João P. G. Magrinho has a total of 71 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Lattice Structures for Orthopedic Metallic Implants

    by Pedro Nogueira, João P. G. Magrinho, Augusto M. Deus, M. Beatriz Silva, M. F. Vaz

  • Open Access

    From Ocean Waste to Injection-Molded Parts: Assessing the Manufacturing with Recycled Fishing Nets

    by João P. G. Magrinho, Mariana V. A. Costa, João F. Caseiro, Ana L. Pires, Nuno Fidelis, Maria Beatriz Silva

    Plastic production and consumption have increased substantially due to the favorable properties of these materials, raising significant environmental concerns because most plastics do not fully decompose. A substantial portion of ocean plastic waste comes from ghost gear, including abandoned fishing nets. In this context, mechanical recycling offers a promising route for recovering these materials and reducing their environmental impact. This study evaluates the feasibility of using recycled fishing nets made of polyamide 6 (PA6) to manufacture injection-molded parts. Injection-molded specimens produced from recycled fishing nets were descriptively compared with specimens obtained from commercially available extruded PA6 plates, used as a commercial processing reference. Both materials were also subjected to an additional post-injection mechanical recycling cycle to evaluate short-term property retention after reprocessing. The feasibility of producing cardholders by injection molding was also examined as a proof of concept. Physical and mechanical characterization showed that the recycled fishing-net PA6 exhibited higher average yield stress and Young’s modulus, but lower stress and strain at break and lower impact toughness than the commercial PA6 reference. The second recycling cycle did not produce a consistent deterioration across the measured properties, although statistical equivalence between the two recycling conditions was not established. The successful production and assembly of cardholders demonstrated the laboratory-scale processability of recovered fishing-net PA6, while further characterization, additional recycling cycles, and process optimization are required to assess long-term recyclability and industrial viability.

  • Design, characterization, modeling and selection of lattice structures for bone repair plates produced by additive manufacturing

    by P Nogueira, B Rodrigues, J Magrinho, P Lopes, Jl Alves, Mb Silva, M Fátima Vaz, Am Deus

    Bone repair plates are crucial in orthopaedics as they provide fixation and stability that promote adequate healing and restore function in fractured or damaged bones. However conventional bone plates can lead to complications and the strategy to overcome such problems relies on the choice of materials, designs, and non-conventional fabrication methods. The current work investigates porous structures for bone plates, obtained by additive manufacturing, featuring two different materials, namely a conventional non-biodegradable (316L stainless steel) and a new possible biodegradable metal (iron). Lattice structures were designed with two different unit cell types, Rhombitruncated Cuboctahedron (RTCO) and Truncated Octahedron (TO), with relative densities of 5%, 25% and 40%. Laser powder bed fusion was used to fabricate such complex structures that would otherwise be difficult to produce. The influence of the thickness of face-sheets and the presence of one or two core layers was also addressed. The mechanical behaviour of plates was evaluated through experimental three-point bending (3PB) and finite element analysis (FEA). A performance index based on mass minimization was proposed to support decision making in parts selection. Plates with RTCO lattices were found to carry higher bending loads than TO samples. An increase in relative density, face-sheet thickness or the number of layers resulted in higher stiffness and yield load values. Deviations between numerical results and experimental data were found, which may be a consequence of the irregularities of the production process.

  • Open Access

    Experimental Determination of the Forming Limits of Steel Thin-Walled Tubes

    by João P. G. Magrinho, Eneko Sáenz-De-Argandoña, Joseba Mendiguren, Maria Beatriz Silva

    This study presents an integrated experimental methodology to determine the forming and fracture limits of welded thin-walled steel tubes, with emphasis on weld-line effects and manufacturing-induced anisotropy. The methodology combines longitudinal and transverse uniaxial tensile tests, using specimens extracted from different positions relative to the weld line, with elastomer-based tube expansion tests. Digital Image Correlation, combined with time-dependent strain analysis, was used to identify the onset of localized necking, while local strain and thickness measurements near the fracture regions supported the determination of fracture limits. This experimental work covered strain paths in the principal strain space ranging from uniaxial tension to near plane-strain expansion within the investigated conditions, enabling the experimental determination of both the Forming Limit Curve and the Fracture Forming Line for the welded tube material. Results reveal a pronounced directional dependence of mechanical response and formability. Transverse specimens exhibited higher yield and ultimate tensile strengths but lower ductility, whereas longitudinal specimens showed greater elongation and strain-hardening capacity. Strain localization and fracture were governed by the combined effects of local thickness variations, weld heterogeneity, and manufacturing-induced anisotropy. In longitudinal specimens, fracture occurred preferentially along the weld line, while in transverse specimens it developed away from the weld region, indicating distinct failure mechanisms depending on the loading direction. These findings highlight the need to account for weld-related heterogeneity and manufacturing history when assessing the formability of welded thin-walled tubes. The proposed methodology provides valuable experimental data for improving failure prediction and supporting the design, simulation, and optimization of welded tubular components.

