Hayrettin Ahlatci
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Hayrettin Ahlatci has a total of 70 co-authors. Here are the top co-authors by number of shared publications:
- Yunus Turen
Necmettin Erbakan University
15 shared publications - Ismail Esen
Karabuk University
14 shared publications - Yavuz Sun
Karabuk University
8 shared publications - Esma Keskin
BUMA Engineering and Consulting Inc
7 shared publications - Levent Elen
Karabuk University
7 shared publications - Bünyamin Çiçek
Hitit University
4 shared publications
Latest Publications
- 7 October 2026
- Published by SAGE Publications in International Journal of Damage Mechanics
Improving rolling contact fatigue behavior in wheel–rail systems using a slag powder–oil mixture friction modifier
This study investigates the effect of different top-of-rail friction modifier (FM) formulations on the rolling contact fatigue (RCF) behavior at the wheel–rail interface. Three different FMs were examined: flange oil, slag powder, and a hybrid oil + slag powder mixture. A twin-disc test was conducted over 700,000 cycles to evaluate crack initiation and propagation. Surface and subsurface damage characteristics were analyzed using scanning electron microscope (SEM) micrographs. The results show that under flange oil conditions, RCF cracks propagate deeper beneath the surface (127 µm), and the presence of liquid oil promotes crack opening and expansion due to hydraulic pressure within the microcracks. In contrast, slag powder (FMA) alone caused severe wear and surface delamination, demonstrating the lack of protective film formation. However, when combined with slag powder + oil (FMB), the cohesive third body layer formed by viscous oil and slag powder particles effectively restricted subsurface crack growth. The FMB formulation reduced the average subsurface crack length by approximately 42% compared to the flange oil condition and by approximately 35% compared to the slag powder-only condition. Similarly, it successfully reduced the average crack depth by up to 77% in rail discs. This improvement demonstrates the hybrid FM's ability to balance local stresses and suppress hydraulic crack propagation. In general, the findings indicate that hybrid FM, composed of oil and solid waste-based particles, can significantly increase RCF resistance by balancing lubrication and surface protection mechanisms. This highlights that it offers a promising approach for extending the service life of wheel/rail systems.
- 7 October 2026
- Published by SAGE Publications in International Journal of Damage Mechanics
Improving rolling contact fatigue behavior in wheel–rail systems using a slag powder–oil mixture friction modifier
This study investigates the effect of different top-of-rail friction modifier (FM) formulations on the rolling contact fatigue (RCF) behavior at the wheel–rail interface. Three different FMs were examined: flange oil, slag powder, and a hybrid oil + slag powder mixture. A twin-disc test was conducted over 700,000 cycles to evaluate crack initiation and propagation. Surface and subsurface damage characteristics were analyzed using scanning electron microscope (SEM) micrographs. The results show that under flange oil conditions, RCF cracks propagate deeper beneath the surface (127 µm), and the presence of liquid oil promotes crack opening and expansion due to hydraulic pressure within the microcracks. In contrast, slag powder (FMA) alone caused severe wear and surface delamination, demonstrating the lack of protective film formation. However, when combined with slag powder + oil (FMB), the cohesive third body layer formed by viscous oil and slag powder particles effectively restricted subsurface crack growth. The FMB formulation reduced the average subsurface crack length by approximately 42% compared to the flange oil condition and by approximately 35% compared to the slag powder-only condition. Similarly, it successfully reduced the average crack depth by up to 77% in rail discs. This improvement demonstrates the hybrid FM's ability to balance local stresses and suppress hydraulic crack propagation. In general, the findings indicate that hybrid FM, composed of oil and solid waste-based particles, can significantly increase RCF resistance by balancing lubrication and surface protection mechanisms. This highlights that it offers a promising approach for extending the service life of wheel/rail systems.
