Michael Lauritzen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Michael Lauritzen has a total of 54 co-authors. Here are the top co-authors by number of shared publications:
Erik Kjeang
Simon Fraser University
11 shared publicationsAlexander Agapov
W. L. Gore & Associates, Inc
7 shared publicationsErin Setzler
W. L. Gore & Associates, Inc
7 shared publications- Monica Dutta
Ballard Power Systems
7 shared publications Nitish Kumar
Fuel Cell Research Lab (FCReL), Simon Fraser University
7 shared publicationsYixuan Chen
Fuel Cell Research Lab (FCReL), Simon Fraser University
7 shared publications
Latest Publications
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02 (41) , 2015
Analysis of Fuel Cell Membrane Buckling into Gas Diffusion Layer Holes and Its Impact on Fuel Cell Durability
Fuel cell membrane durability can be affected by inhomogeneous physical non-uniformities such as holes and depressions in the gas diffusion layers (GDLs). To enhance quality control in fuel cell manufacturing, it is essential to assess the severity of these non-uniformities to implement effective mitigation strategies. A prior study [1] investigating combined chemical and mechanical membrane degradation with artificially induced GDL holes demonstrated that buckling-induced membrane failure is highly dependent on both the size and location of these defects. However, the extensive duration required for degradation experiments constrained the number of testable scenarios. To overcome this limitation, the present study integrates both modeling and experimental approaches to comprehensively analyze membrane deformation and stress distribution across a wider range of GDL hole sizes and locations. The modeling framework is developed to predict membrane deformation and stress distribution, thereby addressing the knowledge gaps identified in previous research [1]. Complementary to this, experimental investigations utilize a micro-XCT visualization system [2] to enable in-situ monitoring of membrane buckling behavior under both wet and dry conditions, providing crucial validation for the modeling predictions. Experimental findings reveal that membrane buckling behavior is strongly influenced by the size and location of GDL holes. Under flow channels, buckling into through-plane GDL holes initiates when the hole diameter reaches approximately 100 μm, identifying this as the critical threshold below which buckling does not occur. Conversely, in the land regions, membrane buckling occurs regardless of hole size due to the higher through-plane compression in these areas. The simulation results closely align with experimental observations. Specifically, in the flow channel regions, the model predicts the onset of membrane buckling at a GDL hole diameter of 120 μm, with a rapid increase in deformation beyond 150 μm. In land regions, the model suggests that the delayed detachment of the catalyst coated membrane (CCM) and the compression retained from the intact GDL on the opposite electrode contribute to early membrane deformation, even for hole diameters below 100 μm, as indicated in the figure. Since membrane buckling is predominantly driven by hygral swelling into interfacial voids between the CCM and GDL, controlling membrane swelling emerges as a potential mitigation strategy. To evaluate this approach, a 20% thinner reinforced membrane, exhibiting similar mechanical properties, is experimentally tested. The results indicate that the critical GDL hole diameters for membrane buckling initiation remain unchanged relative to the thicker membrane. However, the thinner membrane exhibits reduced deformation and consequently lower in-plane strain across most test scenarios. Given that both membranes possess equivalent mechanical properties, this reduction in strain suggests a corresponding decrease in in-plane tension. Overall, this study integrates experimental and simulation analyses to provide critical insights into membrane buckling behavior, stress distribution, and mitigation strategies. The findings suggest that, in addition to minimizing interfacial voids larger than 100 µm through refined GDL and membrane electrode assembly (MEA) design, reducing membrane swelling via thinner reinforced membranes offers a viable approach to mitigating membrane buckling. These insights contribute to improved long-term durability and performance in fuel cell applications. Keywords: fuel cell; membrane durability; membrane buckling; reinforced membrane modeling; X-ray computed tomography Acknowledgements: This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. References: [1] Y. Chen, A. Bahrami, N. Kumar, F.P. Orfino, M. Dutta, E.N. Alvar, M. Lauritzen, E. Setzler, A. Agapov, E. Kjeang, Impact of GDL Hole on Chemo-Mechanical Membrane Degradation Investigated by 4D in-Situ Visualization, Meet. Abstr. MA2023-02 (2023) 1780. https://doi.org/10.1149/MA2023-02371780mtgabs. [2] Y. Chen, M. Bahrami, N. Kumar, F.P. Orfino, M. Dutta, M. Lauritzen, E. Setzler, A.L. Agapov, E. Kjeang, Effect of Accelerated Stress Testing Conditions on Combined Chemical and Mechanical Membrane Durability in Fuel Cells, J. Electrochem. Soc. 170 (2023) 114526. https://doi.org/10.1149/1945-7111/ad0e43. Figure 1
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02 (41) , 2015
Analysis of Fuel Cell Membrane Buckling into Gas Diffusion Layer Holes and Its Impact on Fuel Cell Durability
Fuel cell membrane durability can be affected by inhomogeneous physical non-uniformities such as holes and depressions in the gas diffusion layers (GDLs). To enhance quality control in fuel cell manufacturing, it is essential to assess the severity of these non-uniformities to implement effective mitigation strategies. A prior study [1] investigating combined chemical and mechanical membrane degradation with artificially induced GDL holes demonstrated that buckling-induced membrane failure is highly dependent on both the size and location of these defects. However, the extensive duration required for degradation experiments constrained the number of testable scenarios. To overcome this limitation, the present study integrates both modeling and experimental approaches to comprehensively analyze membrane deformation and stress distribution across a wider range of GDL hole sizes and locations. The modeling framework is developed to predict membrane deformation and stress distribution, thereby addressing the knowledge gaps identified in previous research [1]. Complementary to this, experimental investigations utilize a micro-XCT visualization system [2] to enable in-situ monitoring of membrane buckling behavior under both wet and dry conditions, providing crucial validation for the modeling predictions. Experimental findings reveal that membrane buckling behavior is strongly influenced by the size and location of GDL holes. Under flow channels, buckling into through-plane GDL holes initiates when the hole diameter reaches approximately 100 μm, identifying this as the critical threshold below which buckling does not occur. Conversely, in the land regions, membrane buckling occurs regardless of hole size due to the higher through-plane compression in these areas. The simulation results closely align with experimental observations. Specifically, in the flow channel regions, the model predicts the onset of membrane buckling at a GDL hole diameter of 120 μm, with a rapid increase in deformation beyond 150 μm. In land regions, the model suggests that the delayed detachment of the catalyst coated membrane (CCM) and the compression retained from the intact GDL on the opposite electrode contribute to early membrane deformation, even for hole diameters below 100 μm, as indicated in the figure. Since membrane buckling is predominantly driven by hygral swelling into interfacial voids between the CCM and GDL, controlling membrane swelling emerges as a potential mitigation strategy. To evaluate this approach, a 20% thinner reinforced membrane, exhibiting similar mechanical properties, is experimentally tested. The results indicate that the critical GDL hole diameters for membrane buckling initiation remain unchanged relative to the thicker membrane. However, the thinner membrane exhibits reduced deformation and consequently lower in-plane strain across most test scenarios. Given that both membranes possess equivalent mechanical properties, this reduction in strain suggests a corresponding decrease in in-plane tension. Overall, this study integrates experimental and simulation analyses to provide critical insights into membrane buckling behavior, stress distribution, and mitigation strategies. The findings suggest that, in addition to minimizing interfacial voids larger than 100 µm through refined GDL and membrane electrode assembly (MEA) design, reducing membrane swelling via thinner reinforced membranes offers a viable approach to mitigating membrane buckling. These insights contribute to improved long-term durability and performance in fuel cell applications. Keywords: fuel cell; membrane durability; membrane buckling; reinforced membrane modeling; X-ray computed tomography Acknowledgements: This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. References: [1] Y. Chen, A. Bahrami, N. Kumar, F.P. Orfino, M. Dutta, E.N. Alvar, M. Lauritzen, E. Setzler, A. Agapov, E. Kjeang, Impact of GDL Hole on Chemo-Mechanical Membrane Degradation Investigated by 4D in-Situ Visualization, Meet. Abstr. MA2023-02 (2023) 1780. https://doi.org/10.1149/MA2023-02371780mtgabs. [2] Y. Chen, M. Bahrami, N. Kumar, F.P. Orfino, M. Dutta, M. Lauritzen, E. Setzler, A.L. Agapov, E. Kjeang, Effect of Accelerated Stress Testing Conditions on Combined Chemical and Mechanical Membrane Durability in Fuel Cells, J. Electrochem. Soc. 170 (2023) 114526. https://doi.org/10.1149/1945-7111/ad0e43. Figure 1
