore was performed using wet gravity, followed by sieving. Each sample size’s magnetization (using 10,000 Gauss magnets) is followed by weighing the magnetization results. The sifted and magnetized samples were then analyzed with XRF for composition analysis and XRD for compound determination. FE-SEM was applied to analyze morphology. A microscope was used for metalografi analysis. The fusion temperature of the optimization process was determined using STA. Fusion times were 10, 30, 60, 90, and 150 minutes at 850°C, with a NaOH:Ti ratio (w/w) of 1:2, 2:1, and 4:1, and particle sizes of 0.177-0.149 mm, 0.149-0.105 mm, and 0.105-0.074 mm. The minerals ilmenite (FeTiO3), magnetite (Fe3O4), and coesite (SiO2) dominate the characterization of Banten low-grade ilmenite ore. Sixty minutes of fusion at 850°C with a 2:1 NaOH:Ti ratio (w/w) and 0.177-0.149 mm with 94.44% TiO2 in a product was optimal.
- 13 March 2025
- Published by SAGE Publications in Mineral Processing and Extractive Metallurgy: Transactions of the Institutions of Mining and Metallurgy
- Vol. 134 (1) , 52-66
Advancing the circular economy: green recovery of rare earth elements (REEs) from coal combustion fly ash using biohydrometallurgical techniques with mixotrophic bacteria
Coal remains a crucial energy source, with European countries reactivating coal-fired stations to prevent winter blackouts, highlighting its energy security importance. This research investigates coal fly ash (CFA) from a power plant in Indonesia, which is rich in rare earth elements (REEs) that are vital for contemporary technologies. The analysis reveals that the CFA is primarily composed of Si, Fe, Al and Ca, and is notably concentrated in REEs such as Ce, Y, La, Nd, Sc and Pr. Employing biohydrometallurgical techniques involving mixotrophic bacteria, this study aims to sustainably extract these REEs. The findings indicate effective recovery, especially of heavy REEs like terbium, achieving a maximum extraction rate of 70%. Six bacterial strains demonstrated enhanced efficacy in extracting heavy rather than light REEs. The research emphasises the potential of CFA as a significant secondary source of critical metals, promoting eco-friendly extraction methods as feasible and sustainable alternatives.
- 13 March 2025
- Published by SAGE Publications in Mineral Processing and Extractive Metallurgy: Transactions of the Institutions of Mining and Metallurgy
- Vol. 134 (1) , 52-66
Advancing the circular economy: green recovery of rare earth elements (REEs) from coal combustion fly ash using biohydrometallurgical techniques with mixotrophic bacteria
Coal remains a crucial energy source, with European countries reactivating coal-fired stations to prevent winter blackouts, highlighting its energy security importance. This research investigates coal fly ash (CFA) from a power plant in Indonesia, which is rich in rare earth elements (REEs) that are vital for contemporary technologies. The analysis reveals that the CFA is primarily composed of Si, Fe, Al and Ca, and is notably concentrated in REEs such as Ce, Y, La, Nd, Sc and Pr. Employing biohydrometallurgical techniques involving mixotrophic bacteria, this study aims to sustainably extract these REEs. The findings indicate effective recovery, especially of heavy REEs like terbium, achieving a maximum extraction rate of 70%. Six bacterial strains demonstrated enhanced efficacy in extracting heavy rather than light REEs. The research emphasises the potential of CFA as a significant secondary source of critical metals, promoting eco-friendly extraction methods as feasible and sustainable alternatives.
- Open Access
- 1 January 2025
- Published by Center of Biomass and Renewable Energy Scientia Academy in International Journal of Renewable Energy Development
- Vol. 14 (2) , 322-331
A porous activated carbon derived from banana peel by hydrothermal activation two-step methods
Activated carbon from banana peel waste through two stages of hydrothermal (HT) and physical activation processes has been carried out. The hydrothermal process was carried out at a temperature of 200 oC with a holding time of 2 or 6 hours. The hydrochar that had been obtained was then activated in the second stage with nitrogen gas flow (N2) at a temperature of 700 oC for 1 hour with a flow rate of 100 mL/min. The difference in treatment, without the HT process, two stages of activation, variations in activator agents (water, H3PO4, and PEG6000), water volume ratio and HT process holding time were studied for their effects on the specific surface area (SSA) and structure of activated carbon. SSA was measured using the Brunauer–Emmett–Teller (BET) adsorption method, x-ray crystallography was used to identify the crystalline phase and carbon structure parameters, and the surface morphology of activated carbon was observed using FESEM. The results showed that the activation method and process conditions greatly influenced the (SSA) of activated carbon. HT activation using a combination of activator agents produced an SSA reaching 476.9 m2/g. X-ray diffraction analysis showed that HT activation increased the degree of crystallization of activated carbon. The spherical surface structure of activated carbon was formed when H3PO4 was added, while the layered structure was formed when PEG6000 was used. Overall, the two-step activation preceded by the HT process with the addition of H3PO4 produced activated carbon with better SSA and carbon structure and has the potential to be used in wide applications such as EDLC supercapacitor electrode materials, battery cathodes, and adsorption materials.