- Open Access
- 25 February 2026
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 32 (1) , 42-56
Effect of 0.40 % and 0.20 % Titanium Addition on Microstructure Properties and Corrosion Behavior of CuAl10Ni5Fe4 Alloy
This study examined how post-casting heat treatment (solution treatment and tempering) and forging affected the corrosion and microstructural properties of the nickel aluminium bronze (CuAl10Ni5Fe4) with 0.20 % and 0.40% titanium addition. Heat-treated CuAl10Ni5Fe4 alloy microstructures showed copper-rich α-solid solution, martensitic β-phase, and intermetallic κ-phases, such as flake-shaped κI, fine κIII, and black globular κIV. Adding 0.20 % and 0.40 % titanium to CuAl10Ni5Fe4 alloys reduced dendritic arm thickness and increased κ phase abundance. Additionally, significant κIV and κII precipitations were observed in the tempered β phase. Tempering β may cause martensitic β to split into tiny α and κIII phases. The grain refinement of the CuAl10Ni5Fe4, CuAl10Ni5Fe4-0.20 % Ti, and CuAl10Ni5Fe4-0.40 % Ti alloys was significantly noticeable after forging. The alloys retained the same α, β, and κ phases seen in the heat-treated alloys after forging. Titanium's refining effect increased the hardness of the alloy into which it was incorporated. Increased stiff phases, such as tempered β and fine κIV, contribute to increased hardness. The forging process enhanced the hardness of all three alloys. Forged and heat treated CuAl10Ni5Fe4-0.40 % Ti alloy had the highest hardness with 243.50 HB and 256.18 HB, respectively. The microstructural phases α, β, and κ significantly impact the corrosion behaviour of CuAl10Ni5Fe4 alloy. The CuAl10Ni5Fe4-0.40 % Ti alloy after forging had the lowest 24-hour weight loss of 0.003326 mg/dm2. The CuAl10Ni5Fe4 alloy loses the most weight (0.013659 mg/dm²) following heat treatment (S.T.+T) after 24 hours. The minimal corrosion rate for the CuAl10Ni5Fe4-0.40 % Ti alloy after forging was 0.003916 mg/(dm2·day) after 72 hours. Due to stratification, corrosion creates craters. Pitted or porous structures and craters are common. All alloys show a decrease in these structures after forging. The formation of the CuCl2 phase is believed to occur in regions experiencing pitting corrosion.
- 25 February 2026
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 32 (1) , 42-56
Open AccessEffect of 0.40 % and 0.20 % Titanium Addition on Microstructure Properties and Corrosion Behavior of CuAl10Ni5Fe4 Alloy
This study examined how post-casting heat treatment (solution treatment and tempering) and forging affected the corrosion and microstructural properties of the nickel aluminium bronze (CuAl10Ni5Fe4) with 0.20 % and 0.40% titanium addition. Heat-treated CuAl10Ni5Fe4 alloy microstructures showed copper-rich α-solid solution, martensitic β-phase, and intermetallic κ-phases, such as flake-shaped κI, fine κIII, and black globular κIV. Adding 0.20 % and 0.40 % titanium to CuAl10Ni5Fe4 alloys reduced dendritic arm thickness and increased κ phase abundance. Additionally, significant κIV and κII precipitations were observed in the tempered β phase. Tempering β may cause martensitic β to split into tiny α and κIII phases. The grain refinement of the CuAl10Ni5Fe4, CuAl10Ni5Fe4-0.20 % Ti, and CuAl10Ni5Fe4-0.40 % Ti alloys was significantly noticeable after forging. The alloys retained the same α, β, and κ phases seen in the heat-treated alloys after forging. Titanium's refining effect increased the hardness of the alloy into which it was incorporated. Increased stiff phases, such as tempered β and fine κIV, contribute to increased hardness. The forging process enhanced the hardness of all three alloys. Forged and heat treated CuAl10Ni5Fe4-0.40 % Ti alloy had the highest hardness with 243.50 HB and 256.18 HB, respectively. The microstructural phases α, β, and κ significantly impact the corrosion behaviour of CuAl10Ni5Fe4 alloy. The CuAl10Ni5Fe4-0.40 % Ti alloy after forging had the lowest 24-hour weight loss of 0.003326 mg/dm2. The CuAl10Ni5Fe4 alloy loses the most weight (0.013659 mg/dm²) following heat treatment (S.T.+T) after 24 hours. The minimal corrosion rate for the CuAl10Ni5Fe4-0.40 % Ti alloy after forging was 0.003916 mg/(dm2·day) after 72 hours. Due to stratification, corrosion creates craters. Pitted or porous structures and craters are common. All alloys show a decrease in these structures after forging. The formation of the CuCl2 phase is believed to occur in regions experiencing pitting corrosion.