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02 (41) , 2017
Membrane Integrity in the Presence of Foreign Particles in the Membrane Electrode Assembly
Cost-effective, large-scale production of reliable proton exchange membrane fuel cells (PEMFCs) is crucial to meet growing green energy demands. High-throughput production of PEMFCs relies on heavy machinery, which may inadvertently introduce foreign particles into the membrane electrode assembly (MEA) and affect PEMFC durability and performance 1–3 . A wide variety of particles could conceivably be introduced into the MEA and may or may not be detected. Thus, understanding the potential impacts of these particles is essential. The objective of the present work is to determine the impacts of foreign particle dimensions, shape, hardness, and chemical composition on membrane integrity and durability in PEMFCs. To accommodate a suitably wide range of particles for testing, the study focuses on assessing the nature and extent of membrane damage upon fuel cell assembly, conditioning, and initial operation as well as the prospects of mitigation. Composite material (CM) spheres with diameters of 5, 15, 60, and 100 µm along with 500 µm spherical glass beads, 50 µm slightly oxidized iron (Fe) particles, and stainless steel 316L particles of 50 and 500 µm were selected for this research. The particles were strategically placed between a mechanically reinforced GORE-SELECT® membrane (MemA) and the cathode catalyst layer. An MEA was fabricated using the particle-laden catalyst coated membrane (CCM) and assembled within a small-scale fixture (SSF) fuel cell. Non-invasive 3D characterization through X-ray computed tomography 4 imaging revealed that CM particles completely dissolved when measuring up to 15 µm in diameter, creating pinhole-like voids in the CCM. Additionally, a slightly oxidized Fe particle of approximately 55±5 µm also showed complete dissolution, demonstrating that the dissolution of particles was mainly determined by their chemical composition and, to a lesser extent, their size. Larger particles, specifically those measuring 100 µm or more, caused damage in the MEA structure, including deformation of the gas diffusion layer (GDL) and a torus-shaped void in the catalyst layer. Early fabrication damage during the decal transfer process was commonly noted, especially as the surface features of the particles became increasingly random. Additionally, as the size and hardness of the particles increased, especially the SS316L 500 µm particles, significant permanent membrane rupture, GDL damage, and cavities in the MEA were observed. Figure 1 illustrates the types of observed MEA damage associated with particle sizes. As the particle size increased, the prevalence of some damage types also rose, highlighting the importance of mitigating damage from larger particles. Performance analysis indicated that cyclic voltammetry and polarization curve data could effectively identify early cell failures caused by damage incurred by the particles. Different shapes and surface morphologies of SS316L particles were further tested with a thinner chemically and mechanically reinforced GORE-SELECT® membrane (MemB) for mitigation purposes, as they caused the maximum damage to the MemA MEA. It was found that MemB could accommodate all four selected particles, despite varying degrees of surface randomness, without any membrane ruptures after the decal transfer phase. However, significant permanent damage to other MEA components remained evident. Keywords: Quality control, cost reduction, X-ray computed tomography, foreign particles Acknowledgments This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. References J. Chen, H. Liu, Y. A. Huang, and Z. Yin, J. Manuf. Process. , 23 , 175–182 (2016). M. Bahrami et al., J. Electrochem. Soc., 170 , 114527 (2023). N. Kumar et al., J. Electrochem. Soc. , 171 , 074513 (2024) Y. Singh, F. P. Orfino, M. Dutta, and E. Kjeang, J. Electrochem. Soc. , 164 , F1331–F1341 (2017). Figure 1
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02 (41) , 2017
Membrane Integrity in the Presence of Foreign Particles in the Membrane Electrode Assembly
Cost-effective, large-scale production of reliable proton exchange membrane fuel cells (PEMFCs) is crucial to meet growing green energy demands. High-throughput production of PEMFCs relies on heavy machinery, which may inadvertently introduce foreign particles into the membrane electrode assembly (MEA) and affect PEMFC durability and performance 1–3 . A wide variety of particles could conceivably be introduced into the MEA and may or may not be detected. Thus, understanding the potential impacts of these particles is essential. The objective of the present work is to determine the impacts of foreign particle dimensions, shape, hardness, and chemical composition on membrane integrity and durability in PEMFCs. To accommodate a suitably wide range of particles for testing, the study focuses on assessing the nature and extent of membrane damage upon fuel cell assembly, conditioning, and initial operation as well as the prospects of mitigation. Composite material (CM) spheres with diameters of 5, 15, 60, and 100 µm along with 500 µm spherical glass beads, 50 µm slightly oxidized iron (Fe) particles, and stainless steel 316L particles of 50 and 500 µm were selected for this research. The particles were strategically placed between a mechanically reinforced GORE-SELECT® membrane (MemA) and the cathode catalyst layer. An MEA was fabricated using the particle-laden catalyst coated membrane (CCM) and assembled within a small-scale fixture (SSF) fuel cell. Non-invasive 3D characterization through X-ray computed tomography 4 imaging revealed that CM particles completely dissolved when measuring up to 15 µm in diameter, creating pinhole-like voids in the CCM. Additionally, a slightly oxidized Fe particle of approximately 55±5 µm also showed complete dissolution, demonstrating that the dissolution of particles was mainly determined by their chemical composition and, to a lesser extent, their size. Larger particles, specifically those measuring 100 µm or more, caused damage in the MEA structure, including deformation of the gas diffusion layer (GDL) and a torus-shaped void in the catalyst layer. Early fabrication damage during the decal transfer process was commonly noted, especially as the surface features of the particles became increasingly random. Additionally, as the size and hardness of the particles increased, especially the SS316L 500 µm particles, significant permanent membrane rupture, GDL damage, and cavities in the MEA were observed. Figure 1 illustrates the types of observed MEA damage associated with particle sizes. As the particle size increased, the prevalence of some damage types also rose, highlighting the importance of mitigating damage from larger particles. Performance analysis indicated that cyclic voltammetry and polarization curve data could effectively identify early cell failures caused by damage incurred by the particles. Different shapes and surface morphologies of SS316L particles were further tested with a thinner chemically and mechanically reinforced GORE-SELECT® membrane (MemB) for mitigation purposes, as they caused the maximum damage to the MemA MEA. It was found that MemB could accommodate all four selected particles, despite varying degrees of surface randomness, without any membrane ruptures after the decal transfer phase. However, significant permanent damage to other MEA components remained evident. Keywords: Quality control, cost reduction, X-ray computed tomography, foreign particles Acknowledgments This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. References J. Chen, H. Liu, Y. A. Huang, and Z. Yin, J. Manuf. Process. , 23 , 175–182 (2016). M. Bahrami et al., J. Electrochem. Soc., 170 , 114527 (2023). N. Kumar et al., J. Electrochem. Soc. , 171 , 074513 (2024) Y. Singh, F. P. Orfino, M. Dutta, and E. Kjeang, J. Electrochem. Soc. , 164 , F1331–F1341 (2017). Figure 1
- 22 November 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-02 (44) , 3062
Impact of Irregular Microporous Layer on Chemo-Mechanical Membrane Degradation Investigated by 4D in-Situ Fuel Cell Visualization
