Zhifeng Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Zhifeng Li has a total of 38 co-authors. Here are the top co-authors by number of shared publications:
Xin Liu
State Key Laboratory of Metal Material for Marine Equipment and Application, Anshan, China
5 shared publicationsShuai He
State Key Laboratory of Metal Material for Marine Equipment and Application Anshan Liaoning 114009 China
4 shared publicationsChi Zhang
3 shared publicationsChaoyi Wang
State Key Laboratory of Metal Material for Marine Equipment and Application, Anshan, China
2 shared publicationsGuang-Ming Cao
State Key Laboratory of Rolling and Automation Northeastern University Shenyang Liaoning 110819 China
2 shared publications- Guangming Cao
State Key Laboratory of Digital Steel, Northeastern University, Shenyang, China
2 shared publications
Latest Publications
- Open Access
Microstructural Evolution of Pearlitic Wheel Steel Under Thermal–Mechanical Fatigue
Pearlitic wheel steel subjected to thermal–mechanical fatigue (TMF) during braking can undergo catastrophic fracture. This study clarifies the microstructural evolution governing the macroscopic cyclic hardening/softening behavior of pearlitic wheel steel under thermal–mechanical fatigue (TMF) with a constant mechanical strain range of −0.4% to +0.2%. At lower temperature amplitudes (200–500 °C), the geometrically necessary dislocation (GND) density reaches 20.4 × 1014/m2 during initial cycles, corresponding to cyclic hardening due to dislocation pile-ups at cementite lamellae interfaces. With increasing cycles, the GND density decreases to 12.3 × 1014/m2, concurrent with softening arising from lamellar bending/fracture, partial spheroidization, and dynamic recrystallization of ferrite. At higher temperature amplitudes (200–730 °C), the GND density decreases from 8.8 × 1014/m2 to 3.5 × 1014/m2, reflecting sustained cyclic softening dominated by thermally activated mechanisms, including cementite spheroidization and dislocation annihilation. The resulting softened microstructure consists of ferrite grains, intragranular dispersed cementite, and chain-like coarse cementite at boundaries. Unlike previous studies that focused on single loading conditions (e.g., thermal fatigue, rolling contact fatigue, or wear), the present work addresses the more complex TMF scenario and quantitatively elucidates the interplay between mechanical response and microstructural evolution in pearlitic steel. This work provides theoretical guidance for the development of a fatigue life prediction model for pearlitic wheels under braking.
Open AccessMicrostructural Evolution of Pearlitic Wheel Steel Under Thermal–Mechanical Fatigue
Pearlitic wheel steel subjected to thermal–mechanical fatigue (TMF) during braking can undergo catastrophic fracture. This study clarifies the microstructural evolution governing the macroscopic cyclic hardening/softening behavior of pearlitic wheel steel under thermal–mechanical fatigue (TMF) with a constant mechanical strain range of −0.4% to +0.2%. At lower temperature amplitudes (200–500 °C), the geometrically necessary dislocation (GND) density reaches 20.4 × 1014/m2 during initial cycles, corresponding to cyclic hardening due to dislocation pile-ups at cementite lamellae interfaces. With increasing cycles, the GND density decreases to 12.3 × 1014/m2, concurrent with softening arising from lamellar bending/fracture, partial spheroidization, and dynamic recrystallization of ferrite. At higher temperature amplitudes (200–730 °C), the GND density decreases from 8.8 × 1014/m2 to 3.5 × 1014/m2, reflecting sustained cyclic softening dominated by thermally activated mechanisms, including cementite spheroidization and dislocation annihilation. The resulting softened microstructure consists of ferrite grains, intragranular dispersed cementite, and chain-like coarse cementite at boundaries. Unlike previous studies that focused on single loading conditions (e.g., thermal fatigue, rolling contact fatigue, or wear), the present work addresses the more complex TMF scenario and quantitatively elucidates the interplay between mechanical response and microstructural evolution in pearlitic steel. This work provides theoretical guidance for the development of a fatigue life prediction model for pearlitic wheels under braking.
- 5 September 2024
- Published by Springer Nature in Journal of Materials Research
- Vol. 39 (20) , 2820-2832
Solidification behavior of Ni-based superalloy at different cooling rates
- 5 September 2024
- Published by Springer Nature in Journal of Materials Research
- Vol. 39 (20) , 2820-2832
Solidification behavior of Ni-based superalloy at different cooling rates
- 22 August 2024
- Published by Wiley in Steel Research International
- Vol. 95 (12)
Isothermal Reduction Behavior of Oxide Scale on the Surface of Hot‐Rolled Strip Steel Under Different Hydrogen Concentrations
The oxide scale on the surface of hot‐rolled low‐carbon steel strips is subjected to isothermal reduction in 10 vol%H2–Ar and 20 vol%H2–Ar environments to simulate the reduction process that occurs in a continuous annealing furnace. The influence of hydrogen concentration on the reduction kinetics and the microstructural evolution of the oxide scale after reduction at temperatures ranging from 450 to 850 °C for a duration of 20 min are investigated in detail. The mass changes of the oxide scale in the two gases are quantified using a thermogravimetric analyzer. This data is then employed to calculate the reduction rate constant and the apparent activation energy. To examine the microstructure and element distribution, electron probe microanalysis and energy‐dispersive spectrometry are employed. An novel approach is also undertaken to assess the reduction degree of the oxide scale by measuring surface microhardness. In the findings, it is indicated that an increase in hydrogen concentration served primarily to accelerate the reduction reaction within the temperature ranges of 450–550 and 800–850 °C. Meanwhile, the mechanism of physical transformation of oxide scale, the microstructure of reduction layer, and hydrogen concentration on reduction efficiency under different reaction stages are proposed.