- 3 February 2026
- Published by Trans Tech Publications, Ltd. in Journal of Biomimetics, Biomaterials and Biomedical Engineering
- Vol. 71, 1-15
Cytotoxic and Genotoxic Investigation of Nd and Ce Crossover in Cast EZ43 Magnesium Alloy Enriched Using Rare Elements
This study focuses on the development of magnesium-zinc (Mg-Zn) matrix alloys enriched with rare earth elements (RE), aiming to evaluate both their structural characteristics and in vitro biological responses. The designed alloys incorporated varying amounts of Zn, Nd, Ce, Gd, Zr, and Ca. Two specific EZ43 alloy compositions were synthesized using an induction-heated furnace under a protective gas atmosphere, differing in their Nd-to-Ce weight ratios (1:2 and 2:1). Following casting, the alloys were homogenized at 400 °C for 24 hours to eliminate dendritic structures and minimize elemental segregation. X-ray fluorescence (XRF) was employed to assess the chemical compositions, while scanning electron microscopy (SEM) provided detailed insight into microstructural features and potential intermetallic phases. Biocompatibility was evaluated through cytotoxicity and genotoxicity tests, conducted in accordance with internationally recognized standards to ensure reliability. Results indicated no genotoxic effects and demonstrated high cell viability up to 142% particularly in Nd-enriched samples. Statistical analysis revealed significant differences in biological behavior between the Nd-rich and Ce-rich alloys, with Nd contributing positively to cellular responses. These findings emphasize the importance of RE composition in influencing biocompatibility and suggest that Nd-enriched Mg-Zn alloys hold strong promise for biomedical applications requiring both structural integrity and favorable biological interaction.
- 3 February 2026
- Published by Trans Tech Publications, Ltd. in Journal of Biomimetics, Biomaterials and Biomedical Engineering
- Vol. 71, 1-15
Cytotoxic and Genotoxic Investigation of Nd and Ce Crossover in Cast EZ43 Magnesium Alloy Enriched Using Rare Elements
This study focuses on the development of magnesium-zinc (Mg-Zn) matrix alloys enriched with rare earth elements (RE), aiming to evaluate both their structural characteristics and in vitro biological responses. The designed alloys incorporated varying amounts of Zn, Nd, Ce, Gd, Zr, and Ca. Two specific EZ43 alloy compositions were synthesized using an induction-heated furnace under a protective gas atmosphere, differing in their Nd-to-Ce weight ratios (1:2 and 2:1). Following casting, the alloys were homogenized at 400 °C for 24 hours to eliminate dendritic structures and minimize elemental segregation. X-ray fluorescence (XRF) was employed to assess the chemical compositions, while scanning electron microscopy (SEM) provided detailed insight into microstructural features and potential intermetallic phases. Biocompatibility was evaluated through cytotoxicity and genotoxicity tests, conducted in accordance with internationally recognized standards to ensure reliability. Results indicated no genotoxic effects and demonstrated high cell viability up to 142% particularly in Nd-enriched samples. Statistical analysis revealed significant differences in biological behavior between the Nd-rich and Ce-rich alloys, with Nd contributing positively to cellular responses. These findings emphasize the importance of RE composition in influencing biocompatibility and suggest that Nd-enriched Mg-Zn alloys hold strong promise for biomedical applications requiring both structural integrity and favorable biological interaction.
- 28 January 2026
- Published by Taylor & Francis in Tribology Transactions
- Vol. 69 (2) , 260-282
Rolling Contact Fatigue and Wear Characteristics of ER9 Wheel and R350HT Rail under Sand, Oil, and Leaves Contamination
- 28 January 2026
- Published by Taylor & Francis in Tribology Transactions
- Vol. 69 (2) , 260-282
Rolling Contact Fatigue and Wear Characteristics of ER9 Wheel and R350HT Rail under Sand, Oil, and Leaves Contamination
- 29 November 2025
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 31 (4) , 510-520
Tribological Effects of 0.30% Titanium in NAB Alloy Post-Casting, Heat Treatment and Forging
This study explores the effects of solution treatment, tempering, and forging on the microstructure and tribological properties of 0.30 % Ti-alloyed nickel–aluminum bronze. The modified NAB alloy exhibited a refined microstructure comprising a copper-rich α-phase, martensitic β-phase, and various intermetallic κ (kappa) phases. Titanium addition enhanced nucleation during solidification, reduced dendritic arm spacing, and promoted the formation of discrete κ phases, thereby improving grain refinement and phase uniformity. Notably, tempering the β-phase facilitated its partial decomposition into α and κIII, with further precipitation of κIV and κII phases. Forging significantly altered the alloy's morphology, fragmenting dendritic arms into near-spherical forms and increasing the formation of secondary κIV phases while preserving the fundamental α, β, and κ phases. Hardness analysis revealed that Ti addition markedly improved hardness, with NAB-0.30 %Ti achieving 239.53 HB and 254.06 HB after heat treatment and forging, respectively. Enhanced hardness and improved wear resistance have been attributed to the presence of intermetallic κ phases, increased dislocation density, and grain refinement. Tribological testing confirmed that the forged NAB-0.30 %Ti alloy demonstrated the lowest friction coefficient (0.097), minimal weight loss (0.0035 g), and the best wear rate (1.17 × 10⁻⁸ g/N·m) over 10,000 meters of sliding distance. The findings highlight titanium’s role in refining microstructure and enhancing both hardness and tribological performance of NAB, making it a promising candidate for applications demanding superior wear resistance.
