Esma Keskin
Research Subjects
Esma Keskin has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Hayrettin Ahlatci
Karabuk University
7 shared publications - Ismail Esen
Department of Mechanical Engineering Karabuk University Karabuk Turkey
7 shared publications - Selami Sagiroglu
Karabuk University
2 shared publications - Volkan Karakurt
Sağlam Metal San. ve Tic. A.Ş
2 shared publications - Abdulsalam Saier
Mechanical Engineering Department, Karabuk University, Karabuk 78050, Turkey
1 shared publication - Abubaker J. A. Irhayim
Karabuk University
1 shared publication
Latest Publications
- Open Access
- 25 February 2026
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 32 (1) , 42-56
Effect of 0.40 % and 0.20 % Titanium Addition on Microstructure Properties and Corrosion Behavior of CuAl10Ni5Fe4 Alloy
This study examined how post-casting heat treatment (solution treatment and tempering) and forging affected the corrosion and microstructural properties of the nickel aluminium bronze (CuAl10Ni5Fe4) with 0.20 % and 0.40% titanium addition. Heat-treated CuAl10Ni5Fe4 alloy microstructures showed copper-rich α-solid solution, martensitic β-phase, and intermetallic κ-phases, such as flake-shaped κI, fine κIII, and black globular κIV. Adding 0.20 % and 0.40 % titanium to CuAl10Ni5Fe4 alloys reduced dendritic arm thickness and increased κ phase abundance. Additionally, significant κIV and κII precipitations were observed in the tempered β phase. Tempering β may cause martensitic β to split into tiny α and κIII phases. The grain refinement of the CuAl10Ni5Fe4, CuAl10Ni5Fe4-0.20 % Ti, and CuAl10Ni5Fe4-0.40 % Ti alloys was significantly noticeable after forging. The alloys retained the same α, β, and κ phases seen in the heat-treated alloys after forging. Titanium's refining effect increased the hardness of the alloy into which it was incorporated. Increased stiff phases, such as tempered β and fine κIV, contribute to increased hardness. The forging process enhanced the hardness of all three alloys. Forged and heat treated CuAl10Ni5Fe4-0.40 % Ti alloy had the highest hardness with 243.50 HB and 256.18 HB, respectively. The microstructural phases α, β, and κ significantly impact the corrosion behaviour of CuAl10Ni5Fe4 alloy. The CuAl10Ni5Fe4-0.40 % Ti alloy after forging had the lowest 24-hour weight loss of 0.003326 mg/dm2. The CuAl10Ni5Fe4 alloy loses the most weight (0.013659 mg/dm²) following heat treatment (S.T.+T) after 24 hours. The minimal corrosion rate for the CuAl10Ni5Fe4-0.40 % Ti alloy after forging was 0.003916 mg/(dm2·day) after 72 hours. Due to stratification, corrosion creates craters. Pitted or porous structures and craters are common. All alloys show a decrease in these structures after forging. The formation of the CuCl2 phase is believed to occur in regions experiencing pitting corrosion.
