Wisut Kaewsakul
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Wisut Kaewsakul has a total of 35 co-authors. Here are the top co-authors by number of shared publications:
- Kannika Sahakaro
Department of Rubber Technology and Polymer Science, Faculty of Science and Technology, Prince of Songkla University, Pattani 94000, Thailand
5 shared publications Anke Blume
4 shared publications- Ekwipoo Kalkornsurapranee
Division of Physical Sciences, Faculty of Science, Prince of Songkla University, Hat-Yai 90110, Thailand
4 shared publications - Jacques W. M. Noordermeer
Department of Elastomer Technology and Engineering, University of Twente, P.O. Box 217, 7500 ae Enschede, the Netherlands
4 shared publications - Wilma K. Dierkes
Sustainable Elastomer Systems, Department of Mechanics of Solids, Surfaces and Systems, Faculty of Engineering Technology, University of Twente, P.O. Box 217, 7500 AE Enschede, The Netherlands
4 shared publications - Ammarin Kraibut
Department of Rubber Technology and Polymer Science, Faculty of Science and Technology, Prince of Songkla University, Pattani 94000, Thailand
3 shared publications
Latest Publications
- Open Access
- 2 September 2026
- Published by Elsevier in Results in Materials
- Vol. 31
Identifying polymer networks structures in S-SBR tyre tread compounds by Temperature Scanning Stress Relaxation (TSSR)
- 2 September 2026
- Published by Elsevier in Results in Materials
- Vol. 31
Open AccessIdentifying polymer networks structures in S-SBR tyre tread compounds by Temperature Scanning Stress Relaxation (TSSR)
- Open Access
- 14 December 2025
- Published by MDPI AG in Journal of Composites Science
- Vol. 9 (12) , 698
Exploring Bio-Based Plasticizer as Alternative to Phthalates for Technical Rubber Goods
The rubber industry uses phthalates as plasticizers in technical rubber goods due to their excellent compatibility, low volatility and cost-effectiveness. Growing concerns over their environmental and health impact have driven the search for sustainable alternatives. Bio-based plasticizers offer a promising solution due to their renewable nature, non-toxicity and biodegradability. This study explores the feasibility of replacing a conventional petroleum-based Di-Iso-Nonyl Phthalate (DINP) with a bio-based phthalate-free plasticizer, Aurora PHFree, in Nitrile Butadiene Rubber (NBR) compounds filled with semi-reinforcing carbon black N660. Aurora PHFree achieves similar processing behavior, cure characteristics, and mechanical properties as well as aging performance by using only half of the amount by weight of DINP. This efficiency is attributed to the improved plasticizing effects, which enable polymer chain mobility, without altering the overall crosslink density, as well as the enhanced dispersion of the carbon black (CB) fillers of the rubber compounds. This research supports the development of more sustainable rubber materials and contributes to reducing the dependence on fossil-based materials while maintaining high-quality standards.
- 14 December 2025
- Published by MDPI AG in Journal of Composites Science
- Vol. 9 (12) , 698
Open AccessExploring Bio-Based Plasticizer as Alternative to Phthalates for Technical Rubber Goods
The rubber industry uses phthalates as plasticizers in technical rubber goods due to their excellent compatibility, low volatility and cost-effectiveness. Growing concerns over their environmental and health impact have driven the search for sustainable alternatives. Bio-based plasticizers offer a promising solution due to their renewable nature, non-toxicity and biodegradability. This study explores the feasibility of replacing a conventional petroleum-based Di-Iso-Nonyl Phthalate (DINP) with a bio-based phthalate-free plasticizer, Aurora PHFree, in Nitrile Butadiene Rubber (NBR) compounds filled with semi-reinforcing carbon black N660. Aurora PHFree achieves similar processing behavior, cure characteristics, and mechanical properties as well as aging performance by using only half of the amount by weight of DINP. This efficiency is attributed to the improved plasticizing effects, which enable polymer chain mobility, without altering the overall crosslink density, as well as the enhanced dispersion of the carbon black (CB) fillers of the rubber compounds. This research supports the development of more sustainable rubber materials and contributes to reducing the dependence on fossil-based materials while maintaining high-quality standards.
