Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Hein Zaw Oo has a total of 12 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Effects of preheating on the joint integrity of enclosed arc welded rails

    by Anuchit Teherng, Hein Zaw Oo, Prapas Muangjunburee

  • Open Access

    Microstructure and Abrasive Wear Behavior of Fe–Cr–C Hardfacing on Hammer Tips for Sugarcane Shredders

    by Buntoeng Srikarun, Hein Zaw Oo, Anuchit Teherng, Shayfull Zamree Abd Rahim, Prapas Muangjunburee

    This study investigates the influence of an austenitic buffer layer on the microstructure, hardness, and abrasive wear resistance of Fe–Cr–C hardfacing applied to high-chromium white cast iron (HCWCI) hammer tips used in sugarcane shredders. Hardfacing was performed by shielded metal arc welding with two Fe–Cr–C layers deposited directly on the HCWCI substrate and with an austenitic buffer layer followed by an Fe–Cr–C hardfacing layer. Microstructural characterization was carried out using optical microscopy, scanning electron microscopy with energy-dispersive X-ray spectroscopy, while hardness profiles were determined by micro-Vickers testing. Abrasive wear behavior was evaluated using a dry sand–rubber wheel test according to ASTM G65. The non-buffered hardfacing layer exhibited a hypereutectic Fe–Cr–C microstructure consisting of coarse primary chromium carbides, resulting in high hardness values of approximately 840 HV. In contrast, the buffered sample showed an austenite-rich matrix with finer eutectic carbides and reduced hardness of around 600 HV. Abrasive wear tests of the non-buffered sample showed a lower mass loss, whereas the buffered sample exhibited a substantially higher mass loss. These results demonstrate that Fe–Cr–C hardfacing without a buffer layer provides superior wear resistance.

  • Friction stir welded AA6082-T6 joints repaired by cold metal transfer process under different heat inputs

    by Muhamad Tehyo, Prapas Muangjunburee, Hein Zaw Oo, Sasirat Chaideesungnoen, Thanate Ratanawilai

    This research studied the effects of cold metal transfer (CMT) repair welding with varying heat inputs on the mechanical properties and corrosion resistance of friction stir welded AA6082-T6 aluminum alloy joints. The original friction stir welding (FSW) joint and repaired joints by CMT were investigated by metallurgical characterization, microhardness tests, tensile tests, three-point bending tests, and electrochemical corrosion tests. The results indicated that CMT repair welding affected the mechanical properties. Notably, the CMT-155 showed the best performance, retaining 97.7% of the original FSW joint’s tensile strength. The location of the fracture after tensile tests changed from the thermo-mechanical affected zone of the FSW joint to the heat affected zone (HAZ) of the CMT repair joint. The microhardness in the weld metal (WM) and HAZ of the CMT repaired joints was lower than that of the base metal (BM). The CMT-155 and CMT-160 had higher hardness than the CMT-150. The highest bending strengths for both face bend and root bend were found in the repaired joint using 155 A. Electrochemical corrosion results of the WM in CMT repaired joints exhibited lower corrosion resistance compared to the stir zone of FSW joint and the BM. Corrosion rates increased with higher CMT welding currents.

  • Influence of post-weld heat treatment on microstructure and hardness of inconel 625 laser-cladded repair welds

    by Janetira Chankaew, Sasirat Chaideesungnoen, Prapas Muangjunburee, Hein Zaw Oo

    This research examines the microstructural evolution of Inconel 625 (nickel-based superalloy) laser-cladded onto a 2.25Cr-1Mo steel substrate (low-alloy steel) for the steam turbine rotor restoration, exposed to post-weld heat treatment (PWHT) at 690 °C for 0 (as-cladded), 1, 2, and 4 h. Scanning electron microscopy with energy-dispersive x-ray spectroscopy (SEM/EDS), x-ray diffraction (XRD) analysis, and microhardness tests were used to assess the clad characteristics. Results indicated that prolonged PWHT duration led to a reduction in the hardness of the 2.25Cr-1Mo steel heat-affected zone (HAZ) (from 296.6 ± 11.9 to 187.8 ± 3.5 HV 0.2 ), while simultaneously increasing the Inconel 625 clad hardness (from 271.5 ± 3.4 to 287.6 ± 5.0 HV 0.2 ). Following PWHT, the bainitic HAZ converted into tempered bainite; conversely, the clad layer, mostly consisting of an austenitic phase, provided increased precipitation of secondary phases. Further microstructural analysis of the clad layer proved that the as-cladded condition included an austenitic matrix and an intermetallic phase, identified as carbides enriched with carbon (C), niobium (Nb), and molybdenum (Mo). PWHT promoted the precipitation of Nb/Mo-rich carbides within the face-centered cubic (FCC) austenitic matrix. Quantitative XRD investigation revealed a significant reduction in the austenite lattice parameter ( a ), reaching a minimum after 4 h (from 3.5954 to 3.5895 Å). This crystallographic shrinkage offers visible evidence of solute depletion, as Nb and Mo atoms migrate from the solid solution to form secondary phases. These findings suggest that precipitation hardening, influenced by carbide kinetics, is the primary process responsible for the enhancement of the clad’s mechanical properties.