Membrane durability is critical to the performance and safe operation of proton exchange membrane fuel cells (PEMFC). To address chemical and mechanical membrane degradation mechanisms, substantial mitigation strategies have been developed to enhance the strength of membranes. However, as a system, it is also important to make sure that the membrane electrode assembly (MEA) subcomponents and their integration do not produce unexpected non-uniformities in the manufacturing process, which may lead to premature membrane failure. The interaction between the membrane and gas diffusion media, such as gas diffusion layers (GDLs) and microporous layers (MPLs), was deemed as one of the major root causes for many membrane failure modes [1]. Previously reported mechanisms include elevated membrane buckling induced by micro sags or voids on MPL surface, and local impingement due to GDL fiber protrusion [1]. These non-uniformity features within the MPL and GDL can be natural irregularities from manufacturing, or unexpected damage during handling, and are difficult to control and characterize due to the random nature of the porous fibrous structure of the GDL. In a previous talk [2], the impact of though-plane GDL holes was discussed as they may relate or contribute to the combined chemo-mechanical membrane degradation mechanism. Both accelerated stress testing (AST) and X-ray computed tomography (XCT) imaging results suggest that GDL holes can be harmful to chemical and mechanical membrane degradation and the level of severity depends on their size and location. As a result, further in-depth research is warranted to capture the salient interactions between membrane degradation mechanisms and GDL non-uniformities. The objective of the present work is to determine the influences of missing MPL spots on fuel cell membrane chemo-mechanical durability. Compared to through-plane GDL holes, the fiber structure of the GDL was left intact, while only the MPL layer was completely removed at select locations. The study was carried out using a previously disclosed four dimensional (three spatial dimensions plus one temporal dimension) in-situ XCT visualization technique [3], where membrane degradation was traced at different life stages over time. The MEAs used in this work were composed of GORE-SELECT® membrane, crack free Pt based catalyst layers (CLs), and AvCarb® GDLs with customized smooth and crack free MPL. Circular missing MPL spots were artificially created by laser micromachining, with precisely controlled laser beam energy to only remove the MPL without damaging the GDL substrate. Missing MPLs of multiple controlled sizes were placed at strategic locations, both under flow channels and lands, on anode or cathode GDLs. The MEAs were custom designed small scale MEAs [3] for in-situ XCT visualization, and were subjected to a custom AST protocol imparting combined chemo-mechanical stresses [3] in an alternating pattern. The results confirmed that missing MPL spots are indeed harmful to the membrane durability, mainly through GDL fiber impingement. The impact level of the missing MPL non-uniformity highly depends on its location. Under flow channels, membrane buckling and associated CL crack formation were the major failure modes induced by missing MPL. Regardless of which electrode had the missing MPL, CL cracks tended to initiate either from GDL impinging locations or within voids of the GDL substrate. However, both membrane buckling and CL cracks were moderate, and their influence on MEA performance and durability was minor. Under the supporting lands, GDL impinging and membrane penetration became the major failure modes instead of membrane buckling and CL cracks, which was assessed to be due to the elevated through-plane compression. GDL impinging can be detrimental to MEA performance and membrane durability by penetrating through the membrane and raise electrode shorting, which was validated through a control experiment with MPL-free GDL. Keywords: fuel cell; membrane durability; gas diffusion layer; mechanical degradation; chemical degradation; X-ray computed tomography Acknowledgements: This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. References: [1] D. Ramani, N.S. Khattra, Y. Singh, F.P. Orfino, M. Dutta, E. Kjeang, Journal of Power Sources 512 (2021) 230431. [2] Y. Chen, A. Bahrami, N. Kumar, F.P. Orfino, M. Dutta, E.N. Alvar, M. Lauritzen, E. Setzler, A. Agapov, E. Kjeang, Meet. Abstr. MA2023-02 (2023) 1780. [3] Y. Chen, M. Bahrami, N. Kumar, F.P. Orfino, M. Dutta, M. Lauritzen, E. Setzler, A.L. Agapov, E. Kjeang, J. Electrochem. Soc. 170 (2023) 114526. Figure 1
- 22 November 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-02 (44) , 3062
Impact of Irregular Microporous Layer on Chemo-Mechanical Membrane Degradation Investigated by 4D in-Situ Fuel Cell Visualization
Membrane durability is critical to the performance and safe operation of proton exchange membrane fuel cells (PEMFC). To address chemical and mechanical membrane degradation mechanisms, substantial mitigation strategies have been developed to enhance the strength of membranes. However, as a system, it is also important to make sure that the membrane electrode assembly (MEA) subcomponents and their integration do not produce unexpected non-uniformities in the manufacturing process, which may lead to premature membrane failure. The interaction between the membrane and gas diffusion media, such as gas diffusion layers (GDLs) and microporous layers (MPLs), was deemed as one of the major root causes for many membrane failure modes [1]. Previously reported mechanisms include elevated membrane buckling induced by micro sags or voids on MPL surface, and local impingement due to GDL fiber protrusion [1]. These non-uniformity features within the MPL and GDL can be natural irregularities from manufacturing, or unexpected damage during handling, and are difficult to control and characterize due to the random nature of the porous fibrous structure of the GDL. In a previous talk [2], the impact of though-plane GDL holes was discussed as they may relate or contribute to the combined chemo-mechanical membrane degradation mechanism. Both accelerated stress testing (AST) and X-ray computed tomography (XCT) imaging results suggest that GDL holes can be harmful to chemical and mechanical membrane degradation and the level of severity depends on their size and location. As a result, further in-depth research is warranted to capture the salient interactions between membrane degradation mechanisms and GDL non-uniformities. The objective of the present work is to determine the influences of missing MPL spots on fuel cell membrane chemo-mechanical durability. Compared to through-plane GDL holes, the fiber structure of the GDL was left intact, while only the MPL layer was completely removed at select locations. The study was carried out using a previously disclosed four dimensional (three spatial dimensions plus one temporal dimension) in-situ XCT visualization technique [3], where membrane degradation was traced at different life stages over time. The MEAs used in this work were composed of GORE-SELECT® membrane, crack free Pt based catalyst layers (CLs), and AvCarb® GDLs with customized smooth and crack free MPL. Circular missing MPL spots were artificially created by laser micromachining, with precisely controlled laser beam energy to only remove the MPL without damaging the GDL substrate. Missing MPLs of multiple controlled sizes were placed at strategic locations, both under flow channels and lands, on anode or cathode GDLs. The MEAs were custom designed small scale MEAs [3] for in-situ XCT visualization, and were subjected to a custom AST protocol imparting combined chemo-mechanical stresses [3] in an alternating pattern. The results confirmed that missing MPL spots are indeed harmful to the membrane durability, mainly through GDL fiber impingement. The impact level of the missing MPL non-uniformity highly depends on its location. Under flow channels, membrane buckling and associated CL crack formation were the major failure modes induced by missing MPL. Regardless of which electrode had the missing MPL, CL cracks tended to initiate either from GDL impinging locations or within voids of the GDL substrate. However, both membrane buckling and CL cracks were moderate, and their influence on MEA performance and durability was minor. Under the supporting lands, GDL impinging and membrane penetration became the major failure modes instead of membrane buckling and CL cracks, which was assessed to be due to the elevated through-plane compression. GDL impinging can be detrimental to MEA performance and membrane durability by penetrating through the membrane and raise electrode shorting, which was validated through a control experiment with MPL-free GDL. Keywords: fuel cell; membrane durability; gas diffusion layer; mechanical degradation; chemical degradation; X-ray computed tomography Acknowledgements: This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. References: [1] D. Ramani, N.S. Khattra, Y. Singh, F.P. Orfino, M. Dutta, E. Kjeang, Journal of Power Sources 512 (2021) 230431. [2] Y. Chen, A. Bahrami, N. Kumar, F.P. Orfino, M. Dutta, E.N. Alvar, M. Lauritzen, E. Setzler, A. Agapov, E. Kjeang, Meet. Abstr. MA2023-02 (2023) 1780. [3] Y. Chen, M. Bahrami, N. Kumar, F.P. Orfino, M. Dutta, M. Lauritzen, E. Setzler, A.L. Agapov, E. Kjeang, J. Electrochem. Soc. 170 (2023) 114526. Figure 1