- Open Access
- 19 August 2025
- Published by Wiley in Polymer Engineering & Science
- Vol. 65 (10) , 5611-5626
Elucidating Degradation Phenomena During Mixing of Silica‐Natural Rubber Compounds: The Interplay of Viscoelastic Behavior and Silane Microstructures
Various commercial silica‐silane coupling agent combinations are used these days for synthetic rubber‐based passenger car tire treads with high silica‐loadings. For truck tire treads, much lower silica‐loadings are employed in combination with Natural Rubber (NR). The present study examines the impact of various commercial silane coupling agents on degradation phenomena during mixing of silica‐filled NR compounds by analyzing changes in viscoelastic response, with a focus on different silane microstructures. A novel approach using delta–delta (Δδ) values to quantify branch formation caused by degradation‐induced chain modifications has been adopted. Unfilled NR compounds primarily undergo polymer chain scission from thermo‐mechanical and thermo‐oxidative influences. During mixing, bis‐(3‐TriEthoxySilylPropyl) Tetrasulfide (TESPT) silane creates silica‐rubber coupling and lightly crosslinked materials partly based on polysulfidic bonds. The lightly crosslinked rubber essentially sustains the reinforcement level in the compounds, counterbalancing the degradation effect. However, predominant degradation at 180°C significantly deteriorates the mechanical and dynamic properties of compounds containing both TESPT and TESPD (bis‐(3‐Triethoxysilylpropyl) disulfide). OTPTES (3‐OctanoylThioPropylTriEthoxySilane) and MTCO (Mercapto‐ThioCarboxylate Oligomer) silane‐based compounds exhibit notable plasticization effects along with degradation. The choice of OTPTES in particular demonstrates excellent thermal stability, preserving mechanical properties even till 180°C. MTCO, with one reactive mercaptan group, couples efficiently with rubber at low dump temperatures, 130°C and 150°C, enhancing vulcanizate properties. At high dump temperatures of 170°C and 180°C, though, MTCO releases plasticizing moieties during mixing, leading to inferior final properties. The present study highlights the intricate balance between rubber degradation, crosslinking, branching, network formation, rubber‐filler interactions, and plasticization effects specifically in silica‐filled NR compounds for truck tire tread applications.
- 19 August 2025
- Published by Wiley in Polymer Engineering & Science
- Vol. 65 (10) , 5611-5626
Open AccessElucidating Degradation Phenomena During Mixing of Silica‐Natural Rubber Compounds: The Interplay of Viscoelastic Behavior and Silane Microstructures
Various commercial silica‐silane coupling agent combinations are used these days for synthetic rubber‐based passenger car tire treads with high silica‐loadings. For truck tire treads, much lower silica‐loadings are employed in combination with Natural Rubber (NR). The present study examines the impact of various commercial silane coupling agents on degradation phenomena during mixing of silica‐filled NR compounds by analyzing changes in viscoelastic response, with a focus on different silane microstructures. A novel approach using delta–delta (Δδ) values to quantify branch formation caused by degradation‐induced chain modifications has been adopted. Unfilled NR compounds primarily undergo polymer chain scission from thermo‐mechanical and thermo‐oxidative influences. During mixing, bis‐(3‐TriEthoxySilylPropyl) Tetrasulfide (TESPT) silane creates silica‐rubber coupling and lightly crosslinked materials partly based on polysulfidic bonds. The lightly crosslinked rubber essentially sustains the reinforcement level in the compounds, counterbalancing the degradation effect. However, predominant degradation at 180°C significantly deteriorates the mechanical and dynamic properties of compounds containing both TESPT and TESPD (bis‐(3‐Triethoxysilylpropyl) disulfide). OTPTES (3‐OctanoylThioPropylTriEthoxySilane) and MTCO (Mercapto‐ThioCarboxylate Oligomer) silane‐based compounds exhibit notable plasticization effects along with degradation. The choice of OTPTES in particular demonstrates excellent thermal stability, preserving mechanical properties even till 180°C. MTCO, with one reactive mercaptan group, couples efficiently with rubber at low dump temperatures, 130°C and 150°C, enhancing vulcanizate properties. At high dump temperatures of 170°C and 180°C, though, MTCO releases plasticizing moieties during mixing, leading to inferior final properties. The present study highlights the intricate balance between rubber degradation, crosslinking, branching, network formation, rubber‐filler interactions, and plasticization effects specifically in silica‐filled NR compounds for truck tire tread applications.
