Fernando Henrique Gruber Colaço
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Fernando Henrique Gruber Colaço has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Giuseppe Pintaude
Surface and Contact Lab (LASC), Academic Department of Mechanics, Universidade Tecnológica Federal do Paraná, Curitiba 81280-340, Brazil
4 shared publications - Alexandre Galiotto
Department of Mechanics, Instituto Federal de Santa Catarina - IFSC 1 , Rua dos Imigrantes, 445, Jaraguá do Sul, Santa Catarina 89254-430
2 shared publications - Almir Turazi
Department of Mechanics, Instituto Federal de Santa Catarina - IFSC 1 , Rua dos Imigrantes, 445, Jaraguá do Sul, Santa Catarina 89254-430
2 shared publications - Gil Magno Portal Chagas
Department of Mechanics, Instituto Federal de Santa Catarina - IFSC 1 , Rua dos Imigrantes, 445, Jaraguá do Sul, Santa Catarina 89254-430
2 shared publications - Joel Stryhalski
Federal Institute of Santa Catarina, Jaragu do Sul, Santa Catarina, Brazil
2 shared publications Arthur Henrique Ribeiro Souto
Instituto Federal de Santa Catarina, Brasil
1 shared publication
Latest Publications
- 15 September 2023
- Published by ASTM International in Materials Performance and Characterization
- Vol. 12 (3) , 396-404
Wear Resistance of Fe–Cr–C Hardfacing Deposited by Flux-Core-Double-Wire GTAW in Rubber Wheel Abrasion Test
The wear resistance of metals can be improved by using the hardfacing technique. Different processes can produce it with the desirable microstructures and mechanical properties. This study presents an original method, flux-core-double-wire of gas-shielded tungsten arc welding, in which wires of different compositions are used simultaneously to obtain different microstructures. The deposition was controlled through the following parameters: welding speed, deposition current, standoff distance, torch angle, and pulse frequency of wire feed. Four coatings were deposited on AISI 1020 steel substrate by combining the cored wires: Fe–Cr–C, Fe–Cr–C–Nb, Fe–Cr–C–Mo–Nb, and Fe–Cr–C–Mo–Ti. The combination of these wires resulted in a hypoeutectic microstructure with niobium and titanium carbides, with an average hardness of 650 HV0.3. The hypereutectic microstructures were formed by different niobium contents, with a microhardness range from 820 to 1,020 HV0.3. The performance of the hardfacing was evaluated in the rubber wheel abrasion test described by ASTM G65, Standard Test Method for Measuring Abrasion Using the Dry Sand/Rubber Wheel Apparatus (Superseded), procedure B. The results revealed that the carbide cracking distinguished the wear resistance, and the hardness was not enough to separate the wear behavior. Still, the volume fraction of carbides was a decisive microstructural parameter.
- 15 September 2023
- Published by ASTM International in Materials Performance and Characterization
- Vol. 12 (3) , 396-404
Wear Resistance of Fe–Cr–C Hardfacing Deposited by Flux-Core-Double-Wire GTAW in Rubber Wheel Abrasion Test
The wear resistance of metals can be improved by using the hardfacing technique. Different processes can produce it with the desirable microstructures and mechanical properties. This study presents an original method, flux-core-double-wire of gas-shielded tungsten arc welding, in which wires of different compositions are used simultaneously to obtain different microstructures. The deposition was controlled through the following parameters: welding speed, deposition current, standoff distance, torch angle, and pulse frequency of wire feed. Four coatings were deposited on AISI 1020 steel substrate by combining the cored wires: Fe–Cr–C, Fe–Cr–C–Nb, Fe–Cr–C–Mo–Nb, and Fe–Cr–C–Mo–Ti. The combination of these wires resulted in a hypoeutectic microstructure with niobium and titanium carbides, with an average hardness of 650 HV0.3. The hypereutectic microstructures were formed by different niobium contents, with a microhardness range from 820 to 1,020 HV0.3. The performance of the hardfacing was evaluated in the rubber wheel abrasion test described by ASTM G65, Standard Test Method for Measuring Abrasion Using the Dry Sand/Rubber Wheel Apparatus (Superseded), procedure B. The results revealed that the carbide cracking distinguished the wear resistance, and the hardness was not enough to separate the wear behavior. Still, the volume fraction of carbides was a decisive microstructural parameter.