- 22 November 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-02 (43) , 2957
Simulation of in-Situ Chemical Membrane Degradation in the Presence of Fe and Ce Cations in Reinforced Fuel Cell Membranes
A PEM fuel cell’s durability and lifetime are affected by various degradation phenomena, among which chemical degradation of PEM material exerts the most damage. Chemical degradation of PEM occurs when reactive radicals such as hydroxyl (·OH) and hydroperoxyl (·OOH) are generated from the decomposition of hydrogen peroxide. The radicals chemically attack the main and side chains of the perfluorosulfonic acid-based PEM and change its internal chemical structure. This leads to excessive membrane thinning and pinhole formation that causes higher gas crossover and electrode shorting inside the PEM fuel cell1. The generation of harmful radicals accelerates in the presence of Fenton’s metal, such as iron (Fe)2. Evaluation of PEM fuel cell chemical degradation durability is performed using long-term pure chemical accelerated stress test (AST) under high temperature (T), low relative humidity (RH), and open circuit voltage (OCV) conditions3. Physical characterization of a membrane sample used in a fuel cell can help to visualize and assess damage incurred during an AST. These results, however, fail to encompass the formation rate of radicals and intermediate degradation products generated during the AST3. To overcome these issues, computational fluid dynamics models are developed that simulate the evolution of degraded products and predict the lifetime of PEM fuel cells4,5. The present work aims to develop an in-situ one-dimensional (1-D) transient chemical degradation model that describes reaction-transport phenomena within the membrane electrode assembly (MEA) in the presence of Fe and Ce cations. This work considers mechanically reinforced GORE-SELECT® 15 µm baseline (MemA) and chemically and mechanically reinforced 12 µm (MemB-Ce) membranes. The developed in-situ model simulates pure chemical AST operating conditions with variable Fe ion loading and follows the computational algorithms originally presented by Wong and Kjeang4. The model successfully predicted that side chain scission is followed by main chain unzipping, as reported in the literature6. The evaluation of the change in ionomer structure by chemical degradation was done by computing the temporal concentration profile of intermediate degraded ionomer species, hydrogen peroxide, and membrane thickness reduction. The 1-D model also encapsulates the concentration profile of Fe2+ and Fe3+ ions across the PEM and predicts their temporal distribution throughout the simulated AST duration under OCV conditions. It was observed that the MemA thickness decreased rapidly in the presence of Fe ions, as shown in Figure 1. The computational parameters and results were calibrated and validated using in-house AST results for MEAs with embedded Fe metallic particles, which were shown to completely dissolve during conditioning and hence treated as uniformly distributed Fe cations with an initial concentration of 900 ppm at the beginning-of-life7. The model identified a limiting Fe ion concentration limit of 100 ppm that accentuates the chemical attack. Experimentally, a low Fe concentration of 10 ppm was determined in the baseline MemA, which also reduced the membrane thickness within 1125 h of operation, as shown in Figure 1. It is known that cerium (Ce) ions can scavenge harmful radicals and increase the lifetime of PEM fuel cells8. The model, therefore, simulates the effectiveness of Ce ions in the MemB-Ce membrane and the temporal distribution of Ce3+/Ce4+ ions and shows a lower rate of membrane thickness reduction, as shown in Figure 1. The modelling framework was, therefore, able to predict PEM fuel cell lifetime in conjunction with the transport behaviour of both harmful and beneficial cations as well as their interactions during the chemical degradation process at OCV conditions. Keywords: PEM fuel cell, fuel cell durability, chemical degradation model, in-situ modelling, iron, cerium Acknowledgements This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. It was also undertaken in part thanks to funding from the Canada Research Chairs program. References J. Healy et al., Fuel Cells, 5, 302–308 (2005). S. Kundu, L. C. Simon, and M. W. Fowler, Polym. Degrad. Stab., 93, 214–224 (2008). Y. Singh, F. P. Orfino, M. Dutta, and E. Kjeang, J. Electrochem. Soc., 164, F1331–F1341 (2017). K. H. Wong and E. Kjeang, J. Electrochem. Soc., 161, F823–F832 (2014). R. B. Ferreira, D. S. Falcão, and A. M. F. R. Pinto, Int. J. Hydrogen Energy, 46, 1106–1120 (2021). L. Ghassemzadeh, K. D. Kreuer, J. Maier, and K. Müller, J. Phys. Chem. C, 114, 14635–14645 (2010). N. Kumar et al., ECS Meet. Abstr., MA2023-02, 1919–1919 (2023). S. M. Stewart, D. Spernjak, R. Borup, A. Datye, and F. Garzon, ECS Electrochem. Lett., 3, F19–F22 (2014). Figure 1
- 22 November 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-02 (43) , 2957
Simulation of in-Situ Chemical Membrane Degradation in the Presence of Fe and Ce Cations in Reinforced Fuel Cell Membranes
A PEM fuel cell’s durability and lifetime are affected by various degradation phenomena, among which chemical degradation of PEM material exerts the most damage. Chemical degradation of PEM occurs when reactive radicals such as hydroxyl (·OH) and hydroperoxyl (·OOH) are generated from the decomposition of hydrogen peroxide. The radicals chemically attack the main and side chains of the perfluorosulfonic acid-based PEM and change its internal chemical structure. This leads to excessive membrane thinning and pinhole formation that causes higher gas crossover and electrode shorting inside the PEM fuel cell1. The generation of harmful radicals accelerates in the presence of Fenton’s metal, such as iron (Fe)2. Evaluation of PEM fuel cell chemical degradation durability is performed using long-term pure chemical accelerated stress test (AST) under high temperature (T), low relative humidity (RH), and open circuit voltage (OCV) conditions3. Physical characterization of a membrane sample used in a fuel cell can help to visualize and assess damage incurred during an AST. These results, however, fail to encompass the formation rate of radicals and intermediate degradation products generated during the AST3. To overcome these issues, computational fluid dynamics models are developed that simulate the evolution of degraded products and predict the lifetime of PEM fuel cells4,5. The present work aims to develop an in-situ one-dimensional (1-D) transient chemical degradation model that describes reaction-transport phenomena within the membrane electrode assembly (MEA) in the presence of Fe and Ce cations. This work considers mechanically reinforced GORE-SELECT® 15 µm baseline (MemA) and chemically and mechanically reinforced 12 µm (MemB-Ce) membranes. The developed in-situ model simulates pure chemical AST operating conditions with variable Fe ion loading and follows the computational algorithms originally presented by Wong and Kjeang4. The model successfully predicted that side chain scission is followed by main chain unzipping, as reported in the literature6. The evaluation of the change in ionomer structure by chemical degradation was done by computing the temporal concentration profile of intermediate degraded ionomer species, hydrogen peroxide, and membrane thickness reduction. The 1-D model also encapsulates the concentration profile of Fe2+ and Fe3+ ions across the PEM and predicts their temporal distribution throughout the simulated AST duration under OCV conditions. It was observed that the MemA thickness decreased rapidly in the presence of Fe ions, as shown in Figure 1. The computational parameters and results were calibrated and validated using in-house AST results for MEAs with embedded Fe metallic particles, which were shown to completely dissolve during conditioning and hence treated as uniformly distributed Fe cations with an initial concentration of 900 ppm at the beginning-of-life7. The model identified a limiting Fe ion concentration limit of 100 ppm that accentuates the chemical attack. Experimentally, a low Fe concentration of 10 ppm was determined in the baseline MemA, which also reduced the membrane thickness within 1125 h of operation, as shown in Figure 1. It is known that cerium (Ce) ions can scavenge harmful radicals and increase the lifetime of PEM fuel cells8. The model, therefore, simulates the effectiveness of Ce ions in the MemB-Ce membrane and the temporal distribution of Ce3+/Ce4+ ions and shows a lower rate of membrane thickness reduction, as shown in Figure 1. The modelling framework was, therefore, able to predict PEM fuel cell lifetime in conjunction with the transport behaviour of both harmful and beneficial cations as well as their interactions during the chemical degradation process at OCV conditions. Keywords: PEM fuel cell, fuel cell durability, chemical degradation model, in-situ modelling, iron, cerium Acknowledgements This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. It was also undertaken in part thanks to funding from the Canada Research Chairs program. References J. Healy et al., Fuel Cells, 5, 302–308 (2005). S. Kundu, L. C. Simon, and M. W. Fowler, Polym. Degrad. Stab., 93, 214–224 (2008). Y. Singh, F. P. Orfino, M. Dutta, and E. Kjeang, J. Electrochem. Soc., 164, F1331–F1341 (2017). K. H. Wong and E. Kjeang, J. Electrochem. Soc., 161, F823–F832 (2014). R. B. Ferreira, D. S. Falcão, and A. M. F. R. Pinto, Int. J. Hydrogen Energy, 46, 1106–1120 (2021). L. Ghassemzadeh, K. D. Kreuer, J. Maier, and K. Müller, J. Phys. Chem. C, 114, 14635–14645 (2010). N. Kumar et al., ECS Meet. Abstr., MA2023-02, 1919–1919 (2023). S. M. Stewart, D. Spernjak, R. Borup, A. Datye, and F. Garzon, ECS Electrochem. Lett., 3, F19–F22 (2014). Figure 1
