Ivana Cvijović-Alagić
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Ivana Cvijović-Alagić has a total of 147 co-authors. Here are the top co-authors by number of shared publications:
Z. Cvijović
11 shared publications- Vesna Maksimović
Vinča Institute of Nuclear Sciences, National Institute of the Republic of Serbia, University of Belgrade, Mike Petrovića Alasa 12-14, 11000 Belgrade, Serbia
10 shared publications M. Rakin
9 shared publicationsMarko Rakin
Faculty of Technology and Metallurgy, University of Belgrade, Belgrade, Serbia
8 shared publications- Branko Matović
Vinča Institute of Nuclear Sciences,Vinča,Serbia, Serbia
7 shared publications - Ivana Dimic
Faculty of Technology and Metallurgy, Innovation Centre, Belgrade
7 shared publications
Latest Publications
- 5 September 2026
- Published by Elsevier in Ceramics International
- Vol. 52 (27) , 53436-53444
Effect of Ti2AlC MAX phase additions on microstructure and oxyacetylene ablation behavior of B4C-SiC ceramics
- 5 September 2026
- Published by Elsevier in Ceramics International
- Vol. 52 (27) , 53436-53444
Effect of Ti2AlC MAX phase additions on microstructure and oxyacetylene ablation behavior of B4C-SiC ceramics
- Open Access
- 1 January 2026
- Published by Centre for Evaluation in Education and Science (CEON/CEES)
- p. 30
Effects of 3d metal doping on local and electronic structure of CeO2 nanopowders
- 1 January 2026
- Published by Centre for Evaluation in Education and Science (CEON/CEES)
- p. 30
Open AccessEffects of 3d metal doping on local and electronic structure of CeO2 nanopowders
- Open Access
- 1 January 2025
- Published by Udruženje inženjera Srbije za koroziju i zaštitu materijala
- p. 32-33
Influence of processing-induced changes on the performance of Ti-based alloy in biological systems
- 1 January 2025
- Published by Udruženje inženjera Srbije za koroziju i zaštitu materijala
- p. 32-33
Open AccessInfluence of processing-induced changes on the performance of Ti-based alloy in biological systems
- 3 August 2024
- Published by Elsevier in Ceramics International
- Vol. 50 (21) , 42188-42194
Fabrication of boron carbide ceramics reinforced with silicon carbide fibers
- 3 August 2024
- Published by Elsevier in Ceramics International
- Vol. 50 (21) , 42188-42194
Fabrication of boron carbide ceramics reinforced with silicon carbide fibers
- 9 May 2024
- Published by Royal Society of Chemistry (RSC) in CrystEngComm
- Vol. 26 (22) , 2989-3004
Mechanical properties and behavior of the Ti–45Nb alloy subjected to extreme conditions
Ti–45Nb alloy biomechanical compatibility was evaluated by a multidisciplinary approach and improved by extreme condition processing. Ab initio calculations of mechanical properties are in very good agreement with experimental observations.
- 9 May 2024
- Published by Royal Society of Chemistry (RSC) in CrystEngComm
- Vol. 26 (22) , 2989-3004
Mechanical properties and behavior of the Ti–45Nb alloy subjected to extreme conditions
Ti–45Nb alloy biomechanical compatibility was evaluated by a multidisciplinary approach and improved by extreme condition processing. Ab initio calculations of mechanical properties are in very good agreement with experimental observations.
- 22 April 2024
- Published by Elsevier in Acta Metallurgica Sinica (English Letters)
- Vol. 37 (7) , 1215-1230
Impact of Microstructural and Surface Modifications on the Ti-45Nb Alloy’s Response to Bio-Environment
- 22 April 2024
- Published by Elsevier in Acta Metallurgica Sinica (English Letters)
- Vol. 37 (7) , 1215-1230
Impact of Microstructural and Surface Modifications on the Ti-45Nb Alloy’s Response to Bio-Environment
- Open Access
- 1 January 2024
- Published by National Library of Serbia in Science of Sintering
- Vol. 56 (1) , 123-130
Synthesis and characterization of high-entropy A2B2O7 pyrochlore with multiple elements at A and B sites
Single nano high-entropy pyrochlore-type compound (A2B2O7) with 7 different rareearth cations at site A and 3 different metal cations at site B with equiatomic amounts (7A1/7)2(3B1/3)2O7 is successfully obtained. The powder with nominal composition (La1/7Sm1/7Nd1/7Pr1/7Y1/7Gd1/7Yb1/7)2(Sn1/3Hf1/3Zr1/3)2O7 was fabricated by reacting metal nitrates (site A) and metal chlorides (site B) with glycine during the combustion reaction. The XRD analysis revealed that the powder attained during synthesis is in an amorphous state. To induce crystallization of the obtained pyrochlore structure, the post-calcination process at 600-1500?C was conducted and studied. Results of this study showed that the monophase pyrochlore (A2B2O7) structure is obtained during the calcination at 900?C. The high-density ceramic pellet with 97% of theoretical density and free of any additives was obtained through pressureless sintering at 1650?C for 4 h in the air using the powder calcined at 900?C.