- Open Access
- 1 January 2023
- Published by FapUNIFESP (SciELO) in Materials Research
- Vol. 26 (suppl 1) , e20220600
Dry Sliding Wear Resistance of Fe-Cr-C hardfacing Deposited by Flux-Core-Double-Wire GTAW
Gas-Shielded Tungsten Arc Welding (GTAW) was modified to a Flux-Cored-Double-Wire GTAW (FCDW-GTAW); in this technique, wires of different compositions are used simultaneously to obtain different microstructures. In the modified GTAW, automatic flux-cored double-wire was used with a combination of four different wires deposited in AISI1020 steel, allowing different microstructures. Pin-on-disk wear tests described by ASTM G99 was used to evaluate the wear coefficients of four hardfacing materials combining Fe–Cr–C, Fe-Cr-C-Nb, Fe-Cr-C-Mo-Nb, and Fe-Cr-C-Mo-Ti alloys. The combination of these wires resulted in a hypoeutectic microstructure with niobium and titanium carbides, with an average hardness of 650 HV0.3, and hypereutectic microstructures formed by different niobium contents, with a microhardness range from 820 to 1020 HV0.3. The wear tests were performed without lubrication at room temperature, using a 6.0 mm diameter polished alumina sphere as a counter-body. The total distance covered was 1000 m with a speed of 0.1 m/s, a track radius of 6.0 cm, and an applied load of 10 N. Hardness, microstructure, wear coefficient, and wear mechanisms were compared. The results showed that wear resistance could be differentiated by the predominant wear mechanism: polishing for the hypoeutectic hardfacing and cracking for the hypereutectic ones.
- 1 January 2023
- Published by FapUNIFESP (SciELO) in Materials Research
- Vol. 26 (suppl 1) , e20220600
Open AccessDry Sliding Wear Resistance of Fe-Cr-C hardfacing Deposited by Flux-Core-Double-Wire GTAW
Gas-Shielded Tungsten Arc Welding (GTAW) was modified to a Flux-Cored-Double-Wire GTAW (FCDW-GTAW); in this technique, wires of different compositions are used simultaneously to obtain different microstructures. In the modified GTAW, automatic flux-cored double-wire was used with a combination of four different wires deposited in AISI1020 steel, allowing different microstructures. Pin-on-disk wear tests described by ASTM G99 was used to evaluate the wear coefficients of four hardfacing materials combining Fe–Cr–C, Fe-Cr-C-Nb, Fe-Cr-C-Mo-Nb, and Fe-Cr-C-Mo-Ti alloys. The combination of these wires resulted in a hypoeutectic microstructure with niobium and titanium carbides, with an average hardness of 650 HV0.3, and hypereutectic microstructures formed by different niobium contents, with a microhardness range from 820 to 1020 HV0.3. The wear tests were performed without lubrication at room temperature, using a 6.0 mm diameter polished alumina sphere as a counter-body. The total distance covered was 1000 m with a speed of 0.1 m/s, a track radius of 6.0 cm, and an applied load of 10 N. Hardness, microstructure, wear coefficient, and wear mechanisms were compared. The results showed that wear resistance could be differentiated by the predominant wear mechanism: polishing for the hypoeutectic hardfacing and cracking for the hypereutectic ones.