- 25 February 2026
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 32 (1) , 42-56
Open AccessEffect of 0.40 % and 0.20 % Titanium Addition on Microstructure Properties and Corrosion Behavior of CuAl10Ni5Fe4 Alloy
This study examined how post-casting heat treatment (solution treatment and tempering) and forging affected the corrosion and microstructural properties of the nickel aluminium bronze (CuAl10Ni5Fe4) with 0.20 % and 0.40% titanium addition. Heat-treated CuAl10Ni5Fe4 alloy microstructures showed copper-rich α-solid solution, martensitic β-phase, and intermetallic κ-phases, such as flake-shaped κI, fine κIII, and black globular κIV. Adding 0.20 % and 0.40 % titanium to CuAl10Ni5Fe4 alloys reduced dendritic arm thickness and increased κ phase abundance. Additionally, significant κIV and κII precipitations were observed in the tempered β phase. Tempering β may cause martensitic β to split into tiny α and κIII phases. The grain refinement of the CuAl10Ni5Fe4, CuAl10Ni5Fe4-0.20 % Ti, and CuAl10Ni5Fe4-0.40 % Ti alloys was significantly noticeable after forging. The alloys retained the same α, β, and κ phases seen in the heat-treated alloys after forging. Titanium's refining effect increased the hardness of the alloy into which it was incorporated. Increased stiff phases, such as tempered β and fine κIV, contribute to increased hardness. The forging process enhanced the hardness of all three alloys. Forged and heat treated CuAl10Ni5Fe4-0.40 % Ti alloy had the highest hardness with 243.50 HB and 256.18 HB, respectively. The microstructural phases α, β, and κ significantly impact the corrosion behaviour of CuAl10Ni5Fe4 alloy. The CuAl10Ni5Fe4-0.40 % Ti alloy after forging had the lowest 24-hour weight loss of 0.003326 mg/dm2. The CuAl10Ni5Fe4 alloy loses the most weight (0.013659 mg/dm²) following heat treatment (S.T.+T) after 24 hours. The minimal corrosion rate for the CuAl10Ni5Fe4-0.40 % Ti alloy after forging was 0.003916 mg/(dm2·day) after 72 hours. Due to stratification, corrosion creates craters. Pitted or porous structures and craters are common. All alloys show a decrease in these structures after forging. The formation of the CuCl2 phase is believed to occur in regions experiencing pitting corrosion.
- 29 November 2025
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 31 (4) , 510-520
Tribological Effects of 0.30% Titanium in NAB Alloy Post-Casting, Heat Treatment and Forging
This study explores the effects of solution treatment, tempering, and forging on the microstructure and tribological properties of 0.30 % Ti-alloyed nickel–aluminum bronze. The modified NAB alloy exhibited a refined microstructure comprising a copper-rich α-phase, martensitic β-phase, and various intermetallic κ (kappa) phases. Titanium addition enhanced nucleation during solidification, reduced dendritic arm spacing, and promoted the formation of discrete κ phases, thereby improving grain refinement and phase uniformity. Notably, tempering the β-phase facilitated its partial decomposition into α and κIII, with further precipitation of κIV and κII phases. Forging significantly altered the alloy's morphology, fragmenting dendritic arms into near-spherical forms and increasing the formation of secondary κIV phases while preserving the fundamental α, β, and κ phases. Hardness analysis revealed that Ti addition markedly improved hardness, with NAB-0.30 %Ti achieving 239.53 HB and 254.06 HB after heat treatment and forging, respectively. Enhanced hardness and improved wear resistance have been attributed to the presence of intermetallic κ phases, increased dislocation density, and grain refinement. Tribological testing confirmed that the forged NAB-0.30 %Ti alloy demonstrated the lowest friction coefficient (0.097), minimal weight loss (0.0035 g), and the best wear rate (1.17 × 10⁻⁸ g/N·m) over 10,000 meters of sliding distance. The findings highlight titanium’s role in refining microstructure and enhancing both hardness and tribological performance of NAB, making it a promising candidate for applications demanding superior wear resistance.
- 29 November 2025
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 31 (4) , 510-520
Tribological Effects of 0.30% Titanium in NAB Alloy Post-Casting, Heat Treatment and Forging
This study explores the effects of solution treatment, tempering, and forging on the microstructure and tribological properties of 0.30 % Ti-alloyed nickel–aluminum bronze. The modified NAB alloy exhibited a refined microstructure comprising a copper-rich α-phase, martensitic β-phase, and various intermetallic κ (kappa) phases. Titanium addition enhanced nucleation during solidification, reduced dendritic arm spacing, and promoted the formation of discrete κ phases, thereby improving grain refinement and phase uniformity. Notably, tempering the β-phase facilitated its partial decomposition into α and κIII, with further precipitation of κIV and κII phases. Forging significantly altered the alloy's morphology, fragmenting dendritic arms into near-spherical forms and increasing the formation of secondary κIV phases while preserving the fundamental α, β, and κ phases. Hardness analysis revealed that Ti addition markedly improved hardness, with NAB-0.30 %Ti achieving 239.53 HB and 254.06 HB after heat treatment and forging, respectively. Enhanced hardness and improved wear resistance have been attributed to the presence of intermetallic κ phases, increased dislocation density, and grain refinement. Tribological testing confirmed that the forged NAB-0.30 %Ti alloy demonstrated the lowest friction coefficient (0.097), minimal weight loss (0.0035 g), and the best wear rate (1.17 × 10⁻⁸ g/N·m) over 10,000 meters of sliding distance. The findings highlight titanium’s role in refining microstructure and enhancing both hardness and tribological performance of NAB, making it a promising candidate for applications demanding superior wear resistance.
