Dmitry Naumenko
Dmitry Naumenko has a total of 51 co-authors. Here are the top co-authors by number of shared publications:
- Willem Joseph Quadakkers
Institute for Energy and Climate Research, IEK-2, Forschungszentrum Jülich GmbH, Jülich, Germany
6 shared publications - Heike Hattendorf
Research and Development Department VDM Metals International GmbH Altena Germany
3 shared publications - Elena Yazhenskikh
Forschungszentrum Jülich GmbH, IWV-2, D-52425 Jülich, Germany
2 shared publications - Ivan Povstugar
Max Planck Society
2 shared publications L. Singheiser
Forschungszentrum Jülich GmbH, Institut für Energieforschung, 52425, Jülich, Germany
2 shared publications- Martin Frommherz
Schadensanalyse, Tribologie und Korrosion (TEWS) MTU Aero Engines, AG Dachauer Strasse 665 München 80995 Germany
2 shared publications
Latest Publications
- Open Access
- 5 August 2026
- Published by Elsevier in Corrosion Science
- Vol. 271
Origin of subsurface voids in additively manufactured Ni-base alloy IN625 induced by oxidation
- 5 August 2026
- Published by Elsevier in Corrosion Science
- Vol. 271
Open AccessOrigin of subsurface voids in additively manufactured Ni-base alloy IN625 induced by oxidation
- Open Access
- 25 September 2025
- Published by Elsevier in Journal of Power Sources
- Vol. 659
Towards sustainable interconnects for solid oxide cells: An integrated technical and environmental evaluation of coating methods
- 25 September 2025
- Published by Elsevier in Journal of Power Sources
- Vol. 659
Open AccessTowards sustainable interconnects for solid oxide cells: An integrated technical and environmental evaluation of coating methods
- Open Access
- 17 March 2025
- Published by Elsevier in Corrosion Science
- Vol. 249
Effect of MgSO4 addition on alkali sulphates induced hot corrosion of a β-NiAl coating
- 17 March 2025
- Published by Elsevier in Corrosion Science
- Vol. 249
Open AccessEffect of MgSO4 addition on alkali sulphates induced hot corrosion of a β-NiAl coating
- 10 June 2023
- Published by Elsevier in Corrosion Science
- Vol. 221
Effect of gas composition on the oxide scale growth mechanisms in a ferritic steel for solid oxide cell interconnects
- 10 June 2023
- Published by Elsevier in Corrosion Science
- Vol. 221
Effect of gas composition on the oxide scale growth mechanisms in a ferritic steel for solid oxide cell interconnects
- Open Access
- 6 February 2020
- Published by Wiley in Advanced Engineering Materials
- Vol. 22 (6)
Role of Temperature in Na2SO4–K2SO4 Deposit Induced Type II Hot Corrosion of NiAl Coating on a Commercial Ni‐Based Superalloy
The life span of gas turbine coatings may be restricted by type II hot corrosion when exposed at elevated temperatures in aggressive environments during service. Herein, the temperature dependence of corrosion morphologies and kinetics of NiAl coating on a second‐generation single crystalline Ni‐based superalloy is studied to provide an insight into the possible corrosion mechanisms. A series of tests are performed at 600–800 °C in air‐300 ppm SO2 atmosphere with Na2SO4–20% K2SO4 salt mixture as deposit. Severe attack is observed at both 700 and 750 °C after 24 h exposure, whereas at 600 and 800 °C, only a minor attack is found. The results indicate that the corrosion rate is strongly governed by Na2SO4–NiSO4 liquid formation, and temperature affects the attack rate of the outer coating (mainly β‐NiAl phase) primarily by changing the required minimum SO3 partial pressure to stabilize this liquid. The influence of temperature and on phase equilibrium of the salt and oxide mixture is calculated with an in‐house developed thermodynamic database. The predicted minimum for liquid formation calculated with the database is consistent with the experimental results.