- 1 January 2024
- Published by National Library of Serbia in Science of Sintering
- Vol. 56 (1) , 123-130
Open AccessSynthesis and characterization of high-entropy A2B2O7 pyrochlore with multiple elements at A and B sites
Single nano high-entropy pyrochlore-type compound (A2B2O7) with 7 different rareearth cations at site A and 3 different metal cations at site B with equiatomic amounts (7A1/7)2(3B1/3)2O7 is successfully obtained. The powder with nominal composition (La1/7Sm1/7Nd1/7Pr1/7Y1/7Gd1/7Yb1/7)2(Sn1/3Hf1/3Zr1/3)2O7 was fabricated by reacting metal nitrates (site A) and metal chlorides (site B) with glycine during the combustion reaction. The XRD analysis revealed that the powder attained during synthesis is in an amorphous state. To induce crystallization of the obtained pyrochlore structure, the post-calcination process at 600-1500?C was conducted and studied. Results of this study showed that the monophase pyrochlore (A2B2O7) structure is obtained during the calcination at 900?C. The high-density ceramic pellet with 97% of theoretical density and free of any additives was obtained through pressureless sintering at 1650?C for 4 h in the air using the powder calcined at 900?C.
- Open Access
- 1 January 2023
- Published by National Library of Serbia in Processing and Application of Ceramics
- Vol. 17 (2) , 113-117
Heavily doped high-entropy A2B2O7 pyrochlore
A novel class of high-entropy pyrochlore compounds with multiple elements at the A and B site positions (A2B2O7) was successfully obtained. Powders with (La1/7Sm1/7Nd1/7Pr1/7Y1/7Gd1/7Yb1/7)2(Sn1/3Hf1/3Zr1/3)2O7 nominal composition were fabricated from pure metal oxides obtained through a reaction of metal nitrates (for site A) and metal chlorides (for site B) with sodium hydroxide during the solid-state displacement reaction (SSDR). The phase evolution was analyzed using XRD method. During the thermal treatment of ten individual metal oxides, the single pyrochlore phase was created. The present study showed that the highdensity (98%TD) ceramics with a hardness of 8.1GPa was successfully obtained after pressureless sintering at 1650 ?C for 4 h. Results of the Raman study and the Rietveld structural refinement showed that sintered highentropy ceramics is characterized by a single-phase pyrochlore structure, which was investigated in detail.
- 1 January 2023
- Published by National Library of Serbia in Processing and Application of Ceramics
- Vol. 17 (2) , 113-117
Open AccessHeavily doped high-entropy A2B2O7 pyrochlore
A novel class of high-entropy pyrochlore compounds with multiple elements at the A and B site positions (A2B2O7) was successfully obtained. Powders with (La1/7Sm1/7Nd1/7Pr1/7Y1/7Gd1/7Yb1/7)2(Sn1/3Hf1/3Zr1/3)2O7 nominal composition were fabricated from pure metal oxides obtained through a reaction of metal nitrates (for site A) and metal chlorides (for site B) with sodium hydroxide during the solid-state displacement reaction (SSDR). The phase evolution was analyzed using XRD method. During the thermal treatment of ten individual metal oxides, the single pyrochlore phase was created. The present study showed that the highdensity (98%TD) ceramics with a hardness of 8.1GPa was successfully obtained after pressureless sintering at 1650 ?C for 4 h. Results of the Raman study and the Rietveld structural refinement showed that sintered highentropy ceramics is characterized by a single-phase pyrochlore structure, which was investigated in detail.