- 22 December 2023
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2023-02 (38) , 1843
Impact of Reinforced Polymer Electrolyte Membrane Scratch on Fuel Cell Durability Using 4D X-Ray Computed Tomography Technique
PEMFCs, or Polymer Electrolyte Membrane Fuel Cells, can be used in both stationary power and transportation applications and are promising for use in heavy duty electric vehicles due to their high energy density, ability to be refueled quickly, and extended range, which are key challenges for battery-powered vehicles [1]. Despite these advantages, there are still obstacles preventing the widespread commercialization of PEMFCs, one of which is production cost [2]. To reduce manufacturing costs, it is imperative to ensure that quality control rejects and scraps are minimized. Moreover, enhancing component integration defect detection would ensure the durability of the fuel cell and enhance its operational lifetime. However, robust quality control requires a thorough understanding of potential non-uniformities and their effects on fuel cell performance and operational degradation. Non-uniformities of the membrane electrolyte assembly (MEA) can result in durability issues by damaging the membrane and making it more vulnerable to mechanical and chemical stress during the operation [3]. Several studies have been done on cation contamination and membrane pinholes and their effect on fuel cell performance and durability [4,5] but little attention has been paid to other types of non-uniformities such as membrane scratches and foreign particles, which may also conceivably affect durability [6]. By implementing 4D in-situ X-ray computed tomography (XCT) [7,8], the current work aims to track the evolution of scratches that appear on a reinforced membrane surface during fabrication and its specific objective is to determine the impacts of membrane scratches on membrane durability in fuel cells. The study was conducted by using small-scale fuel cells with GORE-SELECT® membranes that were intentionally scratched with a razor blade, subjecting them to combined chemomechanical membrane accelerated stress test (AST), and monitoring the membrane degradation and evolution of the scratches using 4D-XCT throughout the AST. During the fabrication step, the depth of scratches was regulated by a weak bond between the reinforcement layer and the perfluorosulfonic acid (PFSA) layer, i.e., the scratches did not tear through the reinforcement. Furthermore, the scratches did not adversely impact the initial cell performance. However, during AST operation the evolution of the scratched region was affected by several factors, including the friction between the layers of the membrane electrode assembly, the width of the scratch (Figure 1), the presence of membrane debris, and the extent of membrane strain. Additionally, it was observed that changes in the quality of catalyst layer transfer onto the scratched region can alter the degradation pattern and potentially create a self-mitigating mechanism. These findings may be used to develop more optimized quality control measures for membrane scratches in fuel cell production. Acknowledgements This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. Keywords: fuel cell; membrane durability; X-ray computed tomography; membrane scratch; manufacturing References [1] Cullen DA, Neyerlin KC, Ahluwalia RK, Mukundan R, More KL, Borup RL, et al. New roads and challenges for fuel cells in heavy-duty transportation. Nat Energy 2021;6:462–74. https://doi.org/10.1038/s41560-021-00775-z. [2] Whiston MM, Azevedo IL, Litster S, Whitefoot KS, Samaras C, Whitacre JF. Expert assessments of the cost and expected future performance of proton exchange membrane fuel cells for vehicles. Proc Natl Acad Sci U S A 2019;116:4899–904. [3] De Bruijn FA, Dam VAT, Janssen GJM. Review: Durability and degradation issues of PEM fuel cell components. Fuel Cells 2008;8:3–22. [4] Tavassoli A, Lim C, Kolodziej J, Lauritzen M, Knights S, Wang GG, et al. Effect of catalyst layer defects on local membrane degradation in polymer electrolyte fuel cells. J Power Sources 2016;322:17–25. [5] Lü W, Liu Z, Wang C, Mao Z, Zhang M. The effects of pinholes on proton exchange membrane fuel cell performance. Int J Energy Res 2011;35:24–30. [6] Kundu S, Fowler MW, Simon LC, Grot S. Morphological features (defects) in fuel cell membrane electrode assemblies. J Power Sources 2006;157:650–6. [7] Ramani D, Singh Y, White RT, Wegener M, Orfino FP, Dutta M, et al. 4D in situ visualization of mechanical degradation evolution in reinforced fuel cell membranes. Int J Hydrogen Energy 2020;45:10089–103. [8] White RT, Eberhardt SH, Singh Y, Haddow T, Dutta M, Orfino FP, et al. Four-dimensional joint visualization of electrode degradation and liquid water distribution inside operating polymer electrolyte fuel cells. Sci Rep 2019;9:1–12. Figure 1
- 22 December 2023
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2023-02 (38) , 1843
Impact of Reinforced Polymer Electrolyte Membrane Scratch on Fuel Cell Durability Using 4D X-Ray Computed Tomography Technique
PEMFCs, or Polymer Electrolyte Membrane Fuel Cells, can be used in both stationary power and transportation applications and are promising for use in heavy duty electric vehicles due to their high energy density, ability to be refueled quickly, and extended range, which are key challenges for battery-powered vehicles [1]. Despite these advantages, there are still obstacles preventing the widespread commercialization of PEMFCs, one of which is production cost [2]. To reduce manufacturing costs, it is imperative to ensure that quality control rejects and scraps are minimized. Moreover, enhancing component integration defect detection would ensure the durability of the fuel cell and enhance its operational lifetime. However, robust quality control requires a thorough understanding of potential non-uniformities and their effects on fuel cell performance and operational degradation. Non-uniformities of the membrane electrolyte assembly (MEA) can result in durability issues by damaging the membrane and making it more vulnerable to mechanical and chemical stress during the operation [3]. Several studies have been done on cation contamination and membrane pinholes and their effect on fuel cell performance and durability [4,5] but little attention has been paid to other types of non-uniformities such as membrane scratches and foreign particles, which may also conceivably affect durability [6]. By implementing 4D in-situ X-ray computed tomography (XCT) [7,8], the current work aims to track the evolution of scratches that appear on a reinforced membrane surface during fabrication and its specific objective is to determine the impacts of membrane scratches on membrane durability in fuel cells. The study was conducted by using small-scale fuel cells with GORE-SELECT® membranes that were intentionally scratched with a razor blade, subjecting them to combined chemomechanical membrane accelerated stress test (AST), and monitoring the membrane degradation and evolution of the scratches using 4D-XCT throughout the AST. During the fabrication step, the depth of scratches was regulated by a weak bond between the reinforcement layer and the perfluorosulfonic acid (PFSA) layer, i.e., the scratches did not tear through the reinforcement. Furthermore, the scratches did not adversely impact the initial cell performance. However, during AST operation the evolution of the scratched region was affected by several factors, including the friction between the layers of the membrane electrode assembly, the width of the scratch (Figure 1), the presence of membrane debris, and the extent of membrane strain. Additionally, it was observed that changes in the quality of catalyst layer transfer onto the scratched region can alter the degradation pattern and potentially create a self-mitigating mechanism. These findings may be used to develop more optimized quality control measures for membrane scratches in fuel cell production. Acknowledgements This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. Keywords: fuel cell; membrane durability; X-ray computed tomography; membrane scratch; manufacturing References [1] Cullen DA, Neyerlin KC, Ahluwalia RK, Mukundan R, More KL, Borup RL, et al. New roads and challenges for fuel cells in heavy-duty transportation. Nat Energy 2021;6:462–74. https://doi.org/10.1038/s41560-021-00775-z. [2] Whiston MM, Azevedo IL, Litster S, Whitefoot KS, Samaras C, Whitacre JF. Expert assessments of the cost and expected future performance of proton exchange membrane fuel cells for vehicles. Proc Natl Acad Sci U S A 2019;116:4899–904. [3] De Bruijn FA, Dam VAT, Janssen GJM. Review: Durability and degradation issues of PEM fuel cell components. Fuel Cells 2008;8:3–22. [4] Tavassoli A, Lim C, Kolodziej J, Lauritzen M, Knights S, Wang GG, et al. Effect of catalyst layer defects on local membrane degradation in polymer electrolyte fuel cells. J Power Sources 2016;322:17–25. [5] Lü W, Liu Z, Wang C, Mao Z, Zhang M. The effects of pinholes on proton exchange membrane fuel cell performance. Int J Energy Res 2011;35:24–30. [6] Kundu S, Fowler MW, Simon LC, Grot S. Morphological features (defects) in fuel cell membrane electrode assemblies. J Power Sources 2006;157:650–6. [7] Ramani D, Singh Y, White RT, Wegener M, Orfino FP, Dutta M, et al. 4D in situ visualization of mechanical degradation evolution in reinforced fuel cell membranes. Int J Hydrogen Energy 2020;45:10089–103. [8] White RT, Eberhardt SH, Singh Y, Haddow T, Dutta M, Orfino FP, et al. Four-dimensional joint visualization of electrode degradation and liquid water distribution inside operating polymer electrolyte fuel cells. Sci Rep 2019;9:1–12. Figure 1