- 1 January 2025
- Published by Center of Biomass and Renewable Energy Scientia Academy in International Journal of Renewable Energy Development
- Vol. 14 (2) , 322-331
Open AccessA porous activated carbon derived from banana peel by hydrothermal activation two-step methods
Activated carbon from banana peel waste through two stages of hydrothermal (HT) and physical activation processes has been carried out. The hydrothermal process was carried out at a temperature of 200 oC with a holding time of 2 or 6 hours. The hydrochar that had been obtained was then activated in the second stage with nitrogen gas flow (N2) at a temperature of 700 oC for 1 hour with a flow rate of 100 mL/min. The difference in treatment, without the HT process, two stages of activation, variations in activator agents (water, H3PO4, and PEG6000), water volume ratio and HT process holding time were studied for their effects on the specific surface area (SSA) and structure of activated carbon. SSA was measured using the Brunauer–Emmett–Teller (BET) adsorption method, x-ray crystallography was used to identify the crystalline phase and carbon structure parameters, and the surface morphology of activated carbon was observed using FESEM. The results showed that the activation method and process conditions greatly influenced the (SSA) of activated carbon. HT activation using a combination of activator agents produced an SSA reaching 476.9 m2/g. X-ray diffraction analysis showed that HT activation increased the degree of crystallization of activated carbon. The spherical surface structure of activated carbon was formed when H3PO4 was added, while the layered structure was formed when PEG6000 was used. Overall, the two-step activation preceded by the HT process with the addition of H3PO4 produced activated carbon with better SSA and carbon structure and has the potential to be used in wide applications such as EDLC supercapacitor electrode materials, battery cathodes, and adsorption materials.
- Open Access
- 1 March 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (1) , 127-132
Composition of tailings after selective reduction of laterite
The selective reduction process generates products in the form of concentrates and tailing/by-products. There is high percentage of iron and other elements in the tailings that are not extracted in selective reduction process. Properties of by-products of selective reduction were investigated using X-ray diffraction (XRD), inductively coupled plasma optical emission spectroscopy (ICP–OES), ultraviolet-visible (UV–VIS), and scanning electron microscopy energy dispersion spectroscopy (SEM–EDS). Based on the results of this study, the properties of iron-sulfur, iron-magnesium-aluminium, and silica phases in the tailings can be interpreted experimentally. For future research, it can be the reference for such processes as acid and base leaching. Pure iron extracted from tailings can be used for metal fuel in the future. The tailings composition data will help future researchers to find optimal processes for the tailings.
- 1 March 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (1) , 127-132
Open AccessComposition of tailings after selective reduction of laterite
The selective reduction process generates products in the form of concentrates and tailing/by-products. There is high percentage of iron and other elements in the tailings that are not extracted in selective reduction process. Properties of by-products of selective reduction were investigated using X-ray diffraction (XRD), inductively coupled plasma optical emission spectroscopy (ICP–OES), ultraviolet-visible (UV–VIS), and scanning electron microscopy energy dispersion spectroscopy (SEM–EDS). Based on the results of this study, the properties of iron-sulfur, iron-magnesium-aluminium, and silica phases in the tailings can be interpreted experimentally. For future research, it can be the reference for such processes as acid and base leaching. Pure iron extracted from tailings can be used for metal fuel in the future. The tailings composition data will help future researchers to find optimal processes for the tailings.