- 22 August 2024
- Published by Wiley in Steel Research International
- Vol. 95 (12)
Isothermal Reduction Behavior of Oxide Scale on the Surface of Hot‐Rolled Strip Steel Under Different Hydrogen Concentrations
The oxide scale on the surface of hot‐rolled low‐carbon steel strips is subjected to isothermal reduction in 10 vol%H2–Ar and 20 vol%H2–Ar environments to simulate the reduction process that occurs in a continuous annealing furnace. The influence of hydrogen concentration on the reduction kinetics and the microstructural evolution of the oxide scale after reduction at temperatures ranging from 450 to 850 °C for a duration of 20 min are investigated in detail. The mass changes of the oxide scale in the two gases are quantified using a thermogravimetric analyzer. This data is then employed to calculate the reduction rate constant and the apparent activation energy. To examine the microstructure and element distribution, electron probe microanalysis and energy‐dispersive spectrometry are employed. An novel approach is also undertaken to assess the reduction degree of the oxide scale by measuring surface microhardness. In the findings, it is indicated that an increase in hydrogen concentration served primarily to accelerate the reduction reaction within the temperature ranges of 450–550 and 800–850 °C. Meanwhile, the mechanism of physical transformation of oxide scale, the microstructure of reduction layer, and hydrogen concentration on reduction efficiency under different reaction stages are proposed.
- 26 July 2024
- Published by Elsevier in Materials Letters
- Vol. 372
Effect of microstructure evolution on impact toughness in advanced ultra-high strength steel
- 26 July 2024
- Published by Elsevier in Materials Letters
- Vol. 372
Effect of microstructure evolution on impact toughness in advanced ultra-high strength steel
- 27 May 2024
- Published by Wiley in Steel Research International
- Vol. 95 (8)
Carbide Precipitation Behavior of High‐Alloy Steel During Solidification and Cooling Process
The precipitation, growth, and transformation of carbides rich in Cr and Mo during solidification and cooling process of high‐alloy steel for cold working dies are investigated. The Fe–C pseudobinary phase diagram of high‐alloy steel is calculated by Thermo‐Calc software to ascertain the critical phase transformation temperatures. The temperatures of phase transformation during the solidification process are determined by a differential scanning calorimeter. Then the microstructure of the samples at these characteristic temperatures is observed in situ by high‐temperature confocal microscope. The results show that the characteristic temperatures for phase transformation and carbide precipitation are 1380, 1315, 1140, and 980 °C, respectively. At 1315 °C, thick rod‐like or island‐like M7C3 carbides enriched in Cr and Fe are formed. At 1140 °C, secondary M7C3, adhering to the primary eutectic M7C3, grows rapidly in a rod‐like morphology and maintains a similar composition. The secondary M6C carbides of segregated Mo elements precipitate in fan‐shaped clusters near M7C3 through the dissolution of M7C3 and the conversion of M2C. Thermodynamic calculation further indicates that the eutectic Cr7C3 precipitates at 1213 °C, and secondary Cr7C3 remains under conditions favorable for precipitation below the solidus, preceding the precipitation of secondary carbides Cr23C6 and Mo2C.
- 27 May 2024
- Published by Wiley in Steel Research International
- Vol. 95 (8)
Carbide Precipitation Behavior of High‐Alloy Steel During Solidification and Cooling Process
The precipitation, growth, and transformation of carbides rich in Cr and Mo during solidification and cooling process of high‐alloy steel for cold working dies are investigated. The Fe–C pseudobinary phase diagram of high‐alloy steel is calculated by Thermo‐Calc software to ascertain the critical phase transformation temperatures. The temperatures of phase transformation during the solidification process are determined by a differential scanning calorimeter. Then the microstructure of the samples at these characteristic temperatures is observed in situ by high‐temperature confocal microscope. The results show that the characteristic temperatures for phase transformation and carbide precipitation are 1380, 1315, 1140, and 980 °C, respectively. At 1315 °C, thick rod‐like or island‐like M7C3 carbides enriched in Cr and Fe are formed. At 1140 °C, secondary M7C3, adhering to the primary eutectic M7C3, grows rapidly in a rod‐like morphology and maintains a similar composition. The secondary M6C carbides of segregated Mo elements precipitate in fan‐shaped clusters near M7C3 through the dissolution of M7C3 and the conversion of M2C. Thermodynamic calculation further indicates that the eutectic Cr7C3 precipitates at 1213 °C, and secondary Cr7C3 remains under conditions favorable for precipitation below the solidus, preceding the precipitation of secondary carbides Cr23C6 and Mo2C.