- Open Access
- 1 January 2023
- Published by National Library of Serbia in Hemijska industrija
- Vol. 77 (2) , 155-165
Microstructure, hardness and fracture resistance of P235TR1 seam steel pipes of different diameters
Steel pipelines in industrial plants consist of different elements, including seamless and/or welded (seam) pipes. Properties of welded pipes, including their fracture behaviour, depend on the characteristics of both, the base metal, and the weld metal. In this work, two seam pipes are considered having different diameters and manufactured of P235TR1 steel. Hardness and microstructure were examined on the samples which contained the seam zone, to capture the influence of heterogeneity. Fracture resistance of the pipeline material, i.e. of both base metals and both seams, was determined by experimental examination of the recently proposed Pipe ring notch bending specimens with sharp stress concentrators. Differences between the two tested pipes, including the influence of the heterogeneity caused by the welded joint, were determined by comparison of the crack growth resistance curves. Effects of the initial stress concentrator shape, sharp machined notch or fatigue pre-crack are discussed.
- 1 January 2023
- Published by National Library of Serbia in Hemijska industrija
- Vol. 77 (2) , 155-165
Open AccessMicrostructure, hardness and fracture resistance of P235TR1 seam steel pipes of different diameters
Steel pipelines in industrial plants consist of different elements, including seamless and/or welded (seam) pipes. Properties of welded pipes, including their fracture behaviour, depend on the characteristics of both, the base metal, and the weld metal. In this work, two seam pipes are considered having different diameters and manufactured of P235TR1 steel. Hardness and microstructure were examined on the samples which contained the seam zone, to capture the influence of heterogeneity. Fracture resistance of the pipeline material, i.e. of both base metals and both seams, was determined by experimental examination of the recently proposed Pipe ring notch bending specimens with sharp stress concentrators. Differences between the two tested pipes, including the influence of the heterogeneity caused by the welded joint, were determined by comparison of the crack growth resistance curves. Effects of the initial stress concentrator shape, sharp machined notch or fatigue pre-crack are discussed.
- Open Access
- 1 January 2023
- Published by National Library of Serbia in Science of Sintering
- Vol. 55 (2) , 145-158
Novel basalt-stainless steel composite materials with improved fracture toughness
This paper presents the technological process for obtaining basalt-stainless steel composite materials and testing their physical and mechanical properties. The phases of the technological process consist of: milling, homogenization, pressing, and sintering to obtain composite materials with improved fracture toughness. Andesite basalt from the deposit site "Donje Jarinje", Serbia, was used as a matrix in the composites, while commercial austenitic stainless steel 316L in the amount of 0-30 wt.% was used as a reinforcement. Although the increase of 316L amount caused a continuous decrease in the relative density of sintered samples, the relative density of sample containing 30 wt.% of 316L was above 94%. The 316L grains, which possess a larger coefficient of thermal expansion than the basalt matrix, shrinking faster during cooling from sintering temperature resulting in the formation of compressive residual stress in the basalt matrix surrounding the spherical steel grains. The presence of this stress activated toughening mechanisms such as crack deflection and toughening due to compressive residual stress. The addition of 20 wt.% of reinforcing 316L particles increased the fracture toughness of basalt by more than 30%. The relative density of these samples was measured to be 97%, whereas macrohardness was found to be 6.2 GPa.
- 1 January 2023
- Published by National Library of Serbia in Science of Sintering
- Vol. 55 (2) , 145-158
Open AccessNovel basalt-stainless steel composite materials with improved fracture toughness
This paper presents the technological process for obtaining basalt-stainless steel composite materials and testing their physical and mechanical properties. The phases of the technological process consist of: milling, homogenization, pressing, and sintering to obtain composite materials with improved fracture toughness. Andesite basalt from the deposit site "Donje Jarinje", Serbia, was used as a matrix in the composites, while commercial austenitic stainless steel 316L in the amount of 0-30 wt.% was used as a reinforcement. Although the increase of 316L amount caused a continuous decrease in the relative density of sintered samples, the relative density of sample containing 30 wt.% of 316L was above 94%. The 316L grains, which possess a larger coefficient of thermal expansion than the basalt matrix, shrinking faster during cooling from sintering temperature resulting in the formation of compressive residual stress in the basalt matrix surrounding the spherical steel grains. The presence of this stress activated toughening mechanisms such as crack deflection and toughening due to compressive residual stress. The addition of 20 wt.% of reinforcing 316L particles increased the fracture toughness of basalt by more than 30%. The relative density of these samples was measured to be 97%, whereas macrohardness was found to be 6.2 GPa.