- 22 December 2023
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2023-02 (37) , 1780
Impact of GDL Hole on Chemo-Mechanical Membrane Degradation Investigated by 4D in-Situ Visualization
Membrane electrode assembly (MEA) is the core unit of a fuel cell system, which is composed of proton exchange membrane (PEM), sandwiched on both sides by catalyst layers (CLs) and gas diffusion layers (GDLs). The membrane is subjected to various chemical and mechanical stresses during fuel cell operation, and these stresses will cause membrane degradation over time. Also, the interaction between membrane and other fuel cell components such as CLs and GDLs contributes uncertainty to the membrane degradation process. Previous morphological studies [1] on CLs and GDLs discovered common non-uniform features in these materials such as clusters, sags, cracks, and holes. In addition, such features could also appear during the MEAs assembly [1] process. Previous membrane degradation study discovered buckling driven membrane failure [2], which is strongly related to CL or GDL sags, cracks, and holes. Additionally, impinging driven membrane failure was also reported [2], which is caused by clusters and peaks on CL or GDL surfaces. Models were also developed to understand the mechanism of mechanical membrane degradation related to buckling. For instance, Ramani et al. [2] created a model to simulate membrane buckling into GDL surface pores, and identified stress concentration at the buckling center as the root cause of crack formation. Comparing MEAs made with high and low surface roughness GDLs, it was confirmed that GDL with low surface roughness has significant mitigatory impact on mechanical membrane durability. However, to the authors’ best knowledge, the level of impact of such non-uniform features under combined chemo-mechanical degradation, which is the most common form of membrane degradation during regular fuel cell operation, has not yet been reported. In this work, the objective is to understand the specific impacts of GDL holes as they relate or contribute to the combined chemo-mechanical membrane degradation mechanism and associated membrane durability in polymer electrolyte fuel cells. The study was carried out using a four dimensional (three spatial dimensions plus one temporal dimension) in-situ methodology achieved through X-ray computed tomography (XCT) visualization [3], and the MEAs were made of GORE-SELECT® membrane, Pt based CLs, and AvCarb® GDLs with smooth and crack free microporous layer (MPL). Through-thickness circular GDL holes were introduced with multiple controlled sizes at multiple strategic locations, on anode or cathode GDL. The MEAs were custom designed small scale MEAs with 0.39 cm2 active area for in-situ XCT visualization, and the cells were subjected to a custom accelerated stress test (AST) protocol imparting combined chemo-mechanical stresses in an alternating pattern [3]. The graphite endplates had narrower flow field compared to previously used ones [3], which can reduce membrane degradation rate and better deliver compressive stress to the MEA. A baseline MEA without GDL hole was first tested, with only minor membrane thinning observed. For the GDL hole MEAs, it was discovered that smaller holes were more impactful on membrane durability than larger holes. Among the three selected hole sizes (2.0, 0.5, and 0.2 mm2), through-plane membrane cracks were only observed under the smallest holes, both at the hole center and edge, which are the two stress concentration locations. On the CL surface, cracks were observed at the GDL hole center as a crack network, and along the hole edge, as indicated in the figure. Although the GDL holes are expected to mainly alter mechanical membrane degradation, it was discovered that MEAs with through-plane membrane cracks also had higher membrane thinning rate compared to the baseline. However, the non-uniformity MEAs without through-plane membrane cracks had similar membrane thinning rate as the baseline test. Therefore, the through-plane membrane cracks likely elevated chemical stressors as well; hypothetically, through increased gas crossover. The AST results suggest that GDL holes can be harmful to membrane chemo-mechanical degradation and the level of severity depends on their size and location. Keywords: fuel cell; membrane durability; gas diffusion layer defect; mechanical degradation; chemical degradation; X-ray computed tomography Acknowledgements: This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. References: [1] S. Prass, S. Hasanpour, P.K. Sow, A.B. Phillion, W. Mérida, Journal of Power Sources. 319 (2016) 82–89. [2] D. Ramani, N.S. Khattra, Y. Singh, F.P. Orfino, M. Dutta, E. Kjeang, Journal of Power Sources. 512 (2021) 230431. [3] Y. Chen, Y. Singh, D. Ramani, F.P. Orfino, M. Dutta, E. Kjeang, Journal of Power Sources. 520 (2022) 230674. Figure 1
- 22 December 2023
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2023-02 (37) , 1780
Impact of GDL Hole on Chemo-Mechanical Membrane Degradation Investigated by 4D in-Situ Visualization
Membrane electrode assembly (MEA) is the core unit of a fuel cell system, which is composed of proton exchange membrane (PEM), sandwiched on both sides by catalyst layers (CLs) and gas diffusion layers (GDLs). The membrane is subjected to various chemical and mechanical stresses during fuel cell operation, and these stresses will cause membrane degradation over time. Also, the interaction between membrane and other fuel cell components such as CLs and GDLs contributes uncertainty to the membrane degradation process. Previous morphological studies [1] on CLs and GDLs discovered common non-uniform features in these materials such as clusters, sags, cracks, and holes. In addition, such features could also appear during the MEAs assembly [1] process. Previous membrane degradation study discovered buckling driven membrane failure [2], which is strongly related to CL or GDL sags, cracks, and holes. Additionally, impinging driven membrane failure was also reported [2], which is caused by clusters and peaks on CL or GDL surfaces. Models were also developed to understand the mechanism of mechanical membrane degradation related to buckling. For instance, Ramani et al. [2] created a model to simulate membrane buckling into GDL surface pores, and identified stress concentration at the buckling center as the root cause of crack formation. Comparing MEAs made with high and low surface roughness GDLs, it was confirmed that GDL with low surface roughness has significant mitigatory impact on mechanical membrane durability. However, to the authors’ best knowledge, the level of impact of such non-uniform features under combined chemo-mechanical degradation, which is the most common form of membrane degradation during regular fuel cell operation, has not yet been reported. In this work, the objective is to understand the specific impacts of GDL holes as they relate or contribute to the combined chemo-mechanical membrane degradation mechanism and associated membrane durability in polymer electrolyte fuel cells. The study was carried out using a four dimensional (three spatial dimensions plus one temporal dimension) in-situ methodology achieved through X-ray computed tomography (XCT) visualization [3], and the MEAs were made of GORE-SELECT® membrane, Pt based CLs, and AvCarb® GDLs with smooth and crack free microporous layer (MPL). Through-thickness circular GDL holes were introduced with multiple controlled sizes at multiple strategic locations, on anode or cathode GDL. The MEAs were custom designed small scale MEAs with 0.39 cm2 active area for in-situ XCT visualization, and the cells were subjected to a custom accelerated stress test (AST) protocol imparting combined chemo-mechanical stresses in an alternating pattern [3]. The