- Open Access
- 15 July 2025
- Published by Elsevier in European Polymer Journal
- Vol. 236
Insight into the interactions of functionalised rubber-modified silica in tyre tread compounds
- 15 July 2025
- Published by Elsevier in European Polymer Journal
- Vol. 236
Open AccessInsight into the interactions of functionalised rubber-modified silica in tyre tread compounds
- Open Access
Degradation during Mixing of Silica-Reinforced Natural Rubber Compounds
The optimal mixing conditions for silica-filled NR compounds dictate the need to proceed at a high temperature, i.e., 150 °C, to achieve a sufficient degree of silanization. On the other hand, natural rubber is prone to degradation due to mechanical shear and thermal effects during mixing, particularly at long exposure times. The present work investigates NR rubber degradation during mixing in relation to prolonged silanization times. The Mooney viscosity and stress relaxation rates, bound rubber content, storage modulus (G’), and delta δ were investigated to indicate the changes in the elastic/viscous responses of NR molecules related to rubber degradation, molecular chain modifications, and premature crosslinking/interaction. In Gum NR (unfilled), an increase in the viscous response with increasing mixing times indicates a major chain scission that causes a decreased molecular weight and risen chain mobility. For silica-filled NR, an initial decrease in the Mooney viscosity with increasing silanization time is attributed to the chain scission first, but thereafter the effect of the degradation is counterbalanced by a sufficient silanization/coupling reaction which leads to leveling off of the viscous response. Finally, the higher viscous response due to degradation leads to the deterioration of the mechanical properties and rolling resistance performance of tire treads made from such silica-filled NR, particularly when the silanization time exceeds 495 s.
Open AccessDegradation during Mixing of Silica-Reinforced Natural Rubber Compounds
The optimal mixing conditions for silica-filled NR compounds dictate the need to proceed at a high temperature, i.e., 150 °C, to achieve a sufficient degree of silanization. On the other hand, natural rubber is prone to degradation due to mechanical shear and thermal effects during mixing, particularly at long exposure times. The present work investigates NR rubber degradation during mixing in relation to prolonged silanization times. The Mooney viscosity and stress relaxation rates, bound rubber content, storage modulus (G’), and delta δ were investigated to indicate the changes in the elastic/viscous responses of NR molecules related to rubber degradation, molecular chain modifications, and premature crosslinking/interaction. In Gum NR (unfilled), an increase in the viscous response with increasing mixing times indicates a major chain scission that causes a decreased molecular weight and risen chain mobility. For silica-filled NR, an initial decrease in the Mooney viscosity with increasing silanization time is attributed to the chain scission first, but thereafter the effect of the degradation is counterbalanced by a sufficient silanization/coupling reaction which leads to leveling off of the viscous response. Finally, the higher viscous response due to degradation leads to the deterioration of the mechanical properties and rolling resistance performance of tire treads made from such silica-filled NR, particularly when the silanization time exceeds 495 s.