- 29 November 2025
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 31 (4) , 510-520
Tribological Effects of 0.30% Titanium in NAB Alloy Post-Casting, Heat Treatment and Forging
This study explores the effects of solution treatment, tempering, and forging on the microstructure and tribological properties of 0.30 % Ti-alloyed nickel–aluminum bronze. The modified NAB alloy exhibited a refined microstructure comprising a copper-rich α-phase, martensitic β-phase, and various intermetallic κ (kappa) phases. Titanium addition enhanced nucleation during solidification, reduced dendritic arm spacing, and promoted the formation of discrete κ phases, thereby improving grain refinement and phase uniformity. Notably, tempering the β-phase facilitated its partial decomposition into α and κIII, with further precipitation of κIV and κII phases. Forging significantly altered the alloy's morphology, fragmenting dendritic arms into near-spherical forms and increasing the formation of secondary κIV phases while preserving the fundamental α, β, and κ phases. Hardness analysis revealed that Ti addition markedly improved hardness, with NAB-0.30 %Ti achieving 239.53 HB and 254.06 HB after heat treatment and forging, respectively. Enhanced hardness and improved wear resistance have been attributed to the presence of intermetallic κ phases, increased dislocation density, and grain refinement. Tribological testing confirmed that the forged NAB-0.30 %Ti alloy demonstrated the lowest friction coefficient (0.097), minimal weight loss (0.0035 g), and the best wear rate (1.17 × 10⁻⁸ g/N·m) over 10,000 meters of sliding distance. The findings highlight titanium’s role in refining microstructure and enhancing both hardness and tribological performance of NAB, making it a promising candidate for applications demanding superior wear resistance.
- Open Access
- 25 June 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 819-828
Effects of Yttrium and Lanthanum Elements on the Microstructure and Wear Behaviour of Magnesium
This research investigates the impact of yttrium and lanthanum reinforcement on the dry wear, friction, and microstructure of magnesium alloy. The research investigates the effects of the processes such as as-casting and post-homogenization. The alloys MgY3.21La3.15 and MgY4.71La3.98 were created using a process of controlled melting and casting in an atmosphere-controlled environment. The MgY3.21La3.15 alloy, after undergoing homogenization, has a maximum hardness of 93.70 HB from 81.61 HB for the as- cast alloy. The MgY3.21La3.15 alloy exhibits a weight reduction of 0.024 g and a wear rate of 2.44×10–6 g/Nm, which demonstrates exceptional resistance to wear. The MgY4.71La3.98 alloy exhibits a weight loss of 0.053 g and a wear rate of 5.3×10–6 g/Nm. Friction occurs in parallel due to wearing, thus the MgY3.21La3.15 alloy has the lowest friction coefficient with 0.090.
- 25 June 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 819-828
Open AccessEffects of Yttrium and Lanthanum Elements on the Microstructure and Wear Behaviour of Magnesium
This research investigates the impact of yttrium and lanthanum reinforcement on the dry wear, friction, and microstructure of magnesium alloy. The research investigates the effects of the processes such as as-casting and post-homogenization. The alloys MgY3.21La3.15 and MgY4.71La3.98 were created using a process of controlled melting and casting in an atmosphere-controlled environment. The MgY3.21La3.15 alloy, after undergoing homogenization, has a maximum hardness of 93.70 HB from 81.61 HB for the as- cast alloy. The MgY3.21La3.15 alloy exhibits a weight reduction of 0.024 g and a wear rate of 2.44×10–6 g/Nm, which demonstrates exceptional resistance to wear. The MgY4.71La3.98 alloy exhibits a weight loss of 0.053 g and a wear rate of 5.3×10–6 g/Nm. Friction occurs in parallel due to wearing, thus the MgY3.21La3.15 alloy has the lowest friction coefficient with 0.090.