graphite endplates had narrower flow field compared to previously used ones [3], which can reduce membrane degradation rate and better deliver compressive stress to the MEA. A baseline MEA without GDL hole was first tested, with only minor membrane thinning observed. For the GDL hole MEAs, it was discovered that smaller holes were more impactful on membrane durability than larger holes. Among the three selected hole sizes (2.0, 0.5, and 0.2 mm2), through-plane membrane cracks were only observed under the smallest holes, both at the hole center and edge, which are the two stress concentration locations. On the CL surface, cracks were observed at the GDL hole center as a crack network, and along the hole edge, as indicated in the figure. Although the GDL holes are expected to mainly alter mechanical membrane degradation, it was discovered that MEAs with through-plane membrane cracks also had higher membrane thinning rate compared to the baseline. However, the non-uniformity MEAs without through-plane membrane cracks had similar membrane thinning rate as the baseline test. Therefore, the through-plane membrane cracks likely elevated chemical stressors as well; hypothetically, through increased gas crossover. The AST results suggest that GDL holes can be harmful to membrane chemo-mechanical degradation and the level of severity depends on their size and location. Keywords: fuel cell; membrane durability; gas diffusion layer defect; mechanical degradation; chemical degradation; X-ray computed tomography Acknowledgements: This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. References: [1] S. Prass, S. Hasanpour, P.K. Sow, A.B. Phillion, W. Mérida, Journal of Power Sources. 319 (2016) 82–89. [2] D. Ramani, N.S. Khattra, Y. Singh, F.P. Orfino, M. Dutta, E. Kjeang, Journal of Power Sources. 512 (2021) 230431. [3] Y. Chen, Y. Singh, D. Ramani, F.P. Orfino, M. Dutta, E. Kjeang, Journal of Power Sources. 520 (2022) 230674. Figure 1
- 22 December 2023
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2023-02 (39) , 1919
Chemo-Mechanical Durability of Reinforced Fuel Cell Membranes in the Presence of Metallic Foreign Particles
High-throughput production is vital to achieve cost-effective proton exchange membrane fuel cells (PEMFCs) at scale1. The high-volume mass production of PEMFCs using industrial manufacturing machinery may however introduce unwanted material in the final product due to the wear and tear of the machinery. As an example, roll-to-roll processes applied to the manufacture of catalyst coated membrane (CCM) generally use Fe alloys such as stainless steel2 components that could release fine metallic particles or related debris that may affect the product quality3,4. Therefore, it is important to understand the fundamental impact of such non-uniformities on PEMFC performance and durability. This work focusses on the impact of slightly oxidized iron (Fe) and stainless steel 316L (SS316L) micro-particles entrapped between the cathode catalyst layer (CCL) and a GORE-SELECT® Membrane A. Fe cations are considered as Fenton’s catalyst/reagent which enhance harmful radical generation and ionomer attack, known to weaken its mechanical strength and ionic conductivity5. Therefore, membrane electrode assemblies (MEAs) containing solid Fe and SS316L particles were prepared to conduct in-situ PEMFC experiments and identify their impact on membrane degradation and durability. The chosen particles were placed carefully on the bare membrane at selected locations based on the flow field design of the graphite bipolar plates. Later, the assembled MEAs were tested using a small-scale fixture (SSF) fuel cell in a combined chemical and mechanical AST after beginning-of-life (BOL) conditioning and diagnostics6. X-ray computed tomography (XCT) has been shown to be a powerful and non-invasive 3D characterization tool for analyzing membrane degradation7,8. Thus, periodic same-location XCT visualization of the CCL-membrane interface was performed after every 10 AST cycles. According to the Fe Pourbaix diagram9, Fe oxidizes to Fe2+ at 0.77 V and indeed, in this work, complete dissolution of the Fe-50µm particles was observed leaving cavities at the CCL-membrane interface. This dissolution manifested as a distinct black spot in CT imaging, as highlighted by the enclosed red circle in Figure 1. In contrast, corrosion of SS316L particles is usually prevented by a native oxide layer formation during fuel cell operational conditions10. The Fe particle laden AST reached membrane failure within 30 cycles and indicates an escalation of degradation by global membrane thinning. This is substantially lower than the baseline AST without particles. The XCT images for Fe-50µm AST seen in Figure 1 show that severe global membrane thinning occurred in the Fe-50µm MEA, which contributed to a high electrochemical leak detection (ELDT) signal exceeding test failure criteria. In contrast, the SS316L MEA did not reach the threshold failure criteria for the AST duration, however, the average OCV remained lower as compared to the baseline MEA AST. XCT imaging showed that the SS316L- 50µm particles did not dissolve throughout the AST duration and the membrane thinning was more pronounced near the particle rather than globally. Additionally, we have evaluated whether chemically and mechanically mitigated GORE-SELECT Membrane® B could enable more robustness and minimize impact of multiple metallic particles. Analysis of combined chemo-mechanical AST with a larger dimension SS316L-500µm present on mitigated GORE-SELECT® Membrane B suggest that chemical and mechanical mitigation can reduce impact of large particles and enable lifetime response at the level close to baseline. In conclusion, the membrane lifetime and failure mode were found to be strongly dependent on the particle chemical composition and membrane degradation mitigation strategies, which are therefore should be considered at PEM design stages to reduce risks and improve CCM and MEA production quality. Keywords: PEM durability, quality control, cost reduction, XCT Acknowledgments This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. References H. Tsuchiya and O. Kobayashi, Int. J. Hydrogen Energy, 29, 985–990 (2004). J. Chen, H. Liu, Y. A. Huang, and Z. Yin, J. Manuf. Process., 23, 175–182 (2016). A. Phillips et al., Fuel Cells, 20, 60–69 (2020). A. Phillips, M. Ulsh, K. C. Neyerlin, J. Porter, and G. Bender, Int. J. Hydrogen Energy, 43, 6390–6399. J. G. Goodwin, K. Hongsirikarn, S. Greenway, and S. Creager, J. Power Sources, 195, 7213–7220 (2010). Y. Chen et al., J. Power Sources, 520, 230673 (2022). Y. Chen et al., J. Power Sources, 520, 230674 (2022). Y. Singh et al., J. Power Sources, 412, 224–237 (2019). R. Tolouei et al., Phys. Chem. Chem. Phys., 18, 19637–19646 (2016). N. Kumar et al., Int. J. Energy Res., 44, 6804–6818 (2020). Figure 1
- 22 December 2023
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2023-02 (39) , 1919
Chemo-Mechanical Durability of Reinforced Fuel Cell Membranes in the Presence of Metallic Foreign Particles
High-throughput production is vital to achieve cost-effective proton exchange membrane fuel cells (PEMFCs) at scale1. The high-volume mass production of PEMFCs using industrial manufacturing machinery may however introduce unwanted material in the final product due to the wear and tear of the machinery. As an example, roll-to-roll processes applied to the manufacture of catalyst coated membrane (CCM) generally use Fe alloys such as stainless steel2 components that could release fine metallic particles or related debris that may affect the product quality3,4. Therefore, it is important to understand the fundamental impact of such non-uniformities on PEMFC performance and durability. This work focusses on the impact of slightly oxidized iron (Fe) and stainless steel 316L (SS316L) micro-particles entrapped between the cathode catalyst layer (CCL) and a GORE-SELECT® Membrane A. Fe cations are considered as Fenton’s catalyst/reagent which enhance harmful radical generation and ionomer attack, known to weaken its mechanical strength and ionic conductivity5. Therefore, membrane electrode assemblies (MEAs) containing solid Fe and SS316L particles were prepared to conduct in-situ PEMFC experiments and identify their impact on membrane degradation and durability. The chosen particles were placed carefully on the bare membrane at selected locations based on the flow field design of the graphite bipolar plates. Later, the assembled MEAs were tested using a small-scale fixture (SSF) fuel cell in a combined chemical and mechanical AST after beginning-of-life (BOL) conditioning and diagnostics6. X-ray computed tomography (XCT) has been shown to be a powerful and non-invasive 3D characterization tool for analyzing membrane degradation7,8. Thus, periodic same-location XCT visualization of the CCL-membrane interface was performed after every 10 AST cycles. According to the Fe Pourbaix diagram9, Fe oxidizes to Fe2+ at 0.77 V and indeed, in this work, complete dissolution of the Fe-50µm particles was observed leaving cavities at the CCL-membrane interface. This dissolution manifested as