  • Open Access

    Extending the Process Window of Sheet Injection in AW6082-T6 Aluminium via Localised Laser Heat Treatment

    by João P.G. Magrinho, Angela Cusanno, Miguel Jesus, Antonio Piccininni, Gianfranco Palumbo, Maria Beatriz Silva

    Integrating functional features into lightweight aluminium components remains a key challenge in advanced manufacturing, particularly when forming operations impose severe local deformation. This study focuses on the sheet injection process, a variant of Sheet-Bulk Forming (SBF), where thickening and lateral extrusion occur in previously bent aluminium sheets. The material investigated is AW6082-T6, a medium-strength Al-Mg-Si alloy widely used in transportation and structural applications due to its good strength-to-weight ratio and corrosion resistance. To improve formability and reduce the risk of defects such as fracture and folding, an approach based on Tailored Heat-Treated Blanks (THTB) was employed. Localised Laser Heat Treatment (LHT) was applied to selectively reduce strength and enhance ductility in critical deformation zones. Mechanical characterisation was performed via compression tests on both as-received (T6) and heat-treated (HT) materials. Experiments were conducted on a flexible SBF demonstrator using a two-stage process: bending followed by sheet injection. Numerical simulations were performed to guide LHT pattern design and predict material flow. Among the tested LHT strategies, one demonstrated superior performance, enabling higher injection volumes and reducing process forces while avoiding failure. The experimental results confirm that THTB are an effective method for extending the process window of sheet injection in AW6082-T6, offering a promising solution for the production of complex aluminium components with enhanced functionality.

  • Open Access

    Mechanical Characterization by Profilometry-Based Indentation Plastometry of Locally Heat-Treated Blanks for Sheet Injection Applications

    by Angela Cusanno, João P.G. Magrinho, Antonio Piccininni, Pasquale Guglielmi, Donato Sorgente, Gianfranco Palumbo, Maria Beatriz Silva

    The sheet injection process, a hybrid sheet-bulk forming technique that integrates bending and injection to create complex features such as ribs, offers significant potential for advanced manufacturing applications. However, its implementation with lightweight aluminium alloys is hindered by their limited room-temperature formability. To address this, locally softened, tailored heat-treated blanks produced via laser heat treatment (LHT) can enhance local ductility while maintaining global strength. This study investigates the mechanical property gradients induced by LHT in 3 mm thick AW6082-T6 aluminium alloy sheets using Profilometry-based Indentation Plastometry (PIP). The laser treatment, performed with a 2.5 kW CO 2 laser, produced localized heat treated regions, whose effectiveness was evaluated through microhardness testing. PIP enabled the direct extraction of local stress-strain curves without the need for specimen extraction and was validated against conventional tensile tests. Results showed that PIP accurately captured local variations in mechanical properties, with heat treated zones exhibiting increased ductility compared to the T6 condition.

  • Open Access

    Formability Test for Characterizing the Mode II–III Fracture Transition

    by Inês M. Almeida, João P.G. Magrinho, Paulo A.F. Martins, Maria Beatriz Silva

    The transition between different shear fracture modes is still not well understood, especially in the case of mode II to mode III fracture. While transitions involving mode I have been investigated in previous studies, the interaction between in-plane and out-of-plane shear fracture remains largely unexplored. This work presents an ongoing study aimed at analysing this transition through a newly proposed formability test based on the compression of a thick sheet. The test is intended to investigate the transition region between the shear fracture forming limit (SFFL) and the out-of-plane shear fracture forming limit (OSFFL), associated with fracture mechanics modes II and III, respectively. A new specimen geometry was developed by combining features of existing configurations designed to activate each fracture mode separately. Finite element simulations were carried out to support the design of the specimen and to provide an initial analysis of the strain loading paths in the ligament region. Preliminary numerical results indicate that the proposed test can promote in-plane shear, out-of-plane shear, as well as mixed fracture mechanisms. The predicted fracture initiation sites and corresponding strain paths were examined in the effective strain–stress triaxiality space to provide initial insight into the role of stress state on fracture behaviour. The influence of notch orientation on the resulting fracture mode is discussed, highlighting the potential of the proposed approach for studying mixed shear fracture conditions.