- Open Access
- 29 May 2025
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 32 (2) , 147-154
The Effect of Ce and Nd Addition on Dry/Corrosive Wear Behavior of Newly Developed EZ43 Grade Mg Alloys
This study is concerned with the production of EZ43A and EZ43B alloys by induction melting/casting method and their microstructure, mechanical, and dry/corrosive wear properties. The investigated EZ43A and EZ43B alloys were alloyed with 1 % Ce – 2 % Nd and 2 % Ce – 1 % Nd, respectively. According to the XRD results, ternary Mg0.97Zn0.03/Mg41Nd5/Mg3Gd eutectic phases were present in the microstructure of EZ43A alloy, while quaternary Mg0.97Zn0.03/Mg41Nd5/Mg3Gd/Mg17Ce2 eutectic phase was formed in the microstructure of EZ43B alloy. The hardness increased from 60.41 to 63.34 by increasing Ce from 1 % to 2 %, representing a 5 % improvement in hardness. As the Ce/Nd ratio increased, the yield/tensile strength and modulus of elasticity increased by 2 %, 6 %, and 3 %, respectively. With the increase in Ce, the relative dry wear loss of EZ43A was 1.00, while that of EZ43B was 0.93, and the corrosive relative wear loss of EZ43A was 2.44 and that of EZ43B was 1.56. Accordingly, the dry and corrosive wear resistance of EZ43B increased by 7 % and 36 %, respectively, compared to that of EZ43A.
- 29 May 2025
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 32 (2) , 147-154
Open AccessThe Effect of Ce and Nd Addition on Dry/Corrosive Wear Behavior of Newly Developed EZ43 Grade Mg Alloys
This study is concerned with the production of EZ43A and EZ43B alloys by induction melting/casting method and their microstructure, mechanical, and dry/corrosive wear properties. The investigated EZ43A and EZ43B alloys were alloyed with 1 % Ce – 2 % Nd and 2 % Ce – 1 % Nd, respectively. According to the XRD results, ternary Mg0.97Zn0.03/Mg41Nd5/Mg3Gd eutectic phases were present in the microstructure of EZ43A alloy, while quaternary Mg0.97Zn0.03/Mg41Nd5/Mg3Gd/Mg17Ce2 eutectic phase was formed in the microstructure of EZ43B alloy. The hardness increased from 60.41 to 63.34 by increasing Ce from 1 % to 2 %, representing a 5 % improvement in hardness. As the Ce/Nd ratio increased, the yield/tensile strength and modulus of elasticity increased by 2 %, 6 %, and 3 %, respectively. With the increase in Ce, the relative dry wear loss of EZ43A was 1.00, while that of EZ43B was 0.93, and the corrosive relative wear loss of EZ43A was 2.44 and that of EZ43B was 1.56. Accordingly, the dry and corrosive wear resistance of EZ43B increased by 7 % and 36 %, respectively, compared to that of EZ43A.
- Open Access
Effect of 0.20% Beryllium (Be)-Added CuAl10Ni5Fe4 Alloy on Tribological Behavior and Microstructural Properties After Post-Casting Heat Treatment and Forging Process
This study explored how post-casting heat treatment and forging affected the tribological and microstructural characteristics of 0.20% beryllium (Be)-added CuAl10Ni5Fe4 alloys. The heat-treated CuAl10Ni5Fe4 microstructure exhibits a copper-rich α (alpha)-solid-solution phase, a martensitic β (beta)-phase, and diverse intermetallic κ (kappa)-phases, such as leaf-shaped κI, thin κIII, and black globs. Adding 0.20% beryllium to CuAl10Ni5Fe4 alloys enhanced the dendritic arm thickness, needle-like shape, and κ-phase quantities. Significant κIV- and κII-phase precipitation was observed in the tempered β-phase. Beryllium improves the aluminum matrix’s microstructure. Forging greatly reduced the microstructural thickness of CuAl10Ni5Fe4 and CuAl10Ni5Fe4-0.20% Be alloys. The forging process also developed new κIV-phases. Wear resistance and hardness improved with beryllium. The CuAl10Ni5Fe4-0.20% Be alloy had the highest hardness values (235.29 and 255.08 HB) after solution treatment (ST) and tempering (T) after casting and forging (F). The CuAl10Ni5Fe4-0.20% alloy with Be added had the best wear after solution treatment, tempering, and forging. The CuAl10Ni5Fe4-0.20% Be alloy demonstrated a 0.00272 g weight loss, a 1.36 × 10−8 g/N*m wear rate, and a 0.059 friction coefficient at 10,000 m after forging (F).