a distinct black spot in CT imaging, as highlighted by the enclosed red circle in Figure 1. In contrast, corrosion of SS316L particles is usually prevented by a native oxide layer formation during fuel cell operational conditions10. The Fe particle laden AST reached membrane failure within 30 cycles and indicates an escalation of degradation by global membrane thinning. This is substantially lower than the baseline AST without particles. The XCT images for Fe-50µm AST seen in Figure 1 show that severe global membrane thinning occurred in the Fe-50µm MEA, which contributed to a high electrochemical leak detection (ELDT) signal exceeding test failure criteria. In contrast, the SS316L MEA did not reach the threshold failure criteria for the AST duration, however, the average OCV remained lower as compared to the baseline MEA AST. XCT imaging showed that the SS316L- 50µm particles did not dissolve throughout the AST duration and the membrane thinning was more pronounced near the particle rather than globally. Additionally, we have evaluated whether chemically and mechanically mitigated GORE-SELECT Membrane® B could enable more robustness and minimize impact of multiple metallic particles. Analysis of combined chemo-mechanical AST with a larger dimension SS316L-500µm present on mitigated GORE-SELECT® Membrane B suggest that chemical and mechanical mitigation can reduce impact of large particles and enable lifetime response at the level close to baseline. In conclusion, the membrane lifetime and failure mode were found to be strongly dependent on the particle chemical composition and membrane degradation mitigation strategies, which are therefore should be considered at PEM design stages to reduce risks and improve CCM and MEA production quality. Keywords: PEM durability, quality control, cost reduction, XCT Acknowledgments This research was supported by the Natural Sciences and Engineering Research Council of Canada, Canada Foundation for Innovation, British Columbia Knowledge Development Fund, Western Economic Diversification Canada, Ballard Power Systems, and W.L. Gore & Associates. This research was undertaken, in part, thanks to funding from the Canada Research Chairs program. References H. Tsuchiya and O. Kobayashi, Int. J. Hydrogen Energy, 29, 985–990 (2004). J. Chen, H. Liu, Y. A. Huang, and Z. Yin, J. Manuf. Process., 23, 175–182 (2016). A. Phillips et al., Fuel Cells, 20, 60–69 (2020). A. Phillips, M. Ulsh, K. C. Neyerlin, J. Porter, and G. Bender, Int. J. Hydrogen Energy, 43, 6390–6399. J. G. Goodwin, K. Hongsirikarn, S. Greenway, and S. Creager, J. Power Sources, 195, 7213–7220 (2010). Y. Chen et al., J. Power Sources, 520, 230673 (2022). Y. Chen et al., J. Power Sources, 520, 230674 (2022). Y. Singh et al., J. Power Sources, 412, 224–237 (2019). R. Tolouei et al., Phys. Chem. Chem. Phys., 18, 19637–19646 (2016). N. Kumar et al., Int. J. Energy Res., 44, 6804–6818 (2020). Figure 1
- 1 November 2020
- Published by Elsevier in Journal of Power Sources
- Vol. 477
Residual fatigue life modeling of fuel cell membranes
- 1 November 2020
- Published by Elsevier in Journal of Power Sources
- Vol. 477
Residual fatigue life modeling of fuel cell membranes
- Open Access
- 16 December 2019
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 167 (1) , 013528
Estimating the Durability of Polymer Electrolyte Fuel Cell Membranes Using a Fracture Percolation Model
During fuel cell operation, the polymer electrolyte membranes are subjected to chemical and mechanical degradation that have an adverse impact on the membrane lifetime and thus overall durability of the fuel cell. To understand the synergistic effect of these two fundamentally different modes of degradation, it is therefore essential to consider both these effects when modeling membrane failure. A kinetic approach using a fracture percolation model is presented in this work that takes into consideration the hazard rates of chemical and mechanical degradation of the membrane incorporated into a two-dimensional membrane lattice network. While the chemical hazard rate is based on the rate of mass loss occurring during fuel cell operation, the mechanical hazard rate is evaluated based on a stress-induced, thermally activated process. The model captures the characteristic mechanisms of failure under the action of these fundamentally different modes, and converts the hazard functions into realistic time scale. The individual effects of the two modes are then incorporated in the model to predict in agreement with measured data, the time to fracture initiation in the membrane for a given combination of chemical and mechanical load.
- 16 December 2019
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 167 (1) , 013528
Open AccessEstimating the Durability of Polymer Electrolyte Fuel Cell Membranes Using a Fracture Percolation Model
During fuel cell operation, the polymer electrolyte membranes are subjected to chemical and mechanical degradation that have an adverse impact on the membrane lifetime and thus overall durability of the fuel cell. To understand the synergistic effect of these two fundamentally different modes of degradation, it is therefore essential to consider both these effects when modeling membrane failure. A kinetic approach using a fracture percolation model is presented in this work that takes into consideration the hazard rates of chemical and mechanical degradation of the membrane incorporated into a two-dimensional membrane lattice network. While the chemical hazard rate is based on the rate of mass loss occurring during fuel cell operation, the mechanical hazard rate is evaluated based on a stress-induced, thermally activated process. The model captures the characteristic mechanisms of failure under the action of these fundamentally different modes, and converts the hazard functions into realistic time scale. The individual effects of the two modes are then incorporated in the model to predict in agreement with measured data, the time to fracture initiation in the membrane for a given combination of chemical and mechanical load.
- Open Access
- 9 October 2015
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 162 (14) , F1461-F1469
Microstructural and Mechanical Characterization of Catalyst Coated Membranes Subjected to In Situ Hygrothermal Fatigue
Catalyst coated membranes (CCMs) in polymer electrolyte fuel cells are subjected to mechanical stresses in the form of fatigue and creep that deteriorate the durability and lifetime of the cells. The present article aims to determine the effect of in-situ hygrothermal fatigue on the microstructure and mechanical properties of the CCM. The fatigue process is systematically explored by the application of two custom-developed accelerated mechanical stress test (AMST) experiments with periodic extraction of partially degraded CCMs. Cross sectional and top surface scanning electron microscope (SEM) images of the end-of-test CCMs reveal the formation of mechanically induced cracks and delamination due to cyclic tensile and compressive fatigue stress. Tensile and expansion tests are conducted at different stages of degradation to evaluate the evolution in the mechanical and hygrothermal properties of the CCM. The tensile test results indicate gradual reductions in final strain, ultimate tensile strength, and fracture toughness with increasing number of fatigue cycles. The decay in tensile properties is attributed to the microstructural damage and micro-cracks formed during the AMST. Moreover, it is shown that the hygrothermal expansion of the CCM is more sensitive to conditioning than mechanical degradation.
- 9 October 2015
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 162 (14) , F1461-F1469
Open AccessMicrostructural and Mechanical Characterization of Catalyst Coated Membranes Subjected to In Situ Hygrothermal Fatigue
Catalyst coated membranes (CCMs) in polymer electrolyte fuel cells are subjected to mechanical stresses in the form of fatigue and creep that deteriorate the durability and lifetime of the cells. The present article aims to determine the effect of in-situ hygrothermal fatigue on the microstructure and mechanical properties of the CCM. The fatigue process is systematically explored by the application of two custom-developed accelerated mechanical stress test (AMST) experiments with periodic extraction of partially degraded CCMs. Cross sectional and top surface scanning electron microscope (SEM) images of the end-of-test CCMs reveal the formation of mechanically induced cracks and delamination due to cyclic tensile and compressive fatigue stress. Tensile and expansion tests are conducted at different stages of degradation to evaluate the evolution in the mechanical and hygrothermal properties of the CCM. The tensile test results indicate gradual reductions in final strain, ultimate tensile strength, and fracture toughness with increasing number of fatigue cycles. The decay in tensile properties is attributed to the microstructural damage and micro-cracks formed during the AMST. Moreover, it is shown that the hygrothermal expansion of the CCM is more sensitive to conditioning than mechanical degradation.