- Open Access
- 4 December 2023
- Published by Elsevier in Surfaces and Interfaces
- Vol. 44
Interfacial coupling efficiency of functionalised rubbers on silica surfaces
- 4 December 2023
- Published by Elsevier in Surfaces and Interfaces
- Vol. 44
Open AccessInterfacial coupling efficiency of functionalised rubbers on silica surfaces
- Open Access
Dynamic Response and Molecular Chain Modifications Associated with Degradation during Mixing of Silica-Reinforced Natural Rubber Compounds
Mixing silica-reinforced rubber for tire tread compounds involves high shear forces and temperatures to obtain a sufficient degree of silanization. Natural Rubber (NR) is sensitive to mastication and chemical reactions, and thus, silica–NR mixing encounters both mechanical and thermal degradation. The present work investigates the degradation phenomena during the mixing of silica-reinforced NR compounds in-depth. The Mooney stress relaxation rates, the dynamic properties with frequency sweep, a novel characterization of branch formation on NR using Δδ values acc. Booij and van Gurp-Palmen plots, together, indicate two major competitive reactions taking place: chain scission or degradation and preliminary cross-linking or branch formation. For masticated pure NR and gum compounds, the viscous responses increase, and the changes in all parameters indicate the dominance of chain scission with increasing dump temperature. It causes molecular weight decrease, broader molecular weight distribution, and branched structures. Different behavior is observed for silica-filled NR compounds in which both physical and chemical cross-links are promoted by silanization and coupling reactions. At high dump temperatures above 150 °C, the results indicate a significant increase in branching due to preliminary cross-linking. These molecular chain modifications that cause network heterogeneity deteriorate the mechanical properties of resulting vulcanizates.
Open AccessDynamic Response and Molecular Chain Modifications Associated with Degradation during Mixing of Silica-Reinforced Natural Rubber Compounds
Mixing silica-reinforced rubber for tire tread compounds involves high shear forces and temperatures to obtain a sufficient degree of silanization. Natural Rubber (NR) is sensitive to mastication and chemical reactions, and thus, silica–NR mixing encounters both mechanical and thermal degradation. The present work investigates the degradation phenomena during the mixing of silica-reinforced NR compounds in-depth. The Mooney stress relaxation rates, the dynamic properties with frequency sweep, a novel characterization of branch formation on NR using Δδ values acc. Booij and van Gurp-Palmen plots, together, indicate two major competitive reactions taking place: chain scission or degradation and preliminary cross-linking or branch formation. For masticated pure NR and gum compounds, the viscous responses increase, and the changes in all parameters indicate the dominance of chain scission with increasing dump temperature. It causes molecular weight decrease, broader molecular weight distribution, and branched structures. Different behavior is observed for silica-filled NR compounds in which both physical and chemical cross-links are promoted by silanization and coupling reactions. At high dump temperatures above 150 °C, the results indicate a significant increase in branching due to preliminary cross-linking. These molecular chain modifications that cause network heterogeneity deteriorate the mechanical properties of resulting vulcanizates.
- Open Access
- 3 August 2022
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 31 (9) , 095034
Design and performance of flexible polymeric piezoelectric energy harvesters for battery-less tyre sensors
A piezoelectric energy harvester for battery-less tyre sensors has been developed. It consists of two key elements: (a) a piezoelectric material—polyvinylidene difluoride (PVDF) film and (b) an electrode—a conductive elastomer filled with carbon black and single-wall carbon nanotubes (SWCNTs). It was designed as a flexible patch in a sandwich-like configuration, which can be mounted onto the inner liner of a tyre. The patch was fabricated by inserting a PVDF film in between two conductive elastomer sheets. The development started with improving the conductivity of the elastomer by adding 6 wt% of SWCNT masterbatch. The adhesion between the interfaces was improved through surface modification of the PVDF film by introducing oxygen functional groups via a plasma treatment and further modification with a thiocyanate silane. The successful surface modification of the PVDF film was affirmed by x-ray photoelectron spectroscopy. T-peel and fatigue tests showed durable and stable adhesion between PVDF and conductive elastomer, confirming that the silane can effectively bridge the two components. A glueing method is proposed to adhere the patch to the tyre inner liner compound. The harvester is estimated to sufficiently power a reference tyre sensor, producing 28 μW cm−2.