- Open Access
- 25 June 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 819-828
Effects of Yttrium and Lanthanum Elements on the Microstructure and Wear Behaviour of Magnesium
This research investigates the impact of yttrium and lanthanum reinforcement on the dry wear, friction, and microstructure of magnesium alloy. The research investigates the effects of the processes such as as-casting and post-homogenization. The alloys MgY3.21La3.15 and MgY4.71La3.98 were created using a process of controlled melting and casting in an atmosphere-controlled environment. The MgY3.21La3.15 alloy, after undergoing homogenization, has a maximum hardness of 93.70 HB from 81.61 HB for the as- cast alloy. The MgY3.21La3.15 alloy exhibits a weight reduction of 0.024 g and a wear rate of 2.44×10–6 g/Nm, which demonstrates exceptional resistance to wear. The MgY4.71La3.98 alloy exhibits a weight loss of 0.053 g and a wear rate of 5.3×10–6 g/Nm. Friction occurs in parallel due to wearing, thus the MgY3.21La3.15 alloy has the lowest friction coefficient with 0.090.
- 25 June 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 819-828
Open AccessEffects of Yttrium and Lanthanum Elements on the Microstructure and Wear Behaviour of Magnesium
This research investigates the impact of yttrium and lanthanum reinforcement on the dry wear, friction, and microstructure of magnesium alloy. The research investigates the effects of the processes such as as-casting and post-homogenization. The alloys MgY3.21La3.15 and MgY4.71La3.98 were created using a process of controlled melting and casting in an atmosphere-controlled environment. The MgY3.21La3.15 alloy, after undergoing homogenization, has a maximum hardness of 93.70 HB from 81.61 HB for the as- cast alloy. The MgY3.21La3.15 alloy exhibits a weight reduction of 0.024 g and a wear rate of 2.44×10–6 g/Nm, which demonstrates exceptional resistance to wear. The MgY4.71La3.98 alloy exhibits a weight loss of 0.053 g and a wear rate of 5.3×10–6 g/Nm. Friction occurs in parallel due to wearing, thus the MgY3.21La3.15 alloy has the lowest friction coefficient with 0.090.
- Open Access
Effect of 0.20% Beryllium (Be)-Added CuAl10Ni5Fe4 Alloy on Tribological Behavior and Microstructural Properties After Post-Casting Heat Treatment and Forging Process
This study explored how post-casting heat treatment and forging affected the tribological and microstructural characteristics of 0.20% beryllium (Be)-added CuAl10Ni5Fe4 alloys. The heat-treated CuAl10Ni5Fe4 microstructure exhibits a copper-rich α (alpha)-solid-solution phase, a martensitic β (beta)-phase, and diverse intermetallic κ (kappa)-phases, such as leaf-shaped κI, thin κIII, and black globs. Adding 0.20% beryllium to CuAl10Ni5Fe4 alloys enhanced the dendritic arm thickness, needle-like shape, and κ-phase quantities. Significant κIV- and κII-phase precipitation was observed in the tempered β-phase. Beryllium improves the aluminum matrix’s microstructure. Forging greatly reduced the microstructural thickness of CuAl10Ni5Fe4 and CuAl10Ni5Fe4-0.20% Be alloys. The forging process also developed new κIV-phases. Wear resistance and hardness improved with beryllium. The CuAl10Ni5Fe4-0.20% Be alloy had the highest hardness values (235.29 and 255.08 HB) after solution treatment (ST) and tempering (T) after casting and forging (F). The CuAl10Ni5Fe4-0.20% alloy with Be added had the best wear after solution treatment, tempering, and forging. The CuAl10Ni5Fe4-0.20% Be alloy demonstrated a 0.00272 g weight loss, a 1.36 × 10−8 g/N*m wear rate, and a 0.059 friction coefficient at 10,000 m after forging (F).