  • Open Access

    The electrochemical corrosion performance of aluminum alloys grade 6082-T6 weld repair

    by Porntep Sareekumtorn, Sasirat Chaideesungnoen, Prapas Muangjunburee, Hein Zaw Oo

    This research investigated the corrosion behavior of standard current metal inert gas weld repair for 6082-T6 aluminum alloy using ER5356 filler metal. The new and repaired (NW and RW) welds were studied. The welds comprised the weld metal (WM), the heat affected zone (HAZ) (solid solution and softened zones), and the base metal (BM). The study focused on investigating electrochemical corrosion using polarization and electrochemical impedance spectroscopy (EIS) methods in 3.5% NaCl solutions, especially in HAZ, including metallurgical and mechanical examinations. The BM containing an α-Al matrix with Al(Fe,Mn)Si and Mg2Si phases exhibited the maximum hardness (70–104 HV0.1). The WM hardness decreased (67–76 HV0.1) with the α-Al, β-Mg3Al2, and Mg2Si phases. Despite having comparable phases to BM, HAZs showed lower hardness (Solid HAZ: 70–82 HV0.1) due to more intermetallic phases. The RW’s softened HAZ revealed the minimum hardness (52–63 HV0.1) compared to that of the NW (55–70 HV0.1). Besides, the tensile strength of the RW (179.7 MPa) was also lower than that of the NW (174.4 MPa) because of the reheating effect. The electrochemical corrosion results indicated that the BM exhibited the maximum corrosion resistance (the lowest corrosion current density (icorr), the highest corrosion potential (Ecorr), and the charge transfer resistance (Rct)), followed by the HAZ and the WM, respectively. The softened HAZ demonstrated better corrosion resistance than the solid solution HAZ. Conversely, the over-aging effect reduced the softened zone’s pitting corrosion resistance (Ep) compared to the solid solution zone. The RW exhibited inferior corrosion resistance compared to the NW due to increased intermetallic phases, which was consistent with the mechanical results. However, the RW’s softened HAZ corrosion characteristics were inconsistent with its mechanical properties; its hardness and tensile strength were the lowest, but its corrosion resistance was not. Pitting corrosion was observed on the weld surfaces using the SEM.


  • Open Access

    Influences of preheating parameters on the quality of weld by thermite rail welding

    by Romadorn Burapa, Hein Zaw Oo, Wissarut Sangwiman, Prapas Muangjunburee

    The major goal of this study is to enhance the mechanical and metallurgical characteristics of rail steel grade R260 joined by thermite welding under various preheating conditions, including preheating time and gas pressure. Mainly two conditions, referred to as the Normal Condition and Improved Condition, are carried out for experiments. Prior to welding, the Normal Condition was preheated using liquefied petroleum gas (LPG) and oxygen gas pressures of 1 bar and 4.5 bar for 3 min, and the Improved Condition was preheated using liquefied petroleum gas and oxygen gas pressures of 1.2 bar and 4.5 bar for 6 min and 30 s. To investigate the mechanical and physical properties, micro-Vickers hardness tests, tensile tests and slow bending tests were also carried out. Welded metal in Normal Condition has many defects, including gas holes and shrinkage cavities. When comparing the Normal Condition to the Improved Condition, the Improved Condition demonstrates significantly more bending load and deflection. Specifically, the thermite welded rail sample of Improved Condition demonstrated a remarkable ability to endure bending loads of 108 tonnes and a deflection of 16 mm, and this sample remained unbroken until it exceeded 50% of the standardized deflection limit (10 mm). In addition, the average hardness values for the Improved Condition of the weld metal zone and the heat-affected zone were 331 HV and 289 HV, respectively. The Normal Condition produced an unsatisfactory fracture surface after slow bending test. This was caused by weld defects at the thermite weld due to inappropriate preheating.