Open AccessEffect of 0.20% Beryllium (Be)-Added CuAl10Ni5Fe4 Alloy on Tribological Behavior and Microstructural Properties After Post-Casting Heat Treatment and Forging Process
This study explored how post-casting heat treatment and forging affected the tribological and microstructural characteristics of 0.20% beryllium (Be)-added CuAl10Ni5Fe4 alloys. The heat-treated CuAl10Ni5Fe4 microstructure exhibits a copper-rich α (alpha)-solid-solution phase, a martensitic β (beta)-phase, and diverse intermetallic κ (kappa)-phases, such as leaf-shaped κI, thin κIII, and black globs. Adding 0.20% beryllium to CuAl10Ni5Fe4 alloys enhanced the dendritic arm thickness, needle-like shape, and κ-phase quantities. Significant κIV- and κII-phase precipitation was observed in the tempered β-phase. Beryllium improves the aluminum matrix’s microstructure. Forging greatly reduced the microstructural thickness of CuAl10Ni5Fe4 and CuAl10Ni5Fe4-0.20% Be alloys. The forging process also developed new κIV-phases. Wear resistance and hardness improved with beryllium. The CuAl10Ni5Fe4-0.20% Be alloy had the highest hardness values (235.29 and 255.08 HB) after solution treatment (ST) and tempering (T) after casting and forging (F). The CuAl10Ni5Fe4-0.20% alloy with Be added had the best wear after solution treatment, tempering, and forging. The CuAl10Ni5Fe4-0.20% Be alloy demonstrated a 0.00272 g weight loss, a 1.36 × 10−8 g/N*m wear rate, and a 0.059 friction coefficient at 10,000 m after forging (F).
- Open Access
- 24 September 2024
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 69 (3) , 911-921
Effect of Zinc and Silicon on TriboCorrosive Wear Behaviors of Hot Forged CuZn3Fe2Si3 and CuZn15Si4 Alloys
The production and characterization of UNS C65620 (CuZn3Fe2Si3) and UNS C87800 (CuZn15Si4) coded alloys were investigated. The alloys poured into the gravity die casting method were hot forged with a ram, followed by stress relief annealing heat treatment. While the formation of Cu4Si, Cu0.83Si0.17 and Cu5Zn8 phases were detected in the structure of the UNS C65620 coded alloy, Cu12.75SiZn2.92 and Cu3Zn intermetallics with the phases given above were observed in the structure of the alloy containing more Zn and Si. The formation of phases containing more Si and Zn resulted in an increase in both the hardness and strength of the UNS C87800 coded alloy, while the decrease in the % reduction of area and the observation of dynamic deformation aging caused the increase in both the wear rate and deformation hardening rate, which led to embrittlement of the alloy. The deterioration of the corrosion resistance of the UNS C87800 coded alloy can be attributed to the formation of Zn-rich corrosion products on the surface during corrosion.
- 24 September 2024
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 69 (3) , 911-921
Open AccessEffect of Zinc and Silicon on TriboCorrosive Wear Behaviors of Hot Forged CuZn3Fe2Si3 and CuZn15Si4 Alloys
The production and characterization of UNS C65620 (CuZn3Fe2Si3) and UNS C87800 (CuZn15Si4) coded alloys were investigated. The alloys poured into the gravity die casting method were hot forged with a ram, followed by stress relief annealing heat treatment. While the formation of Cu4Si, Cu0.83Si0.17 and Cu5Zn8 phases were detected in the structure of the UNS C65620 coded alloy, Cu12.75SiZn2.92 and Cu3Zn intermetallics with the phases given above were observed in the structure of the alloy containing more Zn and Si. The formation of phases containing more Si and Zn resulted in an increase in both the hardness and strength of the UNS C87800 coded alloy, while the decrease in the % reduction of area and the observation of dynamic deformation aging caused the increase in both the wear rate and deformation hardening rate, which led to embrittlement of the alloy. The deterioration of the corrosion resistance of the UNS C87800 coded alloy can be attributed to the formation of Zn-rich corrosion products on the surface during corrosion.
- 27 August 2024
- Published by Taylor & Francis in Canadian Metallurgical Quarterly
- Vol. 64 (3) , 914-926
Bio-properties of Mg-RE alloys: an applied study on cytotoxicity and genotoxicity
- 27 August 2024
- Published by Taylor & Francis in Canadian Metallurgical Quarterly
- Vol. 64 (3) , 914-926
Bio-properties of Mg-RE alloys: an applied study on cytotoxicity and genotoxicity