Open AccessEffect of 0.20% Beryllium (Be)-Added CuAl10Ni5Fe4 Alloy on Tribological Behavior and Microstructural Properties After Post-Casting Heat Treatment and Forging Process
This study explored how post-casting heat treatment and forging affected the tribological and microstructural characteristics of 0.20% beryllium (Be)-added CuAl10Ni5Fe4 alloys. The heat-treated CuAl10Ni5Fe4 microstructure exhibits a copper-rich α (alpha)-solid-solution phase, a martensitic β (beta)-phase, and diverse intermetallic κ (kappa)-phases, such as leaf-shaped κI, thin κIII, and black globs. Adding 0.20% beryllium to CuAl10Ni5Fe4 alloys enhanced the dendritic arm thickness, needle-like shape, and κ-phase quantities. Significant κIV- and κII-phase precipitation was observed in the tempered β-phase. Beryllium improves the aluminum matrix’s microstructure. Forging greatly reduced the microstructural thickness of CuAl10Ni5Fe4 and CuAl10Ni5Fe4-0.20% Be alloys. The forging process also developed new κIV-phases. Wear resistance and hardness improved with beryllium. The CuAl10Ni5Fe4-0.20% Be alloy had the highest hardness values (235.29 and 255.08 HB) after solution treatment (ST) and tempering (T) after casting and forging (F). The CuAl10Ni5Fe4-0.20% alloy with Be added had the best wear after solution treatment, tempering, and forging. The CuAl10Ni5Fe4-0.20% Be alloy demonstrated a 0.00272 g weight loss, a 1.36 × 10−8 g/N*m wear rate, and a 0.059 friction coefficient at 10,000 m after forging (F).
- Open Access
Microstructural Characterization, Tribological and Corrosion Behavior of H111 Hot-Rolled AA5754 after Homogenization and Aging
In this study, the microstructural properties, wear resistance, and corrosion behavior of H111 hot-rolled AA5754 alloy before heat treatment, after homogenization, and after aging were examined. The microstructure was mainly composed of the scattered forms of black and gray contrast particles on the matrix and precipitations were observed at the boundaries of the grain. The as-rolled material exhibited a dense pancake-shaped grain structure, which is typical of as-rolled material. Observation along the L-direction did not yield distinct demarcations among the grains and was not uniformly distributed, with precipitates at the grain boundary. When they aged, there was a parallel increase in fine and huge black and gray contrast particles in the zone. Therefore, it could be stated that the amount of fine grains increased due to the rise in the homogenization process. The rolled base metal with the grain orientation was found to be parallel to the rolling direction. On the other hand, the coarse grains were clearly observed in the aging heat-treatment condition. The grains had an elongated morphology consistent with the rolling process of the metal before the heat-treatment process. The aged alloy had the highest hardness with a value of 86.83 HB; the lowest hardness was seen in the alloy before heat treatment with a value of 68.67 HB. The weight loss and wear rate of this material at the end of 10,000 m were, respectively, 1.01 × 10−3 g and 5.07 × 10−9 g/Nm. It was observed that the alloy had the highest weight loss and worst wear resistance before heat treatment. Weight loss and wear rates at the end of 10,000 m were, respectively, 3.42 × 10−3 g and 17.08 × 10−9 g/Nm. According to these results, the friction coefficients during wear were parallel and the material with the lowest friction coefficient after aging was 0.045. While the alloys corroded after aging showed more weight loss, the alloys corroded before heat treatment exhibited better corrosion behavior. Among the alloys, the least weight loss after 24 h was observed in the alloy that was corroded before heat treatment and this value was 0.69 × 10−3 mg/dm2. The highest weight loss was observed in the aged alloy with a value of 1.37 × 10−3 mg/dm2. The alloy before heat treatment, which corroded after casting, showed the lowest corrosion rate with a value of 0.39 × 10−3 mg/(dm2·day) after 72 h. The alloy that was corroded before heat treatment showed the best corrosion behavior by creating a corrosion potential of 1.04 ± 1.5 V at a current density of −586 ± 0.04 μA/cm2. However, after aging, the corroded alloy showed the worst corrosion behavior with a corrosion potential of 5.16 ± 3.3 V at a current density of −880 ± 0.01 μA/cm2.