- Open Access
- 6 March 2021
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 113 (11-12) , 3569-3583
Investigations on quality characteristics in gas tungsten arc welding process using artificial neural network integrated with genetic algorithm
Gas tungsten arc welding (GTAW) technology is widely used in industry and has advantages, including high precision, excellent welding quality, and low equipment cost. However, the inclusion of a large number of process parameters hinders its application on a wider scale. Therefore, there is a need to implement the prediction and optimization models that effectively enhance the process performance of the GTAW process in different applications. In this study, a five-factor five-level central composite design (CCD) matrix was used to conduct GTAW experiments. AISI 1020 steel blank was used as a substrate; UTP AF Ledurit 60 and UTP AF Ledurit 68 were used as the materials of two tubular wires. Further, an artificial neural network (ANN) was used to simulate the GTAW process and then combined with a genetic algorithm (GA) to determine welding parameters that can provide an optimal weld. In welding experiments, five different welding current levels, welding speed, distance to the nozzle, angle of movement, and frequency of the wire feed pulses were used. Using GA, optimal welding parameters were determined: welding current = 222 A, welding speed = 25 cm/min, nozzle deflection distance = 8 mm, travel angle = 25°, wire feed pulse frequency = 8 Hz. The determination coefficient (R2) and RMSE value of all response parameters are satisfactory, and the R2 of all the data remained higher than 0.65.
- 6 March 2021
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 113 (11-12) , 3569-3583
Open AccessInvestigations on quality characteristics in gas tungsten arc welding process using artificial neural network integrated with genetic algorithm
Gas tungsten arc welding (GTAW) technology is widely used in industry and has advantages, including high precision, excellent welding quality, and low equipment cost. However, the inclusion of a large number of process parameters hinders its application on a wider scale. Therefore, there is a need to implement the prediction and optimization models that effectively enhance the process performance of the GTAW process in different applications. In this study, a five-factor five-level central composite design (CCD) matrix was used to conduct GTAW experiments. AISI 1020 steel blank was used as a substrate; UTP AF Ledurit 60 and UTP AF Ledurit 68 were used as the materials of two tubular wires. Further, an artificial neural network (ANN) was used to simulate the GTAW process and then combined with a genetic algorithm (GA) to determine welding parameters that can provide an optimal weld. In welding experiments, five different welding current levels, welding speed, distance to the nozzle, angle of movement, and frequency of the wire feed pulses were used. Using GA, optimal welding parameters were determined: welding current = 222 A, welding speed = 25 cm/min, nozzle deflection distance = 8 mm, travel angle = 25°, wire feed pulse frequency = 8 Hz. The determination coefficient (R2) and RMSE value of all response parameters are satisfactory, and the R2 of all the data remained higher than 0.65.
- Open Access
- 1 January 2021
- Published by FapUNIFESP (SciELO) in Matéria (Rio de Janeiro)
- Vol. 26 (4)
Combined effects on Fe-Cr-C hardfacing deposited by new technique FCDW-GTAW
- 1 January 2021
- Published by FapUNIFESP (SciELO) in Matéria (Rio de Janeiro)
- Vol. 26 (4)
Open AccessCombined effects on Fe-Cr-C hardfacing deposited by new technique FCDW-GTAW
- 19 August 2015
- Published by Taylor & Francis in Welding International
- Vol. 30 (4) , 283-292
Evaluation of mass loss of weld-deposited hardfacing with cored wire Ti-FeCrC alloy
In this article, we have studied the mass loss of hardfacing applied by flux-cored arc welding. Heat input, shielding gas and number of layers of coating were changed to application of Fe–Cr–Ti–C self-shielded tubular wire. Overlapping beads were deposited on plates of carbon steel AISI 1020 to analyse the mass loss, hardness and microstructure. For the analysis of mass loss, beads were deposited forming overlapping layers of coatings. Hardness measurements were performed on the surface of the specimens of wear. A rubber wheel abrasion tester was used to access the mass loss of coatings. The coatings had retained austenite and martensite microstructure with carbides finely dispersed in the matrix. The main factors that contributed to the increase in mass loss were the cracks due to higher cooling rate of the samples deposited with low heat input, the dilution in the first layer of all samples also contributed to the increase in mass loss. The smallest mass losses were those deposited coatings with high heat input, the second and fourth layers, the samples AC2, AC4 and AS2. The volume fraction of titanium carbides contributed to the decrease in the mean free path between the particles of carbides and increased the wear resistance of the coatings.
