KKKyung Kim

Kyung Kim

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Kyung Kim has a total of 22 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Subnanoscale Investigation of the Interface Between c-Si and PECVD AlOxand Its Effect on Surface Passivation

    by Kyung Kim, Naomi Nandakumar, Xin Zheng, Sean Lim, Ziv Hameiri

    We present a subnanometer scale study of the interface between crystalline silicon (c-Si) and aluminum oxide (AlO x ) deposited by an industrial type, remotely plasma-enhanced chemical vapor deposition (PECVD) system. We investigate the origin of the negative charge density within the AlO x layer and the interface defect density. In order to elucidate the source of the negative charge in subnanoscale, we study various AlO x layers with different properties, such as total charge (Q tot ) and interface defect density (D it ) in both as-deposited and thermally treated conditions using scanning transmission electron microscopy and electron energy loss spectroscopy (EELS). The spatially resolved EELS analysis of aluminum (Al) at the c-Si/AlO x interface reveals changes in its chemical configuration through the thermal process. It is found that the ratio of tetrahedrally- to octahedrally-coordinated Al at the c-Si/AlO x interface is a key factor that linearly correlates with the resulting Q tot . However, the ratio in the AlO x layer (far from the interface) stays constant and is the same for both as-deposited and thermally-treated samples, which seems to show a different aspect of PECVD AlO x layers to those presented in previous reports regarding plasma-assisted atomic layer deposited Al 2 O 3 . We also highlight the possibility of the combined impact on D it from the interfacial layer's thickness and the ratio of silicon dioxide to the tetrahedral Al peaks.


  • Investigation of industrial PECVD AlOx films with very low surface recombination

    by Kyung Kim, Nino Borojevic, Saul Winderbaum, Shubham Duttagupta, Xueyun Zhang, Jongsung Park, Ziv Hameiri


  • Degradation of Surface Passivation and Bulk in p-Type Monocrystalline Silicon Wafers at Elevated Temperature

    by Kyung Kim, Ran Chen, Daniel Chen, Phillip Hamer, Alison Ciesla Nee Wenham, Stuart Wenham, Ziv Hameiri

    The surface passivation quality and the bulk lifetime of boron-doped p-type Czochralski silicon wafers were studied in response to dark annealing at 175 °C, using in situ effective lifetime measurements. We investigated non-fired and fired silicon nitride (SiN $_{\rm x}$ ), aluminum oxide (AlO $_{\rm x}$ ) capped with SiN $_{\rm x}$ , and thermally-grown silicon oxide (SiO $_{2}$ ). Modulation in surface passivation quality and bulk lifetime was detected only in cases where hydrogen is assumed to be released into the silicon wafer from the dielectric (AlO $_{\rm x}$ /SiN $_{\rm x}$ stack and fired SiN $_{\rm x}$ layer). Interestingly, the degradation of both the surface and the bulk were followed by a recovery. It is also interesting to note that the changes in the surface and the bulk seem to be related, as the surface degradation starts when the initial bulk degradation ends. This study indicates a possible involvement of hydrogen in both the degradation and the recovery processes. The evolution of the effective lifetime as a function of time is similar to that reported for carrier-induced degradation in multicrystalline wafers; however, occurring on a different time scale. Hence, these findings may also be valuable for investigation of other degradation mechanisms in different silicon materials.


  • Carrier-Induced Degradation in Multicrystalline Silicon: Dependence on the Silicon Nitride Passivation Layer and Hydrogen Released During Firing

    by Carlos Vargas, Kyung Kim, Gianluca Coletti, David Payne, Catherine Chan, Stuart Wenham, Ziv Hameiri

    Carrier-induced degradation (CID) of multicrystalline silicon (mc-Si) solar cells has been receiving significant attention; however, despite this increasing interest, the defect (or defects) responsible for this degradation has not been determined yet. Previous studies have shown that the surface passivation layer and the firing temperature have a significant impact on the rate and extent of this degradation. In this paper, we further study this impact through an investigation of the CID behavior of the mc-Si wafers passivated with six different silicon nitride layers, each fired at four different peak temperatures. At low firing temperatures, no significant difference in the CID was identified between the samples with different passivation layers; however, a large range of degradation extents was observed at higher firing temperatures. Using Fourier transform infrared spectroscopy, a correlation was found between the degradation extent and the amount of hydrogen released from the dielectric during firing. We verified that no degradation of the surface passivation quality occurred, indicating that the degradation is primarily associated with a bulk defect.


  • Low-Absorbing and Thermally Stable Industrial Silicon Nitride Films With Very Low Surface Recombination

    by Ziv Hameiri, Nino Borojevic, Ly Mai, Naomi Nandakumar, Kyung Kim, Saul Winderbaum

    Amorphous silicon nitride has become the state-of-the-art antireflection coating for silicon solar cells. Optimization of silicon nitride films requires consideration of both the film's optical and electrical properties. It is commonly assumed that silicon-rich silicon nitride films (films with high refractive index) provide better surface passivation, compared to that obtained by films with lower indices. However, silicon-rich films are usually very absorptive in the short (and even medium) wavelength range. Development of low absorption silicon nitride films, that provide good surface passivation, is therefore highly valuable. In this study we compare nine different industrial silicon nitride films, all with similarly low refractive index of 2.09 ± 0.01 measured at 633 nm. We demonstrate that these films exhibit very different electrical, chemical, and optical properties despite their similar refractive index values and correlate these differences with the specific deposition conditions. As a result of this investigation, we have developed industrial thermally stable low-absorbing silicon nitride films that provide excellent surface passivation, with surface saturation current density of 7 fA/cm 2 on both n- and p-type wafers. We demonstrate that the developed low absorption films provide surface passivation with equal quality to that obtained by industrial silicon-rich silicon nitride films.