Open AccessMicrostructural Characterization, Tribological and Corrosion Behavior of H111 Hot-Rolled AA5754 after Homogenization and Aging
In this study, the microstructural properties, wear resistance, and corrosion behavior of H111 hot-rolled AA5754 alloy before heat treatment, after homogenization, and after aging were examined. The microstructure was mainly composed of the scattered forms of black and gray contrast particles on the matrix and precipitations were observed at the boundaries of the grain. The as-rolled material exhibited a dense pancake-shaped grain structure, which is typical of as-rolled material. Observation along the L-direction did not yield distinct demarcations among the grains and was not uniformly distributed, with precipitates at the grain boundary. When they aged, there was a parallel increase in fine and huge black and gray contrast particles in the zone. Therefore, it could be stated that the amount of fine grains increased due to the rise in the homogenization process. The rolled base metal with the grain orientation was found to be parallel to the rolling direction. On the other hand, the coarse grains were clearly observed in the aging heat-treatment condition. The grains had an elongated morphology consistent with the rolling process of the metal before the heat-treatment process. The aged alloy had the highest hardness with a value of 86.83 HB; the lowest hardness was seen in the alloy before heat treatment with a value of 68.67 HB. The weight loss and wear rate of this material at the end of 10,000 m were, respectively, 1.01 × 10−3 g and 5.07 × 10−9 g/Nm. It was observed that the alloy had the highest weight loss and worst wear resistance before heat treatment. Weight loss and wear rates at the end of 10,000 m were, respectively, 3.42 × 10−3 g and 17.08 × 10−9 g/Nm. According to these results, the friction coefficients during wear were parallel and the material with the lowest friction coefficient after aging was 0.045. While the alloys corroded after aging showed more weight loss, the alloys corroded before heat treatment exhibited better corrosion behavior. Among the alloys, the least weight loss after 24 h was observed in the alloy that was corroded before heat treatment and this value was 0.69 × 10−3 mg/dm2. The highest weight loss was observed in the aged alloy with a value of 1.37 × 10−3 mg/dm2. The alloy before heat treatment, which corroded after casting, showed the lowest corrosion rate with a value of 0.39 × 10−3 mg/(dm2·day) after 72 h. The alloy that was corroded before heat treatment showed the best corrosion behavior by creating a corrosion potential of 1.04 ± 1.5 V at a current density of −586 ± 0.04 μA/cm2. However, after aging, the corroded alloy showed the worst corrosion behavior with a corrosion potential of 5.16 ± 3.3 V at a current density of −880 ± 0.01 μA/cm2.