- 3 August 2022
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 31 (9) , 095034
Open AccessDesign and performance of flexible polymeric piezoelectric energy harvesters for battery-less tyre sensors
A piezoelectric energy harvester for battery-less tyre sensors has been developed. It consists of two key elements: (a) a piezoelectric material—polyvinylidene difluoride (PVDF) film and (b) an electrode—a conductive elastomer filled with carbon black and single-wall carbon nanotubes (SWCNTs). It was designed as a flexible patch in a sandwich-like configuration, which can be mounted onto the inner liner of a tyre. The patch was fabricated by inserting a PVDF film in between two conductive elastomer sheets. The development started with improving the conductivity of the elastomer by adding 6 wt% of SWCNT masterbatch. The adhesion between the interfaces was improved through surface modification of the PVDF film by introducing oxygen functional groups via a plasma treatment and further modification with a thiocyanate silane. The successful surface modification of the PVDF film was affirmed by x-ray photoelectron spectroscopy. T-peel and fatigue tests showed durable and stable adhesion between PVDF and conductive elastomer, confirming that the silane can effectively bridge the two components. A glueing method is proposed to adhere the patch to the tyre inner liner compound. The harvester is estimated to sufficiently power a reference tyre sensor, producing 28 μW cm−2.
- Open Access
- 1 April 2021
- Published by SAGE Publications in Plastics, Rubber and Composites: Macromolecular Engineering
- Vol. 50 (7) , 315-328
Enabling reprocessability of ENR-based vulcanisates by thermochemically exchangeable ester crosslinks
A reprocessable elastomeric vulcanisate based on Epoxidised Natural Rubber with 50 mol-% epoxide content (ENR-50) was evloved by applying a self-assembled network based on thermochemically exchangeable ester crosslinks to the system. Hydrolysed Maleic Anhydride (HMA) as crosslinking substance in the presence of 1,2-DiMethylImidazole (DMI) as esterification accelerator and Zinc Acetate Dihydrate (ZAD) as transesterification catalyst was employed to generate the exchangeable ester crosslinking system. A sulphur-cured ENR-50 vulcanisate possessing a permanent sulphide crosslinking network was prepared as reference. Based on the results from cure characteristic and chemical structure analyses, the ENR-50 crosslinked with HMA behaves as a dynamic network because of a transesterification reaction catalysed by ZAD, promoting an exchangeable crosslinking network in the system. This dynamic network contributes to an intermolecular rearrangement of the ester crosslinking bonds at elevated temperatures, enabling interfacial self-adhesion and so reprocessability of the vulcanisates. The obtainable vulcanisates can be reprocessed, yielding relatively high retention of mechanical properties compared to their pristine counterpart. The interfacial self-adhesion and reprocessability of the vulcanisates have shown to significantly be improved with a higher loading of ZAD and elevated temperatures. This concept essentially shows a prospect towards developing e.g. novel recyclable and self-healing systems for elastomers.
- 1 April 2021
- Published by SAGE Publications in Plastics, Rubber and Composites: Macromolecular Engineering
- Vol. 50 (7) , 315-328
Open AccessEnabling reprocessability of ENR-based vulcanisates by thermochemically exchangeable ester crosslinks
A reprocessable elastomeric vulcanisate based on Epoxidised Natural Rubber with 50 mol-% epoxide content (ENR-50) was evloved by applying a self-assembled network based on thermochemically exchangeable ester crosslinks to the system. Hydrolysed Maleic Anhydride (HMA) as crosslinking substance in the presence of 1,2-DiMethylImidazole (DMI) as esterification accelerator and Zinc Acetate Dihydrate (ZAD) as transesterification catalyst was employed to generate the exchangeable ester crosslinking system. A sulphur-cured ENR-50 vulcanisate possessing a permanent sulphide crosslinking network was prepared as reference. Based on the results from cure characteristic and chemical structure analyses, the ENR-50 crosslinked with HMA behaves as a dynamic network because of a transesterification reaction catalysed by ZAD, promoting an exchangeable crosslinking network in the system. This dynamic network contributes to an intermolecular rearrangement of the ester crosslinking bonds at elevated temperatures, enabling interfacial self-adhesion and so reprocessability of the vulcanisates. The obtainable vulcanisates can be reprocessed, yielding relatively high retention of mechanical properties compared to their pristine counterpart. The interfacial self-adhesion and reprocessability of the vulcanisates have shown to significantly be improved with a higher loading of ZAD and elevated temperatures. This concept essentially shows a prospect towards developing e.g. novel recyclable and self-healing systems for elastomers.