- 19 August 2015
- Published by Taylor & Francis in Welding International
- Vol. 30 (4) , 283-292
Evaluation of mass loss of weld-deposited hardfacing with cored wire Ti-FeCrC alloy
In this article, we have studied the mass loss of hardfacing applied by flux-cored arc welding. Heat input, shielding gas and number of layers of coating were changed to application of Fe–Cr–Ti–C self-shielded tubular wire. Overlapping beads were deposited on plates of carbon steel AISI 1020 to analyse the mass loss, hardness and microstructure. For the analysis of mass loss, beads were deposited forming overlapping layers of coatings. Hardness measurements were performed on the surface of the specimens of wear. A rubber wheel abrasion tester was used to access the mass loss of coatings. The coatings had retained austenite and martensite microstructure with carbides finely dispersed in the matrix. The main factors that contributed to the increase in mass loss were the cracks due to higher cooling rate of the samples deposited with low heat input, the dilution in the first layer of all samples also contributed to the increase in mass loss. The smallest mass losses were those deposited coatings with high heat input, the second and fourth layers, the samples AC2, AC4 and AS2. The volume fraction of titanium carbides contributed to the decrease in the mean free path between the particles of carbides and increased the wear resistance of the coatings.
- Open Access
- 1 March 2014
- Published by FapUNIFESP (SciELO) in Soldagem & Inspeção
- Vol. 19 (1) , 58-68
Avaliação da perda de massa de revestimento duro depositado por soldagem com arame tubular de liga FeCrC-Ti
Neste trabalho estudou-se a perda de massa de revestimento duro aplicado pelo processo de soldagem com arame tubular com a variação de energia de soldagem, gás de proteção e número de camadas do revestimento. Com arame tubular autoprotegido de liga Fe-Cr-C-Ti foram depositados cordões sobrepostos na formação de camadas de revestimento sobre chapas de aço ao Carbono AISI 1020 para a análise da perda de massa, dureza, microestrutura. Foram realizadas medições de dureza na superfície dos corpos de prova de desgaste. Abrasômetro tipo roda de borracha foi usado para determinar a perda de massa dos revestimentos. Os revestimentos apresentaram microestrutura martensítica e austenita retida com carbonetos finamente dispersos na matriz. Os principais fatores que contribuíram para o aumento na perda de massa foram as trincas devido a maior taxa de resfriamento das amostras depositadas com baixa energia de soldagem, a diluição na primeira camada de todas as amostras também contribuiu para o aumento na perda de massa. As menores perdas de massa foram dos revestimentos de duas e quatro camadas depositados com alta energia de soldagem. A fração volumétrica de carbonetos de Titânio contribuiu para a diminuição do caminho livre médio entre as partículas de carbonetos aumentando a resistência ao desgaste dos revestimentos.
- 1 March 2014
- Published by FapUNIFESP (SciELO) in Soldagem & Inspeção
- Vol. 19 (1) , 58-68
Open AccessAvaliação da perda de massa de revestimento duro depositado por soldagem com arame tubular de liga FeCrC-Ti
Neste trabalho estudou-se a perda de massa de revestimento duro aplicado pelo processo de soldagem com arame tubular com a variação de energia de soldagem, gás de proteção e número de camadas do revestimento. Com arame tubular autoprotegido de liga Fe-Cr-C-Ti foram depositados cordões sobrepostos na formação de camadas de revestimento sobre chapas de aço ao Carbono AISI 1020 para a análise da perda de massa, dureza, microestrutura. Foram realizadas medições de dureza na superfície dos corpos de prova de desgaste. Abrasômetro tipo roda de borracha foi usado para determinar a perda de massa dos revestimentos. Os revestimentos apresentaram microestrutura martensítica e austenita retida com carbonetos finamente dispersos na matriz. Os principais fatores que contribuíram para o aumento na perda de massa foram as trincas devido a maior taxa de resfriamento das amostras depositadas com baixa energia de soldagem, a diluição na primeira camada de todas as amostras também contribuiu para o aumento na perda de massa. As menores perdas de massa foram dos revestimentos de duas e quatro camadas depositados com alta energia de soldagem. A fração volumétrica de carbonetos de Titânio contribuiu para a diminuição do caminho livre médio entre as partículas de carbonetos aumentando a resistência ao desgaste dos revestimentos.