- 6 February 2020
- Published by Wiley in Advanced Engineering Materials
- Vol. 22 (6)
Open AccessRole of Temperature in Na2SO4–K2SO4 Deposit Induced Type II Hot Corrosion of NiAl Coating on a Commercial Ni‐Based Superalloy
The life span of gas turbine coatings may be restricted by type II hot corrosion when exposed at elevated temperatures in aggressive environments during service. Herein, the temperature dependence of corrosion morphologies and kinetics of NiAl coating on a second‐generation single crystalline Ni‐based superalloy is studied to provide an insight into the possible corrosion mechanisms. A series of tests are performed at 600–800 °C in air‐300 ppm SO2 atmosphere with Na2SO4–20% K2SO4 salt mixture as deposit. Severe attack is observed at both 700 and 750 °C after 24 h exposure, whereas at 600 and 800 °C, only a minor attack is found. The results indicate that the corrosion rate is strongly governed by Na2SO4–NiSO4 liquid formation, and temperature affects the attack rate of the outer coating (mainly β‐NiAl phase) primarily by changing the required minimum SO3 partial pressure to stabilize this liquid. The influence of temperature and on phase equilibrium of the salt and oxide mixture is calculated with an in‐house developed thermodynamic database. The predicted minimum for liquid formation calculated with the database is consistent with the experimental results.
- 5 August 2019
- Published by Springer Nature in Oxidation of Metals
- Vol. 92 (5-6) , 471-491
Effect of Nb Addition on Oxidation Mechanisms of High Cr Ferritic Steel in Ar–H2–H2O
- 5 August 2019
- Published by Springer Nature in Oxidation of Metals
- Vol. 92 (5-6) , 471-491
Effect of Nb Addition on Oxidation Mechanisms of High Cr Ferritic Steel in Ar–H2–H2O
- Open Access
- 19 October 2017
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 35 (1-3) , 108-119
High-temperature behavior of oxide dispersion strengthening CoNiCrAlY
To fabricate oxide dispersion strengthened bond coatings, commercial Co–30wt-%Ni–20Cr–8Al–0•4Y powder was milled with 2% additions of Al2O3, Y2O3 or Y2O3 + HfO2. Low-pressure plasma sprayed, free-standing specimens were oxidised in air + 10%H2O at 1100 °C both isothermally (100 h) and in 500, 1−h cycles. Dry air cyclic testing conducted at both ORNL and FZJ showed remarkably similar results. In general, the water vapour addition caused more scale spallation. Two LPPS specimens without oxide additions were tested for comparison. The specimens with 2%Al2O3 addition exhibited the best behaviour as the powder already contained 0•4%Y. Additions of 2%Y2O3 and especially 1%Y2O3 + 1%HfO2 resulted in over-doping as evidenced by high mass gains and the formation of Y- and Hf-rich pegs. Scanning transmission electron microscopy of the isothermal specimens showed no Hf and/or Y segregation to the alumina scale grain boundaries in the over-doped specimens.
- 19 October 2017
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 35 (1-3) , 108-119
Open AccessHigh-temperature behavior of oxide dispersion strengthening CoNiCrAlY
To fabricate oxide dispersion strengthened bond coatings, commercial Co–30wt-%Ni–20Cr–8Al–0•4Y powder was milled with 2% additions of Al2O3, Y2O3 or Y2O3 + HfO2. Low-pressure plasma sprayed, free-standing specimens were oxidised in air + 10%H2O at 1100 °C both isothermally (100 h) and in 500, 1−h cycles. Dry air cyclic testing conducted at both ORNL and FZJ showed remarkably similar results. In general, the water vapour addition caused more scale spallation. Two LPPS specimens without oxide additions were tested for comparison. The specimens with 2%Al2O3 addition exhibited the best behaviour as the powder already contained 0•4%Y. Additions of 2%Y2O3 and especially 1%Y2O3 + 1%HfO2 resulted in over-doping as evidenced by high mass gains and the formation of Y- and Hf-rich pegs. Scanning transmission electron microscopy of the isothermal specimens showed no Hf and/or Y segregation to the alumina scale grain boundaries in the over-doped specimens.
- Open Access
- 10 July 2009
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2009-02 (19) , 1833
Oxidation Kinetics of Y/Zr-doped FeCrAl-alloys in Low and High pO2 Gases
- 10 July 2009
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2009-02 (19) , 1833
Open AccessOxidation Kinetics of Y/Zr-doped FeCrAl-alloys in Low and High pO2 Gases
- 1 January 2008
- Published by Elsevier
- p. 129-160
Lifetime extension of FeCrAIRE alloys in air. Potential role of enhanced Al reservoir and surface pre-treatment (SMILER)
- 1 January 2008
- Published by Elsevier
- p. 129-160
Lifetime extension of FeCrAIRE alloys in air. Potential role of enhanced Al reservoir and surface pre-treatment (SMILER)