- Open Access
- 24 February 2023
- Published by Center of Biomass and Renewable Energy Scientia Academy in International Journal of Renewable Energy Development
- Vol. 12 (3) , 459-466
Utilization of the spent catalyst as a raw material for rechargeable battery production: The effect of leaching time, type, and concentration of organic acids
This study examines the potential use of the spent catalyst as a raw material for rechargeable batteries. The spent catalyst Ni/γ-Al2O3 still contains relatively high amounts of nickel. This indicates the potential use of the spent catalyst to be leached and purified for synthesizing nickel-based compounds so that it can be applied to rechargeable battery cathodes. In this study, the spent catalyst leaching process employed four types of organic acids: citric acid, lactic acid, oxalic acid, and acetic acid. The spent catalyst was leached under atmospheric conditions and room temperature. Organic acid concentrations were also varied at 0.1, 0.5, 1, and 2 M. The leaching process took place for 240 minutes, where sampling was conducted periodically at 30, 60, 120, 180, and 240 minutes. Experimental results showed that Ni (II) and Al (III) ions were successfully leached to the maximum when using 2M citric acids at a leaching time of 240 minutes. The conditions succeeded in leaching Ni (II) and Al (III) ions of 357.8 and 1,975.4 ppm, respectively. Organic acid, notably citric acid, has excellent potential for further development. Citric acid, as a solvent, has the ability to leach metal ions with high recovery. In addition, this acid is categorized as an eco-friendly and green solvent compared to inorganic acid. Thus, the leaching process can take place without harming the environment.
- 24 February 2023
- Published by Center of Biomass and Renewable Energy Scientia Academy in International Journal of Renewable Energy Development
- Vol. 12 (3) , 459-466
Open AccessUtilization of the spent catalyst as a raw material for rechargeable battery production: The effect of leaching time, type, and concentration of organic acids
This study examines the potential use of the spent catalyst as a raw material for rechargeable batteries. The spent catalyst Ni/γ-Al2O3 still contains relatively high amounts of nickel. This indicates the potential use of the spent catalyst to be leached and purified for synthesizing nickel-based compounds so that it can be applied to rechargeable battery cathodes. In this study, the spent catalyst leaching process employed four types of organic acids: citric acid, lactic acid, oxalic acid, and acetic acid. The spent catalyst was leached under atmospheric conditions and room temperature. Organic acid concentrations were also varied at 0.1, 0.5, 1, and 2 M. The leaching process took place for 240 minutes, where sampling was conducted periodically at 30, 60, 120, 180, and 240 minutes. Experimental results showed that Ni (II) and Al (III) ions were successfully leached to the maximum when using 2M citric acids at a leaching time of 240 minutes. The conditions succeeded in leaching Ni (II) and Al (III) ions of 357.8 and 1,975.4 ppm, respectively. Organic acid, notably citric acid, has excellent potential for further development. Citric acid, as a solvent, has the ability to leach metal ions with high recovery. In addition, this acid is categorized as an eco-friendly and green solvent compared to inorganic acid. Thus, the leaching process can take place without harming the environment.
- Open Access
- 27 July 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (7) , 471-478
Thermal upgrading of nickel from limonite by means of selective reduction
X-ray diffraction (XRD), X-ray fluorescence (XRF), scanning electron microscopy energy dispersion spectroscopy (SEM–EDS), and differential thermal analysis (DTA) measurements were used to investigate the mineralogical characteristics and distribution of data set in limonite soil from Indonesia. The findings point to a complicated inner core in laterite ore. Ni, Fe, Mg, Al, and Si levels in limonite are 1.4, 50.5, 1.81, 4.86 and 16.5 wt %, respectively. The iron oxide/oxyhydroxide content of limonite is 94.4 and 5.6 % silicate. DTA shows that limonite has a phase transition in the low temperature (200 – 300 °C) with the goethite transformation to hematite. This phase is good optimalization for nickel diffusion in the iron. Moreover, for this limonite, the thermal upgrading was used as a good method.
- 27 July 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (7) , 471-478
Open AccessThermal upgrading of nickel from limonite by means of selective reduction
X-ray diffraction (XRD), X-ray fluorescence (XRF), scanning electron microscopy energy dispersion spectroscopy (SEM–EDS), and differential thermal analysis (DTA) measurements were used to investigate the mineralogical characteristics and distribution of data set in limonite soil from Indonesia. The findings point to a complicated inner core in laterite ore. Ni, Fe, Mg, Al, and Si levels in limonite are 1.4, 50.5, 1.81, 4.86 and 16.5 wt %, respectively. The iron oxide/oxyhydroxide content of limonite is 94.4 and 5.6 % silicate. DTA shows that limonite has a phase transition in the low temperature (200 – 300 °C) with the goethite transformation to hematite. This phase is good optimalization for nickel diffusion in the iron. Moreover, for this limonite, the thermal upgrading was used as a good method.