- Open Access
Effect of Oxidation Process on Mechanical and Tribological Behaviour of Titanium Grade 5 Alloy
In this study, microstructural characterization, mechanical (tensile and compressive) properties, and tribological (wear) properties of Titanium Grade 5 alloy after the oxidation process were examined. While it is observed that the grey contrast coloured α grains are coaxial in the microstructures, it is seen that there are black contrast coloured β grains at the grain boundaries. However, in oxidised Titanium Grade 5, it is possible to observe that the α structure becomes larger, and the number and density of the structure increases. Small-sized structures can be seen inside the growing α particles and on the β particles. These structures are predicted to be Al-Ti/Al-V secondary phases. The nonoxidised alloy matrix and the OL layer exhibited a macrolevel hardness of 335 ± 3.21 HB and 353 ± 1.62 HB, respectively. The heat treatment increased Vickers microhardness by 13% in polished and etched nonoxidised and oxidised alloys, from 309 ± 2.08 HV1 to 352 ± 1.43 HV1. The Vickers microhardness value of the oxidised sample was 528 ± 1.74 HV1, as a 50% increase was noted. According to their tensile properties, oxidised alloys showed a better result compared to nonoxidised alloys. While the peak stress in the oxidised alloy was 1028.40 MPa, in the nonoxidised alloy, this value was 1027.20 MPa. It is seen that the peak stresses of both materials are close to each other, and the result of the oxidised alloy is slightly better. When we look at the breaking strain to characterise the deformation behaviour in the materials, it is 0.084 mm/mm in the oxidised alloy; In the nonoxidised alloy, it is 0.066 mm/mm. When we look at the stress at offset yield of the two alloys, it is 694.56 MPa in the oxidised alloy; it was found to be 674.092 MPa in the nonoxidised alloy. According to their compressive test properties, the maximum compressive strength is 2164.32 MPa in the oxidised alloy; in the nonoxidised alloy, it is 1531.52 MPa. While the yield strength is 972.50 MPa in oxidised Titanium Grade 5, it was found to be 934.16 MPa in nonoxidised Titanium Grade 5. When the compressive deformation oxidised alloy is 100.01%, in the nonoxidised alloy, it is 68.50%. According to their tribological properties, the oxidised alloy provided the least weight loss after 10,000 m and had the best wear resistance. This material’s weight loss and wear coefficient at the end of 10,000 m are 0.127 ± 0.0002 g and (63.45 ± 0.15) × 10−8 g/Nm, respectively. The highest weight loss and worst wear resistance have been observed in the nonoxidised alloy. The weight loss and wear coefficients at the end of 10,000 m are 0.140 ± 0.0003 g and (69.75 ± 0.09) × 10−8 g/Nm, respectively. The oxidation process has been shown to improve the tribological properties of Titanium Grade 5 alloy.
Open AccessEffect of Oxidation Process on Mechanical and Tribological Behaviour of Titanium Grade 5 Alloy
In this study, microstructural characterization, mechanical (tensile and compressive) properties, and tribological (wear) properties of Titanium Grade 5 alloy after the oxidation process were examined. While it is observed that the grey contrast coloured α grains are coaxial in the microstructures, it is seen that there are black contrast coloured β grains at the grain boundaries. However, in oxidised Titanium Grade 5, it is possible to observe that the α structure becomes larger, and the number and density of the structure increases. Small-sized structures can be seen inside the growing α particles and on the β particles. These structures are predicted to be Al-Ti/Al-V secondary phases. The nonoxidised alloy matrix and the OL layer exhibited a macrolevel hardness of 335 ± 3.21 HB and 353 ± 1.62 HB, respectively. The heat treatment increased Vickers microhardness by 13% in polished and etched nonoxidised and oxidised alloys, from 309 ± 2.08 HV1 to 352 ± 1.43 HV1. The Vickers microhardness value of the oxidised sample was 528 ± 1.74 HV1, as a 50% increase was noted. According to their tensile properties, oxidised alloys showed a better result compared to nonoxidised alloys. While the peak stress in the oxidised alloy was 1028.40 MPa, in the nonoxidised alloy, this value was 1027.20 MPa. It is seen that the peak stresses of both materials are close to each other, and the result of the oxidised alloy is slightly better. When we look at the breaking strain to characterise the deformation behaviour in the materials, it is 0.084 mm/mm in the oxidised alloy; In the nonoxidised alloy, it is 0.066 mm/mm. When we look at the stress at offset yield of the two alloys, it is 694.56 MPa in the oxidised alloy; it was found to be 674.092 MPa in the nonoxidised alloy. According to their compressive test properties, the maximum compressive strength is 2164.32 MPa in the oxidised alloy; in the nonoxidised alloy, it is 1531.52 MPa. While the yield strength is 972.50 MPa in oxidised Titanium Grade 5, it was found to be 934.16 MPa in nonoxidised Titanium Grade 5. When the compressive deformation oxidised alloy is 100.01%, in the nonoxidised alloy, it is 68.50%. According to their tribological properties, the oxidised alloy provided the least weight loss after 10,000 m and had the best wear resistance. This material’s weight loss and wear coefficient at the end of 10,000 m are 0.127 ± 0.0002 g and (63.45 ± 0.15) × 10−8 g/Nm, respectively. The highest weight loss and worst wear resistance have been observed in the nonoxidised alloy. The weight loss and wear coefficients at the end of 10,000 m are 0.140 ± 0.0003 g and (69.75 ± 0.09) × 10−8 g/Nm, respectively. The oxidation process has been shown to improve the tribological properties of Titanium Grade 5 alloy.