  • Open Access

    Innovation trends in hybrid additive manufacturing: A bibliometric and technology life cycle analysis

    by João P.G. Magrinho

    The manufacturing industry is undergoing a profound transformation driven by increasing demands for efficiency, customization, and sustainability. Although Additive Manufacturing (AM) offers significant advantages, its industrial adoption remains constrained by limitations in precision, productivity, and repeatability. Hybrid Additive Manufacturing (HAM), which integrates additive and conventional manufacturing processes, has emerged as a promising pathway to overcome these limitations. This study goes beyond descriptive literature mapping by combining bibliometric science mapping with Technology Life Cycle (TLC) modelling to analyse the evolution, technological maturity, and industrial positioning of HAM. Using a Scopus dataset and the Gompertz growth model, the study interprets publication and citation dynamics. The results indicate that HAM is currently in an early growth phase, with differentiated maturity trajectories across process families and a projected inflection point around 2030. By linking bibliometric clusters to technological maturity, the study reveals mismatches between scientific activity and industrial deployment, as well as the role of international collaboration in shaping impact and specialization. Based on this integrated analysis, the paper derives actionable research priorities and industrial implications, addressing process reliability, hybrid process planning, material–process co-optimization, and certification challenges. Rather than providing a purely descriptive overview, this study offers an analytical framework that supports strategic decision-making for researchers, industry stakeholders, and policymakers, contributing to the advancement of hybrid manufacturing technologies.

  • Open Access

    Selection of Processing Parameters in Laser Powder Bed Fusion for the Production of Iron Cellular Structures

    by Pedro Nogueira, João P. G. Magrinho, Rodolfo L. Batalha, Maria J. Rosa, Ana Cabral, Paulo J. Morais, Luis Reis, Catarina Santos, Maria J. Carmezim, Ricardo Cláudio, et al.

    Metal additive manufacturing (AM) offers promising advancements in producing implants with complex geometry for biomedical applications, where accuracy and near-net-shape production are essential. Metal AM by laser powder bed fusion (PBF-LB) is a promising route to produce biodegradable iron implants made of complex lattice structures. However, processing windows for pure iron remain poorly defined. This work focuses on optimizing PBF-LB parameters for pure iron using a design of experiments (DoE) approach on bulk samples of different geometries to evaluate different parameters. Hatch laser power, scanning speed, hatch distance and point distance were varied and their effect on porosity, surface roughness and dimensional accuracy was evaluated. This was followed by the fabrication of rhombitruncated cuboctahedron (RTCO) lattice structures with the best parameters previously defined for the bulk samples. The best parameter set (hatch laser power 180 W, scanning speed 600 mm/s, hatch distance 110 µm and point distance 12 µm, corresponding to a volumetric energy density of 90.9 J/mm3) produced bulk samples with a porosity as low as 0.07% (99.93% density) measured in polished sections. Using these parameters, RTCO lattices with designed relative densities of 10.28%, 35.29% and 65.16% were successfully manufactured with small geometric deviations and good control of strut thickness and relative density. The results of this study define a robust PBF-LB processing window for pure iron and demonstrate the feasibility of producing geometrically controlled, biodegradable iron lattice structures suitable for future load-bearing biomedical applications.


  • Open Access

    Formability Limits in Square Tubes and L-Section Profiles

    by Inês M. Almeida, João P. G. Magrinho, Maria Beatriz Silva

    Understanding the formability limits of thin-walled tubes with square cross-sections and L-section profiles is crucial for improving manufacturing efficiency and ensuring structural reliability in industries such as automotive and aerospace. Unlike the usually studied circular tubes, square tubes and L-section profiles geometries present unique deformation and fracture behaviours that require specific analysis. To address this gap, this research establishes a novel methodology combining digital image correlation (DIC) with a time-dependent approach and precise thickness measurements, enabling accurate strain measurements essential to the onset of necking and fracture strain identification. Two experimental tests under different forming conditions allowed capturing a distinct range of strain paths leading to failure. This approach allowed the determination of the forming limit points associated with necking and the fracture forming lines associated with crack opening by tension (mode I) and by in-plane shear (mode II). The findings highlight the strong influence of geometry on the fracture mechanisms and provide valuable data for optimizing tube-forming processes for square tubes and L-section profiles, ultimately enhancing the design and performance of lightweight structural components.