  • Open Access

    Improving Microstructure and Hardness of Softening Area at Haz of Thermite Welding on Rail Running Surface

    by Hein Zaw Oo, Prapas Muangjunburee

    Thermite welding is widely used to join rails to get a continuous welded rail. The HAZ formed on two sides of the thermite welded joint. The soft zones in the HAZ of thermite weld are weaknesses that must be strengthened for the rails to give good service. A groove was machined on the running surface of the rail in the HAZ of the thermite weld, and it was filled using the FCAW process to improve the microstructures and hardnesses of the soft region, without adversely affecting the thermite welded rail. In this paper, the improvements of FCAW over the original HAZ of thermite weld determined through the differences in the microstructures and hardnesses are discussed. An optical microscope and a field emission scanning electron microscope (FESEM) were used to characterize the microstructures and an atomic force microscope (AFM) was used to analyze the interlamellar spacing of pearlite. The micro-Vickers hardness profiles are also compared between the original HAZ zone and that obtained after improvements obtained by FCAW. The spheroidized microstructures of the original HAZ were changed to very fine pearlite microstructures by the FCAW process. The hardness of the soft zone was approximately 250 HV, whereas the value of the improved zone was approximately 330 HV. The conclusion is clear that the FCAW process can effectively improve the microstructures and hardnesses of the soft regions found in the HAZ of conventional thermite welds.

  • Effectiveness of metal powder additions for martensitic hardfacing alloy on its wear properties

    by Buntoeng Srikarun, Hein Zaw Oo, Prapas Muangjunburee

    Selecting welding consumables to get satisfactory results in hard facing weld repair jobs at a low cost is an important consideration. The standard martensitic welding electrodes used for hardfacing are expensive, so an investigation into finding suitable substitutes is a worthwhile activity. The objective of this study was to analyze the hardfacing deposits on using a low carbon steel welding electrode with metal powders added to the weld pool. Four different samples were hardfaced applying a submerged arc welding setup with constant heat input. Single and three layers of hardfacing samples were welded using a standard martensitic electrode and compared to using low carbon steel electrodes with added metal powders. An optical emission spectrometer was used to obtain the chemical compositions of welded metal layers. A scanning electron microscope was used to characterize the metallurgical structures of deposits. SEM images of worn surfaces were also obtained. Microhardnessand abrasive testing were used to examine the mechanical properties of the hardfaced surfaces. The results showed that martensitic microstructures were obtained in the hardfaced deposits using a low carbon steel welding electrode with added metal powders. However, hardness and abrasive wear resistance of both single and three layers of hardfacing using low carbon steel welding electrode with added metal powder were below those achieved by welding with a standard martensitic electrode.


  • The effects of heat input and polarity on wear resistance of Fe-3.5% Cr steel hardfaced using submerged arc welding

    by Hein Zaw Oo, Buntoeng Srikarun, Prapas Muangjunburee

    In this research, four samples of 3.5% Cr steel plates were hardfaced using austenitic stainless-steel buffer electrodes and martensitic steel hardfacing electrodes with a submerged arc welding process. This research seeks to the optimum welding parameters to get maximum wear resistance in the hardfaced layer. Heat inputs of 15 kJ/cm to 18 kJ/cm and Direct Current Electrode Positive (DC+) and Alternating Current Electrode (AC) welding polarities were applied. The microstructural analysis was conducted using an optical microscope (OM) and a scanning electron microscope (SEM). Microhardness values of the hardfaced samples were obtained using a Vickers hardness tester, and abrasive wear mass loss was measured using a dry sand rubber wheel apparatus, following ASTM G65 A standard. It was seen that the hardness profiles across the cross-section of the top hardfaced layer and along the top surface were different. The microstructure in the deposited layers, especially the quantity of martensite phase played a major influence on the wear resistance. Hardfaced layers applied with low heat input showed the highest amount of martensite phase and lowest abrasive mass loss. The hardfaced layers using AC polarity contained higher amount of martensite and lower abrasive mass loss than the layers applied using DC+ polarity.