- 3 August 2023
- Published by Springer Nature in High Temperature Corrosion of Materials
- Vol. 100 (3-4) , 251-264
Lamellar Spacing Characteristics of Eutectoids in Oxide Scale Formed on Iron After Holding at 300–500℃
- 3 August 2023
- Published by Springer Nature in High Temperature Corrosion of Materials
- Vol. 100 (3-4) , 251-264
Lamellar Spacing Characteristics of Eutectoids in Oxide Scale Formed on Iron After Holding at 300–500℃
- Open Access
- 10 July 2023
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 25, 5855-5870
SAG usage wear-resistant steel with rare retained austenite achieve trade-off between impact toughness and strength
- 10 July 2023
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 25, 5855-5870
Open AccessSAG usage wear-resistant steel with rare retained austenite achieve trade-off between impact toughness and strength
- 28 September 2019
- Published by Wiley in Steel Research International
- Vol. 91 (1)
Reduction Behavior of Oxide Scales Containing Different Structures on the Surface of Hot‐Rolled Steel Strip in Gas Mixture H2/Ar at 400–625 °C
The reduction behavior of the oxide scales with two different microstructures in the gas of H2:Ar = 1:2 at 400–625 °C is investigated in detail. The mass change in the scale is measured by thermogravimetric analysis, and a function between reduction degree, reduction temperature, and reaction time is established. The experiment results show that the increase in temperature has an accelerating influence on the reduction reaction of the scale with eutectoid (Fe3O4/α‐Fe) until reaching 550 °C, and then the further increase in temperature decelerates the reduction. For the scale without eutectoid, the reduction rate at 450 °C is extremely high, and then the rate decreases with the increase in temperatures. Additionally, the reduction rate in the scale with eutectoid is faster than that without eutectoid at the temperature range of this study. At 400–550 °C, a large number of phase interfaces appear within the scale with eutectoid, which can provide diffusion channels for hydrogen atoms and water molecules within the Fe oxides. When the temperature reaches 575–625 °C, the phase transformation in the scale (Fe3O4 + α‐Fe → FeO) is accompanied by the reduction reaction, which is believed to be responsible for the lower reaction rate.
- 28 September 2019
- Published by Wiley in Steel Research International
- Vol. 91 (1)
Reduction Behavior of Oxide Scales Containing Different Structures on the Surface of Hot‐Rolled Steel Strip in Gas Mixture H2/Ar at 400–625 °C
The reduction behavior of the oxide scales with two different microstructures in the gas of H2:Ar = 1:2 at 400–625 °C is investigated in detail. The mass change in the scale is measured by thermogravimetric analysis, and a function between reduction degree, reduction temperature, and reaction time is established. The experiment results show that the increase in temperature has an accelerating influence on the reduction reaction of the scale with eutectoid (Fe3O4/α‐Fe) until reaching 550 °C, and then the further increase in temperature decelerates the reduction. For the scale without eutectoid, the reduction rate at 450 °C is extremely high, and then the rate decreases with the increase in temperatures. Additionally, the reduction rate in the scale with eutectoid is faster than that without eutectoid at the temperature range of this study. At 400–550 °C, a large number of phase interfaces appear within the scale with eutectoid, which can provide diffusion channels for hydrogen atoms and water molecules within the Fe oxides. When the temperature reaches 575–625 °C, the phase transformation in the scale (Fe3O4 + α‐Fe → FeO) is accompanied by the reduction reaction, which is believed to be responsible for the lower reaction rate.
- Open Access
- 20 September 2019
- Published by Association for Computing Machinery (ACM)
- Vol. 19, 605-610
Design and Kinematics Analysis of Four-linkage Excavator
- 20 September 2019
- Published by Association for Computing Machinery (ACM)
- Vol. 19, 605-610
Open AccessDesign and Kinematics Analysis of Four-linkage Excavator
- 17 September 2019
- Published by Springer Nature in Journal of Materials Science
- Vol. 55 (4) , 1826-1839
High-efficiency reduction behavior for the oxide scale formed on hot-rolled steel in a mixed atmosphere of hydrogen and argon
- 17 September 2019
- Published by Springer Nature in Journal of Materials Science
- Vol. 55 (4) , 1826-1839
High-efficiency reduction behavior for the oxide scale formed on hot-rolled steel in a mixed atmosphere of hydrogen and argon