- Open Access
Effect of Rare Earth Elements (Y, La) on Microstructural Characterization and Corrosion Behavior of Ternary Mg-Y-La Alloys
In this study, the microstructural properties and corrosion behavior of RE elements (Y, La) added to magnesium in varying minors after casting and homogenization heat treatment were investigated. Three-phase structures, such as α-Mg, lamellae-like phases, and network-shaped eutectic compounds, were seen in the microstructure results. The dendrite-like phases were evenly distributed from the eutectic compounds to the interior of the α-Mg grains, while the eutectic compounds (α-Mg + Mg) RE (La/Y)) were distributed at the grain boundaries. According to the corrosion results, the typical hydroxide formation for lanthanum content caused the formation of crater structures in the material, and with the increase in lanthanum content, these crater structures increased both in depth and in density. In addition, the corrosion products formed by Y2O3 and Y(OH)3 in the Mg-3.21Y-3.15 La alloy increased the thickness of the corrosion film and formed a barrier that protects the material against corrosion. The thinness of the protective barrier against corrosion in the Mg-4.71 Y-3.98 La alloy is due to the increased lanthanum and yttrium ratios. In addition, the corrosion resistance of both Mg-3.21Y-3.15 La and Mg-4.71 Y-3.98 La alloys decreases after homogenization. This negative effect on corrosion is due to the coaxial distribution of oxide/hydroxide layers formed by yttrium and lanthanum after homogenization.
Open AccessEffect of Rare Earth Elements (Y, La) on Microstructural Characterization and Corrosion Behavior of Ternary Mg-Y-La Alloys
In this study, the microstructural properties and corrosion behavior of RE elements (Y, La) added to magnesium in varying minors after casting and homogenization heat treatment were investigated. Three-phase structures, such as α-Mg, lamellae-like phases, and network-shaped eutectic compounds, were seen in the microstructure results. The dendrite-like phases were evenly distributed from the eutectic compounds to the interior of the α-Mg grains, while the eutectic compounds (α-Mg + Mg) RE (La/Y)) were distributed at the grain boundaries. According to the corrosion results, the typical hydroxide formation for lanthanum content caused the formation of crater structures in the material, and with the increase in lanthanum content, these crater structures increased both in depth and in density. In addition, the corrosion products formed by Y2O3 and Y(OH)3 in the Mg-3.21Y-3.15 La alloy increased the thickness of the corrosion film and formed a barrier that protects the material against corrosion. The thinness of the protective barrier against corrosion in the Mg-4.71 Y-3.98 La alloy is due to the increased lanthanum and yttrium ratios. In addition, the corrosion resistance of both Mg-3.21Y-3.15 La and Mg-4.71 Y-3.98 La alloys decreases after homogenization. This negative effect on corrosion is due to the coaxial distribution of oxide/hydroxide layers formed by yttrium and lanthanum after homogenization.
- 1 June 1999
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 9 (2) , 2452-2455
Defects in YBCO relevant for RF superconductivity: T-, f- and H-dependencies
- 1 June 1999
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Applied Superconductivity
- Vol. 9 (2) , 2452-2455
Defects in YBCO relevant for RF superconductivity: T-, f- and H-dependencies